Modification of alkyne-functionalized asymmetric phthalocyanines by CuI-catalyzed azide-alkyne cycloaddition
Explore the source record for details and available documents.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
We report a facile combustion method synthesis of reduced graphene oxide/CuI composites as a photocatalyst, in which CuI nanoparticles were homogeneously distributed on the surface of reduced graphene oxide (rGO), showing a good visible light response. The rGO-supported and unsupported CuI hybrids were tested over the photocatalytic reduction of CO{sub 2} for methanol evolution in visible light. In the current study rGO-CuI composites have shown excellent yields (19.91 μmol g-cat{sup −1}). rGO provides a light-weight, charge complementary and two-dimensional material that interacts effectively with the CuI nanoparticles. - Graphical abstract: A facile reduced graphene oxide(rGO)/ CuI nanoparticles complexes hybrid material was prepared by a naked flame. This method can be simple and rapid preparation of composite materials which exhibit excellent catalytic performance. It is not only can improve the light absorption but also can be highly efficient reduction of CO{sub 2} to methanol in visible light. So the rGO-CuI composite will find potential applications as catalysts in organic photosynthetic reaction. Display Omitted - Highlights: • Reduced graphene oxide-CuI composites have been prepared by a facile method. • This method can produce reduced graphene oxide from graphene oxide without any reducing agent. • The absorption efficiency of rGO-CuI composites is significantly higher than rGO and CuI.
Oxidative stress has been suggested to contribute to neuronal apoptosis associated with Alzheimer's disease (AD). Copper may participate in oxidative stress through redox-cycling between its +2 and +1 oxidation states to generate reactive oxygen species (ROS). In vitro, copper binds to the amyloid-? peptide of AD, and in vivo, copper is associated with amyloid plaques characteristic of AD. As a result, the A?CuI complex may be a critical reactant involved in ROS associated with AD etiology. To characterize the A?CuI complex, we have pursued X-ray absorption (XAS) and electron paramagnetic resonance (EPR) spectroscopy of A?CuII and A?CuI (produced by ascorbate reduction of A?CuII). The A?CuII complex Cu K-edge XAS spectrum is indicative of a square-planar CuII center with mixed N/O ligation. Multiple scattering analysis of the extended X-ray absorption fine structure (EXAFS) data for A?CuII indicates that two of the ligands are imidazole groups of histidine ligands, indicating a (NIm)2(N/O)2 CuII ligation sphere for A?CuII. After reduction of the A?CuII complex with ascorbate, the edge region decreases in energy by 4 eV. The X-ray absorption near-edge spectrum region of A?CuI displays an intense pre-edge feature at 8984.1(2) eV. EXAFS data fitting yielded a two-coordinate geometry, with two imidazole ligands coordinated to CuI at 1.877(2) A in a linear geometry. Ascorbate reduction of A?CuII under inert atmosphere and subsequent air oxidation of A?CuI to regenerate A?CuII was monitored by low-temperature EPR spectroscopy. Slow reappearance of the A?CuII EPR signal indicates that O2 oxidation of the A?CuI complex is kinetically sluggish and A? damage is occurring following reoxidation of A?CuI by O2. Together, these results lead us to hypothesize that CuI is ligated by His13 and His14 in a linear coordination environment in ??, that A? may be playing a neuroprotective role, and that metal-mediated oxidative damage of A? occurs over multiple redox cycles.
Herein, we present a new series of CuI-based hybrid materials with tunable structures and semiconducting properties. Furthermore, the CuI inorganic modules can be tailored into a one-dimensional (1D) chain and two-dimensional (2D) layer and confined/stabilized in coordination frameworks of potassium isonicotinic acid (HINA) and its derivatives (HINA-R, R = OH, NO 2 , and COOH). The resulting CuI-based hybrid materials exhibit interesting semiconducting behaviors associated with the dimensionality of the inorganic module; for instance, the structures containing the 2D-CuI module demonstrate significantly enhanced photoconductivity with a maximum increase of five orders of magnitude compared to that of the structures containing the 1D-CuI module. They also represent the first CuI-bearing hybrid chemiresistive gas sensors for NO 2 with boosted sensing performance and sensitivity at multiple orders of magnitude over that of the pristine CuI. Particularly, the sensing ability of CuI-K-INA containing both 1D- and 2D-CuI modules is comparable to those of the best NO 2 chemiresistors reported thus far.
Graphical abstract: - Highlights: • CuI nanostructures were prepared via a simple precipitation method. • Glucose as a green capping agent and reductant was applied. • The effect of glucose concentration on the morphology of CuI was investigated. • According to XRD results, pure cubic phase CuI have been formed by using glucose. - Abstract: In this work, CuI micro/nanostructures have been successfully prepared via a simple precipitation route at room temperature. By using glucose as a clean reducing agent with different concentrations, CuI micro/nanostructures with various morphologies were obtained. Besides glucose, Na{sub 2}SO{sub 3}, KBH{sub 4} and N{sub 2}H{sub 4}·H{sub 2}O have been applied as reductant. X-ray diffraction (XRD), scanning electron microscopy (SEM), photoluminescence spectroscopy, X-ray energy dispersive spectroscopy (EDS) and Fourier transformed infrared (FT-IR) spectroscopy were used to characterize the as-produced CuI micro/nanostructures. According to the XRD results, it was found that pure cubic phase CuI have been formed by using glucose.
Highlights: • Large and transparent γ-CuI single crystal with the size over 20 mm was successfully obtained for the first time. • The intensities of near-band-edge emissions of γ-CuI single crystal are greatly enhanced by Li and I dopants. • The 430 nm emission decay time is less than 450 ps under pulsed X-ray irradiation. - Abstract: Large-sized γ-CuI single crystals with ultrafast scintillation property were grown in LiI acetonitrile solvent through evaporation technique. The LiI exhibits unique properties to γ-CuI single crystal preparation. One is that it increases the solubility of CuI in the solvent, which gives rise to a largest-sized (23 × 14 × 2 mm{sup 3}) single crystal with the high optical transmission (over 60%) in the wavelength region of 435–800 nm. The other feature is that it acts as an effective isoelectronic dopant and improves the molar ratio of copper to iodine, which greatly enhances the near-band-edge emissions (411 and 432 nm) and suppresses the broadband emission (680 nm). The decay time of the fast emission under pulsed X-ray excitation is shorter than 450 ps. The results will give a guidance for optimizing the properties of γ-CuI single crystal as an ultrafast scintillator.
Cuprous iodide (CuI) crystals are grown by slow evaporation technique in three different solvents. Large CuI single crystals with dimensions of 7.5 mm x 5 mm x 3 mm are obtained in pure acetonitrile solvent at 40 {sup o}C. The as-grown crystals are analyzed by X-ray diffraction, energy-dispersive X-ray analysis, differential scanning calorimetry, current-voltage characteristic and photoluminescence spectrum. The results show that the CuI crystal has the zinc-blende structure with no secondary phase. The elemental Cu/I ratio is 1.09:1. The melting point of the crystal is 875 K and two phase transitions occur from room temperature to its melting point. The electrical conductivity of CuI platelet crystal is in the range of 1.11-2.38 {Omega}{sup -1} cm{sup -1}. Under ultraviolet excitation, the CuI crystals exhibit three emission bands with peak positions at 426, 529 and 671 nm. The nature of the luminescence is discussed.
The electronic structures were calculated for BiTeBr and BiTeI using the density-functional theory approach and accounting for the strong spin-orbital interaction. Qualitatively, the band structures for two compounds are similar, showing strong mixing of the p states of all elements in vicinity of the Fermi level, with the band gaps of 0.595 and 0.478 eV for BiTeBr and BiTeI, respectively. The optimized crystal structures show a tendency for the Bi-X (X=Br, I) bond elongation compared to the Bi-Te one. Both compounds are intrinsic n-type semiconductors but display a metallic-like conductivity coupled to rather large thermopower, which is rationalized within the frames of the acoustic phonons scattering model. Because of larger thermopower BiTeBr exhibits a twice higher thermoelectric figure-of-merit near room temperature, ZT=0.17, compared to BiTeI. The addition of 1 mass% of BiI{sub 3} or CuI to BiTeI decreases the mobility of electrons by two orders of magnitude, leading to significantly lower electrical conductivity, but at the same time effectively reduces the thermal conductivity. The prospects of further enhancing the thermoelectric efficiency are briefly discussed. - Graphical abstract: View of the crystal structure of BiTeBr is shown in the figure The optimized crystal structures show a tendency for the Bi-X (X=Br, I) bond elongation compared to the Bi-Te one. The electronic structures were calculated for BiTeBr and BiTeI using the density-functional theory approach and accounting for the strong spin-orbital interaction. Qualitatively, the band structures for two compounds are similar, showing strong mixing of the p states of all elements in vicinity of the Fermi level, with the band gaps of 0.595 and 0.478 eV for BiTeBr and BiTeI, respectively. Both compounds are intrinsic n-type semiconductors but display a metallic-like conductivity coupled to rather large thermopower, which is rationalized within the frames of the acoustic phonons scattering model. The addition of 1 mass% of BiI{sub 3} or CuI to BiTeI effectively reduces the thermal conductivity. The prospects of further enhancing the thermoelectric efficiency are briefly discussed. Highlights: Black-Right-Pointing-Pointer BiTeBr and BiTeI feature mixing of p states of Bi, Te, and halogen near Fermi level. Black-Right-Pointing-Pointer BiTeBr has thermoelectric figure-of-merit ZT=0.17, two times that of BiTeI. Black-Right-Pointing-Pointer 1% CuI or BiI{sub 3} decrease dramatically electron mobility in BiTeI. Black-Right-Pointing-Pointer 1% CuI decreases thermal conductivity of BiTeI by a factor of 4, reaching 0.5 W m{sup -1} K.
Reaction of equimolar pyridine (Py) solutions BiI 3 and CuI produces the Py-supported 1:1 bimetallic complex BiCuI 4 (Py) 5 in quantitative yield. The title complex is only the second neutral complex to feature Cu–I–Bi bridging and shows an octahedral trans-[BiI 4 (Py) 2 ] unit joined to a distorted tetrahedral CuI(Py) 3 unit by an iodide bridge. The complex shows low thermal stability, decomposing under modest heating or vacuum to produce a mixture of BiI 3 and CuI. Thus, it is a potential entry/precursor to BiI 3 /CuI chemistry. Natural Localized Molecular Orbital (NLMO) calculations were performed to analyze the nature of the Cu–I–Bi bonds, revealing that the title compound lies on the cusp of being [Cu(Py) 3 ] + [BiI 4 (Py) 2 ] – . Diffuse reflectance spectroscopy measurements show a strong absorption band with an optical bandgap energy of 1.94 eV. Theoretical density of states (DOS) and time-dependent density functional theory (TD-DFT) experiments to map the electronic structure assign the primary electronic transition as a mixed halide/metal-to-ligand charge transfer between Cu–I–Bi donor orbitals and Py π* acceptor orbitals.
The CuI-derived inorganic–organic hybrid compounds are considered as promising phosphors for the lighting industry. Herein, exploiting N-monoalkylated hexaminium salts, [R-HMTA]X (R = Me, Et, Pr, and propargyl; X = Cl and I), as multibridging ligands, we have designed and synthesized a unique class of one-dimensional and two-dimensional hybrid CuI-materials. The reactions of these salts with CuI give rise to All-in-One (AIO) type compounds combining ionic and dative bonds between inorganic and organic components. The latter is formed by structurally unique inorganic [Cu x I y ] (y–x)– clusters, chains, or sheets interconnected through [R-HMTA] + cations via multiple Cu–N bonds. The so-designed compounds at ambient temperature exhibit tunable luminescence spanning from deep blue to red color (λ em = 430–625 nm) with microsecond lifetimes and the quantum efficiency of up to 78%. Remarkably, the AIO materials feature nontrivial excitation- (ED) and temperature-dependent (TD) luminescence, allowing their emission color to be finely adjusted from deep blue to red through changing the excitation wavelength and/or temperature. Based on the TD emission spectroscopy and theoretical calculations, a possible mechanism of the luminescence has been proposed. In conclusion, the very interesting luminescence characteristics coupled with good thermal and photostability render these AIO hybrid materials possible candidates for applications in energy-efficient lighting devices.
We demonstrate a new approach for utilizing CuI coordination complexes as emissive layers in organic light-emitting diodes that involves in situ codeposition of CuI and 3,5-bis(carbazol-9-yl)pyridine (mCPy). With a simple three-layer device structure, pure green electroluminescence at 530 nm from a Cu(I) complex was observed. A maximum luminance and external quantum efficiency (EQE) of 9700 cd/m2 and 4.4%, respectively, were achieved. The luminescent species was identified as [CuI(mCPy)2]2 on the basis of photophysical studies of model complexes and X-ray absorption spectroscopy.
We report the fabrication of high power conversion efficiency (PCE) polymer/fullerene bulk heterojunction (BHJ) photovoltaic cells using solution-processed Copper (I) Iodide (CuI) as hole transport layer (HTL). Our devices exhibit a PCE value of ∼5.5% which is equivalent to that obtained for control devices based on the commonly used conductive polymer poly(3,4-ethylenedioxythiophene): polystyrenesulfonate as HTL. Inverted cells with PCE >3% were also demonstrated using solution-processed metal oxide electron transport layers, with a CuI HTL evaporated on top of the BHJ. The high optical transparency and suitable energetics of CuI make it attractive for application in a range of inexpensive large-area optoelectronic devices.
CuI is lead oxide structured and crystallizes in the tetragonal P4/nmm space group. The structure is two-dimensional and consists of one CuI sheet oriented in the (0, 0, 1) direction. Cu1+ is bonded to four equivalent I1- atoms to form a mixture of edge and corner-sharing CuI4 tetrahedra. All Cu–I bond lengths are 2.67 Å. I1- is bonded in a 4-coordinate geometry to four equivalent Cu1+ atoms.
CuI is lead oxide-like structured and crystallizes in the trigonal P3m1 space group. The structure is two-dimensional and consists of one CuI sheet oriented in the (0, 0, 1) direction. there are two inequivalent Cu1+ sites. In the first Cu1+ site, Cu1+ is bonded to four I1- atoms to form a mixture of edge and corner-sharing CuI4 tetrahedra. There are one shorter (2.61 Å) and three longer (2.68 Å) Cu–I bond lengths. In the second Cu1+ site, Cu1+ is bonded to four I1- atoms to form a mixture of edge and corner-sharing CuI4 tetrahedra. There are one shorter (2.60 Å) and three longer (2.69 Å) Cu–I bond lengths. There are two inequivalent I1- sites. In the first I1- site, I1- is bonded in a 4-coordinate geometry to four Cu1+ atoms. In the second I1- site, I1- is bonded in a 4-coordinate geometry to four Cu1+ atoms.
CuI is lead oxide-like structured and crystallizes in the trigonal P3m1 space group. The structure is two-dimensional and consists of three CuI sheets oriented in the (0, 0, 1) direction. there are two inequivalent Cu1+ sites. In the first Cu1+ site, Cu1+ is bonded to four equivalent I1- atoms to form a mixture of edge and corner-sharing CuI4 tetrahedra. There are one shorter (2.61 Å) and three longer (2.68 Å) Cu–I bond lengths. In the second Cu1+ site, Cu1+ is bonded to four equivalent I1- atoms to form a mixture of edge and corner-sharing CuI4 tetrahedra. There are one shorter (2.62 Å) and three longer (2.68 Å) Cu–I bond lengths. I1- is bonded in a 4-coordinate geometry to four equivalent Cu1+ atoms. There are one shorter (2.61 Å) and three longer (2.68 Å) I–Cu bond lengths.
CuI crystallizes in the orthorhombic Cmcm space group. The structure is one-dimensional and consists of two CuI ribbons oriented in the (0, 0, 1) direction. Cu1+ is bonded in a distorted trigonal planar geometry to three equivalent I1- atoms. There are two shorter (2.60 Å) and one longer (2.63 Å) Cu–I bond lengths. I1- is bonded in a 3-coordinate geometry to three equivalent Cu1+ atoms.
We have determined the critical surface density of the CuI buffer layer inserted to change the preferred orientation of copper phthalocyanine (CuPc) crystals grown on the buffer layer. X-ray reflectivity measurements were performed to obtain the density profiles of the buffer layers and out-of-plane and 2D grazing-incidence X-ray diffraction measurements were performed to determine the preferred orientations of the molecular crystals. Remarkably, it was found that the preferred orientation of the CuPc film is completely changed from edge-on (1 0 0) to face-on (1 1 −2) by a CuI buffer layer with a very low surface density, so low that a large proportion of the substrate surface is bare.
In this paper, we report the properties of the reported transparent conductor CuI, including the effect of heavy p-type doping. The results, based on first-principles calculations, include an analysis of the electronic structure and calculations of optical and dielectric properties. We find that the origin of the favorable transparent conducting behavior lies in the absence in the visible of strong interband transitions between deeper valence bands and states at the valence-band maximum that become empty with p-type doping. Instead, strong interband transitions to the valence-band maximum are concentrated in the infrared with energies below 1.3 eV. This is contrast to the valence bands of many wide-band-gapmaterials. Turning to the mobility,we find that the states at the valence-band maximum are relatively dispersive. This originates from their antibonding Cu d–I p character. We find a modest enhancement of the Born effective charges relative to nominal values, leading to a dielectric constant ε(0) = 6.3. This is sufficiently large to reduce ionized impurity scattering, leading to the expectation that the properties of CuI can still be significantly improved through sample quality.