Atomic faulting drives exceptional toughness in low thermal expansion chromium alloys

Endowing functional properties with mechanical responses in traditional metals has been a frontier topic, akin to transforming base metal into gold. Chromium and its alloys, with their functional deficiencies and limited ductility, serve as typical examples. Herein, we report a Cr96Fe4Ge1.3B1 alloy that unifies low thermal expansion (LTE, αl = 1.79 × 10-6 K-1, 200 − 315 K) with exceptional toughness (240.2 J·cm-3). The enhancement in mechanical responses is primarily attributed to layered Cr2B intermetallic precipitates, which ameliorate interfacial cohesion and simultaneously refine the grain structure. The weakened interlayer interactions within the Cr-B layers facilitate the nucleation and movement of numerous tiny stacking faults in precipitates, efficiently alleviating strain energy and resulting in marked work-hardening ability. Additionally, antiferromagnetic fluctuations in the BCC matrix contribute to the unique LTE behavior. This paves the way for the design of high-performance alloys featuring layered-symmetry precipitates.

Yu, Chengyi [University of Science and Technology

Cr plasma-material-interaction in PISCES-RF: D thermal release, retention, and erosion

Pure chromium (Cr) targets were exposed to high-flux deuterium (D) plasmas in the Pisces-RF linear plasma device, and measurements of D retention, release, and erosion were subsequently performed. Post-exposure D retention was quantified using temperature-programmed desorption on Cr targets irradiated by 50 eV ions over a broad range of exposure temperatures (423–873 K) and ion fluences (3 × 10 24 – 3 × 10 26 m −2 ). The retained D inventory was observed to decrease rapidly with increased exposure temperature, from approximately ∼7 × 10 20 m −2 at ∼ 420 K, to then saturate near ∼ 10 20 m −2 for exposure temperatures above ∼550 K. Separately, at fixed exposure temperature (∼450 K), D retention was found to have only a weak dependence on increasing ion fluence. Lastly, the erosion of Cr in D plasma was investigated for ion impact energies in the range 40 ≤ E i ≤ 250 eV. Erosion was inferred using optical emission spectroscopy (OES) from the ratio of emission lines (Cr I (425.4 nm)/D I (656.1 nm)) measured close to the target. Conversion of the OES yield data to net erosion yield was made with singular ion energy target mass-loss measurements. These net erosion yield data were then further corrected to obtain gross erosion yield by accounting for a re-deposition factor, computed using a simple model. The gross erosion yield is found to be 2–4 times lower than predicted by SDTrimSP, consistent with that typically observed for light-ion sputtering under high-flux plasma conditions.

Chromium

Feasibility of Nitrogen as a Carrier Gas for Inconel Cold Spray in Hydropower Application

Cold spray deposition of Inconel nickel alloys has emerged as a promising strategy for mitigating cavitation erosion in hydropower facilities. Most prior developments employ helium (He) as the carrier gas because it enables high particle velocities and the formation of dense coatings. However, He is nearly two orders of magnitude more expensive than nitrogen (N2), which limits its widespread adoption in the hydropower sector. Although He-based cold spray can be justified for high value repairs, the lower cost and broad availability of N2 make it an attractive alternative. This study assesses the feasibility of N2-based cold spray of Inconel 625 powders for hydropower applications. Cavitation erosion testing shows that He-based coating exhibits cavitation resistance of ~398% relative to the 304L stainless steel (SS304L) substrate. In contrast, N2-based coating shows substantially lower cavitation resistance, reaching only ~69% of the SS304L substrate, even when higher carrier gas temperature and pressure are applied. When the Inconel 625 powder size is reduced from 44 to 22 µm under N2-based cold spray conditions, cavitation resistance increases significantly to ~148% of the SS304L substrate. Additional improvement can be obtained by incorporating fine chromium carbide powders into the feedstock, resulting in cavitation resistance of ~172% of the SS304L substrate. Overall, with optimized feedstock design, N2-based cold spray offers a practical and cost-effective approach for producing cavitation resistant coatings on hydropower components, although He-based cold spray continues to deliver higher cavitation resistance.

Wang, Tianhao

A comparison of wrought and powder metallurgical FeCrAl claddings under simulated LWR accident transients

Iron-chromium-aluminum (FeCrAl) alloys are potential accident tolerant fuel (ATF) cladding candidates for light-water reactors but are difficult to fabricate as thin-walled tubes via conventional cast-and-wrought routes. Powder metallurgy (PM) offers a manufacturing alternative with improved compositional control, but its transient accident performance has not been directly benchmarked against wrought variants. This study evaluates the burst behavior of commercially developed PM-processed FeCrAl alloys, PM-C26M (Fe-12Cr-6Al-2Mo) and the high precipitate density FA-SMT (Fe-22Cr-5Al-3Mo), under simulated light-water reactor accident transient conditions. Burst testing was conducted using the Severe Accident Test Station with heating rates of 5 °C/s and 50 °C/s and internal pressures ranging from 25 MPa to 100 MPa. PM-C26M reproduced wrought C26M burst behavior within 7–37 °C across the stress range, indicating that PM processing does not compromise transient strength. FA-SMT exhibited markedly higher burst temperatures and reduced heating-rate sensitivity, consistent with its engineered precipitate strengthening. FA-SMT rupture exhibited axial "unzipping" rather than the lateral tearing characteristic of PM- and wrought C26M. Post-test EBSD and fractography indicate that this behavior is strongly correlated with strain-gated intergranular void nucleation associated with the dense precipitate architecture of FA-SMT, a response absent in the comparatively clean PM-C26M matrix and consistent with rupture morphologies reported for oxide-dispersion strengthened (ODS) FeCrAl of similar base-matrix chemistry to PM-C26M. These findings highlight the potential of powder metallurgy as a viable fabrication route for ATF claddings from an accident performance standpoint.

Bell, Sam [ORNL] (ORCID:0000000251905657)

Identifying Strain Stacking Boundaries between Multiphase Domains in Atomically Thin Two-Dimensional Magnets

Stacking engineering of van der Waals materials is an important strategy to control the materials’ properties, such as electronic correlations, ferroelectricity, and layer-dependent two-dimensional magnetism. A timely testbed for the study of the latter is atomically thin chromium trihalides (CrX 3 , X = Cl, Br, I). Notably, by understanding the sliding mechanism between different stacking sequences, control of the stacking arrangement, and thus magnetic properties in CrX 3 , can be achieved. Such insight, however, is currently lacking. Here, in this study, advanced electron microscopy methods are used to identify multiple stacking sequences corresponding to different bulk phases in atomically thin CrX 3 (X = Cl and Br) down to bilayer thickness and with lateral domain sizes as small as tens of nanometers. Indications of nanometer scale transitions and interactions at the stacking boundaries are found, including a universally preferred sliding direction that is consistent with density functional theory calculations and the strain fields at lateral heterostructure boundaries. This study demonstrates the necessity to consider local stacking structures when interpreting averaged magnetic properties measured with macroscale probes. Additionally, the preferred sliding direction insight from this study provides a strategy to control stacking sequence in atomically thin CrX 3 samples during the exfoliation and sample fabrication process.

DFT calculations

Influence of Powder Characteristics and Processing Methods on Creep Performance of Powder Metallurgy Hot Isostatic Pressed SS316

The U.S. nuclear energy expansion goals are driving the demand for manufacturing routes that can rapidly produce large, complex, near net shape components. Powder metallurgy hot isostatic pressing (PM HIP) is an advanced manufacturing technique that can be economically scaled-up, while alleviating the supply chain challenges that forging and casting face in terms of cost and lead time constraints. This makes PM-HIP a viable technology to aid and accelerate large-scale part manufacturing for nuclear applications. However, large-scale qualification and deployment of this technology require a thorough understanding of the influence of powder feedstock quality, powder handling history, hot isostatic pressing (HIP) parameters, and subsequent heat treatment on microstructural evolution and elevated temperature mechanical performance. The present work focusses on 316 austenitic stainless steel (SS316) which is most commonly used in high temperature environments for nuclear applications Results from this study show that PM HIPed SS316 meets ASME tensile requirements at room temperature and at elevated temperature. However, creep performance of PM-HIPed SS316 remains inferior to its wrought counterpart, demonstrating that tensile performance alone is not a reliable metric for long duration high temperature integrity. Further, this report delineates powder derived microstructural features that govern creep damage, with key evidences pointing to “microstructural inheritance” from gas atomized powder feedstocks. Commercial SS316 powders of varying chemical compositions and recycling histories were studies, and the results showed large differences in elemental segregation, oxide surface layers and secondary phase distributions. Multi-scale characterization revealed segregation of chromium, molybdenum, manganese and silicon at the boundaries and the precipitation of manganese-, silicon-, and molybdenum-oxides. During HIP consolidation, these surface oxides transform into decorated prior particle boundaries (PPBs) and grain boundary inclusions that persist through conventional post-HIP solution annealing treatment. The retained oxides in post-HIP microstructures were found to influence grain growth, precipitation behavior, and ultimately creep cavitation and fracture. Such post-HIP heat treatments are therefore limited by a complex trade-off between grain growth, and oxide coarsening which aggravate creep damage by acting as nucleation sites for cavities. The objective of this work is to establish an integrated processing–structure–property framework for PM-HIP 316 stainless steel by investigating the influence of powder feedstock characteristics in pre- and post-HIP processing as well as to understand the significance of post-HIP heat treatment on microstructural evolution and creep properties. The results from this report emphasize the significance of powder feedstock integrity in improving creep performance of PM-HIPed SS316, by highlight the effect of rapid solidification, elemental segregation, oxide formation and powder recycling on microstructural defect inheritance following HIP consolidation. Rather than considering HIP processing, solution annealing, and mechanical performance independently, this report treats powder production, HIP consolidation, post-HIP thermal processing, and creep deformation as interconnected stages within a continuous metallurgical process. The resulting framework will provide a scientific basis for developing feedstock engineering strategies capable of improving long-term reliability of PM-HIP stainless steels and accelerating their qualification for advanced nuclear applications.

Ajjarapu, Pavan [Oak Ridge National Laboratory (OR