Search NASA⌕ Search

SEARCH · Search NASA

Results for “DMTA”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

Exploring the in vitro formation of trimethylarsine sulfide from dimethylthioarsinic acid in anaerobic microflora of mouse cecum using HPLC-ICP-MS and HPLC-ESI-MS

Although metabolism of arsenicals to form methylated oxoarsenical species has been extensively studied, less is known about the formation of thiolated arsenical species that have recently been detected as urinary metabolites. Indeed, their presence suggests that the metabolism of ingested arsenic is more complex than previously thought. Recent reports have shown that thiolated arsenicals can be produced by the anaerobic microflora of the mouse cecum, suggesting that metabolism prior to systemic absorption may be a significant determinant of the pattern and extent of exposure to various arsenic-containing species. Here, we examined the metabolism of {sup 34}S labeled dimethylthioarsinic acid ({sup 34}S-DMTA{sup V}) by the anaerobic microflora of the mouse cecum using HPLC-ICP-MS and HPLC-ESI-MS/MS to monitor for the presence of various oxo- and thioarsenicals. The use of isotopically enriched {sup 34}S-DMTA{sup V} made it possible to differentiate among potential metabolic pathways for production of the trimethylarsine sulfide (TMAS{sup V}). Upon in vitro incubation in an assay containing anaerobic microflora of mouse cecum, {sup 34}S-DMTA{sup V} underwent several transformations. Labile {sup 34}S was exchanged with more abundant {sup 32}S to produce {sup 32}S-DMTA{sup V}, a thiol group was added to yield DMDTA{sup V}, and a methyl group was added to yield {sup 34}S-TMAS{sup V}. Because incubation of {sup 34}S-DMTA{sup V} resulted in the formation of {sup 34}S-TMAS{sup V}, the pathway for its formation must preserve the arsenic-sulfur bond. The alternative metabolic pathway postulated for formation of TMAS{sup V} from dimethylarsinic acid (DMA{sup V}) would proceed via a dimethylarsinous acid (DMA{sup III}) intermediate and would necessitate the loss of {sup 34}S label. Structural confirmation of the metabolic product was achieved using HPLC-ESI-MS/MS. The data presented support the direct methylation of DMTA{sup V} to TMAS{sup V}. Additionally, the detection of isotopically pure {sup 34}S-TMAS{sup V} raises questions about the sulfur exchange properties of TMAS{sup V} in the cecum material. Therefore, {sup 34}S-TMAS{sup V} was incubated and the exchange was monitored with respect to time. The data suggest that the As-S bond associated with TMAS{sup V} is less labile than the As-S bond associated with DMTA{sup V}.

60 APPLIED LIFE SCIENCES↗

Contribution of Catalytic Transesterification Reactions to the Compatibilization of Poly(lactic acid)/Polycarbonate Blends: Thermal, Morphological and Viscoelastic Characterization

Samarium acetylacetonate (Sm-Acac) was added to catalyze interchange reactions between poly(lactic acid) (PLA) and polycarbonate (PC) in order to promote compatibilization and enhance the performances of the PLA/PC blend. The effects of the composition and catalyzed transesterification reactions were investigated using differential scanning calorimetry (DSC), thermogravimetry (TG), dynamic mechanical thermal analysis (DMTA) and scanning electron microscopy (SEM). DMTA and DSC analysis revealed the immiscibility of the uncatalyzed PLA/PC blends for the studied compositions because the glass transition temperatures of PC and PLA were unchanged after blending. In the PLA glassy region, PLA/PC blends exhibited lower storage moduli which increased upon heating due to the cold crystallization process. During melt mixing with Sm-Acac catalyst, PLA/PC blends were submitted to two competing processes. In one hand, Sm-Acac acted as a plasticizer and contributed in decreasing significantly the glass transition, crystallization and melting temperatures of PLA phase. In the other hand, Sm-Acac proved its efficiency in catalyzing the transesterification reactions that were evidenced by the decrease of the PLA aptitude to crystallization due to the hindering effect of the PC units inserted into the PLA chains. PLA/PC blends melt mixed with 0.25% of Sm-Acac showed a significant strengthening effect, corresponding to an increase in the storage modulus in the temperature range comprised between 70 and 90 °C. This indicated the formation of a copolymer at the interface and the promotion of adhesion as it is confirmed from the decrease in the height of the PLA Tan δ peak. At 0.5% of Sm-Acac, (90/10) PLA/PC blend revealed a new peak assigned to the glass transition of the PLA-PC copolymer, whereas the (50/50) PLA/PC blend was converted into a new random copolymer. TG analysis proved the presence of a copolymer structure presenting an intermediate thermal stability in both the catalyzed and uncatalyzed blends.

36 MATERIALS SCIENCE↗

Glutaraldehyde as Ambient Temperature Crosslinking Agent of Latex Films from Natural Rubber Grafted with Poly(diacetone acrylamide)

The concept of using glutaraldehyde (GTA) to crosslink natural rubber (NR) particles bearing diacetone acrylamide (DAAM) functional groups during film formation was investigated in the present work. The primary advantage of this curing system is that it is feasible under ambient conditions, which can lower operating costs of the curing process. Graft copolymers of NR and poly(diacetone acrylamide) prepared with 5 wt% of DAAM (NR–g–PDAAM5) were synthesized by seeded emulsion polymerization at 50 °C. Then, the tensile properties were measured for cast films formed from NR–g–PDAAM5 latex in the absence and presence of GTA. The results revealed increased tensile strength of the NR–g–PDAAM5 film, when GTA was added into the latex prior to film casting. The crosslinking of NR–g–PDAAM5 latex film by reaction with GTA, after film casting, was also investigated using attenuated total reflection Fourier transform infrared (ATR–FTIR) and dynamic mechanical thermal analysis (DMTA). ATR–FTIR analysis demonstrated that crosslinking reactions formed conjugated C=C double bonds between the active carbonyl groups of DAAM and GTA. The complementary use of DMTA also corroborated that crosslinking reactions took place involving the grafted PDAAM chains on the NR particles. This was evidenced by a clear shift towards higher temperatures of the tan δ peak, corresponding to the T{sub g} of NR–g–PDAAM phase, when GTA was incorporated into the NR–g–PDAAM5 latex before film formation. Additionally, a noticeable increase in thermal stability of the NR–g–PDAAM5 film was also observed with added GTA. Hence, it can be concluded that GTA is an efficient room-temperature crosslinker for NR particles functionalized with DAAM. This curing system can also be considered an alternative, simple, and inexpensive method for curing NR latex compounds, as only one component (GTA) is required in the curing process.

36 MATERIALS SCIENCE↗

Reversible Interlayer Sliding and Conductivity Changes in Adaptive Tetrathiafulvalene-Based Covalent Organic Frameworks

Ordered interlayer stacking is intrinsic in two-dimensional covalent organic frameworks (2D COFs) and has strong implications on COF's optoelectronic properties. Reversible interlayer sliding, corresponding to shearing of 2D layers along their basal plane, is an appealing dynamic control of both structures and properties, yet it remains unexplored in the 2D COF field. In this paper, we demonstrate that the reversible interlayer sliding can be realized in an imine-linked tetrathiafulvalene (TTF)-based COF TTF-DMTA. The solvent treatment induces crystalline phase changes between the proposed staircase-like sql net structure and a slightly slipped eclipsed sql net structure. The solvation-induced crystallinity changes correlate well with reversible spectroscopic and electrical conductivity changes as demonstrated in oriented COF thin films. In contrast, no reversible switching is observed in a related TTF-TA COF, which differs from TTF-DMTA in terms of the absence of methoxy groups on the phenylene linkers. This work represents the first 2D COF example of which eclipsed and staircase-like aggregated states are interchangeably accessed via interlayer sliding, an uncharted structural feature that may enable applications such as chemiresistive sensors.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Miscible blends of biobased poly(lactide) with poly(methyl methacrylate): Effects of chopped glass fiber incorporation

Poly(lactide) (PLA) and poly(methyl methacrylate) (PMMA) are melt compounded with chopped glass fiber using laboratory scale twin-screw extrusion. Physical properties are examined using differential scanning calorimetry (DSC), dynamic mechanical thermal analysis (DMTA), thermogravimetric analysis (TGA), tensile testing, impact testing, X-ray computed tomography (CT) scanning, and field emission scanning electron microscopy (FE-SEM). Molecular weight is determined using gel permeation chromatography (GPC). Miscibility of the blends is implied by the presence of a single glass transition temperature and homogeneous morphology. PLA/PMMA blends tend to show positive deviations from a simple linear mixing rule in their mechanical properties (e.g., tensile toughness, modulus, and stress at break). The addition of 40 wt % glass fiber to the system dramatically increases physical properties. Across all blend compositions, the tensile modulus increases from roughly 3 GPa to roughly 10 GPa. Estimated heat distortion temperatures (HDTs) are also greatly enhanced; the pure PLA sample HDT increases from 75 degrees C to 135 degrees C. Fiber filled polymer blends represent a sustainable class of earth abundant materials which should prove useful across a range of applications.

36 MATERIALS SCIENCE↗

Rheology, Mechanical Properties and Morphology of Poly(lactic acid)/Ethylene Vinyl Acetate Blends

In this work, the effect of ethylene vinyl acetate (EVA) content on the rheology, mechanical properties, and morphology of poly (lactic acid) (PLA)/EVA blends was investigated. Differential Scanning Calorimetry (DSC) showed that the addition of EVA to PLA decreased the degree of crystallinity of PLA. Dynamic Mechanical Thermal Analysis (DMTA) results showed that the presence of EVA copolymer increased the cold crystallization temperature (T{sub cc}) of PLA. The addition of 10% of EVA to PLA substantially increased the impact strength. Morphology analysis by Scanning Electron Microscopy (SEM) indicated the immiscibility between PLA and EVA phases and an in increase the EVA average dispersed phase domains size with the increase in EVA content. Rheological measurements under oscillatory shear flow showed that storage modulus (G′) increased with the increase in the EVA content at low frequencies and is related to the increase in the EVA dispersed phase domains size, as also observed by relaxation spectrum analysis. Cole–Cole plots of imaginary viscosity (η″) versus real viscosity (η′) and Han plots of storage modulus (G′) versus loss modulus (G″) indicated that PLA and EVA phases are immiscible, as also observed by SEM.

36 MATERIALS SCIENCE↗

Bio-based PA5.10 for Industrial Applications: Improvement of Barrier and Thermo-mechanical Properties with Rice Husk Ash and Nanoclay

Composites consisting of renewable PA5.10 were obtained from melt compounding with a modified clay (CL) and/or a by-product obtained from the combustion of rice husk (RHA). Two different industrialized lab-scale machines were used to obtain the final shape: a film extrusion machine and an injection moulding apparatus. The industrial application requirements for polyamides generally need good barrier properties and high thermo-mechanical strength. Considering the barrier properties, the CL was able to decrease the oxygen permeability to less than half with respect to neat PA5.10. DMTA demonstrated that the addition of RHA caused a consistent enhancement (+ 46 °C) in the heat deflection temperature (HDT) compared to the neat PA5.10 matrix, increasing the possible areas of interest. Furthermore, the simultaneous presence of RHA and CL provided the best result reaching an extraordinary HDT of 131 °C. A complete discussion taking into account the morphology, crystallinity and filler-matrix adhesion evaluation was reported as well as comparison of performances with other bio-PAs composites. These two fillers can therefore be used separated or together combined in PA5.10 for functional purposes in a sustainable scenario.

36 MATERIALS SCIENCE↗

Preparation and properties of UV-cured acrylated silane intercalated polymer/LDH nanocomposite

A novel UV-cured polymer/layered double hydroxide (LDH) nanocomposite was prepared by modifying the LDH with sodium dodecyl sulfate (SDS) and [3-(methyl-acroloxy)propyl]trimethoxysilane (KH570) followed by UV irradiation after blended into a acrylate system. From the XRD analyses, the SDS-modified LDH-DS presented the basal spacing of 2.67 nm, whereas the further KH570-intercalated LDH-KH showed a slight decrease to 2.41 nm. After UV irradiated the exfoliated microstructure was formed, and observed by TEM and HR-TEM, showing the fine dispersion and random orientation of LDH in the polymer matrix. The storage modulus and glass transition temperature of the nanocomposite containing 5% LDH-KH increased to 47.5 MPa and 67.8 {sup o}C, respectively, from 39.7 MPa and 66 {sup o}C of the pure polymer from DMTA measurements. The tensile strength and Persoz hardness were enhanced to 10.6 MPa and 111 s, respectively, from 7.7 MPa and 85 s of the pure polymer.

36 MATERIALS SCIENCE↗

Environmentally friendly preparation of nanoparticles for organic photovoltaics

Aqueous nanoparticle dispersions were prepared from a conjugated polymer poly[thiophene-2,5-diyl-alt-5,10-bis((2-hexyldecyl)oxy)dithieno[3,2-c:3',2'-h][1,5]naphthyridine-2,7-diyl] (PTNT) and fullerene blend utilizing chloroform as well as a non-chlorinated and environmentally benign solvent, o-xylene, as the miniemulsion dispersed phase solvent. The nanoparticles (NPs) in the solid-state film were found to coalesce and offered a smooth surface topography upon thermal annealing. Organic photovoltaics (OPVs) with photoactive layer processed from the nanoparticle dispersions prepared using chloroform as the miniemulsion dispersed phase solvent were found to have a power conversion efficiency (PCE) of 1.04%, which increased to 1.65% for devices utilizing NPs prepared from o-xylene. Physical, thermal and optical properties of NPs prepared using both chloroform and o-xylene were systematically studied using dynamic mechanical thermal analysis (DMTA) and photoluminescence (PL) spectroscopy and correlated to their photovoltaic properties. The PL results indicate different morphology of NPs in the solid state were achieved by varying miniemulsion dispersed phase solvent.

14 SOLAR ENERGY↗

Engineering Two-Phase and Three-Phase Microstructures from Water-Based Dispersions of Nanoparticles for Eco-Friendly Polymer Solar Cell Applications

Nanoparticle organic photovoltaics, a subfield of organic photovoltaics (OPV), has attracted increasing interest in recent years due to the eco-friendly fabrication of solar modules afforded by colloidal ink technology. Importantly, using this approach it is now possible to engineer the microstructure of the light absorbing/charge generating layer of organic photovoltaics; decoupling film morphology from film deposition. In this study, single-component nanoparticles of poly(3-hexylthiophene) (P3HT) and phenyl-C 61 butyric acid methyl ester (PC 61 BM) were synthesized and used to generate a two-phase microstructure with control over domain size prior to film deposition. Scanning transmission X-ray microscopy (STXM) and electron microscopy were used to characterize the thin film morphology. Uniquely, the measured microstructure was a direct input for a nanoscopic kinetic Monte Carlo (KMC) model allowing us to assess exciton transport properties that are experimentally inaccessible in these single-component particles. Photoluminescence, UV-vis spectroscopy measurements, and KMC results of the nanoparticle thin films enabled the calculation of an experimental exciton dissociation efficiency (η ED ) of 37% for the two-phase microstructure. The glass transition temperature (T g ) of the materials was characterized with dynamic mechanical thermal analysis (DMTA) and thermal annealing led to an increase in ηED to 64% due to an increase in donor-acceptor interfaces in the thin film from both sintering of neighboring opposite-type particles in addition to the generation of a third mixed phase from diffusion of PC 61 BM into amorphous P3HT domains. Finally, this study demonstrates the higher level of control over donor-acceptor film morphology enabled by customizing nanoparticulate colloidal inks, where the optimal three-phase film morphology for an OPV photoactive layer can be designed and engineered.

36 MATERIALS SCIENCE↗

Robust Self-Healing Adhesives Based on Dynamic Urethane Exchange Reactions

Thermoset polyurethanes (PUs) have been successfully reprocessed as covalent adaptable networks (CANs) by catalyzing carbamate exchange. Here we extend bond exchange beyond the internal network cross-links to create a dynamic urethane adhesive. Interfacing PU CANs to substrates with nucleophilic functional groups creates adhesives capable of reversible transcarbamoylation with the substrate, which has not been demonstrated previously by CAN adhesives. Two types of thermoset PU films were synthesized, one containing the green carbamate exchange catalyst Zr(tmhd)4 and the other containing no catalyst. Although otherwise identical in chemical and network properties, as indicated by FT-IR spectroscopy and dynamic mechanical thermal analysis (DMTA), the film containing catalyst showed dynamic bond exchange behavior through stress relaxation analysis. When evaluated as an adhesive, the CAN film exhibited self-healing properties and retained its adhesive strength for five cycles, which is attributed to reversible covalent bonding to the glass substrate. Furthermore, this work expands industrially relevant CANs to structural adhesives and demonstrates their potential value in an application that presently employs PUs as single-use materials.

adhesive↗

Study on process and characterization of high-temperature resistance polyimide composite

A novel polyimide composite with upper-use temperature of 420°C was prepared by autoclave process. The thermogravimetic analysis and rheological properties of uncured polyimide resin powders were analyzed. The influences of process parameters and post-treatment process on the properties of composites were also investigated. The morphologies of polyimide composites after shear fracture were observed by scanning electron microscope (SEM). The high-temperature resistance of composite was characterized by dynamic mechanical thermal analyzer (DMTA). Results showed that the imidization reaction mainly occurred in the temperature range of 100°C~220°C, and the largest weight loss rate appearing at 145°C indicated a drastic imidization reaction occurred. The melt viscosity of polyimide resin decreased with increasing the temperature between 220°C ∼305°C, and then increased with the increase of temperature due to the molecular crosslinking reactions. The fiber volume contents and void contents could be effectively controlled by applying the pressure step by step. The fiber volume content was sensitive to the initial pressure (P{sub i}) during the imidization. The second-stage pressure (P{sub 2}) and the temperature for applying the P{sub 2} (T{sub 2}) during the imidization had a great effect on the void content of composite. Good mechanical properties and interfacial adhesion of polyimide composite could obtain by optimized process. The post-treatment process can obviously increase the high-temperature resistance of polyimide composite. The polyimide composite treated at 420°C exhibited good retention of mechanical properties at 420°C and had a glass transition temperature (Tg) of 456°C. The retentions of flexible strength, flexible modulus and short beam shear strength of polyimide composite at 420°C were 65%, 84% and 62% respectively.

36 MATERIALS SCIENCE↗

Evaluation of Common Thermoplastic Polymers in High-Pressure Cycling Hydrogen Under Ambient and Cold Environments as Applicable to the Hydrogen Infrastructure

Thermoplastic polymers are required to perform unfailingly under stringent conditions of changing pressures (35 MPa to 70 MPa) and temperatures (-40°C to +85°C) in storage and fueling operations. Although diffusivity in glassy polymers appear to be an order of magnitude lower than elastomers, polymer microstructural attributes such as degree of crystallinity and presence of polar and non-polar groups on the main chain with and without branching can play a substantial role in influencing their behaviors in hydrogen environments. In the work described here, the effect of high-pressure hydrogen cycling on PEEK, PTFE, PA11, HDPE, POM (and different commercial grades of these polymers) under ambient and cold (-40°C) conditions is addressed. Ex-situ characterization for polymer changes included density measurements for impact of hydrogen retention, hardness changes using nanoindentation, storage modulus and glass transition changes using dynamic mechanical and thermal analysis (DMTA), degree of crystallization with Differential Scanning Calorimetry (DSC) and tensile testing following ASTM D412. In other evaluations, solid-state nuclear magnetic resonance (NMR), attenuated total reflectance Fourier transform infra-red spectroscopy (ATRFTIR), X-ray diffraction (XRD), and X-ray CT results are presented. The overall impact of these evaluations is to establish a technical basis for the behaviors of common thermoplastics in cycling hydrogen environments under ambient and cold temperatures while establishing the relationship between polymer structure-based properties and hydrogen transport effects.

Menon, Nalini C.↗

Compatibility of polymers in super-critical carbon dioxide for power generation systems: High level findings for low temperatures and pressure conditions

Polymers such as PTFE (polytetrafluorethylene or Teflon), PEEK (polyetheretherketone), EPDM (ethylene propylene cliene monomer) rubber, Viton, EPR (ethylene propylene rubber), Nylon, Nitrile rubber, and perfluoroelastomers are commonly employed in super critical CO 2 (sCO2) energy conversion systems. O-rings and gaskets made from these polymers face stringent performance conditions such as elevated temperatures, high pressures, pollutants and corrosive humid environments. Critical knowledge gaps about polymer degradation from sCO2 exposure need to be addressed. To understand these effects, we have studied nine commonly used polymers subjected to elevated temperatures under isobaric conditions of sCO2 pressure. The polymers (PEEK, Nylon, PTFE, EPDM, Nitrile rubber, EPR, Neoprene, perfluoroelastomer FF 202 and Viton) were exposed for 1000 hours at 100°C to 25 MPa sCO2 pressure in an autoclave. In a second study, elastomers perfluoroelastomer (FF202) and EPDM were exposed to 25 MPa sCO2 for 1000 hours at 150°C. Samples were extracted for ex-situ characterization at t = 200 hours and then at the completion of the test at t=1000 hours. The polymer samples were examined for physical and chemical changes by Dynamic Mechanical and Thermal Analysis (DMTA), Fourier Transform Infrared (FTIR) spectroscopy, and compression set. Density and mass changes immediately after removal from test and 48 hours later, and optical microscopy techniques were also used. Microcomputer tomography (micro CI) data was generated on select specimens. Super-critical CO 2 effects have been identified as either physical or chemical effects. For each polymer, the dominance of one type of effect over the other was evaluated. Attempts were also made to qualitatively link sCO2 effects such as lowering or increase in glass transition temperatures, storage modulus changes, mass and compression set changes, chemical changes seen in FTIR analyses and blister and void formation seen post-exposure to polymer microstructure-related mechanisms such as plasticization of the polymer matrix, escape of volatiles from the polymer during depressurization, and filler and plasticizer effects on microstructure with rapid depressurization rates.

36 MATERIALS SCIENCE↗

Collective Summary of sCO2 Materials Development (Supercritical Transformational Electric Power Generation (STEP) Level 2 Milestone Report) (Parts I - II)

Polymers such as PTFE (polytetrafluorethylene or Teflon), EPDM (ethylene propylene diene monomer) rubber, FKM fluoroelastomer (Viton), Nylon 11, Nitrile butadiene (NBR) rubber, hydrogenated nitrile rubber (HNBR) and perfluoroelastomers (FF_202) are commonly employed in super critical CO 2 (sCO2) energy conversion systems. O-rings and gaskets made from these polymers face stringent performance conditions such as elevated temperatures, high pressures, pollutants, and corrosive humid environments. In FY 2019, we conducted experiments at high temperatures (100°C and 120°C) under isobaric conditions (20 MPa). Findings showed that elevated temperatures accelerated degradation of polymers in sCO2, and that certain polymer microstructures are more susceptible to degradation over others. In FY 2020, the focus was to understand the effect of sCO2 on polymers at low (10 MPa) and high pressures (40 MPa) under isothermal conditions (100°C). It was clear that the same selectivity was observed in these experiments wherein certain polymeric functionalities showed more propensity to failure over others. Fast diffusion, supported by higher pressures and long exposure times (1000 hours) at the test temperature, caused increased damage in sCO2 environments to even the most robust polymers. We also looked at polymers under compression in sCO2 at 100°C and 20 MPa pressure to imitate actual sealing performance required of these materials in sCO2 systems. Compression worsened the physical damage that resulted from chemical attack of the polymers under these test conditions. In FY 2021, the effect of cycling temperature (from 50°C to 150°C to 50°C) for polymers under a steady sCO2 pressure of 20 MPa was studied. The aim was to understand the influence of cycling temperatures of sCO2 for typical polymers under isobaric (20 MPa) conditions. Thermoplastic polymers (Nylon, and PTFE) and elastomers (EPDM, Viton, Buna N, Neoprene, FF202, and HNBR) were subjected to 20 MPa sCO2 pressure for 50 cycles and 100 cycles in separate experiments. Samples were extracted for ex-situ characterization at 50 cycles and upon the completion of 100 cycles. Each cycle constituted of 175 minutes of cycling from 50°C to 150°C. The polymer samples were examined for physical and chemical changes by Dynamic Mechanical and Thermal Analysis (DMTA), Fourier Transform Infrared (FTIR) spectroscopy, and compression set. Density and mass changes immediately after removal from test were measured for degree of swell comparisons. Optical microscopy techniques and micro computer tomography (micro CT) images were collected on select specimens. Evaluations conducted showed that exposures to super-critical CO2 environments resulted in combinations of physical and/or chemical changes. For each polymer, the dominance of cycling temperatures under sCO2 pressures, were evaluated. Attempts were made to qualitatively link the permanent sCO2 effects to polymer micro- structure, free volume, backbone substitutions, presence of polar groups, and degree of crystallinity differences. This study has established that soft polymeric materials are conducive to failure in sCO2 through mechanisms of failure that are dependent on polymer microstructure and chemistry. Polar pendant groups, large atom substitutions on the backbone are some of the factors that are influential structural factors.

36 MATERIALS SCIENCE↗

Dynamic Mechanical Thermal Analysis of Virgin TR-55 Silicone Rubber

Dynamic mechanical thermal analysis (DMTA) of virgin TR-55 silicone rubber specimens was conducted. Dynamic frequency/temperature sweep tests were conducted over the ranges 0.1-100 rad/s and 30-100 C using a parallel plate test geometry. A strain of 0.2% was used, which was near the upper limit of the linear viscoelastic region of the material based on initial dynamic strain sweep tests. Master curves of G{prime} and G{double_prime} as a function of frequency were generated using time-temperature superposition (horizontal shift with initial vertical correction). The activation energy calculated from an Arrhenius fit to the horizontal shift factors was 178-355 kJ/mol. The calculated percent load retention at {approx}50 years was 61-68%.

36 MATERIALS SCIENCE↗

Crystallization Behavior of Virgin TR-55 Silicone Rubber Measured Using Dynamic Mechanical Thermal Analysis with Liquid Nitrogen Cooling

Dynamic mechanical thermal analysis (DMTA) of virgin TR-55 silicone rubber specimens was conducted. Two dynamic temperature sweep tests, 25 to -100 C and 25 to -70 to 0 C (ramp rate = 1 C/min), were conducted at a frequency of 6.28 rad/s (1 Hz) using a torsion rectangular test geometry. A strain of 0.1% was used, which was near the upper limit of the linear viscoelastic region of the material based on an initial dynamic strain sweep test. Storage (G{prime}) and loss (G{double_prime}) moduli, the ratio G{double_prime}/G{prime} (tan {delta}), and the coefficient of linear thermal expansion ({alpha}) were determined as a function of temperature. Crystallization occurred between -40 and -60 C, with G{prime} increasing from {approx}6 x 10{sup 6} to {approx}4 x 10{sup 8} Pa. The value of {alpha} was fairly constant before ({approx}4 x 10{sup -4} mm/mm- C) and after ({approx}3 x 10{sup -4} mm/mm- C) the transition, and peaked during the transition ({approx}3 x 10{sup -3} mm/mm- C). Melting occurred around -30 C upon heating.

36 MATERIALS SCIENCE↗