Search NASA⌕ Search

SEARCH · Search NASA

Results for “DOUBLE BONDS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Organic Compounds Produced by Photolysis of Realistic Interstellar and Cometary Ice Analogs Containing Methanol

The InfraRed (IR) spectra of UltraViolet (UV) and thermally processed, methanol-containing interstellar / cometary ice analogs at temperatures from 12 to 300 K are presented. Infrared spectroscopy, H-1 and C-13 Nuclear Magnetic Resonance (NMR) spectroscopy, and gas chromatography-mass spectrometry indicate that CO (carbon monoxide), CO2 (carbon dioxide), CH4 (methane), HCO (the formyl radical), H2CO (formaldehyde), CH3CH2OH (ethanol), HC([double bond]O)NH2 (formamide), CH3C([double bond]O)NH2 (acetamide), and R[single bond]C[triple bond]N (nitriles) are formed. In addition, the organic materials remaining after photolyzed ice analogs have been warmed to room temperature contain (in rough order of decreasing abundance), (1) hexamethylenetetramine (HMT, C6H12N4), (2) ethers, alcohols, and compounds related to PolyOxyMethylene (POM, ([single bond]CH2O[single bond](sub n)), and (3) ketones (R[single bond]C([double bond]O)[single bond]R') and amides (H2NC([double bond]O)[single bond]R). Most of the carbon in these residues is thought to come from the methanol in the original ice. Deuterium and C-13 isotopic labeling demonstrates that methanol is definitely the source of carbon in HMT. High concentrations of HMT in interstellar and cometary ices could have important astrophysical consequences. The ultraviolet photolysis of HMT frozen in H2O ice readily produces the 'XCN' band observed in the spectra of protostellar objects and laboratory ices, as well as other nitriles. Thus, HMT may be a precursor of XCN and a source of CN in comets and the interstellar medium. Also, HMT is known to hydrolyze under acidic conditions to yield ammonia, formaldehyde, and amino acids. Thus, HMT may be a significant source of prebiogenic compounds on asteroidal parent bodies. A potential mechanism for the radiative formation of HMT in cosmic ices is outlined.

Bernstein, Max P.↗

Fundamental flame velocities of pure hydrocarbons II : alkadienes

Data are presented for the fundamental flame velocities of 10 pure alkadienes that have isolated, conjugated, or cumulative double-bond systems. On the basis of this limited amount of data and the flame velocities previously reported, it is concluded that unsaturation changes the flame velocity in the order alkanes ? alkenes ? alkadienes with isolated double bonds ?= alkadienes with conjugated double bonds ? alkadienes with cumulative double bonds ?= alkynes. There were no significant differences in the flame velocities of cis and trans 1,3-pentadiene. The alkadienes 1,2-pentadiene and 2,3-pentadiene, with different positions of the cumulative double bond in the straight chain, have similar flame velocities. Methyl substitution in a hydrocarbon reduces the flame velocity; the extent of the reduction increases with the degree of unsaturation of the hydrocarbon.

Levine, Oscar↗

Thermal Rearrangements of Polybutadienes with Different Vinyl Contents

A study was made of the loss of double bonds in equibinary (1,4-1,2) polybutadiene (EB) and in polybutadienes with 30% 1,2, 70% 1,4 (FI), and 10% 1,2, 90% 1,4 (DI) double-bond content, when heated in vacuum under nonpyrolitic conditions (temperature range 220-280 C). These polymers were found to undergo second-order loss of 1,2 unsaturation with similar activation energies (E(sub a) = 34.0 +/- 3 kcal/mole), by analogy to the previously reported thermally induced loss of double bonds in 1,2-polybutadiene (VB) (E(sub a) = 33.6 +/- 3 kcal/mole). Moreover, EB and Fl exhibited also second-order loss of 1,4 unsaturation, with E(sub a) ca. 36 and 40 kcal/mole, respectively, while DI showed negligible loss of 1,4 unsaturation below 260 C, in common with cis-1,4-polybutadiene (CB) (with 2% 1,2 double bonds) examined earlier. The loss of 1,2 double bonds in the various polybutadienes with different vinyl contents is accompanied by substantial methyl production, ranging from about one methyl group formed for every 4-5 vinyl units lost in VB, to one methyl for every two vinyls lost in EB,and to almost one methyl for each vinyl lost in DI or CB. Mechanisms are proposed for the thermally induced loss of 1,2 and 1,4 unsaturation in various polybutadienes and for the accompanying methyl production.

Golub, Morton A.↗

Adhesive-bonded double-lap joints

Explicit analytical solutions are derived for the static load carrying capacity of double-lap adhesive-bonded joints. The analyses extend the elastic solution Volkersen and cover adhesive plasticity, adherend stiffness imbalance and thermal mismatch between the adherends. Both elastic-plastic and bi-elastic adhesive representations lead to the explicit result that the influence of the adhesive on the maximum potential bond strength is defined uniquely by the strain energy in shear per unit area of bond. Failures induced by peel stresses at the ends of the joint are examined. This failure mode is particularly important for composite adherends. The explicit solutions are sufficiently simple to be used for design purposes

Hart-Smith, L. J.↗

Thermal rearrangements of unsaturated polymers

Thermal anaerobic uncatalyzed cyclizations and cis-trans isomerizations observed in unsaturated hydrocarbon polymers are surveyed. Three main types of cyclizations are described. Type I is a radical reaction which is caused by chain rupture and gives rise to six-membered rings; this reaction occurs during pyrolysis of polymers with double bonds in a 1,5- or 1,6-diene configuration. Type II is a (2 + 2) thermal cycloaddition of double bonds in certain polymers with a 1,6-diene structure; bicycloheptane structures result. Type III is an intramolecular ene reaction. Many polymers containing a double bond linking CH units display thermal cis-trans isomerization. The common activation energy is approximately 130 kJ/mol, and the initial rate constants are lower, for homologous polymers, the greater the separation of the carbon-carbon double bonds.

Golub, M. A.↗

High-temperature resins

The basic chemistry, cure processes, properties, and applications of high temperature resins known as polyimides are surveyed. Condensation aromatic polymides are prepared by reacting aromatic diamines with aromatic dianhydrides, aromatic tetracarboxylic acids, or with dialkyl esters of aromatic tetracarboxylic acids, depending on the intended end use. The first is for coatings or films while the latter two are more suitable for polyimide matrix resins. Prepreg solutions are made by dissolving reactants in an aprotic solvent, and advances in the addition of a diamine on the double bond and radical polymerization of the double bond are noted to have yielded a final cure product with void-free characteristics. Attention is given to properties of the Skybond, Pyralin, and NR-150B polyimide prepreg materials and characteristics of aging in the NP-150 polyimides. Finally, features of the NASA-developed PMR polyimides are reviewed.

Serafini, T. T.↗

Carotenoid diagenesis in a marine sediment

The major carotenoids at three levels (3, 40, and 175 m below the sediment-water interface) in a core from a marine sediment (Cariaco Trench, off Venezuela) have been examined. Mass and electronic spectral data have provided evidence for the onset of a progressive reduction of carotenoids in the geological column. The time scale of the process appears to depend on the particular carotenoid. Reduction of up to two double bonds is observed for the diol, zeaxanthin, in the oldest sediment (about 340,000 years old) but no reduction is observed in the younger samples (about 5000 and 56,000 years old). The diketone, canthaxanthin, shows evidence of reduction of up to two double bonds in the 56,000-yr sample and up to five double bonds in the oldest sample. No reduction of beta-carotene was observed in any of the samples.

Watts, C. D.↗

Tough, high performance, addition-type thermoplastic polymers

A tough, high performance polyimide is provided by reacting a triple bond conjugated with an aromatic ring in a bisethynyl compound with the active double bond in a compound containing a double bond activated toward the formation of a Diels-Adler type adduct, especially a bismaleimide, a biscitraconimide, or a benzoquinone, or mixtures thereof. Addition curing of this product produces a high linear polymeric structure and heat treating the highly linear polymeric structure produces a thermally stable aromatic addition-type thermoplastic polyimide, which finds utility in the preparation of molding compounds, adhesive compositions, and polymer matrix composites.

Pater, Ruth H.↗

Singlet oxygenation of 1,2-poly/1,4-hexadiene/s

The microstructural changes that occur in cis and trans forms of 1,2-poly(1,4-hexadiene) during methylene blue-photosensitized oxidation were examined by infrared and (C-13)-NMR spectroscopy. The singlet oxygenation of these polymers yielded the expected allylic hydroperoxides accompanied by double bond shifts to new vinyl and trans-vinylene double bonds. The photosensitized oxidation exhibited zero-order kinetics; the relative rates for the cis- and trans-1,2-poly(1,4-hexadiene)s were approximately 3.8:1.0.

Golub, M. A.↗

Decrease in the etch rate of polymers in the oxygen afterglow with increasing gas flow rate

This paper reports the variation of the etch rate of polymers in the afterglow of a radio frequency discharge in oxygen as a function of total flow rate in the range 2-10 cu cm (STP)/min. The measurements were made at ambient temperature with the O(P-3) concentration held essentially constant. Results are reported on three polymers: cis-polybutadiene, a polybutadiene with 33 percent 1,2 double bonds, and a polybutadiene with 40 percent 1,2 double bonds. It has been observed that the etch rate of these polymers decreases significantly with increasing flow rate, strongly suggesting that the vapor-phase products of polymer degradation contribute to the degradation process.

Lerner, N. R.↗

Photochemistry of unsaturated polymers.

The mechanisms of the direct photochemical reactions which occur in unsaturated polymers when irradiated as thin films in vacuo are reviewed. Important reactions in 1,4-polyisoprene and 1,4-polybutadiene are cis-trans isomerization, loss of 1,4-unsaturation, formation of new external double bonds (vinylidene and/or vinyl units) and cyclopropyl formation. In 1,2-polybutadiene and 3,4-polyisoprene, on the other hand, the main reaction is consumption of the external double bonds through cyclization. Recent work on the photoinduced microstructural changes in cis and trans polypentenamers is also discussed.

Golub, M. A.↗

The effect of aromatization on the isotopic compositions of hydrocarbons during early diagenesis

Polycyclic aromatic hydrocarbons with varying degrees of aromatization were isolated from the Eocene Messel Shale (Rheingraben, Germany). The high abundances of these compounds and their structural resemblances to cyclic triterpenoid lipids are consistent with derivation from microbial rather than thermal processes. Compounds structurally related to oleanane contain from five to nine double bonds; those within a series of aromatized hopanoids contain from three to nine. All are products of diagenetic reactions that remove hydrogen or methyl groups, and, in several cases, break carbon-carbon bonds to open rings. Aromatized products are on average depleted in 13C relative to possible precursors by l.2% (range: l.5% enrichment to 4% depletion, n = 9). The dependence of 13C content on the number of double bonds is not, however, statistically significant and it must be concluded that there is no strong evidence for isotopic fractionation accompanying diagenetic aromatization. Isotopic differences between series (structures related to ursane, des-A-ursane, des-A-lupane, des-A-arborane, and possibly, des-A-gammacerane are present) are much greater, indicating that 13C contents are controlled primarily by source effects. Fractionations due to chromatographic isotope effects during HPLC ranged from 0.1 to 2.8%.

NASA Discipline Exobiology↗

Thermal rearrangements in polypentenamer and polyoctenamer

Experiments were conducted to show that polypentenamer and polyoctenamer, in common with 1,4-polybutadiene, undergo anaerobic thermal cis-trans isomerization at temperatures as low as 200 degrees C. Their activation energies for isomerization are comparable to that of polybutadiene. The relative rate constants are found to decrease in the order: polybutadiene, polypentenamer, polyoctenamer. When heated in a vacuum at 200 to 270 degrees C, polypentenamer exhibits a loss of double bonds. This disappearance of unsaturation has no counterpart in polybutadiene or polyoctenamer. In polypentenamer, a mechanism for a thermally-induced ring closure that is different from the one shown for the cyclization-depolymerization of various unsaturated polymers is evident. The cyclization-depolymerization process does cause a loss of double bonds in polybutadiene and polyoctenamer at temperatures greater than or equal to 275 degrees C.

Golub, M. A.↗

Reactions of atomic oxygen /O(3P)/ with polymer films

The reactions of polymer films with oxygen atoms are reviewed focusing on laboratory tests on polybutadienes with different amount of 1,4 or 1,2 double bonds and their polyalkenamer homologues, polyimide (Kapton), and a series of polyolefines with increasing fluorine content. It is found that etch rates increase with decrease in -CH=CH- unsaturation, starting with 1,4 -polybutadiene and reaching the maximum rate with polyethylene or ethylene-propylene rubber. IN polybutadienes with both 1,4 and 1,2 double bonds, the rate of O(3P)-induced etching is lower the higher the 1,2 content. The reactions are confined to the polymer surface.

Golub, Morton A.↗

Activation energies for addition of O/3P/ to simple olefins.

Description of relative rate measurements for the addition of O(3P) to C2H4, C2F4, C3H6, and C4H8-1 in liquid argon at 87.5 K. The data strongly indicate that the activation energies for the addition of O(3P) to the double bonds of propylene and butene-1 are identical, probably to within 0.1 kcal/mole. It is very doubtful that differences in pre-exponential factors or other factors such as solvent effects, could invalidate this conclusion. A similar argument holds for the C2H4 and C2F4 reactions. Furthermore, the experiments suggest that the activation energy for addition of O(3P) to the double bond of butene-1 is about 0.1 kcal/mole.

Demore, W. B.↗

Reactions of Atomic Oxygen (O(3P)) with Polybutadienes and Related Polymers

Thin films of the following polymers were exposed at ambient temperature to ground-state oxygen atoms (O(3P)), generated by a radio-frequency glow discharge in O2: cis- and trans-1,4-polybutadienes (CB and TB), amorphous 1,2-polybutadiene (VB), polybutadienes with different 1,4/1,2 contents, trans polypentenamer (TP), cis and trans polyoctenamers (CO and TO), and ethylene-propylene rubber (EPM). Transmission infrared spectra of CB and TB films revealed extensive surface recession, or etching, unaccompanied by any microstructural changes within the films, demonstrating that the reactions were confined to the surface layers. Contrary to the report by Rabek, Lucki, and Ranby (1979), there was no O(3P)-induced cis-trans isomerization in CB or TB. From weight-loss measurements, etch rates for polybutadienes were found to be markedly dependent on vinyl content, decreasing by two orders of magnitude from CB (2% 1,2) to structures with 30 to 40% 1,2 double bonds, thereafter increasing by half an order of magnitude to VB (97% 1,2). Relative etch rates for EMP and the polyalkenamers were in the order: EMP is greater than CO (or TO) is greater than TP is greater than CB. The sole non-elastomer examined, TB, had an etch rate about six times that of CB, ascribable to a morphology difference. Cis/trans content had a negligible effect on the etch rate of the polyalkenamers. Mechanisms involving crosslinking through units are proposed for the unexpected protection imparted to polybutadienes by the 1,2 double bonds.

Golub, Morton A.↗