Materials Data on Co(BMo)3 by Materials Project

Co(MoB)3 crystallizes in the orthorhombic Cmcm space group. The structure is three-dimensional. there are two inequivalent Mo+2.33+ sites. In the first Mo+2.33+ site, Mo+2.33+ is bonded in a 6-coordinate geometry to six B3- atoms. There are a spread of Mo–B bond distances ranging from 2.31–2.53 Å. In the second Mo+2.33+ site, Mo+2.33+ is bonded in a 7-coordinate geometry to seven B3- atoms. There are a spread of Mo–B bond distances ranging from 2.35–2.50 Å. Co2+ is bonded in a square co-planar geometry to four equivalent B3- atoms. All Co–B bond lengths are 2.07 Å. There are two inequivalent B3- sites. In the first B3- site, B3- is bonded in a 9-coordinate geometry to six Mo+2.33+, two equivalent Co2+, and one B3- atom. The B–B bond length is 1.89 Å. In the second B3- site, B3- is bonded in a 9-coordinate geometry to seven Mo+2.33+ and two equivalent B3- atoms.

36 MATERIALS SCIENCE↗

Transient kinetic insights into selective propene oxidation over industrial bismuth molybdate catalysts

Selective oxidation of propene to acrolein over industrial multicomponent bismuth molybdate (BMO) catalysts significantly depends on reaction conditions that include operating parameters and catalyst state. Here, this work investigates selective propene oxidation in the intrinsic kinetic paradigm of Temporal Analysis of Products (TAP) reactor by systematically varying catalyst redox state, temperature, and oxygen-to-propene feed ratio. A 93 % propene conversion with an acrolein yield of 80 % is achieved at elevated temperatures (450 °C) on oxidized catalysts under oxygen-rich conditions (O 2 :C 3 H 6 = 10). However, these conditions diminish acrolein-to-CO 2 selectivity due to enhanced total oxidation to CO 2 . In contrast, a reduced catalyst state, moderate temperature (350 °C), and lower oxygen feed (O 2 :C 3 H 6 = 1) nearly doubles the acrolein to-CO 2 selectivity, albeit at a lower acrolein yield (33 %). Transient kinetic studies together with a kinetic model that simplify the major product formation pathways in lumped non-elementary forms reveal that the availability of surface oxygen species plays a pivotal role in governing reaction pathways. Additionally, density functional theory (DFT) calculations on pure BMO catalysts inform the role of surface redox states on propene and oxygen activation barriers. Lattice oxygen at acrolein-selective sites drives both acrolein and CO 2 formation, while adsorbed oxygen at activation sites favors unselective CO 2 generation. This work establishes a critical relationship between transient product selectivity and surface oxygen availability, which is strongly influenced by catalyst redox state, feed ratio, and reaction temperature. These insights underscore the importance of dynamic reactor operation strategies and offer a foundation for designing next-generation propene oxidation processes with tunable acrolein selectivity.

42 - ENGINEERING↗

Materials Data on Ni(BMo)3 by Materials Project

Ni(MoB)3 crystallizes in the orthorhombic Cmcm space group. The structure is three-dimensional. there are two inequivalent Mo+2.33+ sites. In the first Mo+2.33+ site, Mo+2.33+ is bonded in a 6-coordinate geometry to six B3- atoms. There are a spread of Mo–B bond distances ranging from 2.30–2.56 Å. In the second Mo+2.33+ site, Mo+2.33+ is bonded in a 7-coordinate geometry to seven B3- atoms. There are a spread of Mo–B bond distances ranging from 2.35–2.48 Å. Ni2+ is bonded in a square co-planar geometry to four equivalent B3- atoms. All Ni–B bond lengths are 2.10 Å. There are two inequivalent B3- sites. In the first B3- site, B3- is bonded in a 9-coordinate geometry to six Mo+2.33+, two equivalent Ni2+, and one B3- atom. The B–B bond length is 1.86 Å. In the second B3- site, B3- is bonded in a 9-coordinate geometry to seven Mo+2.33+ and two equivalent B3- atoms.

36 MATERIALS SCIENCE↗

A redox-reversible A/B-site co-doped BaFeO 3 electrode for direct hydrocarbon solid oxide fuel cells

Solid oxide fuel cells (SOFCs) can directly convert the chemical energy in fuel to electrical energy with fuel flexibility; however, the conventional nickel-based anodes face great challenges due to coking upon direct oxidation of hydrocarbon fuels and redox instability. Thus, developing new anode materials which can provide high coking resistance as well as redox stability is crucial. In this work, Ba 0.6 La 0.4 Fe 0.8 Mo 0.1 Ni 0.1 O 3-δ (BLFMN) has been synthesized in air using a sol–gel combustion method, resulting in a dual phase consisting of a cubic BLFMN main phase and scheelite BaMoO 4 (BMO 4 ) secondary phase. By heat-treating the BLFMN dual phase in H 2 at 800 °C for 5 h, a metallic nanoparticle-decorated BLFMN triple phase compound comprising cubic BLFMN, cubic BaMoO 3 (BMO 3 ) and in situ exsolved FeNi 3 alloy was obtained. BLFMN was subsequently investigated as an electrode material for La 0.8 Sr 0.2 Ga 0.83 Mg 0.17 O 3-δ (LSGM) electrolyte (300 μm) supported SOFCs. Symmetrical cells using BLFMN as electrodes with the cell configuration of BLFMN//LSGM//BLFMN showed excellent redox reversibility and a peak power density (PPD) of 1.32 W cm -2 at 850 °C when using H 2 as fuel. Single cell with the cell configuration of BLFMN//LSGM//LSCF (La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3-δ ) reached PPD of 1.61 and 0.41 W cm -2 at 850 °C when operating with H 2 and CH 4 fuel, respectively. Moreover, the single cell exhibit excellent stability (over 300 h) upon direct oxidation of hydrocarbon fuels of CH 4 and C 3 H 8 . This study indicates that BLFMN is a promising redox reversible and coking resistant anode for SOFCs.

08 HYDROGEN↗