Search NASA⌕ Search

SEARCH · Search NASA

Results for “Fluoropolymers”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Fluoropolymer Composites from Partially Perfluoroalkylated Waste Polyethylene

Chemically modified plastics have emerged as practical solutions to plastic waste increases. Here, the inherent novelty of decorating polymer chains with chemical functionality results in distinct properties that expand the available application space. Nevertheless, developing designer materials for specific applications beyond compatibilization or mild property enhancement is difficult due to the synergistic effects of both the polar functionality imparted and the parent materials' intrinsic properties. By incorporating perfluoro-alkyl side-chains onto the backbone of dehydrogenated waste HDPE, unique surface properties intermediate between polytetrafluoroethylene (PTFE, the model fluoropolymer) and HDPE become apparent, while the overall material mechanical and thermal properties result in more LLDPE-like materials. This is demonstrated through moderate decreases in the surface free energy of the perfluoroalkylated polyolefin surface (increase in H 2 O contact angle of ~ 6°) and increased ordering under shear when blended with PTFE nanoparticles where the crossover point occurred at higher strains. Critically, perfluoroalkylated HDPE possesses improved rheological modification properties at elevated temperatures with PTFE nanoparticles, resulting in more thermally robust and stable composite materials.

fluoropolymer↗

Fluoropolymer‐Stabilized Chromophore–Catalyst Assemblies in Aqueous Buffer Solutions for Water‐Oxidation Catalysis

Abstract Here, the application of the fluorinated polymer [Dupont AF, a copolymer of 4,5‐difluoro‐2,2‐bis(trifluoromethyl)‐1,3‐dioxole and tetrafluoroethylene] is described in stabilizing phosphonate‐derivatized molecular assemblies on oxide electrodes. In the procedure, the polymer was dip‐coated onto the surfaces of oxide electrodes with pre‐bound, phosphonate‐derivatized chromophores and assemblies, including assemblies for water oxidation. The results of the experiments showed a high degree of stabilization by the added polymer and a demonstration of its use in stabilizing surface‐bound assemblies for water‐oxidation catalysis.

Eberhart, Michael S.↗

Lifespan Impacts to Infrastructure, Renewable Energy Components and Energy Storage Components Related to Fluoropolymer Use

This report focuses on the use of fluoropolymers in infrastructure materials (building construction materials, transportation, and electrical transmission and distribution); renewable energy generation components (specifically wind and solar); and energy storage components (lithium-ion batteries and fuel cells) and product lifespan impacts if fluoropolymers were no longer available or allowed in commerce. Additionally, environmental considerations for fluoropolymer manufacture, use, and end-of-life disposal are discussed. This document is the second of two companion reports. The first report, Assessment of Fluoropolymer Production and Use With Analysis of Alternative Replacement Materials, contained an analysis of use of fluoropolymers and their potential replacement technologies in aerospace, automotive, battery, building construction, chemical processing, electronics, infrastructure, semiconductor, solar panel, and wind energy industries sectors, along with qualitative life cycle assessment (LCA) and cost-benefit analysis of replacing fluoropolymers. This report does not focus on the lifecycle aspects of use of fluoropolymer or alternatives in the designated applications. For more information on those topics, see aforementioned report.

25 ENERGY STORAGE↗

Methods for manufacturing electrodes including fluoropolymer-based solid electrolyte interface layers

Methods for manufacturing electrodes include applying a fluoropolymer film to a lithium-based host material, defluorinating the fluoropolymer film by heating to produce a lithium electrode having a solid electrolyte interface (SEI) layer including defluorinated fluoropolymers and at least about 5 wt. % LiF. The fluoropolymers can include one or more of fluorinated ethylenepropylene, perfluoroalkoxy alkanes, vinylidenefluoride, and copolymers of perfluoromethylvinylether and tetrafluoroethylene. The fluoropolymers can include one or more fluorinated monomers, including hexafluoropropylene, tetrafluoroethylene, ethylene-tetrafluoroethylene, perfluoroethers, and vinylidene fluoride. The —CF 3 functional groups of the defluorinated fluoropolymers can be about 3 wt. % to about 10 wt. % of the SEI layer. The SEI layer can include about 30 wt. % to about 50 wt. % LiF. The method can include assembling a battery cell by disposing a battery separator between a cathode and the electrode, and disposing the battery separator, the cathode, and the electrode in an electrolyte.

Xiao, Xingcheng↗

Assessment of Fluoropolymer Production and Use With Analysis of Alternative Replacement Materials

This report focuses on fluoropolymers, which are a subgroup of the much larger class of fluorinated chemicals known as per- and polyfluoroalkyl substances (PFAS). Clearly distinguishing fluoropolymers is important to understanding their distinctive chemical properties, associated risks and benefits, and roles in commerce. In this report, the factors that are considered in a lifecycle assessment (LCA) of fluoropolymers will be discussed. These include the manufacturing of fluoropolymers, their use in industry, and available replacement technologies. Emphasis is placed on fluoropolymer plastics because of their extensive use in the commerce sectors considered here, specifically aerospace, automotive, battery, building construction, chemical processing, electronics, infrastructure, semiconductor, solar panel, and wind energy industries.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Phase changes in fluoropolymer binders

Motivation: Understanding fluoropolymer binder structure and aging response continues to be an important goal for the prediction and assessment of polymer bonded explosive compositions within the stockpile. As part of ongoing efforts within NNM, we are developing new methods to quantify crystallization and chemical degradation within aged Fluoropolymer materials. Significance: Time, temperature and radiation are known to alter the mechanical properties of fluoropolymers as crystalline domains nucleate and grow within the material. However, current methods do not accurately quantify and assess the degree or rapidity of these physical aging processes. For this reason, we are developing methods that directly measure crystalline domain, composition, size and shape and cross-correlating them with traditional techniques. Progress: Most recently, we thermally aged fluoropolymer binder, FK800, for various durations up to 23 days at several temperatures including: 25C (red), 35C (green), and 60C (blue). We used wide angle X-ray scattering (WAXS) to observe when crystalline peaks emerged, signaling a phase transition from amorphous to partially crystalline. Some of these data are summarized in Figure 1. As expected, samples held at 25C (red), which is below the glass transition temperature at 28C, remain amorphous – the WAXS data (Figure 1b) lacks sharp peaks indicative of crystallinity and the ultra-small angle X-ray scattering (USAXS) also has a smooth background without peaks indicative of structure (Figure 1a). By contrast, samples held at 35C and 60C have new peaks in both the USAXS and WAXS data. The structure is clearer after subtracting off the amorphous background from the WAXS data (Figure 1c). These data show that samples aged at 60C are more crystalline as determined by the more defined peaks and also have a larger lattice constant as seen by the shift in peak position as compared to the 35C samples. The corresponding USAXS data (Figure 1a) indicate that the size of the crystals was larger at 60C than at 35C as seen by the shift in the knee position to lower q-values. Interestingly, the shape of the scatter curve also changed, which indicates a change in morphology. Atomic force microscopy (AFM) was used to image the fluoropolymer (Figure 1c-e). At 35C, ~50nm long stacked crystal plates are observed. High resolution imaging shows that the stacks consist of 2-6 lamellae that are spaced approximately 3nm apart. At 60C, the individual lamella appear both thicker and longer and are intertwined to fill the surface. Morphological data such as these images help to interpret & model volume averaging techniques like X-ray scattering and NMR. We also expect the shift from isolated islands to intertwined clusters to impact mechanical properties.

36 MATERIALS SCIENCE↗

Optoelectronic devices incorporating fluoropolymer compositions for protection

The fluoropolymer compositions of the present invention generally incorporate ingredients comprising one or more fluoropolymers, an ultraviolet light protection component (hereinafter UV protection component), and optionally one or more additional ingredients if desired. The UV protection component includes a combination of at least one hindered tertiary amine (HTA) compound having a certain structure and a weight average molecular weight of at least 1000. This tertiary amine is used in combination with at least one organic, UV light absorbing compound (UVLA compound) having a weight average molecular weight greater than 500. When the HTA compound and the UVLA compound are selected according to principles of the present invention, the UV protection component provides fluoropolymer compositions with significantly improved weatherability characteristics for protecting underlying materials, features, structures, components, and/or the like. In particular, fluoropolymer compositions incorporating the UV protection component of the present invention have unexpectedly improved ability to resist blackening, coloration, or other de gradation that may be caused by UV exposure. As a consequence, devices protected by these compositions would be expected to have dramatically improved service life. The compositions have a wide range of uses but are particularly useful for forming protective layers in optoelectronic devices.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Evaluating Non-Fluoropolymer-Based Co-Extruded Backsheets Using Combined-Accelerated Stress Testing and Materials Forensics

Co-extruded, non-fluoropolymer backsheet films for photovoltaic (PV) modules have gained popularity in recent years based on their cost competitiveness. However, their viability has been thrown into question as a result of widespread, early-life field-failures of some materials, particularly the polyamide (PA)-based “AAA” backsheet product. Failure to detect weaknesses in those earlier products could be due, in part, to insufficient quality testing practices. New testing protocols have recently been developed to better evaluate such materials. Here we show the testing results for a non-fluoropolymer, co-extruded PA-based backsheet film, which demonstrates greater durability than AAA and some commercial fluoropolymers. Using material characterization techniques including Fourier-transform infrared spectroscopy (FTIR), wide-angle x-ray scattering (WAXS), differential scanning calorimetry (DSC), X-ray photoelectron spectroscopy (XPS), elongation-to-break (ETB), and optical microscopy we perform a comprehensive failure analysis to better understand the materials weaknesses. This analysis can ultimately inform how best to improve the material and extend its lifetime. This work serves as a demonstration that some materials should not be discounted due to a single poorly designed product and that more appropriate qualification testing with subsequent materials analysis can be used to develop better materials.

41 EE - Solar Energy Technologies Office (EE-4S)↗

Degradation Analysis of Field-Exposed Photovoltaic Modules with Non-Fluoropolymer-Based Backsheets

The selection of polymeric materials utilized in photovoltaic (PV) modules has changed relatively little since the inception of the PV industry, with ethylene-vinyl acetate (EVA), polyethylene terephthalate (PET), and fluoropolymer-based laminates being the most widely adopted primary components of the encapsulant and backsheet materials. The backsheet must serve to electrically insulate the solar cells and protect them from the effects of weathering. Due to continued downward pressure on cost, other polymeric materials are being formulated to withstand outdoor exposure for use in backsheets to replace either the PET film, the fluoropoymer film, or both. Because of their relatively recent deployment, less is known about their reliability and if they are durable enough to fulfill the greater than or equal to 25 year warranties of current PV modules. This work presents a degradation analysis of field-exposed modules with polyamide- and polyester-based backsheets. Modules were exposed for up to five years in different geographic locations: USA (Maryland, Ohio), China, and Italy. Surface and cross-sectional analysis included visual inspection, colorimetry, glossimetry, and Fourier-transform infrared spectroscopy. Each module experienced different types of degradation depending on the exposure site, even for the same material and module brand. For instance, the polyamide-based backsheet experienced hairline cracking and greater yellowing and chemical changes in China (Changsu, humid subtropical climate), while in Italy (Rome, hot-summer Mediterranean climate) it underwent macroscopic cracking and greater losses in gloss. Spectroscopic studies have permitted identification of degradation products and changes in polymer structure over time. Comparisons are made to fielded modules with fluoropolymer-based backsheets, as well as backsheet materials in accelerated laboratory exposures. Implications for qualification testing and service life prediction of the non-fluoropolymer-based backsheets are discussed.

14 SOLAR ENERGY↗

Final Report for Project DE-FG02-05ER15718 Fluoropolymers, Electrolytes, Composites and Electrodes

This report is for a project that was initiated under the title “New Proton-Conducting Fluoropolymer Electrolytes for PEM Fuel Cells”, as part of the DOE program titled “Basic Research for the Hydrogen Fuel Cell Initiative”, Program Notice DE-FG01-04ER04-20. The project received 750,000 dollars in initial funding for a three-year term with a start date of August 15, 2005. Creager was PI and co-PIs were DesMarteau and Smith, all from Clemson. The project was renewed for a second three-year term with a start date of June 15 2008, again for 750,000 dollars, with the new title, “Fluoropolymers, Electrolytes, Composites and Electrodes”. Shortly after the renewal was put in place, co-PI Smith left Clemson to accept a position at the University of Texas at Dallas. After a period of no-cost extension the project was renewed on January 1 2013 for another three-year term, this time for a smaller amount ($525,000) and with Thrasher, a new senior hire at Clemson, as co-PI in place of Smith. DesMarteau had retired from Clemson by this time but was retained as a project advisor. After a final one-year no-cost extension for calendar year 2016, the project ended on December 31, 2016, giving it an active period of eleven and one-half years, from August 15 2005 to December 31 2016. The overall objective of this research project has been to create and understand the behavior of new fluoropolymer-based electrolytes and electrodes suitable for use in electrochemical energy storage and conversion devices. The objective was pursued via research on new fluorinated monomers, new polymers and polyelectrolytes (also known as ionomers), and new electrocatalyst supports that in some cases include chemically grafted electrolytes to promote rapid ion transport to electrocatalytically active sites (usually platinum nanoparticles) on the support. The research involved synthesis and characterization of new materials, and creation and use of new measurement techniques that address key properties of the materials, e.g. mixed electronic / ionic conduction in the absence of liquid electrolyte, that are relevant to their use in energy conversion and storage.

30 DIRECT ENERGY CONVERSION↗

Developing experimental methods to measure phase change in fluoropolymer binders (Progress Summary)

Understanding fluoropolymer binder structure and aging response continues to be an important goal for the prediction and assessment of polymer bonded explosive compositions. Fluoropolymer (FP) binders are commonly only a few percent of the composite material - they are thin films that coat explosives, binding them together. Although FPs are a small fraction of the composite, they are essential for the mechanical integrity of the part. As part of ongoing efforts within NNM, we are developing new methods to quantify crystallization and chemical degradation within aged Fluoropolymer materials.

36 MATERIALS SCIENCE↗

Toxicity of Common Fluoropolymers and PFAS on C. Elegans and an Innovative Strategy to Promote in Situ Remediation - 26128

Per- and polyfluoroalkyl substances (PFAS) are a broad class of synthetic chemicals used in a variety of modern technologies and consumer products. PFAS have an alkyl backbone with all or most of the hydrogen (H) atoms replaced with fluorine (F) atoms. PFAS generally fall into one of two categories, they can be non-polymeric with relatively low molecular weights, or long-chain polymers. PFAS are a diverse group of organic compounds that can be solids, liquids, dispersions, or gases. Their mobility and toxicity are influenced by their chain lengths and functional groups. Non-polymeric PFAS are common building blocks for the manufacturing of fluoropolymers. Non-polymeric PFAS are known to be mobile in the environment and some are considered contaminants of emerging concern. Polymeric PFAS, or fluoropolymers, are typically thought to be of low concern, however few systematic investigations into their toxicity have been completed. PFAS, including fluoropolymers and microplastics, have been found in pristine environments and animals located far from site of origin including the arctic and deep ocean.

Jacobs, Stephanie [Savannah River National Laborat↗

Lithium Insertion Mechanism in Iron Fluoride Nanoparticles Prepared by Catalytic Decomposition of Fluoropolymer

Metal fluorides with high redox potential and capacity from strong metal-fluoride bonds and conversion reaction, makes them promising cathodic materials but detailed lithium insertion and extraction mechanisms have not been clearly understood and explained to date. Here we report low temperature synthesis of electrochemically active FeF3/FeF2 nanoparticles by catalytic decomposition of fluoropolymer [perfluoropolyether (PFPE)] using hydrated iron oxalate precursor in air and inert atmosphere. Freshly synthesized FeF3 nanoparticle delivered specific capacity over 210 mAh/g with decent cycling performance as a Li-ion battery cathode. Both in situ and ex situ characterization techniques were used to investigate the detailed PFPE decomposition and fluorination mechanism leading to FeF3/FeF2 formation as well as initial lithium insertion mechanism in FeF3 cathode. Specifically, a detailed understanding was investigated using thermogravimetric - mass spectroscopy (TGA-MS), X-ray diffraction (XRD), Fourier-transform infrared spectroscopy (FTIR), nuclear magnetic resonance (NMR), transmission electron microscopy (TEM), scanning electron microscopy (SEM) - energy dispersive spectroscopy (EDS), and X-ray absorption near edge structure (XANES). The novel synthesis route developed not only offers an access to electrochemically active metal fluorides but also offers a catalytic approach for decomposing highly inert fluoropolymers for environmental protection.

Li-ion Battery, cathode, FeF3, FeF2, Fluoropolumer↗

Distinct Mechanism of Anti-Corrosion and Swelling-Adhesion Modeling of Low-Dimensional Nylon-Fluoropolymer Composite Coatings

Compared to other polymers, composite coatings with fluoropolymers as the matrix have attracted considerable interest due to their mechanical performance, chemical stability, and low surface energy. Herein, we present an anticorrosion mechanism of fluoropolymer composite coatings achieved by dispersing varying amounts of polyamide 12 (PA-12) particles over a poly(vinylidene fluoride-co-hexafluoropropylene) (PVDF-HFP) matrix. The choice of PVDF-HFP as a coating matrix was driven by its superior processability and mechanical properties over Teflon, while PA-12 afforded swelling capacity, preventing electrolyte permeation, and inhibiting matrix stress crack propagation. The corrosion resistance of the coatings was assessed mainly by potentiodynamic polarization and impedance measurements while being immersed in a NaCl solution. Our electrochemical measurement findings showed that 0.75% w/w PA-12 in the PVDF-HFP matrix significantly enhanced corrosion protection even after 21 days of immersion. Microscopy, dielectric spectroscopy, surface analysis, and mechanical testing (American Society for Testing and Materials standards) corroborated the results. PVDF-HFP coatings containing a minimum percolation threshold of 0.75 wt % PA-12 with 1 mil thickness on mild steel exhibited a remarkable increase in resistance and film adhesion, and a notable corrosion rate decrease. Finite element analysis simulation with a bilinear traction-separation law confirmed the swelling mechanism and adhesion behavior. Finally, this study highlights the potential of nylon particle dispersion in PVDF-HFP matrices as a practical approach to developing advanced anticorrosion coatings with promising practical applications in various industries.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Failure Analysis of a New Polyamide-Based Fluoropolymer-Free Backsheet After Combined-Accelerated Stress Testing

The viability of novel coextruded, fluoropolymer-free backsheets for photovoltaic (PV) modules has been questioned as a result of a large number of early-life backsheet failures in PV installations containing one of the earliest co-extruded polyamide (PA)-based backsheet to reach the market, “AAA.” New PV reliability testing protocols have been recently developed and applied to backsheets to reproduce failures observed in the field and evaluate the durability of novel backsheet materials and designs prior to commercialization. A new co-extruded PA-based backsheet was tested using combined-accelerated stress testing (C-AST) and demonstrated a greater lifetime than AAA, and some other fluoropolymer-based backsheets such as polyvinylidene fluoride. The improved PA-based backsheet also eventually failed by through-thickness cracking. Using surface and bulk material characterization techniques, we performed a comprehensive study of material properties before and after the stress testing. Aging of the backsheet resulted in an increase of surface roughness by erosion of the outer PA layer. However the failure is more likely related to an increase in crystallinity of the polyolefin core layer reducing the backsheet tearing energy. The analysis can ultimately inform on the specific weaknesses of the materials so that the manufacturer can improve the backsheet design to extend its lifetime.

14 SOLAR ENERGY↗

Progress Summary: Developing experimental methods to quantify the degree of crystallinity in fluoropolymer binders

Understanding fluoropolymer binder structure and aging response continues to be an important goal for the prediction and assessment of polymer bonded explosive compositions within the stockpile. As part of ongoing efforts within NNM, we are developing new methods to quantify crystallization and chemical degradation within aged Fluoropolymer materials.

36 MATERIALS SCIENCE↗

Fluoropolymer Aging Assessments

Fluoropolymer (FP) binders are commonly only a few percent of polymer bonded explosive compositions but they are essential for the mechanical integrity of the part. Because we are using newly manufactured binders, we need to understand how lot variations might affect processing, aging, and mechanical properties. Time, temperature and radiation induce phase changes in fluoropolymers. These phase changes can rearrange the polymer causing crystalline domains to nucleate and grow that can alter mechanical properties. These studies quantify the aging process so that it may be cross correlated with changes in the adhesion, strength, and other properties important for performance.

36 MATERIALS SCIENCE↗