Search NASA⌕ Search

SEARCH · Search NASA

Results for “FILLER METALS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

AN INITIAL ASSESSMENT OF THE CREEP-RUPTURE STRENGTHS FOR WELDMENTS WITH ALLOY 800H BASE METAL AND ALLOY 617 FILLER METAL

In Section III, Division 5 of the American Society of Mechanical Engineers Boiler and Pressure Vessel Code, Alloy 800H is qualified for elevated-temperature nuclear construction for temperatures up to 760°C (1,400°F) and a maximum service life of 300,000 hours. There are two permissible filler metals for Alloy 800H weldments specified in Division 5: ENiCrFe-2 (Alloy A) and ERNiCr-3 (Alloy 82). Low creep-rupture strengths of these weldments at the upper limits of the qualified temperatures and service lives may restrict the design envelope for elevated-temperature nuclear construction with Alloy 800H. As a result, an alternative filler metal is desired to improve the creep-rupture strengths of Alloy 800H weldments for the qualified temperatures and service lives. This work investigates an overmatched filler metal. Specifically, a weldment with Alloy 800H base metal and Alloy 617 filler metal fabricated by semiautomated gas tungsten arc welding is investigated. A scoping creep-rupture test program was conducted of cross-weld specimens at temperatures ranging from 750 to 1,000°C (1,292 to 1,832°F). Preliminary results on the creep-rupture strengths of the Alloy 800H weldment with Alloy 617 filler metal do not show significant improvement compared to the filler metals currently qualified in Division 5 for Alloy 800H weldments. Consequently, work is in progress to investigate a matching filler metal.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstructure and Mechanical Properties of Stainless Steel/Brass Joints Brazed by Sn-Electroplated Ag Brazing Filler Metals

To develop a high-Sn-content AgCuZnSn brazing filler metal, the BAg50CuZn was used as the base filler metal and a Sn layer was electroplated upon it. Then, the 304 stainless steel and the H62 brass were induction-brazed with the Sn-plated brazing filler metals. The microstructures of the joints were examined with an optical microscope, a scanning electron microscope and an x-ray diffractometer. The corresponding mechanical properties were obtained with a universal tensile testing machine. The results indicated that the induction brazed joints consisted of the Ag phase, the Cu phase and the CuZn phase. When the content of Sn in the Sn-plated Ag brazing filler metal was 6.0 or 7.2 wt.%, the Cu{sub 5}Zn{sub 8}, the Cu{sub 41}Sn{sub 11} and the Ag{sub 3}Sn phases appeared in the brazed joint. The tensile strength of the joints brazed with the Sn-plated filler metal was higher compared to the joints with the base filler metal. When the content of Sn was 6.0 wt.%, the highest tensile strength of the joint reached to 395 MPa. The joint fractures presented a brittle mode, mixed with a low amount of ductile fracture, when the content of Sn exceeded 6.0 wt.%.

36 MATERIALS SCIENCE↗

Interfacial structure and properties of Cu/Al joints brazed with Zn-Al filler metals

Highlights: • The formation mechanism of Cu side interfacial compounds of Cu/Al joints with Zn-Al filler metals are revealed accurately. • The Cu side interfacial structure is uncertain and dependent on brazing parameters, especially cooling rate after brazing. • The close relation among composition, brazing parameters, interfacial structure and mechanical properties is discovered. - Abstract: Seeing that opinions vary, no unanimous conclusion has been drawn on Cu side interfacial structure and its relationship with the mechanical properties of Cu/Al joints brazed with Zn-Al filler metals, XRD, SEM and HAADF-STEM were used to accurately reveal the Cu side interfacial structure and the mechanism concerned. The relationship among the brazing process, interfacial structure and mechanical properties of the joints was systematically studied. The following phenomena and principles were newly found and clarified. The Cu side interfacial structure are uncertain and dependent on brazing parameters, especially cooling rate after brazing, in addition to the composition of Zn-Al filler metal. High cooling rate promotes the formation of CuZn and Al{sub 4.2}Cu{sub 3.2}Zn{sub 0.7} compounds, while slow cooling rate is beneficial for the formation of Cu-Al interfacial compounds at the Cu side interface. Increasing brazing temperature or lengthening holding time enhances the dissolution of base metals, which results in the increase of Al and Cu contents at the Cu side interface, thus promoting the formation of CuAl{sub 2} compound. Besides, increasing Al content in Zn-Al filler metal also promotes the formation of CuAl{sub 2} compound by directly increasing Al content at the Cu side interface. The significant differences in joint strength are caused by the differences of Cu side interfacial compounds essentially. When the thin CuZn and Al{sub 4.2}Cu{sub 3.2}Zn{sub 0.7} layers exist at the Cu side interface, the brazed joint possesses high shear strength. On the contrary, the formation of Cu-Al compound layers at the Cu side interface, especially CuAl{sub 2}, will severely degrade the joint strength.

36 MATERIALS SCIENCE↗

Assessment of UTP A 2133 Mn as a Matching Filler Metal for Alloy 800H in Section III, Division 5 Applications

Six alloys are qualified in the American Society of Mechanical Engineers (ASME) Boiler and Pressure Vessel Code (BPVC) for elevated-temperature nuclear components. Due to reactor design alloy restrictions and motivation to improve operational efficiency and plant lifetimes, it is necessary to maximize the usefulness of qualified alloys. One of these alloys is Alloy 800H, which is qualified for a maximum temperature of 760°C and a maximum 300,000-hour service life. However, the welding filler metals qualified to join Alloy 800H have stress rupture factors that reduce the allowable weldment strength by factors as low as 0.59 times the Alloy 800H base metal. In an effort to improve the weldment creep-rupture performance, or to increase the stress reduction factor, non-code qualified filler metals are under investigation by the Department of Energy?s Advanced Reactor Technologies program. For this investigation, UTP A 2133 Mn filler metal (Fe-Cr-Ni-Mn-Nb) was used to join 0.5 in. thick Alloy 800H plate to demonstrate passing an ASME BPVC Section IX weld qualification. The multi-pass, pulsed GTAW process showed successful weld qualification results, and additional property measurements were conducted to compare previous analyses of Alloy 82 and Alloy 617 filler metals. Future work will evaluate the cross-weld creep-rupture performance of the UTP A 2133 Mn in comparison to Alloy 82 and Alloy 617 filler metals.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstructure evolution of Al/Mg butt joints welded by gas tungsten arc with Zn filler metal

Based on the idea of alloying welding seam, Gas tungsten arc welding method with pure Zn filler metal was chosen to join Mg alloy and Al alloy. The microstructures, phases, element distribution and fracture morphology of welding seams were examined. The results indicate that there was a transitional zone in the width of 80-100 {mu}m between the Mg alloy substrate and fusion zone. The fusion zone was mainly composed of MgZn{sub 2}, Zn-based solid solution and Al-based solid solution. The welding seam presented distinct morphology in different location owning to the quite high cooling rate of the molten pool. The addition of Zn metal could prevent the formation of Mg-Al intermetallics and form the alloyed welding seam during welding. Therefore, the tensile strengths of joints have been significantly improved compared with those of gas tungsten arc welded joints without Zn metal added. Highlights: Black-Right-Pointing-Pointer Mg alloy AZ31B and Al alloy 6061 are welded successfully. Black-Right-Pointing-Pointer Zinc wire is employed as a filler metal to form the alloyed welding seam. Black-Right-Pointing-Pointer An alloyed welding seam is benefit for improving of the joint tensile strength.

36 MATERIALS SCIENCE↗

Interfacial diffusion reactions and mechanical properties of Ti3Al/Ni-based superalloy joints brazed with AgCuPd filler metal

Highlights: • Ti{sub 3}Al alloy to Ni-based superalloy was successfully brazed using Ag-21Cu-25Pd filler metal. • Phases TiPd (fcc), Ti{sub 3}Pd{sub 5} (bct) and AlPd (hcp) formed within the Ti{sub 3}Al/Ni-based superalloy joint. • Diffusion behavior of elements and its influence on joint interfacial microstructure were revealed. • A formation model of interfacial microstructure has been established. • The joint tensile strength at room temperature reached 404MPa, and the strength of 212MPa was maintained at 773 K. - Abstract: Dissimilar joining of a Ti{sub 3}Al-based alloy to a Ni-based superalloy has been conducted using Ag-21Cu-25Pd filler metal. The joint microstructures were analyzed using SEM, EPMA, XRD and TEM. The reaction behaviors between different elements were discussed. Due to the strong affinity, element Pd mainly reacted with Ti{sub 3}Al substrate and formed intermetallic compounds of TiPd, Ti{sub 3}Pd{sub 5} and AlPd. Elements Ni and Ti reacted with each other and caused the formation of Ni{sub 3}Ti in the centre of the joint. Owing to the diffusion effect, element Ag was enriched in the joint central area as (Ag,Cu){sub ss}. With the prolonging of the brazing time varying from 3 min to 15 min at 1253 K, the tensile strength of the joint firstly increased and then decreased. The joints brazed at 1253 K for 10 min presented the maximum strength of 404 MPa at room temperature, and the joint strength of 212 MPa was maintained at 773 K. The total fracture surface covered the most of the reaction zones from the (Ag,Cu){sub ss} to the diffusion effect zone at the Ti{sub 3}Al side.

36 MATERIALS SCIENCE↗

Understanding the reliability of solder joints used in advanced structural and electronics applications: Part 1 - Filler metal properties and the soldering process

Soldering technology has made tremendous strides in the past half-century. Whether structural or electronic, all solder joints must provide a level of reliability that is required by the application. This Part 1 report examines the effects of filler metal properties and soldering process on joint reliability. Solder alloy composition must have the appropriate melting and mechanical properties that suit the product's assembly process(es) and use environment. The filler metal must also optimize solderability (wetting-and-spreading) to realize the proper joint geometry. Here, the soldering process also affects joint reliability. The choice of flux and thermal profile support the solderability performance of the molten filler metal to successfully fill the gap and complete the fillet.

36 MATERIALS SCIENCE↗

Method for eliminating runout of braze filler metal during active brazing

Nanometers thick conformal coatings deposited by atomic-layer deposition (ALD) onto the metal surface of an active braze joint modifies the surface chemistry to eliminate excess braze filler metal flow. Unlike other means used to prevent braze filler metal runout, the thin ALD coating does not hinder next assembly processes, does not require post-braze cleaning, and does not alter the base material mechanical properties.

Goeke, Ronald S.↗

Characterization of Mg/Al butt joints welded by gas tungsten arc filling with Zn–29.5Al–0.5Ti filler metal

The multivariate alloying design of a welding joint is used in the Mg to Al welding process. A Zn–29.5Al–0.5Ti alloy is added as filler metal in gas tungsten arc welding of Mg and Al alloy joint based on the analysis of Al and Mg alloy characteristics. The tensile strength, microstructure, and phase constitution of the weld seam are analyzed. The formation of brittle and hard Mg–Al intermetallic compounds is avoided because of the effects of Zn, Al, and Ti. The average tensile strength of the joint is 148 MPa. Al{sub 3}Ti is first precipitated and functions as the nucleus of heterogeneous nucleation during solidification. Moreover, the precipitated Al–MgZn{sub 2} hypoeutectic phase exhibited a feather-like structure, which enhances the property of the Mg–Al dissimilar joint. - Highlights: • Mg alloy AZ31B and Al alloy 6061 are butt welded by fusion welding. • The effect of Ti in filler metal is investigated. • The formation of Mg–Al intermetallic compounds is avoided.

36 MATERIALS SCIENCE↗

The Effect of Surface Condition on Wetting of HASTELLOY{sup ®} X by Brazing Filler Metal of Ni-Pd-Cr-B-Si System

The paper presents the results of wettability tests by a sessile drop method coupled with residual gas analysis for the HASTELLOY{sup ®} X substrates contact heated with brazing filler metal of Palnicro 36M. The contact angles formed between the substrate and the molten brazing filler metal were recorded by high-speed high-resolution CCD camera using two different heating procedures: (1) fast continuous heating to a temperature of 960 °C; (2) isothermal heating at a temperature of 995 °C for 10 min after step heating to the test temperature. In this study, the reference sample was HASTELLOY{sup ®} X in a delivery state (D1). The base material with a different surface finish was also tested: after polishing (P1), after polishing and oxidation at a temperature of 600 °C for 1 h in the air (U1). The tests confirmed very good wetting properties of Palnicro 36M on HASTELLOY{sup ®} X, independently on its surface finish and the heating procedure used in this study, i.e., after 10 min at 995 °C, the final contact angle values were θ{sub f} = 7.6 ± 0.1°, 6.03 ± 0.07° and 6.2 ± 1.0° for D1, P1 and U1, respectively. However, oxidation of HASTELLOY{sup ®} X surface affects the wetting kinetics and spreading of molten Palnicro 36M on BM substrates by: (1) increasing the initial contact angle values (θ{sub 0} = 51 ± 4°, 65 ± 13° and 83 ± 2° for D1, P1 and U1, respectively), (2) delaying the wetting process and (3) reducing the spreading area since after wettability tests at 960 °C, the largest area covered with solidified Palnicro 36M drop was noted for D1 (92 mm{sup 2}) while the smallest one for U1 (52 mm{sup 2}).

36 MATERIALS SCIENCE↗

High Temperature Strength of YSZ Joints Brazed with Palladium Silver Copper Oxide Filler Metals

The Ag-CuOx system is being investigated as potential filler metals for use in air brazing high-temperature electrochemical devices such as solid oxide fuel cells and gas concentrators. The current study examines the effects of palladium addition on the high temperature joint strength of specimens prepared from yttria stabilized zirconia (YSZ) bars brazed with the binary Ag-CuOx, and 15Pd-Ag-CuO. It was found that while the binary Ag-CuOx system exhibits stronger room temperature strength than the 15Pd system the strength is reduced to values equivalent of the 15Pd system at 800°C. The 15Pd system exhibits a lower ambient temperature strength that is retained at 800°C. In both systems the failure mechanism at high temperature appears to be peeling of the noble metal component from the oxide phases and tearing through the noble metal phase whereas sufficient adhesion is retained at lower temperatures to cause fracture of the YSZ substrate.

30 DIRECT ENERGY CONVERSION↗

Effect of filler metal composition on the strength of yttria stabilized zirconia joints brazed with Pd-Ag-CuOx

The Ag-CuOx system is of interest to be used to be used as an air braze filler metal for joining high temperature electrochemical devices. Previous work has shown that the melting temperatures can be increased by adding palladium to Ag-CuOx and it is expected that this may aid high temperature stability. This work compares the room temperature bend strength of joints made between yttria-stabilized zirconia (YSZ) air brazed using Ag-CuOx without palladium and with 5 and 15mol% palladium additions. It has been found that in general palladium decreases joint strength, especially in low copper oxide compositions filler metals. At high copper oxide contents, brittle fracture through both copper oxide rich phases and the YSZ limits joint strength.

36 MATERIALS SCIENCE↗

Effect of a copper filler metal on the microstructure and mechanical properties of electron beam welded titanium-stainless steel joint

Cracking in an electron beam weld of titanium to stainless steel occurred during the cooling process because of internal thermal stress. Using a copper filler metal, a crack free joint was obtained, which had a tensile strength of 310 MPa. To determine the reasons for cracking in the Ti/Fe joint and the function of the copper filler metal on the improvement of the cracking resistance of the Ti/Cu/Fe joint, the microstructures of the joints were studied by optical microscopy, scanning electron microscopy and X-ray diffraction. The cracking susceptibilities of the joints were evaluated with microhardness tests on the cross-sections. In addition, microindentation tests were used to compare the brittleness of the intermetallics in the welds. The results showed that the Ti/Fe joint was characterized by continuously distributed brittle intermetallics such as TiFe and TiFe(Cr){sub 2} with high hardness ({approx} 1200 HV). For the Ti/Cu/Fe joint, most of the weld consisted of a soft solid solution of copper with dispersed TiFe intermetallics. The transition region between the weld and the titanium alloy was made up of a relatively soft Ti-Cu intermetallic layer with a lower hardness ({approx} 500 HV). The formation of soft phases reduced the cracking susceptibility of the joint. - Highlights: Black-Right-Pointing-Pointer Electron beam welded Ti/Fe joint cracked for the brittleness and residual stress. Black-Right-Pointing-Pointer Electron beam welded Ti/Cu/Fe joint with tensile strength of 310 MPa was obtained. Black-Right-Pointing-Pointer Cu diluted Ti and Fe contents in weld and separated the TiFe{sub 2} into individual blocks. Black-Right-Pointing-Pointer Interfacial hard Ti-Fe compounds were replaced by soft Ti-Cu compounds in the weld. Black-Right-Pointing-Pointer A large amount of solid solution of copper formed in the weld.

36 MATERIALS SCIENCE↗

Effect of mechanical milling on Ni-TiH{sub 2} powder alloy filler metal for brazing TiAl intermetallic alloy: The microstructure and joint's properties

A TiH{sub 2}-50 wt.% Ni powder alloy was mechanically milled in an argon gas atmosphere using milling times up to 480 min. A TiAl intermetallic alloy was joined by vacuum furnace brazing using the TiH{sub 2}-50 wt.% Ni powder alloy as the filler metal. The effect of mechanical milling on the microstructure and shear strength of the brazed joints was investigated. The results showed that the grains of TiH{sub 2}-50 wt.% Ni powder alloy were refined and the fusion temperature decreased after milling. A sound brazing seam was obtained when the sample was brazed at 1140 deg. C for 15 min using filler metal powder milled for 120 min. The interfacial zones of the specimens brazed with the milled filler powder were thinner and the shear strength of the joint was increased compared to specimens brazed with non-milled filler powder. A sample brazed at 1180 deg. C for 15 min using TiH{sub 2}-50 wt.% Ni powder alloy milled for 120 min exhibited the highest shear strength at both room and elevated temperatures.

36 MATERIALS SCIENCE↗

Influence of TiH{sub 2} on Interfacial Reaction Features Between Cubic Boron Nitride and Cu-Sn-Ti Active Filler Metals

Cubic boron nitride (CBN) grains are brazed by Cu-Sn-Ti filler metal in vacuum at 1223 K. Wetting behaviors, reaction layer features, and elemental distribution characteristics have been systematically investigated through scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and X-ray diffraction (XRD). The results show that when the TiH{sub 2} content is 5 wt pct, virtually no sharp-edged, partially coated, and uncoated CBN grains can be observed, indicating that adequate wetting could be achieved. Moreover, a continuous reaction layer with uniform thickness (1.30 μm) consisting of TiN, TiB{sub 2}, and TiB is obtained, which indicates that large numbers of TiN, TiB{sub 2}, and TiB compounds could have been formed at the interface. However, when the TiH{sub 2} content exceeds 5 wt pct, the thickness of the reaction layer is no longer significantly expanding and excessive Ti present in the matrix will lower the volume percentage of Cu{sub 3}Sn{sub 1} phase, which will reduce the bonding strength of the brazing samples. Wear tests indicate that the minimum weight loss also occurs at 5 wt pct TiH{sub 2}.

36 MATERIALS SCIENCE↗

Wetting and Brazing of Chromium Film-Deposited Alumina Using AgCu Filler Metal

Wetting behavior of AgCu filler on chromium film-deposited Al{sub 2}O{sub 3} ceramics was studied by sessile drop method under vacuum, and brazing of chromium-deposited alumina using AgCu was carried out. Cr film can improve the wettability of AgCu filler on alumina ceramics, and the contact angle decreased dramatically. However, with further increase in temperature and extension of wetting time, Cr atom might diffuse excessively to molten alloy or substrate leading to thinned or disappeared Cr film on alumina; thus, the contact angle of AgCu on alumina increased. The reliable alumina joint was obtained via chromium deposition using AgCu filler brazed at 900 °C for 10 min, and no hard or brittle intermetallic compounds formed in the brazed joint. The maximum shear strength of 16.8 MPa was achieved when the thickness of deposited chromium film was 2 μm.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Property Improvement in Laser-Welded TC4 Titanium Alloy and 301L Stainless Steel Joints Without Filler Metal

Pulsed laser welding of Ti alloy to stainless steel (SS) has been applied without filler metal. When the laser beam was focused on the Ti alloy–SS interface, large volumes of Ti-Fe intermetallics were formed in the joint. These Ti-Fe intermetallics were highly brittle, causing the joint to crack spontaneously after welding. The brittle coarse Ti-Fe intermetallics seriously deteriorates the joint strength of Ti alloy and SS; therefore, it is necessary to control the quantities and distributions of brittle Ti-Fe intermetallics in the joint. The amount of melted base materials was controlled by changing laser offset to control the melted proportion and thus control the quantity and distribution of brittle Ti-Fe intermetallics in weld. When laser beam was on the SS side, melting amount of Ti alloy in weld was decreased. When laser beam was on the Ti alloy side, melting amount of SS in weld was decreased. When the laser offset was 0.35 mm away from SS side, the sample realizes the effective connection between Ti alloy and SS. A compound layer was formed at the SS side with the main microstructure of β-Ti and TiFe{sub 2}. The joint fractured at the compound layer with the maximum tensile strength of 182 MPa. Microstructures and mechanical properties of joints were improved by changing laser offset.

36 MATERIALS SCIENCE↗