Model 9975 O-Ring Fixture Long-Term Leak Performance (Tenth Interim Status Report)

A series of experiments to monitor the aging performance of Viton® GLT O-rings used in the Model 9975 package has been ongoing since 2004 at the Savannah River National Laboratory. One approach has been to periodically evaluate the leak performance of O-rings being aged in mock-up 9975 Primary Containment Vessels (PCVs) at elevated temperatures. Other methods such as compression-stress relaxation (CSR) tests and field surveillance are also on-going to evaluate O-ring behavior. Seventy tests using PCV mock-ups were assembled and heated to temperatures ranging from 200 to 450 ºF. They were leak-tested initially and have been tested periodically to determine if they continue to meet the leak-tightness criterion defined in ANSI standard N14.5-97. Due to material substitution, fourteen additional tests were initiated in 2008 with GLT-S O-rings heated to temperatures ranging from 200 to 400 ºF. High temperature aging continues for 23 GLT O-ring fixtures at 200 – 270 ºF. Room temperature leak test failures have been experienced in all of the GLT O-ring fixtures aging at 350 ºF and higher temperatures, and in 8 fixtures aging at 300 ºF. The earliest 300 °F GLT Oring fixture failure was observed at 34 months. The remaining GLT O-ring fixtures aging at 300 ºF have been retired from testing following more than 5 years at temperature without failure. No failures have yet been observed in GLT O-ring fixtures aging at 200 ºF for 84 - 108 months, which bounds O-ring temperatures anticipated during storage in K-Area Complex (KAC). Based on expectations that the 200 ºF fixtures will remain leak-tight for a significant period yet to come, 2 additional fixtures began aging in 2011 at 270 ºF, with hopes that they may reach a failure condition before the 200 ºF fixtures, thus providing additional time to failure data. High temperature aging continues for 5 GLT-S O-ring fixtures at 200 – 300 ºF. Room temperature leak test failures have been experienced in all 8 of the GLT-S O-ring fixtures aging at 350 and 400 ºF, and in one GLT-S O-ring fixture aging at 300 ºF. No failures have yet been observed in GLT-S O-ring fixtures aging at 200 - 250 ºF for 66 months. One O-ring fixture has failed since the last interim report was issued. Both O-rings in one GLTS fixture aging at 300 ºF failed to remain leak-tight after 69 months at temperature. Aging and periodic leak testing will continue for the remaining PCV fixtures. Additional irradiation of several fixtures has been performed in the last year to maintain a balance between thermal and radiation exposures similar to that experienced in storage, and to show the degree of consistency of radiation response between GLT and GLT-S O-rings.

42 ENGINEERING↗

FY2025 Status Report: Model 9975 O Ring Fixture Long-Term Leak Performance

Leak testing experiments to monitor the aging performance of Viton® GLT and GLT-S O-rings used in the model 9975 shipping package have been ongoing since 2004 at Savannah River National Laboratory. Seventy tests using mock-up 9975 primary containment vessels (PCVs) with GLT O-rings were assembled and heated to temperatures ranging from 200 to 450 °F. Due to material substitution, fourteen tests with GLT-S O-rings were initiated in 2008 and heated to temperatures ranging from 200 to 400 °F. The conditioning temperatures are elevated compared to the calculated maximum O-ring temperature in a 9975 package in storage, 158 °F, to accelerate aging and enable observations of O-ring failures in a reasonable time frame. The mock-up PCV fixtures are leak tested periodically, and all GLT O-ring fixtures aged at 350 °F or above have failed to maintain a leak-tight seal. Eight GLT O-ring fixtures aged at 300 °F have failed after 2.8 to 5.7 years at temperature while the remaining fixtures at 300 °F were retired from testing following more than five years of aging without failure. Two of these retired fixtures were returned to testing and heated to 350 °F to evaluate the impact of additional heating at higher temperature for aged O-rings. Fixture #20 failed after 3 months while fixture #18 failed after 9 months at 350 °F. These O-rings demonstrated that aged and in-service O-rings can continue to be used, even at higher temperatures, after being in storage, and their leak performance are consistent with other samples at 350 °F. There has been one GLT O-ring fixture which failed after 13.4 years of aging at 200 °F. However, 20 other GLT O-rings aging at 200 °F have remained leak-tight for over 16.9 years and remain in test. There are two GLT O-ring fixtures at 270 °F; one fixture has failed after 12.9 years while the other fixture remains in test after 12.5 years. All GLT-S O-ring fixtures aged at 300 °F or above have failed their leak test. No failures have yet been observed in GLT-S O-ring fixtures aging at 250 °F for 14.9 years, while one GLT-S O-ring fixture failed after 12.4 years at 200 °F. The leak testing data to date suggest the GLT and GLT-S O-rings aging in the K-Area Complex (KAC) storage at temperatures of 158 °F might maintain a leak-tight seal for up to 59 years. Data from the O-ring fixtures are generally consistent with results from compression stress-relaxation testing and provide confidence in the predictive models based on those results. However, uncertainty exists in extrapolating these elevated temperature results to the lower temperatures of interest for normal storage in KAC. The collective data from these test efforts suggest the minimum O-ring service life at KAC normal storage conditions should be at least 34 years for GLT and GLT-S O-rings. Measurement of compression set in O-rings removed from failed fixtures, compared to that from KAC surveillance O-rings, indicate significant margin remains for O-rings still in service in 9975 packages in KAC. Aging and periodic leak testing will continue for the remaining 24 mock-up PCV fixtures.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Model 9975 PCV O-Ring Fixture Long-Term Leak Performance (Seventh Interim Status Report)

A series of experiments to monitor the aging performance of Viton® GLT O-rings used in the Model 9975 package has been ongoing since 2004 at the Savannah River National Laboratory. Seventy tests using mock-ups of 9975 Primary Containment Vessels (PCVs) were assembled and heated to temperatures ranging from 200 to 450ºF. They were leak-tested initially and have been tested periodically to determine if they meet the criterion of leak-tightness defined in ANSI standard N14.5-97. Fourteen additional tests were initiated in 2008 with GLT-S O-rings heated to temperatures ranging from 200 to 400ºF. High temperature aging continues for 23 GLT O-ring fixtures at 200–270ºF. Room temperature leak test failures have been experienced in all of the GLT O-ring fixtures aging at 350ºF and higher temperatures, and in 8 fixtures aging at 300ºF. The remaining GLT O-ring fixtures aging at 300ºF have been retired from testing following more than 5 years at temperature without failure. No failures have yet been observed in GLT O-ring fixtures aging at 200ºF for 54-72 months, which is still bounding to O-ring temperatures during storage in K-Area Complex (KAC). Based on expectations that the fixtures aging at 200ºF will remain leak-tight for a significant period yet to come, 2 additional fixtures began aging in 2011 at an intermediate temperature of 270ºF, with hopes that they may reach a failure condition before the 200ºF fixtures. High temperature aging continues for 6 GLT-S O-ring fixtures at 200–300ºF. Room temperature leak test failures have been experienced in all 8 of the GLT-S O-ring fixtures aging at 350 and 400ºF. No failures have yet been observed in GLT-S O-ring fixtures aging at 200-300ºF for 30-36 months. For O-ring fixtures that have failed the room temperature leak test and been disassembled, the O-rings displayed a compression set ranging from 51–96%. This is greater than seen to date for any packages inspected during KAC field surveillance (24% average). For GLT O-rings, separate service life estimates have been made based on the O-ring fixture leak test data and based on compression stress relaxation (CSR) data. These two predictive models show reasonable agreement at higher temperatures (350–400ºF). However, at 300ºF, the room temperature leak test failures to date experienced longer aging times than predicted by the CSR-based model. This suggests that extrapolations of the CSR model predictions to temperatures below 300ºF will provide a conservative prediction of service life relative to the leak rate criterion. Leak test failure data at lower temperatures are needed to verify this apparent trend. Insufficient failure data exist currently to perform a similar comparison for GLT-S O-rings. Aging and periodic leak testing will continue for the remaining PCV O-ring fixtures.

36 MATERIALS SCIENCE↗

NINTH INTERIM STATUS REPORT: MODEL 9975 PCV O-RING FIXTURE LONG-TERM LEAK PERFORMANCE

A series of experiments to monitor the aging performance of Viton® GLT O-rings used in the Model 9975 package has been ongoing since 2004 at the Savannah River National Laboratory. One approach has been to periodically evaluate the leak performance of O-rings being aged in mock-up 9975 Primary Containment Vessels (PCVs) at elevated temperatures. Other methods such as compression-stress relaxation (CSR) tests and field surveillance are also on-going to evaluate O-ring behavior. Seventy tests using PCV mock-ups were assembled and heated to temperatures ranging from 200 to 450 ºF. They were leak-tested initially and have been tested periodically to determine if they continue to meet the leak-tightness criterion defined in ANSI standard N14.5-97. Due to material substitution, fourteen additional tests were initiated in 2008 with GLT-S O-rings heated to temperatures ranging from 200 to 400 ºF. High temperature aging continues for 23 GLT O-ring fixtures at 200 – 270 ºF. Room temperature leak test failures have been experienced in all of the GLT O-ring fixtures aging at 350 ºF and higher temperatures, and in 8 fixtures aging at 300 ºF. The earliest 300 °F GLT O-ring fixture failure was observed at 34 months. The remaining GLT O-ring fixtures aging at 300 ºF have been retired from testing following more than 5 years at temperature without failure. No failures have yet been observed in GLT O-ring fixtures aging at 200 ºF for 72 - 96 months, which bounds O-ring temperatures anticipated during storage in K-Area Complex (KAC). Based on expectations that the 200 ºF fixtures will remain leak-tight for a significant period yet to come, 2 additional fixtures began aging in 2011 at 270 ºF, with hopes that they may reach a failure condition before the 200 ºF fixtures, thus providing additional time to failure data. High temperature aging continues for 6 GLT-S O-ring fixtures at 200 – 300 ºF. Room temperature leak test failures have been experienced in all 8 of the GLT-S O-ring fixtures aging at 350 and 400 ºF. No failures have yet been observed in GLT-S O-ring fixtures aging at 200 - 300 ºF for 54 - 57 months. No additional O-ring failures have been observed since the last interim report was issued. Aging and periodic leak testing will continue for the remaining PCV fixtures. Additional irradiation of several fixtures is recommended to maintain a balance between thermal and radiation exposures similar to that experienced in storage, and to show the degree of consistency of radiation response between GLT and GLT-S O-rings.

42 ENGINEERING↗

SIXTH INTERIM STATUS REPORT: MODEL 9975 PCV O-RING FIXTURE LONG-TERM LEAK PERFORMANCE

A series of experiments to monitor the aging performance of Viton{reg_sign} GLT O-rings used in the Model 9975 package has been ongoing for seven years at the Savannah River National Laboratory. Seventy tests using mock-ups of 9975 Primary Containment Vessels (PCVs) were assembled and heated to temperatures ranging from 200 to 450 F. They were leak-tested initially and have been tested periodically to determine if they meet the criterion of leak-tightness defined in ANSI standard N14.5-97. Fourteen additional tests were initiated in 2008 with GLT-S O-rings heated to temperatures ranging from 200 to 400 F. High temperature aging continues for 33 GLT O-ring fixtures at 200-300 F. Room temperature leak test failures have been experienced in all of the GLT O-ring fixtures aging at 350 F and higher temperatures, and in 7 fixtures aging at 300 F. No failures have yet been observed in GLT O-ring fixtures aging at 200 F for 41-60 months, which is still bounding to O-ring temperatures during storage in K-Area Complex (KAC). Based on expectations that the fixtures aging at 200 F will remain leak-tight for a significant period yet to come, 2 additional fixtures began aging within the past year at an intermediate temperature of 270 F, with hopes that they may leak before the 200 F fixtures. High temperature aging continues for 6 GLT-S O-ring fixtures at 200-300 F. Room temperature leak test failures have been experienced in all 8 of the GLT-S O-ring fixtures aging at 350 and 400 F. No failures have yet been observed in GLT-S O-ring fixtures aging at 200-300 F for up to 26 months. For O-ring fixtures that have failed the room temperature leak test and been disassembled, the Orings displayed a compression set ranging from 51-96%. This is greater than seen to date for packages inspected during KAC field surveillance (24% average). For GLT O-rings, separate service life estimates have been made based on the O-ring fixture leak test data and based on compression stress relaxation (CSR) data. These two predictive models show reasonable agreement at higher temperatures (350-400 F). However, at 300 F, the room temperature leak test failures to date experienced longer aging times than predicted by the CSR-based model. This suggests that extrapolations of the CSR model predictions to temperatures below 300 F will provide a conservative prediction of service life relative to the leak rate criterion. Leak test failure data at lower temperatures are needed to verify this apparent trend. Insufficient failure data exist currently to perform a similar comparison for GLT-S O-rings. Aging and periodic leak testing will continue for the remaining fixtures.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Additive Manufacturing of Advanced High Temperature Masking Fixtures for EBPVD TBC Coating

The purpose of this Manufacturing Demonstration Facility (MDF) technical collaboration project between Praxair Surface Technologies, Inc. (PST) and Oak Ridge National Laboratory (ORNL) was to develop an additive manufacturing process to fabricate next generation high temperature masking fixtures for coating of turbine airfoils with ceramic Thermal Barrier Coatings (TBC) by the Electron Beam Physical Vapor Deposition (EBPVD) process. Typical masking fixtures are sophisticated designs and require complex part manipulation in order to achieve the desired coating distribution. Fixtures are typically fabricated from high temperature nickel (Ni) based superalloys. The fixtures are fabricated from conventional processes by welding of thin sheet material into a complex geometry, to decrease the weight load for the manipulator and to reduce the thermal mass of the fixture. Recent attempts have been made in order to fabricate the fixtures through casting, but thin walled sections are difficult to cast and have high scrap rates. This project focused on understanding the potential for fabricating high temperature Ni based superalloy fixtures through additive manufacturing. Two different deposition processes; electron beam melting (EBM) and laser powder bed fusion were evaluated to determine the ideal processing route of these materials. Two different high temperature materials were evaluated. The high temperature materials evaluated were Inconel 718 and another Ni base alloy, designated throughout the remainder of this document as Alloy X, as the alloy composition is sensitive. Inconel 718 is a more widely utilized material for additive manufacturing although it is not currently the material utilized for current fixtures. Alloy X is the alloy currently used for the fixtures, but is not a commercially available alloy for additive manufacturing. Praxair determined it was possible to build the fixture using laser powder bed technology from Inconel 718. ORNL fabricated the fixture geometry using the EBM technology in order to compare deposition features such as surface roughness, geometric accuracy, deposition rate, surface and subsurface porosity, and material quality. It was determined that the laser powder bed technology was ideal for the geometry and requirements of the fixture set by Praxair, and Praxair moved forward with the purchase of a laser powder bed system. The subsequent portion of the project focused on determining the ideal processing parameters for alloy X for the laser powder bed system using ORNL’s Renishaw laser powder bed system. Praxair supplied gas atomized powders of alloy X material with properties specified by ORNL. ORNL printed text cube arrays in order to determine the ideal combination of laser powder and laser travel speed in order to maximize material density, improve surface quality, and maintain geometric accuracy. Additional powder supplied by Praxair was used to fabricate a full-scale fixture component.

42 ENGINEERING↗

Eighth Interim Status Report: Model 9975 PCV O-Ring Fixture Long-Term Leak Performance

A series of experiments to monitor the aging performance of Viton® GLT O-rings used in the Model 9975 package has been ongoing since 2004 at the Savannah River National Laboratory. Seventy tests using mock-ups of 9975 Primary Containment Vessels (PCVs) were assembled and heated to temperatures ranging from 200 to 450 ºF. They were leak-tested initially and have been tested periodically to determine if they meet the criterion of leak-tightness defined in ANSI standard N14.5-97. Fourteen additional tests were initiated in 2008 with GLT-S O-rings heated to temperatures ranging from 200 to 400 ºF. High temperature aging continues for 23 GLT O-ring fixtures at 200 – 270 ºF. Room temperature leak test failures have been experienced in all of the GLT O-ring fixtures aging at 350 ºF and higher temperatures, and in 8 fixtures aging at 300 ºF. The remaining GLT O-ring fixtures aging at 300 ºF have been retired from testing following more than 5 years at temperature without failure. No failures have yet been observed in GLT O-ring fixtures aging at 200 ºF for 61 - 85 months, which is still bounding to O-ring temperatures during storage in KArea Complex (KAC). Based on expectations that the fixtures aging at 200 ºF will remain leaktight for a significant period yet to come, 2 additional fixtures began aging in 2011 at an intermediate temperature of 270 ºF, with hopes that they may reach a failure condition before the 200 ºF fixtures. High temperature aging continues for 6 GLT-S O-ring fixtures at 200 – 300 ºF. Room temperature leak test failures have been experienced in all 8 of the GLT-S O-ring fixtures aging at 350 and 400 ºF. No failures have yet been observed in GLT-S O-ring fixtures aging at 200 - 300 ºF for 41 - 45 months. Aging and periodic leak testing will continue for the remaining PCV fixtures.

42 ENGINEERING↗

Model 9975 O-Ring Fixture Long-Term Leak Performance (FY2022 Status Report)

Leak testing experiments to monitor the aging performance of Viton® GLT and GLT-S O-rings used in the model 9975 shipping package has been ongoing since 2004 at Savannah River National Laboratory. Seventy tests using mock-up 9975 primary containment vessels (PCVs) with GLT O-rings were assembled and heated to temperatures ranging from 200 to 450 °F. Due to material substitution, fourteen tests with GLT-S O-rings were initiated in 2008 and heated to temperatures ranging from 200 to 400 °F. The conditioning temperatures are elevated compared to the calculated maximum O-ring temperature in a 9975 package in storage, 158 °F, to accelerate aging and enable observations of O-ring failures in a reasonable time frame. The fixtures are leak tested periodically and all GLT O-ring fixtures aging at 350 °F or above have failed to maintain a leak-tight seal. Eight GLT O-ring fixtures aging at 300 °F have failed after 2.8 to 5.7 years at temperature while the remaining fixtures at 300 °F were retired from testing following more than five years without failure. There has been one GLT O-ring fixture which failed after 13.4 years aging at 200 °F. However, 20 other GLT O-rings aging at 200 °F have remained leak-tight for over 14 years and remain in test. No failures have yet been observed in GLT O-ring fixtures aging at 270 °F for 10.4 years. All GLT-S O-ring fixtures aging at 300 °F or above have failed their leak test. No failures have yet been observed in GLT-S O-ring fixtures aging at 250 °F for 12.5 years. This year, one GLT-S O-ring fixture failed after 12.4 years aging at 200 °F. Data from the O-ring fixtures are generally consistent with results from compression stress-relaxation testing, and provide confidence in the predictive models based on those results. However, uncertainty exists in extrapolating these elevated temperature results to the lower temperatures of interest for normal storage in K-Area Complex (KAC). Oxygen consumption testing, which includes results from temperatures near KAC normal storage temperatures, is ongoing to provide further confidence and corroborate these extrapolations. The collective data from these test efforts suggest the minimum O-ring service life at KAC normal storage conditions should be at least 34 years for GLT and GLT-S O-rings. Measurement of compression set in O-rings removed from failed fixtures, compared to that from KAC surveillance O-rings, indicate significant margin remains for O-rings still in service in 9975 packages in KAC. Aging and periodic leak testing will continue for the remaining 25 mock-up PCV fixtures.

36 MATERIALS SCIENCE↗

FY2017 status report: Model 9975 O-ring fixture long-term leak performance

A series of experiments to monitor the aging performance of Viton® GLT and GLT-S O-rings used in the Model 9975 shipping package has been ongoing since 2004 at the Savannah River National Laboratory. One approach has been to periodically evaluate the leak performance of O-rings being aged in mock-up 9975 Primary Containment Vessels (PCVs) at elevated temperature. Other methods such as compression-stress relaxation (CSR) tests and field surveillance are also on-going to evaluate O-ring behavior. Seventy tests using PCV mock-ups with GLT O-rings were assembled and heated to temperatures ranging from 200 to 450 ºF. They were leak-tested initially and have been tested periodically to determine if they continue to meet the leak-tightness criterion defined in ANSI standard N14.5-97. Due to material substitution, a smaller test matrix with fourteen additional tests was initiated in 2008 with GLT-S O-rings heated to temperatures ranging from 200 to 400 ºF. Leak test failures have been experienced in all of the GLT O-ring fixtures aging at 350 ºF and higher temperatures, and in 8 fixtures aging at 300 ºF. The 300 °F GLT O-ring fixtures failed after 2.8 to 5.7 years at temperature. The remaining GLT O-ring fixtures aging at 300 ºF were retired from testing following more than 5 years at temperature without failure. No failures have yet been observed in GLT O-ring fixtures aging at 200 ºF for 9 to 10.5 years, or in GLT O-ring fixtures aging at 270 ºF for 5.7 years. These aging temperatures bound O-ring temperatures anticipated during normal storage in K-Area Complex (KAC). Leak test failures have been experienced in all of the GLT-S O-ring fixtures aging at 300 ºF and above. No failures have yet been observed in GLT-S O-ring fixtures aging at 200 and 250 ºF for 6.9 to 7.5 years. Data from the O-ring fixtures are generally consistent with results from compression stress relaxation testing, and provide confidence in the predictive models based on those results. However, uncertainty still exists in extrapolating these elevated temperature results to the lower temperatures of interest for normal storage in KAC. Measurement of compression set in O-rings removed from failed fixtures, compared to that from KAC surveillance O-rings, indicates margin remains for O-rings still in service. Aging and periodic leak testing will continue for the remaining PCV fixtures.

42 ENGINEERING↗

Model 9975 O Ring Fixture LongTerm Leak Performance (FY2021 Status Report)

Leak testing experiments to monitor the aging performance of Viton® GLT and GLT-S O-rings used in the model 9975 shipping package has been ongoing since 2004 at Savannah River National Laboratory. Seventy tests using mock-up 9975 primary containment vessels (PCVs) with GLT O-rings were assembled and heated to temperatures ranging from 200 to 450 °F. Due to material substitution, fourteen tests with GLT-S O-rings were initiated in 2008 and heated to temperatures ranging from 200 to 400 °F. The conditioning temperatures are elevated compared to the calculated maximum O-ring temperature in a 9975 package in storage, 158 °F, to accelerate aging and enable observations of O-ring failures in a reasonable time frame. The fixtures are leak tested periodically and all GLT O-ring fixtures aging at 350 °F or above have failed to maintain a leak-tight seal. Eight GLT O-ring fixtures aging at 300 °F have failed after 2.8 to 5.7 years at temperature while the remaining fixtures at 300 °F were retired from testing following more than five years without failure. There has been one GLT O-ring fixture which failed after 13.4 years aging at 200 °F. However, 19 other GLT O-rings aging at 200 °F have remained leak-tight for over 14 years and remain in test. No failures have yet been observed in GLT O-ring fixtures aging at 270 °F for 9.5 years. All GLT-S O-ring fixtures aging at 300 °F or above have failed their leak test. No failures have yet been observed in GLT-S O-ring fixtures aging at 200 and 250 °F for 11.5 years. Data from the O-ring fixtures are generally consistent with results from compression stress-relaxation testing, and provide confidence in the predictive models based on those results. However, uncertainty exists in extrapolating these elevated temperature results to the lower temperatures of interest for normal storage in K-Area Complex (KAC). Oxygen consumption testing, which includes results from temperatures near KAC normal storage temperatures, is ongoing to provide further confidence and corroborate these extrapolations. The collective data from these test efforts suggest the minimum O-ring service life at KAC normal storage conditions should be at least 34 years for GLT and GLT-S O-rings. Measurement of compression set in O-rings removed from failed fixtures, compared to that from KAC surveillance O-rings, indicate significant margin remains for O-rings still in service in 9975 packages in KAC. Aging and periodic leak testing will continue for the remaining 26 mock-up PCV fixtures.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Graphite Composite Panel Polishing Fixture

The use of high-strength, lightweight composites for the fixture is the novel feature of this innovation. The main advantage is the light weight and high stiffness-to-mass ratio relative to aluminum. Meter-class optics require support during the grinding/polishing process with large tools. The use of aluminum as a polishing fixture is standard, with pitch providing a compliant layer to allow support without deformation. Unfortunately, with meter-scale optics, a meter-scale fixture weighs over 120 lb (.55 kg) and may distort the optics being fabricated by loading the mirror and/or tool used in fabrication. The use of composite structures that are lightweight yet stiff allows standard techniques to be used while providing for a decrease in fixture weight by almost 70 percent. Mounts classically used to support large mirrors during fabrication are especially heavy and difficult to handle. The mount must be especially stiff to avoid deformation during the optical fabrication process, where a very large and heavy lap often can distort the mount and optic being fabricated. If the optic is placed on top of the lapping tool, the weight of the optic and the fixture can distort the lap. Fixtures to support the mirror during fabrication are often very large plates of aluminum, often 2 in. (.5 cm) or more in thickness and weight upwards of 150 lb (68 kg). With the addition of a backing material such as pitch and the mirror itself, the assembly can often weigh over 250 lb (.113 kg) for a meter-class optic. This innovation is the use of a lightweight graphite panel with an aluminum honeycomb core for use as the polishing fixture. These materials have been used in the aerospace industry as structural members due to their light weight and high stiffness. The grinding polishing fixture consists of the graphite composite panel, fittings, and fixtures to allow interface to the polishing machine, and introduction of pitch buttons to support the optic under fabrication. In its operation, the grinding polishing fixture acts as a reaction structure to the polishing tool. It must be stiff enough to avoid imparting a distorted shape to the optic under fabrication and light enough to avoid self-deflection. The fixture must also withstand significant tangential loads from the polishing machine during operations.

Hagopian, John↗

Model 9975 O-Ring Fixture Long-Term Leak Performance (FY2020 Status Report)

Leak testing experiments to monitor the aging performance of Viton GLT and GLT-S O-rings used in the model 9975 shipping package has been ongoing since 2004 at Savannah River National Laboratory. Seventy tests using mock-up 9975 primary containment vessels (PCVs) with GLT O-rings were assembled and heated to temperatures ranging from 200 to 450 °F. In addition, fourteen tests with GLT-S O-rings were initiated in 2008 and heated to temperatures ranging from 200 to 400 °F. The conditioning temperatures are elevated compared to the calculated maximum O-ring temperature in a 9975 package in storage, 158 °F, to accelerate aging and enable observations of O-ring failures in a reasonable time frame. The fixtures are leak tested periodically and all GLT O-ring fixtures aging at 350 °F or above have failed to maintain a leak-tight seal. Eight GLT O-ring fixtures aging at 300 °F have failed after 2.8 to 5.7 years at temperature while the remaining fixtures at 300 °F were retired from testing following more than five years without failure. No failures have yet been observed in GLT O-ring fixtures aging at 200 °F for 12 to 14 years or aging at 270 °F for 8.5 years. All GLT-S O-ring fixtures aging at 300 °F or above have failed their leak test. No failures have yet been observed in GLT-S O-ring fixtures aging at 200 and 250 °F for 10 to 10.5 years. Data from the O-ring fixtures are generally consistent with results from compression stress-relaxation testing, and provide confidence in the predictive models based on those results. However, uncertainty exists in extrapolating these elevated temperature results to the lower temperatures of interest for normal storage in K-Area Complex (KAC). Oxygen consumption testing, which includes results from temperatures near KAC normal storage temperatures, is ongoing to provide further confidence and corroborate these extrapolations. The collective data from these test efforts suggest the minimum O-ring service life at KAC normal storage conditions should be at least 34 years for GLT and GLT-S O-rings. Measurement of compression set in O-rings removed from failed fixtures, compared to that from KAC surveillance O-rings, indicates margin remains for O-rings still in service. Aging and periodic leak testing will continue for the remaining PCV fixtures.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

FIFTH INTERIM STATUS REPORT: MODEL 9975 PCV O-RING FIXTURE LONG-TERM LEAK PERFORMANCE

A series of experiments to monitor the aging performance of Viton{sup reg.} GLT O-rings used in the Model 9975 package has been ongoing for six years at the Savannah River National Laboratory. Sixty-seven mock-ups of 9975 Primary Containment Vessels (PCVs) were assembled and heated to temperatures ranging from 200 to 450 F. They were leak-tested initially and have been tested at nominal six month intervals to determine if they meet the criterion of leaktightness defined in ANSI standard N14.5-97. Fourteen additional tests were initiated in 2008 with GLT-S O-rings heated to temperatures ranging from 200 to 400 F. High temperature aging continues for 36 GLT O-ring fixtures at 200--350 F. Room temperature leak test failures have been experienced in 5 of the GLT O-ring fixtures aging at 300 and 350 F, and in all 3 of the GLT O-ring fixtures aging at higher temperatures. No failures have yet been observed in GLT O-ring fixtures aging at 200 F for 30--48 months, which is still bounding to O-ring temperatures during storage in KAMS. High temperature aging continues for 6 GLT-S O-ring fixtures at 200--300 F. Room temperature leak test failures have been experienced in all 8 of the GLT-S O-ring fixtures aging at 350 and 400 F. No failures have yet been observed in GLT-S O-ring fixtures aging at 200 or 300 F for 19 months. For O-ring fixtures that have failed the room temperature leak test and been disassembled, the O-rings displayed a compression set ranging from 51--95%. This is significantly greater than seen to date for packages inspected during KAMS field surveillance (23% average). For GLT O-rings, service life based on the room temperature leak rate criterion is comparable to that predicted by compression stress relaxation (CSR) data at higher temperatures (350--400 F). While there are no comparable failure data yet at aging temperatures below 300 F, extrapolations of the data for GLT O-rings suggests that CSR model predictions provide a conservative prediction of service life relative to the leak rate criterion. Failure data at lower temperatures is needed to verify this apparent trend. Insufficient failure data exist currently to perform a similar comparison for GLT-S O-rings. Aging and periodic leak testing will continue for the remaining fixtures.

42 ENGINEERING↗

FIFTH INTERIM STATUS REPORT: MODEL 9975 PCV O-RING FIXTURE LONG-TERM LEAK PERFORMANCE

A series of experiments to monitor the aging performance of Viton{reg_sign} GLT O-rings used in the Model 9975 package has been ongoing for six years at the Savannah River National Laboratory. Sixty-seven mock-ups of 9975 Primary Containment Vessels (PCVs) were assembled and heated to temperatures ranging from 200 to 450 F. They were leak-tested initially and have been tested at nominal six month intervals to determine if they meet the criterion of leaktightness defined in ANSI standard N14.5-97. Fourteen additional tests were initiated in 2008 with GLT-S O-rings heated to temperatures ranging from 200 to 400 F. High temperature aging continues for 36 GLT O-ring fixtures at 200-350 F. Room temperature leak test failures have been experienced in 6 of the GLT O-ring fixtures aging at 300 and 350 F, and in all 3 of the GLT O-ring fixtures aging at higher temperatures. No failures have yet been observed in GLT O-ring fixtures aging at 200 F for 30-48 months, which is still bounding to O-ring temperatures during storage in KAMS. High temperature aging continues for 6 GLT-S O-ring fixtures at 200-300 F. Room temperature leak test failures have been experienced in all 8 of the GLT-S O-ring fixtures aging at 350 and 400 F. No failures have yet been observed in GLT-S O-ring fixtures aging at 200 or 300 F for 19 months. For O-ring fixtures that have failed the room temperature leak test and been disassembled, the Orings displayed a compression set ranging from 51-95%. This is significantly greater than seen to date for packages inspected during KAMS field surveillance (23% average). For GLT O-rings, service life based on the room temperature leak rate criterion is comparable to that predicted by compression stress relaxation (CSR) data at higher temperatures (350-400 F). While there are no comparable failure data yet at aging temperatures below 300 F, extrapolations of the data for GLT O-rings suggests the CSR model predictions provide a conservative prediction of service life relative to the leak rate criterion. Failure data at lower temperatures are needed to verify this apparent trend. Insufficient failure data exist currently to perform a similar comparison for GLT-S O-rings. Aging and periodic leak testing will continue for the remaining fixtures.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗