Search NASA⌕ Search

SEARCH · Search NASA

Results for “Commercially pure titanium”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

ECCI based characterization of dislocation shear in polycrystalline arrays during heterogeneous deformation of commercially pure titanium

A new electron channeling contrast imaging (ECCI) based approach for the characterization of heterogeneous plastic deformation across multiple grains in a polycrystal is presented. The nature of the shear accommodation at grain boundaries has been assessed by evaluating the spatial distribution of dislocations and slip system activities near the boundaries and relating these observations to standard slip transfer criteria and the global state of stress. The direction of slip band propagation, and consequently the location of dislocation slip band nucleation, was determined by characterizing the slip band widths across individual grains. This assessment leads to a better understanding of the factors involved in polycrystalline deformation, including the grain boundary shear accommodation associated with both dislocation pile-ups and grain boundary dislocation nucleation. Because ECCI allows study of dislocation structures over large surface areas, and thus larger overall volumes than typically are accessible by other techniques, the overall approach allows the dislocation distribution across individual grains to be understood in terms of the broader polycrystalline constraints.

36 MATERIALS SCIENCE↗

Mechanical Behavior of Commercially Pure Titanium Weldments at Lower Temperatures

Commercially pure titanium is used for low-temperature applications due to good toughness attributed to single-phase microstructure (α). Electron beam welding (EBW) and gas tungsten arc welding (GTAW) processes have been used for welding two grades of commercially pure titanium (Grade 2 and Grade 4). Martensitic microstructure is found to be finer in the case of EBW joint as compared to GTAW joint due to faster rate of cooling in the former process. Weldments have been characterized to study the mechanical behavior at ambient (298 K) and cryogenic temperatures (20 and 77 K). Strength of weldments increases with the decrease in temperature, which is found to be more prominent in case of Grade 4 titanium as compared to Grade 2. Weld efficiency of Grade 4 is found to be higher at all the temperatures (ambient, 77 and 20 K). However, ultimate tensile strength/yield strength ratio is higher for Grade 2 as compared to Grade 4. % Elongation is found to increase/retained at cryogenic temperatures for Grade 2, and it is found to decrease for Grade 4. Electron backscattered diffraction analysis and transmission electron microscopy of deformed samples confirmed the presence of extensive twinning in Grade 2 and the presence of finer martensitic structure in Grade 4. Fractography analysis of tested specimens revealed the presence of cleavage facets in Grade 4 and dimples in specimens of Grade 2. Higher strength in Grade 4 is attributed to higher oxygen restricting the twin-assisted slip, which is otherwise prominent in Grade 2 titanium.

36 MATERIALS SCIENCE↗

Effect of laser power on oxygen and nitrogen concentration of commercially pure titanium manufactured by selective laser melting

Highlights: • The hardness and strength of pure titanium fabricated by SLM were increased with increasing the laser power. • During the SLM processing, the concentrations of oxygen and nitrogen in the SLM parts were increased. • The oxidation and nitriding were thermodynamically possible under SLM. - Abstract: This study analyzed the variation of mechanical properties and its causes with increasing the laser power in the fabrication of pure titanium by selective laser melting (SLM). SLM samples were fabricated using commercially pure titanium grade 1 powder when the scan speed was 1000 mm/s and the laser power as 120, 200, 280, 360, and 440 W, respectively. As the laser power increased, the hardness and strength of the samples increased gradually. During the SLM processing, the concentrations of oxygen and nitrogen in the SLM samples were increased, which resulted in the increase of hardness and strength. The SLM equipment used in this study removed oxygen in the chamber by flowing high purity argon gas and fabricates the sample while preserving the oxygen concentration in the atmosphere to 0.2%. Evaluating the possibility of oxidation and nitriding during the SLM process by thermodynamic analysis, it was found that the process occurred under conditions in which temperature and residual oxygen and nitrogen partial pressure led to oxidation and nitriding.

36 MATERIALS SCIENCE↗

Effect of pre-annealing deformation on the recrystallized texture and grain boundary misorientation in commercial pure titanium

Highlights: • Tailoring the misorientation angle distribution by pre-annealing rolling in CP-Titanium. • Enhancing the inheritance of basal scatter texture by medium pre-annealing rolling. • Moderate pre-annealing rolling produces refined recrystallized grains. - Abstract: The effects of rolling reduction followed by annealing (at 650 °C) on commercial pure titanium sheet are investigated. The microstructure, texture and misorientation angle distributions after rolling and annealing are observed by electron back scatter diffraction (EBSD). It is found that, when the rolling deformation was low (20%) or medium (40%), a fraction of non-TD-split basal texture is inherited from the deformed state and remains even after long time (60 min) annealing. However, heavy rolling deformation (85%) causes a strong and typical TD-split basal texture in the deformed and annealed states. In addition, the misorentation angle distributions are relatively homogeneous for the recrystallized samples with a low or medium pre-annealing deformation. But with heavy pre-annealing deformation, the misorientation angle distributions exhibits two peaks, around 15–30° and 70–80°. The texture and misorientation angle evolution mechanisms are discussed in this work. The study shows the possibility to tailor the texture and the misorientation angle distribution of commercial pure titanium sheet by ordinary rolling process.

36 MATERIALS SCIENCE↗

The Effect of Reduced Pressure on Laser Keyhole Weld Porosity and Weld Geometry in Commercially Pure Titanium and Nickel

Here, the beneficial effect of reduced pressure laser welding in vacuum at 10 -1 mBar was investigated in commercially pure titanium and nickel and compared to atmospheric pressure welding in Ar shielding gas. Partial penetration keyhole welds were made in these materials using a continuous wave disk laser operating at 2-4 kW and travel speeds of 12 and 17 mm/s, where moderate to severe porosity is observed under normal atmospheric pressure welding conditions. Additional welds were made in nickel using an electron beam welding process and the same parameters for comparison. Optical metallography, x-ray radiography, and computed x-ray tomography (CT) were used to characterize the porosity levels in the welds. Quantitative CT results show a monotonically decreasing pore size distribution for all of the welds, and the distributions can be fit with a 2-parameter Wiebull relationship with a beta shape factor that varied between 0.37 and 0.61 depending on the welding conditions. Other results show that laser vacuum essentially eliminates porosity in titanium, and significantly reduces porosity in nickel, but does not completely eliminate porosity in nickel. Laser vacuum welds have increased keyhole penetration and reduced weld widths compared to their atmospheric pressure counterparts, with similar beneficial geometric weld shapes as electron beam welds that are also made in vacuum. Finally, laser vacuum welds showed approximately one-half the volumetric porosity in nickel than electron beam welds, with less porosity at the weld root.

36 MATERIALS SCIENCE↗

Creep Behavior of Commercially Pure Titanium TA2 After Supersonic Fine Particles Bombardment

In this study, the effect of supersonic fine particles bombardment (SFPB) on the creep behavior of commercially pure titanium TA2 was investigated. Microstructural observations with x-ray diffraction and a transmission electron microscope indicated that the grain size of the TA2 surface layer was refined to nanometer scale in the topmost surface layer after SFPB treatment. Indentation creep tests showed that the SFPB-treated sample had a lower maximum depth and higher hardness than the original sample at the same load, indicating an enhancement of the surface strength with SFPB. With lower creep displacements, the creep resistance was also improved after SFPB treatment. The maximum creep rate under different loading conditions showed obvious loading time and load dependencies. The maximum creep rate of the SFPB-treated sample was lower than the original sample for all test conditions, and the maximum creep strain rate of the SFPB-treated sample was similar to that of the original sample. The indentation stress of the SFPB-treated sample was higher than the original sample, while the creep stress exponent of the original sample was slightly higher than for the SFPB-treated sample, with no obvious variation tendency with different loading times or loads.

36 MATERIALS SCIENCE↗

The deformation behavior of commercially pure titanium subjected to electron beam treatment

The effect of low-energy high-current pulsed electron beam treatment on the microstructure and mechanical properties of commercially pure titanium specimens is studied. Plastic deformation mechanisms of the specimens subjected to the electron beam treatment followed by uniaxial tension are demonstrated. The role of the interface between the hardened surface layer and the relatively soft parent metal in the slip band formation in the loaded specimens is revealed.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

In-situ laser ultrasonic measurement of the hcp to bcc transformation in commercially pure titanium

Using a novel in-situ laser ultrasonic technique, the evolution of longitudinal velocity was used to measure the α − β transformation during cyclic heating and cooling in commercially pure titanium. In order to quantify the transformation kinetics, it is shown that changes in texture can not be ignored. This is particularly important in the case of titanium where significant grain growth occurs in the β-phase leading to the ultrasonic wave sampling a decreasing number of grains on each thermal treatment cycle. Electron backscatter diffraction measurements made postmortem in the region where the ultrasonic pulse traveled were used to obtain an estimate of such local texture and grain size changes. An analysis technique for including the anisotropy of wave velocity depending on local texture is presented and shown to give self consistent results for the transformation kinetics. - Highlights: • Laser ultrasound and EBSD interpret the hcp/bcc phase transformation in cp-Ti. • Grain growth and texture produced variation in velocity during similar treatments. • Texture was deconvoluted from phase addition to obtain transformation kinetics.

36 MATERIALS SCIENCE↗

Fabrication of nanotube arrays on commercially pure titanium and their apatite-forming ability in a simulated body fluid

In this study, we investigated self-organized TiO{sub 2} nanotubes that were grown using anodization of commercially pure titanium at 5 V or 10 V in NH{sub 4}F/NaCl electrolyte. The nanotube arrays were annealed at 450 °C for 3 h to convert the amorphous nanotubes to anatase and then they were immersed in simulated body fluid at 37 °C for 0.5, 1, and 14 days. The purpose of this experiment was to evaluate the apatite-formation abilities of anodized Ti nanotubes with different tube diameters and lengths. The nanotubes that formed on the surfaces of Ti were examined using a field emission scanning electron microscope, X-ray diffraction, and X-ray photoelectron spectroscope. When the anodizing potential was increased from 5 V to 10 V, the pore diameter of the nanotube increased from approximately 24–30 nm to 35–53 nm, and the tube length increased from approximately 590 nm to 730 nm. In vitro testing of the heat-treated nanotube arrays indicated that Ca-P formation occurred after only 1 day of immersion in simulated body fluid. This result was particularly apparent in the samples that were anodized at 10 V. It was also found that the thickness of the Ca-P layer increases as the applied potential for anodized c.p. Ti increases. The average thickness of the Ca-P layer on Ti that was anodized at 5 V and 10 V was approximately 170 nm and 190 nm, respectively, after immersion in simulated body fluid for 14 days. - Highlights: • TiO{sub 2} nanotube on Ti surface was formed by anodic oxidation in a NaCl/NH{sub 4}F solution. • TiO{sub 2} layers show a tube length of 590 nm and 730 nm at 5 V and 10 V, respectively. • After soaking in SBF, Ca-P layer completely covered the entire nanotubular surfaces. • The Ca-P layer was thicker on the Ti surface anodized at 10 V.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Damage evolution and ductile fracture of commercially-pure titanium sheets subjected to simple tension and cyclic bending under tension

This paper describes a study into the evolution of damage in commercial-purity titanium (CP–Ti) sheets subjected to cyclic bending under tension (CBT) and uniaxial tension (simple tension, ST). Sections were taken from sheets that were strained to various levels under both methods and were imaged using X-ray computed tomography (XCT) to reveal insights into the size, density, and distribution of microvoids in the sheets. Digital image correlation (DIC) was also used to observe the surface strain of CBT and ST sheets during testing. These results showed that elongation to failure (ETF) for CBT deformation is about 2.5× higher than for ST, local longitudinal strains in the bulk of the CBT sample are around 1.3× higher than the peak strain in the ST necked region, and 1.7× higher in the localized region of CBT failure. It was found that the volume-density of voids in both sheets followed a similar exponential increase with strain, reaching nearly 45× higher in the CBT than the ST sheets before the onset of failure, mainly due to the higher strain levels achieved. A higher volume density of voids developed in the center of sheets at high levels of strain, for both processes, with the density in the sheet center becoming approximately double that found near the edges. Scanning electron microscopy (SEM) was used to examine the fracture surface of CBT and ST sheets after failure. The observations are presented and discussed highlighting the CBT process as effective to delay ductile fracture of the CP-Ti sheets.

Commercially pure titanium↗

Spherical nanoindentation stress-strain curves of commercially pure titanium and Ti-6Al-4V

Spherical nanoindentation combined with electron back-scattered diffraction was employed to characterize the grain-scale elastic and plastic anisotropy of single crystal alpha-Ti for commercially pure (CP-Ti) and alloyed (Ti-64) titanium. In addition, alpha-beta Ti (single colony) grains were characterized. The data set includes the nanoindentation force, displacement, and contact stiffness, the nanoindentation stress-strain analysis, and the alpha-Ti crystal orientations. Details of the samples and experimental protocols can be found in Weaver et al. (2016) Acta Materialia doi:10.1016/j.actamat.2016.06.053.

36 MATERIALS SCIENCE↗

Low-Pressure Diffusion Bonding of Vanadium to Commercially Pure Titanium and Ti-6Al-4V

Modern technology increasingly requires components to be made from specific high-performance materials. To support complex multi-metal structures, a variety of techniques are required to join dissimilar metal parts with precise shapes. This study evaluates vacuum diffusion bonding as a method for joining titanium and vanadium, focusing on both pure titanium and the common alloy Ti-6Al-4V. We employ modest pressure provided by a weight and simple surface preparation to simulate the most commercially applicable process. Here, we show that Ti-6Al-4V alloy bonds readily to V, forming a continuous, clearly defined interdiffusion layer with predictable kinetics. Conversely, commercially pure Ti forms a crack-prone bond with V that fails to improve at higher bonding temperatures or longer times. We attribute this failure to the concentration of stress caused by the ß-to-α phase transformation in Ti. The contrasting bonding efficacy between pure Ti and the alloy provides insight into the crystallographic interactions that occur at the interface during bonding and cooling. These results provide surprising insight into a new method for bonding Ti alloys to V and possibly other metals that share the body-centered cubic crystal structure.

36 MATERIALS SCIENCE↗

Evaluation of the Pressing Characteristics of Commercially Pure Titanium Using an Instrumented Double Acting Die

With recent advances in synthesizing titanium powder by low-cost routes, there has been growing interest in identifying process/material conditions that overcome the powder compaction problems typically found with this reactive metal. The use of instrumented dies in studying the cold pressing process for commercial iron and steel powders has provided greater insight into the complex phenomena that occur and may be used to evaluate constitutive relations that describe the compaction process. Nevertheless, little work has been conducted on the special, more problematic case of reactive metal powders such as titanium. An instrumented die was developed that allows die wall friction to be characterized and the radial stress distribution along the die wall and throughout the compact to be monitored. As will be presented, this tool has been used to investigate titanium compaction and to draw comparisons with results obtained on a baseline commercial iron powder. Both sets of data were systematically collected using various powder/die lubrication combinations.

36 MATERIALS SCIENCE↗

Planar Anisotropy, Tension–Compression Asymmetry, and Deep Drawing Behavior of Commercially Pure Titanium at Room Temperature

The planar anisotropy (PA) and tension–compression asymmetry (TCA) of the CP-Ti were investigated via uniaxial tension and compression tests at room temperature. The formability and the earing behavior of the CP-Ti sheet were studied via deep drawing experiment. The deep drawing simulations using the uniaxial tensile and the compressive curves as the hardening rules were compared with each other and with the experimental results. The CP-Ti sheet showed PA and TCA in yielding and strain hardening. The PA was characterized by the plastic strain ratio r{sub 0}, r{sub 45}, and r{sub 90} of 1.47, 2.06, and 2.05. The TCA showed PA, which showed tension–compression yield strength ratios of 1.12, 1.08, and 1.04 in 0°, 45°, and 90° in the rolling direction, and tensile and compressive hardening exponent ratios of 0.86, 0.8, and 0.62. The orientation distribution functions (ODFs) analysis demonstrated that the tensile and the compressive deformation textures were different and showed PA. The simulative results, including the simulated forming force and the earing profiles using the uniaxial tensile and compressive curves as the hardening rules, were not in agreement with each other. The results were not in good agreement with the experimental results, implying that the TCA had an important effect on the formability of the sheet. The TCA tended to reduce the thickness of the deep drawing parts, increase the earing ratio, and affect the drawing force.

36 MATERIALS SCIENCE↗

Diffusion bonding of commercially pure titanium to low carbon steel using a silver interlayer

Titanium and low carbon steel plates were joined through diffusion bonding using a silver interlayer at various temperatures for various diffusion times. In order to determine the strength of the resulting joints, tensile-shear tests and hardness tests were applied. Additionally, optical, scanning electron microscopy examinations and energy dispersive spectrometry elemental analyses were carried out to determine the interface properties of the joint. The work showed that the highest interface strength was obtained for the specimens joined at 850 deg. C for 90 min. It was seen from the hardness results that the highest hardness value was obtained for the interlayer material and the hardness values on the both sides of the interlayer decreased gradually as the distance from the joint increased. In energy dispersive spectrometry analyses, it was seen that the amount of silver in the interlayer decreased markedly depending on the temperature rise. In addition, increasing diffusion time also caused some slight decrease in the amount of silver.

36 MATERIALS SCIENCE↗

Hardening of the surface layers of commercial pure titanium VT1-0 under combined treatment

The treatment of VT1-0 titanium samples was carried out by concentrated energy fluxes. The combined treatment included surface carburizing with the joint use of powder samples of compounds with high physical and mechanical properties (namely, titanium diboride TiB{sub 2}, silicon carbide SiC and zirconium oxide ZrO{sub 2}) and subsequent electron beam treatment of surface layers formed in electroexplosive treatment. The combined treatment of surface layers resulted in the multifold increase in microhardness, which reduces depending on the depth of hardening zone. After electron-beam treatment, the depth of hardening zone is increased. During electron-beam treatment, the two-layer hardening zone forms.

36 MATERIALS SCIENCE↗