Temperature dependence of diffusion length, lifetime and minority electron mobility in GaInP

The mobility of electrons in double heterostructures of p-type Ga{sub 0.50}In{sub 0.50}P has been determined by measuring minority carrier diffusion length and lifetime. The minority electron mobility increases monotonically from 300 K to 5 K, limited primarily by optical phonon and alloy scattering. Comparison to majority electron mobility over the same temperature range in comparably doped samples shows a significant reduction in ionized impurity scattering at lower temperatures, due to differences in interaction of repulsive versus attractive carriers with ionized dopant sites. These results should be useful in modeling and optimization for multi-junction solar cells and other optoelectronic devices.

36 MATERIALS SCIENCE↗

Proton irradiation effects on minority carrier diffusion length and defect introduction in homoepitaxial and heteroepitaxial n-GaN [Proton irradiation effects on minority carrier diffusion length and defect introduction in homoepitaxial n-GaN]

Here, inherent advantages of wide bandgap materials make GaN-based devices attractive for power electronics and applications in radiation environments. Recent advances in the availability of wafer-scale, bulk GaN substrates have enabled the production of high quality, low defect density GaN devices, but fundamental studies of carrier transport and radiation hardness in such devices are lacking. Here, we report measurements of the hole diffusion length in low threading dislocation density (TDD), homoepitaxial n-GaN, and high TDD heteroepitaxial n-GaN Schottky diodes before and after irradiation with 2.5 MeV protons at fluences of 4–6 × 10 13 protons/cm 2 . We also characterize the specimens before and after irradiation using electron beam-induced-current (EBIC) imaging, cathodoluminescence, deep level optical spectroscopy (DLOS), steady-state photocapacitance, and lighted capacitance-voltage (LCV) techniques. We observe a substantial reduction in the hole diffusion length following irradiation (50%–55%) and the introduction of electrically active defects which could be attributed to gallium vacancies and associated complexes (V Ga -related), carbon impurities (C-related), and gallium interstitials (Ga i ). EBIC imaging suggests long-range migration and clustering of radiation-induced point defects over distances of ~500 nm, which suggests mobile Ga i . Following irradiation, DLOS and LCV reveal the introduction of a prominent optical energy level at 1.9 eV below the conduction band edge, consistent with the introduction of Ga i .

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

The Reactive–Diffusive Length of OH and Ozone in Model Organic Aerosols

We report that a key step in the heterogeneous oxidation of atmospheric aerosols is the reaction of ozone (O 3 ) and hydroxyl radicals (OH) at the gas–particle interface. The formation of reaction products and free radical intermediates and their spatial distribution inside the particle is a sensitive function of the length over which these oxidants diffuse prior to reaction. The reactive–diffusive length of OH and ozone at organic aerosol interfaces is determined by observing the change in the effective uptake coefficient for size-selected model aerosols comprising a reactive core and a thin nanometer-sized (0–12 nm) organic shell. The core and shell materials are selected so that they are immiscible and adopt an assumed core–shell configuration. The results indicate a reactive–diffusive length of 1.4 nm for hydroxyl (OH) radicals in squalane and 1.0 nm for ozone in squalene. Measurements for a purely diffusive system allow for an estimate for diffusion constant (1.6 × 10 -6 cm 2 /s) of ozone in squalane to be determined. In conclusion, the reactive–diffusive length offers a simple first order estimate of how shielding of aerosols by immiscible layers can alter estimates of oxidative lifetimes of aerosols in the atmosphere.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Diffusion length in nanoporous TiO{sub 2} films under above-band-gap illumination

We determined the carrier diffusion lengths in TiO{sub 2} nanoporous layers of dye-sensitized solar cells by using scanning photocurrent microscopy using an ultraviolet laser. Here, we excited the carrier directly in the nanoporous layers where the diffusion lengths were found to 140 μm as compared to that of visible illumination measured at 90 μm. The diffusion length decreased with increasing laser modulation frequency, in which we determined the electron lifetimes and the diffusion coefficients for both visible and UV illuminations. The diffusion lengths have been studied in terms of the sintering temperatures for both cells with and without binding molecules. We found a strong correlation between the diffusion length and the overall light-to-current conversion efficiency, proving that improving the diffusion length and hence the interparticle connections, is key to improving cell efficiency.

36 MATERIALS SCIENCE↗

Charge Carrier Diffusion Length Determination in 4H-SiC Schottky Alpha Detectors

When developing semiconductor radiation detectors detailed characterization of the detector behavior is required. The ability of a semiconductor radiation detector to collect the charge liberated by incident ionizing radiation is a critical characteristic. Several factors influence the charge collection efficiency of a semiconductor radiation detector, including electron-hole trapping, applied electric field strength, and dopant concentrations and dimensions of low doped regions. Applying a reverse bias electric potential to a low doped semiconductor region creates a free charge carrier depleted region and establishes an electric field which can remove subsequently freed charge in the form of an electrical signal. When ionizing radiation is incident upon a semiconductor electron-hole pairs are generated. These charge carriers are created along the path of the ionizing radiation regardless of the doping concentration. However, only the charge freed in the low doped epitaxial region of a detector will be collected as a result of the applied electric field. When the electric field is insufficient to develop a depleted region equal to or larger than the range of the ionizing radiation in the detector material some charge freed by the ionizing radiation outside of the sensitive region will be lost, thus potentially resulting in less than complete charge collection. The incomplete collection of charge complicates the analysis of the incident particle energy spectrum. Charge freed in the highly doped bulk region beyond the low doped epitaxial region may diffuse back into the low doped depleted region and be subsequently included in the integral pulse. The amount of charge collected as a result of this diffusion mechanism is dependent upon the diffusion length of the charge carriers in the material. The diffusion length is subsequently dependent on the material properties of the detector including the number of defects, trapping centers, and temperature. In order to fully characterize the properties of 4H-SiC as a radiation detector the diffusion length was calculated by adjusting the theoretical diffusion length value used in the calculation of the charge collection efficiency to agree with empirically observed charge collection efficiencies. The discrepancy between the observed and theoretical charge collection efficiency at 50 to 150 volts applied bias indicates an unexplained charge collection phenomenon which is contributing to the larger than predicted charge collection efficiency of the detectors. This voltage range corresponds to an intermediate applied bias, indicating that either the theoretical depletion width is too short, the diffusion length varies with the composition of the region that the charge carriers are diffusing through, or some other phenomenon is involved. If the charge carrier diffusion length varies depending on whether or not the diffusing charge is freed in unbiased epitaxy or bulk layer, then a function describing the variation of the diffusion layer could be determined by measuring the diffusion length at the applied voltages used previously, but over a range of epitaxial layer thicknesses. Future work includes the characterization of the effects of high temperature operation on the diffusion length of 4H-SiC in addition to measuring the effects of varying energy alpha emitter electrodeposition on the observed diffusion length. Additional Schottky barrier contacts, namely those with a nickel-platinum contact, will be tested in various sizes which have been developed in order to eliminate certain failure mechanisms and explore the potential effects of Schottky contact size on charge collection efficiency. (authors)

36 MATERIALS SCIENCE↗

Measurement of minority carrier diffusion lengths in GaAs nanowires by a nanoprobe technique

Minority carrier diffusion lengths in both p-type and n-type GaAs nanowires were studied using electron beam induced current by means of a nanoprobe technique without lithographic processing. The diffusion lengths were determined for Au/GaAs rectifying junctions as well as axial p-n junctions. By incorporating a thin lattice-matched InGaP passivating shell, a 2-fold enhancement in the minority carrier diffusion lengths and one order of magnitude reduction in the surface recombination velocity were achieved.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Laser interferometric method for determining the carrier diffusion length in semiconductors

A new laser interferometric method for measuring the carrier diffusion length in semiconductors is proposed. The method is based on the interference–absorption interaction of two laser radiations in a semiconductor. Injected radiation generates additional carriers in a semiconductor, which causes a change in the material’s optical constants and modulation of the probing radiation passed through the sample. When changing the distance between carrier generation and probing points, a decrease in the carrier concentration, which depends on the diffusion length, is recorded. The diffusion length is determined by comparing the experimental and theoretical dependences of the probe signal on the divergence of the injector and probe beams. The method is successfully tested on semiconductor samples with different thicknesses and surface states and can be used in scientific research and the electronics industry.

36 MATERIALS SCIENCE↗

Determination of the Pt spin diffusion length by spin-pumping and spin Hall effect

The spin diffusion length of Pt at room temperature and at 8 K is experimentally determined via spin pumping and spin Hall effect in permalloy/Pt bilayers. Voltages generated during excitation of ferromagnetic resonance from the inverse spin Hall effect and anisotropic magnetoresistance effect were investigated with a broadband approach. Varying the Pt layer thickness gives rise to an evolution of the voltage line shape due to the superposition of the above two effects. By studying the ratio of the two voltage components with the Pt layer thickness, the spin diffusion length of Pt can be directly extracted. We obtain a spin diffusion length of ∼1.2 nm at room temperature and ∼1.6 nm at 8 K.

36 MATERIALS SCIENCE↗

Measurements on the Diffusion Length of Thermal Neutrons in Water from 25 to 296°C

Here, the diffusion length of thermal neutrons has been measured in water over the range 25.9 to 295.3°C in the pressure vessel of the KAPL High Temperature Critical Assembly. The diffusion length was determined by fitting an exponential to the data found by activating manganese foils with neutrons from a small Sb-Be source. The temperature variation of the diffusion length could be fairly well represented by either of two simple approximations—either that the transport cross section of water has a 1/υ behavior, or that the transport cross section is determined from the Radkowsky prescription.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Determination of charge-carrier diffusion length in the photosensing layer of HgCdTe n-on-p photovoltaic infrared focal plane array detectors

In the present paper, we propose a method for evaluating the bulk diffusion length of minority charge carriers in the photosensing layer of photovoltaic focal plane array (FPA) photodetectors. The method is based on scanning a strip-shaped illumination spot with one of the detector diodes at a low level of photocurrents j{sub ph} being registered; such scanning provides data for subsequent analysis of measured spot-scan profiles within a simple diffusion model. The asymptotic behavior of the effective (at j{sub ph} ≠ 0) charge-carrier diffusion length l{sub d} {sub eff} as a function of j{sub ph} for j{sub ph} → 0 inferred from our experimental data proved to be consistent with the behavior of l{sub d} {sub eff} vs j{sub ph} as predicted by the model, while the obtained values of the bulk diffusion length of minority carriers (electrons) in the p-HgCdTe film of investigated HgCdTe n-on-p FPA photodetectors were found to be in a good agreement with the previously reported carrier diffusion-length values for HgCdTe.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Long carrier diffusion length in two-dimensional lead halide perovskite single crystals

Ruddlesden-Popper (RP) perovskites are two-dimensional semiconductors for high-performance optoelectronic devices. In this work, we report a long in-plane carrier diffusion length in 2D RP perovskite single crystals probed by scanning photocurrent microscopy. Carrier diffusion lengths of 7–14μm are observed when the number of PbI 6 –2 octahedra between organic spacers increases from 1 to 3. Using detailed light intensity and electric-field-dependent photocurrent measurements, we attribute the observed long diffusion length to the dominating dissociated free carrier transport. This is further validated by time-resolved photoluminescence measurements, where the decay lifetime increases in the presence of an electric field. From our experiments, we conclude that the in-plane transport in RP perovskites is efficient because of the partial free carrier generation, which overcomes strong excitonic effects. In conclusion, our results suggest that semiconducting devices fabricated from RP perovskite single crystals can be as efficient as their 3D counterparts.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Increase in the diffusion length of minority carriers in Al{sub x}Ga{sub 1–x}N alloys ({sub x} = 0–0.1) fabricated by ammonia molecular beam epitaxy

The room-temperature diffusion length of minority carriers in n-Al{sub 0.1}Ga{sub 0.9}N layers grown by ammonia molecular beam epitaxy on sapphire (0001) substrates used in structures for ultraviolet photodetectors is studied. Measurements were performed using the spectral dependence of the photocurrent recorded in a built-in p–n junction for thin samples and using the induced electron-current procedure for films up to 2 µm thick. The results show that the hole diffusion length in n-AlGaN films is 120–150 nm, which is larger than in GaN films grown under similar growth conditions by a factor of 3–4. This result can be associated with the larger lateral sizes characteristic of hexagonal columns in AlGaN layers grown by molecular beam epitaxy. No increase in the hole diffusion length is observed for thicker films.

36 MATERIALS SCIENCE↗

Strongly extended diffusion length for the nonequilibrium magnons in Y 3 F e 5 O 12 by photoexcitation

Y 3 Fe 5 O 12 (YIG) is known for its long magnon diffusion length. Although it has the known lowest damping rate, an even longer diffusion distance is still highly desired since it may lead to a much more efficient information transmission and processing. While most of previous works focused on the generation and detection of magnons in YIG, here we demonstrate how to depress the damping rate during the diffusion of magnon. By selectively exciting the spin state transition of the Fe ions in YIG, we successfully increase magnon diffusion length by one order of magnitude, i.e., from the previous reported ~10 μm up to ~156 μm (for the sample prepared by liquid phase epitaxy) and ~180 μm (for the sample prepared by pulsed laser deposition) at room temperature. The diffusion length, determined by nonlocal geometry, is ~30 μm for the magnons induced by visible light and above 150 μm for the laser of 980 nm. In addition to thermal gradient, light excitation affects the electron configuration of the Fe 3+ ion in YIG. Long-wavelength laser is more effective since it causes a transition of the Fe 3+ ions in FeO 6 octahedron from a high spin to a low spin state and thus causes a magnon softening which favors a long-distance diffusion. Furthermore, the present work paves the way toward an efficient tuning of magnon transport which is crucially important for magnon spintronics.

36 MATERIALS SCIENCE↗

Measurement of minority-carrier diffusion lengths using wedge-shaped semiconductor photoelectrodes

Measurement of the photocurrent as a function of the thickness of a light absorber has been shown herein both theoretically and experimentally to provide a method for determination of the minority-carrier diffusion length of a sample. To perform the measurement, an illuminated spot of photons with an energy well above the band gap of the material was scanned along the thickness gradient of a wedge-shaped, rear-illuminated semiconducting light absorber. Photogenerated majority carriers were collected through a back-side transparent ohmic contact, and a front-side liquid or Schottky junction collected the photogenerated minority carriers. Calculations showed that the diffusion length could be evaluated from the exponential variation in photocurrent as a function of the thickness of the sample. Good agreement was observed between experiment and theory for a solid-state silicon Schottky junction measured using this method. As an example for the application of the technique to semiconductor/liquid-junction photoelectrodes, the minority-carrier diffusion length was determined for graded thickness, sputtered tungsten trioxide and polished bismuth vanadate films under back-illumination in contact with an aqueous electrolyte. Furthermore, this wedge technique does not require knowledge of the spectral absorption coefficient, doping, or surface recombination velocity of the sample.

42 ENGINEERING↗

Enhancing electron diffusion length in narrow-bandgap perovskites for efficient monolithic perovskite tandem solar cells

Developing multijunction perovskite solar cells (PSCs) is an attractive route to boost PSC efficiencies to above the single-junction Shockley-Queisser limit. However, commonly used tin-based narrow-bandgap perovskites have shorter carrier diffusion lengths and lower absorption coefficient than lead-based perovskites, limiting the efficiency of perovskite-perovskite tandem solar cells. In this work, we discover that the charge collection efficiency in tin-based PSCs is limited by a short diffusion length of electrons. Adding 0.03 molar percent of cadmium ions into tin-perovskite precursors reduce the background free hole concentration and electron trap density, yielding a long electron diffusion length of 2.72 ± 0.15 um. It increases the optimized thickness of narrow-bandgap perovskite films to 1000 nm, yielding exceptional stabilized efficiencies of 20.2 and 22.7% for single junction narrow-bandgap PSCs and monolithic perovskite-perovskite tandem cells, respectively. This work provides a promising method to enhance the optoelectronic properties of narrow-bandgap perovskites and unleash the potential of perovskite-perovskite tandem solar cells.

14 SOLAR ENERGY↗

The spin Hall angle and spin diffusion length of Pd measured by spin pumping and microwave photoresistance

We present the experimental study of the spin Hall angle (SHA) and spin diffusion length of Pd with the spin pumping and microwave photoresistance effects. The Py/Pd bilayer stripes are excited with an out-of-plane microwave magnetic field. The pure spin current is thus pumped and transforms into charge current via the inverse spin Hall effect (ISHE) in Pd layer, yielding an ISHE voltage. The ISHE voltage can be distinguished from the unwanted signal caused by the anisotropic magnetoresistance according to their different symmetries. Together with Pd thickness dependent measurements of in and out-of-plane precessing angles and effective spin mixing conductance, the SHA and spin-diffusion length of Pd are quantified as 0.0056 ± 0.0007 and 7.3 ± 0.7 nm, respectively.