Search NASA⌕ Search

SEARCH · Search NASA

Results for “Dow Corning”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Evaluation of newly formulated Dow Corning 321 dry film lubricant

An evaluation of the newly formulated Dow Corning 321 dry film lubricant was performed. The purpose of the evaluation was to compare lubricating characteristics of Dow Corning 321 (STW4-2955, SCN No. 3) to those of Molykote 321R (STW4-2955). Ten igniter bolts were installed and torqued on test plates using the old formulation thread lubricant (Molykote 321R), and 10 bolts were installed using the new formulation (Dow Corning 321). After bolt removal, no signs of galling were found on any of the bolts or test plates threaded holes. Average torque-load values for each formulation were very close. Test results showed there are no significant differences in lubrication abilities between Molykote 321R and Dow Corning 321. It is recommended that, once current supplies of Molykote 321R are depleted, Dow Corning 321 dry film lubricant be used in place of Molykote 321R as a thread lubricant on redesigned solid rocket motor assemblies.

Cook, M.↗

Advances in the Dow Corning process for solar-grade silicon

The Dow Corning process consists of the carbothermic reduction of silica to produce silicon that is then purified by unidirectional solidification. The process has produced silicon of semiconductor quality with respect to all elements except boron and phosphorus at about 10 ppma and aluminum at 0.1 ppma. Solar cells produced from this silicon gave AM0 conversion efficiencies of 11%. A process cost analysis is presented.

Hunt, L. P.↗

Progress on the Dow Corning process for solar-grade silicon

The Dow Corning approach to increasing the resistivity of solar-grade silicon from about 0.04 ohm-cm (40 ppma B) to greater than 0.1 ohm-cm (10 ppma B) involves the use of high-purity raw materials carbothermically reduced in a specially designed electric arc furnace. Final purification occurs during Czochralski crystal growth of a polycrystalline ingot. This small-scale purification technology has resulted in silicon that has been fabricated into solar cells with a maximum AM1 conversion efficiency of 13.4%.

Hunt, L. P.↗

Gamma Radiation Aging Study of a Dow Corning SE 1700 Porous Structure Made by Direct Ink Writing

Dow Corning SE 1700 (reinforced polydimethylsiloxane) porous structures were made by direct ink writing (DIW). The specimens (~50% porosity) were subjected to a compressive strain of ~25% while exposed to a gamma radiation dose of 1, 5, or 10 Mrad under vacuum. Compression set and load retention of the aged specimens were measured after a ~24 h relaxation period. Compression set (relative to deflection) increased with radiation dose: 11, 35, and 51% after 1, 5, and 10 Mrad, respectively. Load retention was 96-97% for the doses tested. The SE 1700 compared favorably to M9763 cellular silicone tested under the same conditions.

36 MATERIALS SCIENCE↗

Load Deflection of Dow Corning SE 1700 Simple Cubic Direct Ink Write Materials: Effect of Thickness and Filament Spacing

Dow Corning SE 1700 (reinforced polydimethylsiloxane) porous structures were made by direct ink writing (DIW) in a simple cubic (SC) configuration. The filament diameter was 250 μm. Structures consisting of 4, 8, or 12 layers were fabricated with center-to-center filament spacing (“road width” (RW)) of 475, 500, 525, 550, or 575 μm. Three compressive load-unload cycles to 2000 kPa were performed on four separate areas of each sample; three samples of each thickness and filament spacing were tested. Geometry-dependent buckling of the SC structure was evident. At a given strain during the third loading phase, stress varied inversely with porosity. At strains of 25% and higher, the stress varied inversely with the number of layers (i.e., thickness); however, the relationship between stress and number of layers was more complex at lower strains. Intra-and inter-sample variability of the load deflection response was higher for thinner and less porous structures.

36 MATERIALS SCIENCE↗

Load Deflection of Dow Corning SE 1700 Face Centered Tetragonal Direct Ink Write Materials: Effect of Thickness and Filament Spacing

Dow Corning SE 1700 (reinforced polydimethylsiloxane) porous structures were made by direct ink writing (DIW) in a face centered tetragonal (FCT) configuration. The filament diameter was 250 μm. Structures consisting of 4, 8, or 12 layers were fabricated with center-to-center filament spacing (“road width” (RW)) of 475, 500, 525, 550, or 575 μm. Three compressive load-unload cycles to 2000 kPa were performed on four separate areas of each sample; three samples of each thickness and filament spacing were tested. At a given strain during the third loading phase, stress varied inversely with porosity. At 10% strain, the stress was nearly independent of the number of layers (i.e., thickness). At higher strains (20- 40%), the stress was highest for the 4-layer structure; the 8- and 12-layer structures were nearly equivalent suggesting that the load deflection is independent of number of layers above 8 layers. Intra-and inter-sample variability of the load deflection response was higher for thinner and less porous structures.

36 MATERIALS SCIENCE↗

Thermal Aging Study of a Dow Corning SE 1700 Porous Structure Made by Direct Ink Writing: 1-Year Results and Long-Term Predictions

Dow Corning SE 1700 (reinforced polydimethylsiloxane) porous structures were made by direct ink writing (DIW). The specimens (~50% porosity) were subjected to various compressive strains (15, 30, 45%) and temperatures (room temperature, 35, 50, 70°C) in a nitrogen atmosphere (active purge) for 1 year. Compression set and load retention of the aged specimens were measured periodically during the study. Compression set increased with strain and temperature. After 1 year, specimens aged at room temperature, 35, and 50°C showed ~10% compression set (relative to the applied compressive deflection), while those aged at 70°C showed 20-40%. Due to the increasing compression set, load retention decreased with temperature, ranging from ~90% at room temperature to ~60-80% at 70°C. Long-term compression set and load retention at room temperature were predicted by applying time-temperature superposition (TTS). The predictions show compression set relative to the compressive deflection will be ~10-15% with ~70-90% load retention after 50 years at 15-45% strain, suggesting the material will continue to be mechanically functional. Comparison of the results to previously acquired data for cellular (M97*, M9760, M9763) and RTV (S5370) silicone foams suggests that the SE 1700 DIW porous specimens are on par with, or outperform, the legacy foams.

36 MATERIALS SCIENCE↗

STABILITY OF DOW CORNING Q2-3183A ANTIFOAM IN IRRADIATED HYDROXIDE SOLUTION

Researchers at the Savannah River National Laboratory (SRNL) examined the stability of Dow Corning Q2-3183A antifoam to radiation and aqueous hydroxide solutions. Initial foam control studies with Hanford tank waste showed the antifoam reduced foaming. The antifoam was further tested using simulated Hanford tank waste spiked with antifoam that was heated and irradiated (2.1 x 10{sup 4} rad/h) at conditions (90 C, 3 M NaOH, 8 h) expected in the processing of radioactive waste through the Waste Treatment and Immobilization Plant (WTP) at Hanford. After irradiation, the concentration of the major polymer components polydimethylsiloxane (PDMS) and polypropylene glycol (PPG) in the antifoam was determined by gel permeation chromatography (GPC). No loss of the major polymer components was observed after 24 h and only 15 wt% loss of PDMS was reported after 48 h. The presence of degradation products were not observed by gas chromatography (GC), gas chromatography mass spectrometry (GCMS) or high performance liquid chromatography mass spectrometry (HPLC-MS). G values were calculated from the GPC analysis and tabulated. The findings indicate the antifoam is stable for 24 h after exposure to gamma radiation, heat, and alkaline simulated waste.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Solar silicon via the Dow Corning process

Carbon, as a reductant for quartz, must be made available so as to have suitable reactivity in conjunction with high purity, especially with respect to boron and phosphorus. A detailed experimental plan was developed to do this. Different sources of carbon were selected to be subjected to various purification methods and reactivity-enhancement processes. A developmental scale arc furnace was installed to perform quartz-carbon reactivity testing.

Hunt, L. P.↗

Solar silicon via the Dow Corning process

Technical feasibility for high volume production of solar cell-grade silicon is investigated. The process consists of producing silicon from pure raw materials via the carbothermic reduction of quartz. This silicon was then purified to solar grade by impurity segregation during Czochralski crystal growth. Commercially available raw materials were used to produce 100 kg quantities of silicon during 60 hour periods in a direct arc reactor. This silicon produced single crystalline ingot, during a second Czochralski pull, that was fabricated into solar cells having efficiencies ranging from 8.2 percent to greater than 14 percent. An energy analysis of the entire process indicated a 5 month payback time.

Hunt, L. P.↗

Historical Material Analysis of DC745U Pressure Pads

As part of the Enhance Surveillance mission, it is the goal to provide suitable lifetime assessment of stockpile materials. This report is an accumulation of historical publication on the DC745U material and their findings. It is the intention that the B61 LEP program uses this collection of data to further develop their understanding and potential areas of study. DC745U is a commercially available silicone elastomer consisting of dimethyl, methyl-phenyl, and methyl-vinyl siloxane repeat units. Originally, this material was manufactured by Dow Corning as Silastic® DC745U at their manufacturing facility in Kendallville, IN. Recently, Dow Corning shifted this material to the Xiameter® brand product line. Currently, DC745U is available through Xiameter® or Dow Corning's distributor R. D. Abbott Company. DC745U is cured using 0.5 wt% vinyl-specific peroxide curing agent known as Luperox 101 or Varox DBPH-50. This silicone elastomer is used in numerous parts, including two major components (outer pressure pads and aft cap support) in the W80 and as pressure pads on the B61. DC745U is a proprietary formulation, thus Dow Corning provides limited information on its composition and properties. Based on past experience with Dow Corning, DC745U is at risk of formulation changes without notification to the costumer. A formulation change for DC745U may have a significant impact because the network structure is a key variable in determining material properties. The purpose of this report is to provide an overview of historical DC745U studies and identify gaps that need to be addressed in future work. Some of the previous studies include the following: 1. Spectroscopic characterization of raw gum stock. 2. Spectroscopic, thermal, and mechanical studies on cured DC745U. 3. Nuclear Magnetic Resonance (NMR) and solvent swelling studies on DC745U with different crosslink densities. 4. NMR, solvent swelling, thermal, and mechanical studies on thermally aged DC745U. 5. NMR, solvent swelling, thermal, and mechanical studies on radiolytically aged DC745U. Each area is reviewed and further work is suggested to improve our understanding of DC745U for systems engineering, surveillance, aging assessments, and lifetime assessment.

36 MATERIALS SCIENCE↗

EFFECTS OF ALTERNATE ANTIFOAM AGENTS, NOBLE METALS, MIXING SYSTEMS AND MASS TRANSFER ON GAS HOLDUP AND RELEASE FROM NONNEWTONIAN SLURRIES

Gas holdup tests performed in a small-scale mechanically-agitated mixing system at the Savannah River National Laboratory (SRNL) were reported in 2006. The tests were for a simulant of waste from the Hanford Tank 241-AZ-101 and featured additions of DOW Corning Q2-3183A Antifoam agent. Results indicated that this antifoam agent (AFA) increased gas holdup in the waste simulant by about a factor of four and, counter intuitively, that the holdup increased as the simulant shear strength decreased (apparent viscosity decreased). These results raised questions about how the AFA might affect gas holdup in Hanford Waste Treatment and Immobilization Plant (WTP) vessels mixed by air sparging and pulse-jet mixers (PJMs). And whether the WTP air supply system being designed would have the capacity to handle a demand for increased airflow to operate the sparger-PJM mixing systems should the AFA increase retention of the radiochemically generated flammable gases in the waste by making the gas bubbles smaller and less mobile, or decrease the size of sparger bubbles making them mix less effectively for a given airflow rate. A new testing program was developed to assess the potential effects of adding the DOW Corning Q2-3183A AFA to WTP waste streams by first confirming the results of the work reported in 2006 by Stewart et al. and then determining if the AFA in fact causes such increased gas holdup in a prototypic sparger-PJM mixing system, or if the increased holdup is just a feature of the small-scale agitation system. Other elements of the new program include evaluating effects other variables could have on gas holdup in systems with AFA additions such as catalysis from trace noble metals in the waste, determining mass transfer coefficients for the AZ-101 waste simulant, and determining whether other AFA compositions such as Dow Corning 1520-US could also increase gas holdup in Hanford waste. This new testing program was split into two investigations, prototypic sparger-PJM tests and modeling being conducted at the Pacific Northwest National Laboratory (PNNL), and small-scale agitation tests and evaluations of effects waste and AFA ingredients have on gas retention and mass transfer being conducted at SRNL. Only work conducted at SRNL is reported here. Key results are: (1) The unexpected gas holdup behavior reported in 2006 for a small-scale agitation system is confirmed. The gas holdup data from small-scale and bench-scale impeller-type mixing systems reported herein show very different trends than the behavior exhibited by the prototypic sparger-PJM mixing system tested in the PNNL APEL facility. Results obtained from testing this 1/4-scale prototypic mixing system will be reported by PNNL. The reason for this difference in holdup behavior between the two different mixing systems is not known at this time. Consequently, data from the small mechanical agitation systems should not be extrapolated to prototypic plant conditions. (2) Bench-scale and small-scale tests conducted with Dow Corning 1520-US AFA show it to be a viable replacement to Dow Corning Q2-3183A AFA. This alternative AFA will, however, require significantly higher dosage (concentration) to perform the same antifoam function. (3) Addition of noble metals to the AZ-101 waste simulant does not produce a catalytic gas retention effect with the AFA. The Gas holdup is similar whether or not noble metals are present in the AZ-101 simulant. (4) Mass transfer tests were performed in a large (0.76 m diameter) bubble column filled to 1.3, 3.4, and 7.4 m elevations with water and the AZ-101 waste simulant. Mass transfer coefficients for air bubbles emanating from a prototypic 0.051 m diameter sparger were obtained from the transient decay of dissolved oxygen concentration in the initially saturated fluids. Adding AFA to water reduces the mass transfer coefficient slightly. AFA addition reduces the mass transfer coefficient for AZ-101 simulant more than it does for water because the shear strength of the simulant allows for larger bubble sizes, and larger bubbles have smaller surface area for mass transfer than small bubbles for the same void volume.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

PARAMETRIC EFFECTS OF ANTI-FOAM COMPOSITION, SIMULANT PROPERTIES AND NOBLE METALS ON THE GAS HOLDUP AND RELEASE OF A NON-NEWTONIAN WASTE SLURRY SIMULANT

Gas holdup tests were performed in bench-scale and small-scale mechanically-agitated mixing systems at the Savannah River National Laboratory (SRNL) for a simulant of waste from the Hanford Tank 241-AZ-101. These featured additions of DOW Corning Q2-3183A anti-foam agent. Results indicated that this anti-foam agent (AFA) increased gas holdup in the waste simulant by about a factor of four and, counter-intuitively, that the holdup increased as the non-newtonian simulant shear strength decreased (apparent viscosity decreased). Such results raised the potential of increased flammable gas retention in Hanford Waste Treatment and Immobilization Plant (WTP) vessels mixed by air sparging and pulse-jet mixers (PJMs) during a Design Basis Event (DBE). Additional testing was performed to determine the effects of simulant properties, composition of alternate AFAs, and presence of trace noble metals. Key results are that: (1) Increased gas holdup resulting from addition of Q2-3183A is due to a decrease in surface tension that supports small bubbles which have low rise velocities. (2) Dow Corning 1520-US AFA shows it to be a viable replacement to Dow Corning Q2-3183A AFA. This alternative AFA, however, requires significantly higher dosage for the same anti-foam function. (3) Addition of noble metals to the AZ-101 waste simulant does not produce a catalytic gas retention effect with the AFA.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Elastomers that Endure

Through assistance from NASA's Kennedy Space Center, Dow Corning developed a strong, heat-protecting coating with applications in a variety of fields. Previously, NASA used silicate coatings that simply failed to adequately protect, which resulted in the frequent recoating of the damaged areas. The enormous expense of this repeat procedure led Kennedy's Materials Science Laboratory to investigate the possibilities of ablative-type coatings. The investigations resulted in the creation of a silicone ablative material known as the Dow Corning 3-6376 Fast Cure Elastomer. The new product, which does not require a primer coating, is a 100 percent silicone material. It is currently used in the automotive and aerospace industries and serves as an exceptional coating for engine compartment firewalls. Dow Corning's Fast Cure Elastomer has also proved to be an effective sealant. Moreover, it reduces the turnaround time for reuse of the launch structure because of fewer refurbishing operations. This means that NASA is not held up due to repairs when it comes time to launch another Shuttle. To date, the Agency has launched dozens of successful missions without the need for recoating.

Source record↗

Effect of an oxygen plasma on the physical and chemical properties of several fluids for the liquid droplet radiator

The Liquid Droplet Radiator is one of several radiator systems currently under investigation by NASA Lewis Research Center. It involves the direct exposure of the radiator working fluid to the space environment. An area of concern is the potential harmful effects of the low-Earth-orbit atomic oxygen environment on the radiator working fluid. To address this issue, seven candidate fluids were exposed to an oxygen plasma environment in a laboratory plasma asher. The fluids studied included Dow Corning 705 Diffusion Pump Fluid, polymethylphenylsiloxane and polydimethlsiloxane, both of which are experimental fluids made by Dow Corning, Fomblin Z25, made by Montedison, and three fluids from the Krytox family of fluids, Krytox 143AB, 1502, and 16256, which are made by DuPont. The fluids were characterized by noting changes in visual appearance, physical state, mass, and infrared spectra. Of the fluids tested, the Fomblin and the three Krytoxes were the least affected by the oxygen plasma. The only effect noted was a change in mass, which was most likely due to an oxygen-catalyzed deploymerization of the fluid molecule.

Gulino, D. A.↗

Effect of an oxygen plasma on the physical and chemical properties of several fluids for the Liquid Droplet Radiator

The Liquid Droplet Radiator is one of several radiator systems currently under investigation by NASA Lewis Research Center. It involves the direct exposure of the radiator working fluid to the space environment. An area of concern is the potential harmful effects of the low-Earth-orbit atomic oxygen environment on the radiator working fluid. To address this issue, seven candidate fluids were exposed to an oxygen plasma environment in a laboratory plasma asher. The fluids studied included Dow Corning 705 Diffusion Pump Fluid, polymethylphenylsiloxane and polydimethylsiloxane, both of which are experimental fluids made by Dow Corning, Fomblin Z25, made by Montedison, and three fluids from the Krytox family of fluids, Krytox 143AB, 1502, and 16256, which are made by DuPont. The fluids were characterized by noting changes in visual appearance, physical state, mass, and infrared spectra. Of the fluids tested, the Fomblin and the three Krytoxes were the least affected by the oxygen plasma. The only effect noted was a change in mass, which was most likely due to an oxygen-catalyzed depolymerization of the fluid molecule.

Gulino, Daniel A.↗

Post-Cure Studies on Solid Silicone Elastomer: DC745U

DC745U is a silicone elastomer originally manufactured by Dow Corning under the name of Silastic® DC745U at their manufacturing facility in Kendaville, Indiana. Currently DC745U is available through Xiameter® or Dow Corning’s distributor R. D. Abbott Company. This silicone elastomer is used in numerous parts of weapon systems, including outer pressure pads, aft cap support in W80 and pressure pad in the B61. DC745U is a proprietary formulation and limited information about its composition and properties is provided to the customer. Thus, Los Alamos National Laboratory and Lawrence Livermore National Laboratory have performed a variety of characterization experiments on this material.

36 MATERIALS SCIENCE↗

Wabash River Integrated Methanol and Power Production from Clean Coal Technologies (IMPPCCT)

The Wabash River Integrated Methanol and Power Production from Clean Coal Technologies (IMPPCCT) project was established to evaluate integrated electrical power generation and methanol production through clean coal technologies. The project was under the leadership of ConocoPhillips Company (COP), after it acquired Gasification Engineering Corporation (GEC) and the E-Gas gasification technology from Global Energy Inc. in July 2003. The project has completed both Phase 1 and Phase 2 of development. The two project phases include the following: (1) Feasibility study and conceptual design for an integrated demonstration facility at SG Solutions LLC (SGS), previously the Wabash River Energy Limited, Gasification Facility located in West Terre Haute, Indiana, and for a fence-line commercial embodiment plant (CEP) operated at the Dow Chemical Company or Dow Corning Corporation chemical plant locations. (2) Research, development, and testing (RD&T) to define any technology gaps or critical design and integration issues. Phase 1 of this project was supported by a multi-industry team consisting of Air Products and Chemicals, Inc., The Dow Chemical Company, Dow Corning Corporation, Methanex Corporation, and Siemens Westinghouse Power Corporation, while Phase 2 was supported by Gas Technology Institute, TDA Research Inc., and Nucon International, Inc. The SGS integrated gasification combined cycle (IGCC) facility was designed, constructed, and operated under a project selected and co-funded under the Round IV of the United States Department of Energy's (DOE's) Clean Coal Technology Program. In this project, coal and/or other carbonaceous fuel feedstocks are gasified in an oxygen-blown, entrained-flow gasifier with continuous slag removal and a dry particulate removal system. The resulting product synthesis gas (syngas) is used to fuel a combustion turbine generator whose exhaust is integrated with a heat recovery steam generator to drive a refurbished steam turbine generator. The gasifier uses technology initially developed by The Dow Chemical Company (the Destec Gasification Process), and now acquired and offered commercially by COP as the E-Gas technology. In a joint effort with the DOE, a Cooperative Agreement was awarded under the Early Entrance Coproduction Plant (EECP) solicitation. GEC, and later COP and the industrial partners investigated the use of syngas produced by the E-Gas technology in a coproduction environment to enhance the efficiency and productivity of solid fuel gasification combined cycle power plants. The objectives of this effort were to determine the feasibility of an EECP located at a specific site which produces some combination of electric power (or heat), fuels, and/or chemicals from syngas derived from coal, or, coal in combination with some other carbonaceous feedstock. The intended result of the project was to provide the necessary technical, economic, and environmental information that would be needed to move the EECP forward to detailed design, construction, and operation by industry. The EECP study conducted in Phase 1 of the IMPPCCT Project confirmed that the concept for the integration of gasification-based (E-Gas) electricity generation from coal and/or petroleum coke and methanol production (Liquid Phase Methanol or LPMEOH{trademark}) processes was feasible for the coproduction of power and chemicals. The results indicated that while there were minimal integration issues that impact the deployment of an IMPPCCT CEP, the major concern was the removal of sulfur and other trace contaminants, which are known methanol catalyst poisons, from the syngas. However, economic concerns in the domestic methanol market which is driven by periodic low natural gas prices and cheap offshore supplies limit the commercial viability of this more capital intensive concept. The objective of Phase 2 was to conduct RD&T as outlined in the Phase 1 RD&T Plan to enhance the development and commercial acceptance of coproduction technology. Studies were designed to address the technical concerns that would make the IMPPCCT concept competitive with natural gas-based systems in the commercial marketplace. Efforts in Phase 2 investigated the cleanup of the syngas by removing contaminants, particularly sulfur species, to a level acceptable for the methanol synthesis catalyst, and reducing the cost of the current sulfur removal system such as via warm gas cleanup methods. Laboratory testing followed by on-site field testing at SGS with bench-scale slipstream units was conducted. Actual syngas produced by the facility was evaluated at system pressure and temperature.

01 COAL, LIGNITE, AND PEAT↗