High Curie temperature drive layer materials for ion-implanted magnetic bubble devices

Ion implantation of bubble garnets can lower the Curie temperature by 70 C or more, thus limiting high temperature operation of devices with ion-implanted propagation patterns. Therefore, double-layer materials were made with a conventional 2-micron bubble storage layer capped by an ion-implantable drive layer of high Curie temperature, high magnetostriction material. Contiguous disk test patterns were implanted with varying doses of a typical triple implant. Quality of propagation was judged by quasistatic tests on 8-micron period major and minor loops. Variations of magnetization, uniaxial anisotropy, implant dose, and magnetostriction were investigated to ensure optimum flux matching, good charged wall coupling, and wide operating margins. The most successful drive layer compositions were in the systems (SmDyLuCa)3(FeSi)5O12 and (BiGdTmCa)3(FeSi)5O12 and had Curie temperatures 25-44 C higher than the storage layers.

Fratello, V. J.↗

Earth's core-mantle boundary - Results of experiments at high pressures and temperatures

Laboratory experiments document that liquid iron reacts chemically with silicates at high pressures (above 2.4 x 10 to the 10th Pa) and temperatures. In particular, (Mg,Fe)SiO3 perovskite, the most abundant mineral of earth's lower mantle, is expected to react with liquid iron to produce metallic alloys (FeO and FeSi) and nonmetallic silicates (SiO2 stishovite and MgSiO3 perovskite) at the pressures of the core-mantle boundary, 14 x 10 to the 10th Pa. The experimental observations, in conjunction with seismological data, suggest that the lowermost 200 to 300 km of earth's mantle, the D-double-prime layer, may be an extremely heterogeneous region as a result of chemical reactions between the silicate mantle and the liquid iron alloy of earth's core. The combined thermal-chemical-electrical boundary layer resulting from such reactions offers a plausible explanation for the complex behavior of seismic waves near the core-mantle boundary and could influence earth's magnetic field observed at the surface.

Knittle, Elise↗

The Combined Strength of Thermodynamics and Comparative Planetology: Application of Activity Models to Core Formation in Terrestrial Bodies

Recent models for accretion of terrestrial bodies involve metal-silicate equilibrium as the metallic core formed during growth. Most elements considered are either refractory or well studied elements for which effects of pressure, temperature, oxygen fugacity, and metallic liquid composition are well known. There are a large number of elements that are both siderophile and volatile, whose fate in such models is unknown, largely due to a lack of data at comparable conditions and com-positions (FeNi core with light elements such as S, C, Si, and O). We have focused on Ge, In, As, Sb and determined the effect of Si and C on metal-silicate partitioning, and developed a thermo-dynamic model that allows application of these new data to a wide range of planetary bodies. New experiments: We have previously carried out experiments with FeSi metallic liquid at C-saturated conditions at 1600 and 1800 C [4]. In a new series of experiments we investigate the effect of Si in carbon-free systems at 1600 C for comparison. Experiments were carried out at 1 GPa in MgO capsules using the same basaltic starting composition as in previous studies. The MgO capsule reacts with the silicate melt to form more MgO-rich liquids that have 22-26 wt% MgO. Experimental met-als and silicates were analyzed using a combination of electron microprobe analysis and laser ablation ICP-MS. Results: The new results can be interpreted by considering Ge as an example, in the simple exchange equilibrium Fe + GeO = FeO + Ge, where the equilibrium constant Kd can be examined as a function of Si content of the metal. The slope of lnKd vs. (1-XSi) for this new series allows derivation of the epsilon interaction parameter for each of these four elements and Si (both C-saturated and C-free).All four elements have positive epsilon values, indicating that Si causes a decrease in the partition coefficients; values are 6.6, 6.5, 27.8 and 25.2 for In, Ge, As, and Sb, respectively, at 1 GPa and 1600 C. As an example of how large the effect of Si can be, these epsilon values correspond to activity coefficients (gamma) for As of 0.01 when XSi = 0, and up to gamma = 23 when XSi = 0.2. Combining these new results with previous determinations [5,6] of epsilon parameters for S and C for these elements allows us calculate activity of Ge, In, As, and Sb in Fe-Ni-Si-S-C-O metallic liquids. We apply this new model to sever-al terrestrial bodies such as Earth (Si-rich core), Mars (S-rich core), Moon (S-, C-, and Si-poor core), and Vesta, and examine the resulting core and mantle concentrations of these elements. Mantle concentrations of these four elements are well explained for Earth and Mars in models that call for mid-mantle equilibration between Si-bearing and S-bearing FeNi cores, respectively. Modeling results for the Moon and Vesta will also be presented.

Righter, K.↗

Activity Coefficients of Siderophile Elements in Fe-Si Liquids at High Pressure

Metallic core formation in differentiated bodies in the inner solar system can takeplace between low pressures (near 1 bar) to much higher pressures (up to 100 GPa). Mostthermodynamic models of metal-silicate equilibria utilize activity coefficients for metallic tracersin Fe liquids, nearly all of which have been carried out at low pressures. This study focuses onthe effect of pressure on activity coefficients for Au, P, V, Mn, Ga, Zn, Cd, Sn, W, Pb, and Nb inliquid Fe-Si alloys. From a series of experiments at 10 GPa, 2373 K containing variable Sicontent in a metallic liquid we have derived epsilon interaction parametersin FeSi liquids (εMSi). Comparison of 1 GPa and 10 GPa data shows no difference except for Nb. Epsilonparameters derived from low pressure experiments can thus be used to calculate activitycoefficients for application to higher pressure processes (at least to 10 GPa).

K Righter↗