Search NASA⌕ Search

SEARCH · Search NASA

Results for “Fracture instability”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Integrated simulation, machine learning, and experimental approach to characterizing fracture instability in indentation pillar-splitting of materials

Measuring fracture toughness of materials at small scales remains challenging due to limited experimental testing configurations. A recently developed indentation pillar-splitting method has shown promise of improved flexibility in fracture toughness measurements at the microscale, partly due to the occurrence of an unusual fracture instability, i.e., a transition from stable to unstable crack propagation. In spite of growing interest in this method, the underlying mechanism of this phenomenon is yet to be elucidated. Furthermore, we provide a comprehensive description of fracture instability in indentation pillar-splitting by combining in situ experiments with high-fidelity simulations based on cohesive zone and J-integral methods. In addition, a machine-learning-based solution for predicting the critical indentation load of fracture instability is established through Gaussian processes regression for broad use of this method by the community.

36 MATERIALS SCIENCE↗

Phase instability-coupled fracture behavior in garnet LLZO solid electrolytes: a machine learning-enabled atomistic study

Fracture in the garnet-type solid electrolyte Li 7 La 3 Zr 2 O 12 (LLZO) poses a critical threat to both the performance and safety of solid-state batteries. To unravel the coupled chemomechanical processes that govern fracture in LLZO under external loading, we carry out large-scale molecular-dynamics simulations with a validated machine-learning force field. Our results demonstrate that triaxial stresses at crack flanks trigger a localized cubic-to-tetragonal phase transformation, which is accompanied by Li-ion rearrangement. The emergent tetragonal domains feature lattice contraction normal to the fracture plane, imposing coherent misfit strains that provide an additional driving force for further crack propagation. Crucially, introducing Li deficiencies stabilizes the cubic phase, postponing the phase transition and thereby delaying fracture initiation. These findings highlight the role of intrinsic phase instability in dictating LLZO's fracture resistance and its critical connection to local Li concentration. This chemomechanical coupling points toward targeted strategies to enhance the mechanical robustness of garnet electrolytes, including tuning Li content, ensuring dopant homogeneity, and refining processing protocols.

Materials science↗

Crack Growth Rate and Fracture Toughness of Stainless Steel Welds in Light Water Reactor Environment

Austenitic stainless steel welds play a crucial role in maintaining the structural integrity of light water reactors. Within the reactor core, stainless steel welds endure a harsh service environment including elevated temperature, corrosive coolant, and intense neutron irradiation. Long-term exposure to such a severe service environment could lead to performance degradation. To ensure the safe and economic operation of light water reactors, this study performed crack growth rate and fracture toughness tests on irradiated and thermally aged weld samples harvested from decommissioned reactor components. In a low-corrosion-potential environment, stainless steel welds showed resistance to stress corrosion cracking, and the measured crack propagation rates were comparable to those of wrought stainless steels under similar test conditions. However, a marked decline in fracture toughness was observed in weld samples, particularly in irradiated samples. Fracture instability was observed at ~0.8 dpa, significantly lower than those observed in wrought stainless steels. Further research at higher doses is needed to evaluate the dose dependence of irradiation-induced embrittlement, and to understand the interplay between thermal aging and neutron irradiation in stainless steel welds.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

EXPERIMENTAL EVALUATION OF ULTRASONIC VELOCITIES AND ANISOTROPY IN THE TUSCALOOSA MARINE SHALE FORMATION

Tuscaloosa Marine Shale (TMS) formation is a clay- and organic-rich emerging shale play with a considerable amount of hydrocarbon resources. Despite the substantial potential, there have been only a few wells drilled and produced in the formation over the recent years. The analyzed TMS samples contain an average of 50 wt% total clay, 27 wt% quartz and 14 wt% calcite and the mineralogy varies considerably over the small intervals. The high amount of clay leads to pronounced anisotropy and the frequent changes in mineralogy result in the heterogeneity of the formation. We studied the compressional (V P ) and shear-wave (V S ) velocities to evaluate the degree of anisotropy and heterogeneity, which impact hydraulic fracture growth, borehole instabilities, and subsurface imaging. The ultrasonic measurements of P- and S-wave velocities from five TMS wells are the best fit to the linear relationship with R 2 = 0.84 in the least-squares criteria. We observed that TMS S-wave velocities are relatively lower when compared to the established velocity relationships. Most of the velocity data in bedding-normal direction lie outside constant V P /V S lines of 1.6–1.8, a region typical of most organic-rich shale plays. For all of the studied TMS samples, the S-wave velocity anisotropy exhibits higher values than P-wave velocity anisotropy. In the samples in which the composition is dominated by either calcite or quartz minerals, mineralogy controls the velocities and V P /V S ratios to a great extent. Additionally, the organic content and maturity account for the velocity behavior in the samples in which the mineralogical composition fails to do so. The results provide further insights into TMS Formation evaluation and contribute to a better understanding of the heterogeneity and anisotropy of the play.

Geochemistry & Geophysics↗

Graphene coating on silicon anodes enabled by thermal surface modification for high-energy lithium-ion batteries

Silicon is a high-energy density anode material for lithium-ion batteries, but it possesses shortcomings such as poor electronic conductivity, interfacial instability and mechanical fracturing that hinder its battery cycling. Carbon coating has been an important strategy for stabilizing silicon anodes, but the effects of the silicon surface properties on carbon coating morphology and the consequent silicon cycling stability have not been clearly elucidated. Herein, we find that thermal oxidation of the silicon anodes followed by chemical vapor deposition of carbonaceous precursors leads to a well-ordered graphene coating, whereas disordered graphite coating is formed on the native silicon surface. Graphene-coated silicon exhibits superior cycling performance, retaining a discharge capacity of ~1300 mAh g -1 after 300 cycles, whereas the disordered graphite-coated silicon suffers continuous degradation, retaining only~600 mAh g -1 after 300 cycles. Cryogenic electron microscopy reveals the mechanism behind the difference in cycling stabilities; graphene coated silicon is able to withstand the large mechanical strains induced during extended cycling, whereas disordered graphite coating is ruptured, exposing silicon surfaces to the electrolyte, leading to extensive buildup of SEI and poor cycling performance. Characterization of the silicon surface reveals that thermal treatment yields an oxygen-rich surface layer, which is hypothesized to play a decisive role in dictating the carbon coating. This work highlights the effect of silicon surface properties on carbon coating microstructure, and presents thermal treatment as a facile avenue to attain graphene coating on silicon anodes.

25 ENERGY STORAGE↗

A study of adhesive bonding in metal–metal, metal–CFRP, and CFRP–CFRP material combinations under shear deformation: Fracture morphologies and damage mechanisms

Safe design of adhesive joining in multi-materials in engineered structures requires the accumulation of numerous experimental data on the failure behavior of various adhesively-bonded material combinations under different loading conditions. The deep understanding of mechanical performance, fracturing morphologies, and main damage mechanisms is also quintessential for accelerating the development of proper physics-based and multi-scale models for assisting the design. Towards this goal, this work presents a comprehensive characterization of the failure behavior of adhesively-bonded metal–metal, metal–CFRP, and CFRP–CFRP material combinations under global shear deformation via single lap shear testing. Thanks to a synergistic combination of measurement methods by using Digital Imaging Correlation (DIC) and 3D optical profilometry, adhesive features on the adherend after failure were quantified and the main progressive damage mechanisms were identified. The characterization performed in this work provides quantitative data that contributes to a better understanding of shear failure in adhesive bonding across different bi-material combinations. Finally, the obtained results have practical implications, including the potential to enhance adhesive bonding design, identify failure causes in adhesive joints, and develop or validate computational models capable of capturing the observed behavior in various adhesively-bonded materials under global shear deformation.

36 MATERIALS SCIENCE↗

On the Cutting of Metals: A Mechanics Viewpoint

The mechanics of large-strain deformation in cutting of metals is discussed, primarily from viewpoint of recent developments in in situ analysis of plastic flow and microstructure characterization. It is shown that a broad range of deformation parameters can be accessed in chip formation—strains of 1–10, strain rates of 10–10 5 /s, and temperatures up to 0.7T m —and controlled. This range is far wider than achievable by any other single-stage, severe plastic deformation (SPD) process. The resulting extreme deformation conditions produce a rich variety of microstructures in the chip. Four principal types of chip formation—continuous, shear-localized, segmented, and mushroom-type—as elucidated first by Nakayama (1974, “The Formation of ‘Saw-Toothed Chip’ in Metal Cutting,” Proceedings of International Conference on Production Engineering, Tokyo, pp. 572–577) are utilized to emphasize the diverse plastic flow phenomena, especially unsteady deformation modes that prevail in cutting. These chip types are intimately connected with the underlying flow, each arising from a distinct mode and triggered by an instability phenomenon. The role of plastic flow instabilities such as shear banding, buckling, and fracture in mediating unsteady flow modes is expounded, along with consequences of the flow modes and chip types for the cutting. Sinuous flow is shown to be the reason why gummy (highly strain-hardening) metals, although relatively soft, are so difficult to cut. Synthesizing the various observations, a hypothesis is put forth that it is the stability of flow modes that determines the mechanics of cutting. Furthermore, this leads to a flow-stability phase diagram that could provide a framework for predicting chip types and process attributes.

42 ENGINEERING↗

Revisiting the first Sandia Fracture Challenge with transient deformation heating and strain localization considerations

In this study, we present a systematic experimental study and accompanying theoretical analysis of the dependence of ductile fracture on strain localization, strain hardening rates, deformation-induced thermal softening, and transient heat conduction under spatially uniform as well as spatially heterogeneous deformation. Spatially uniform cases are studied via standard dogbone shaped specimens subject to uniaxial tension. Spatially heterogeneous deformation is studied via the so-called Sandia Fracture Challenge (SFC) specimen, which is a standard compact tension specimen modified with three machined holes in front of a blunt notch. We utilize the same precipitation hardened martensitic stainless steel used in the first SFC experiments, i.e. 15-5 PH with an H1075 heat treatment. We also study 15-5 PH in Condition A and with the H900 heat treatment, each of which has a different hardening behavior and ductility. We find that the ductility does not correlate with the deformation to first crack initiation in the SFC specimen. Instead, hardening rates are better correlated. Moreover, a re-examination finds that an accurate calibration of the hardening rates is strongly correlated with accurate blind predictions of ductile fracture in the SFC specimens. Given that thermal softening can greatly affect hardening rates, we provided a thermographic analysis of deformation-induced heating and transient heat transfer in both the dogbone shaped samples and the SFC specimens. Transient heating in stainless steels is found to have first-order effects on the strain at the onset of necking, strain to fracture, as well as strain localization and ductile fracture in complex geometries even under so-called quasi-static loading rates.

42 ENGINEERING↗

Irradiation hardening and ductility loss of Eurofer97 steel variants after neutron irradiation to ITER-TBM relevant conditions

Ten Eurofer97 steel variants, produced by non-standard fabrication-processing routes and modified alloying chemistries, were studied by neutron irradiations in the high flux isotope reactor. The irradiations were performed to ITER-TBM relevant conditions of ~255–350 °C, 2.94–3.24 dpa. We quantified the irradiation-induced degradation of the steels using mechanical property tests. All the steels suffered from irradiation hardening, where a significant increase in Vickers microhardness and yield stress (σ YS ) occurred, accompanied with severe loss of tensile elongation. The extent of hardening was material dependent. For T irr = 300±30 °C, most steels showed σ YS increase in the range of ~30% to as high as ~66%, except for a low temperature tempered steel with σYS increase below 15%. Despite large losses in elongation, most failures were ductile. Significant post-necking ductility was retained with reduction in area (RA) between 65–75%, but <50% for low temperature tempered steels. The ultimate tensile stress to yield stress (σ UTS /σ YS ) ratios decreased significantly after irradiation, highlighting irradiation-induced strain hardening capacity reduction. No major effect of irradiation on the plastic instability stress (σ PIS ) and true fracture stress of the steels was observed. By comparing the tensile stresses in true stress units and with literature, the results suggest that RAFM steel designing should target materials with a large separation between σ PIS and σ YS , to ensure the materials can maintain large work hardening and uniform deformation capability after irradiation. The tensile data of the steels additionally revealed a compelling evidence of an inverse trend between the change in RA and increase in σ YS of the neutron irradiated Eurofer97 type steels.

36 MATERIALS SCIENCE↗

Exceptional fracture toughness of CrCoNi-based medium- and high-entropy alloys at 20 kelvin

Medium- and high-entropy alloys based on the CrCoNi-system have been shown to display outstanding strength, tensile ductility and fracture toughness (damage-tolerance properties), especially at cryogenic temperatures. Here we examine the J Ic and (back-calculated) K JIc fracture toughness values of the face-centered cubic, equiatomic CrCoNi and CrMnFeCoNi alloys at 20 K. At flow stress values of ~1.5 GPa, crack-initiation K JIc toughnesses were found to be exceptionally high, respectively 235 and 415 MPa√m for CrMnFeCoNi and CrCoNi, with the latter displaying a crack-growth toughness K ss exceeding 540 MPa√m after 2.25 mm of stable cracking, which to our knowledge is the highest such value ever reported. Characterization of the crack-tip regions in CrCoNi by scanning electron and transmission electron microscopy reveal deformation structures at 20 K that are quite distinct from those at higher temperatures and involve heterogeneous nucleation, but restricted growth, of stacking faults and fine nanotwins, together with transformation to the hexagonal closed-packed phase. The coherent interfaces of these features can promote both the arrest and transmission of dislocations to generate respectively strength and ductility which strongly contributes to sustained strain hardening. Indeed, we believe that these nominally single-phase, concentrated solid-solution alloys develop their fracture resistance through a progressive synergy of deformation mechanisms, including dislocation glide, stacking-fault formation, nano-twinning and eventually in situ phase transformation, all of which serve to extend continuous strain hardening which simultaneously elevates strength and ductility (by delaying plastic instability), leading to truly exceptional resistance to fracture.

36 MATERIALS SCIENCE↗

Crack Stability in Breached Fuel

This report describes the fracture mechanics formalism to evaluate the stability of cracks in a fuel cladding. Recognized consensus-body linear elastic fracture mechanics (LEFM) was applied to identify the crack instability length, or the length at which unstable mechanical crack extension would occur, as a function of pellet swelling loading (radial strain and fraction conversion from UO 2 to U 3 O 8 ) at the local cracked cladding region for two postulated fracture toughness (K IC ) values of the cladding. The crack opening displacement (COD) and the crack opening area (COA) were also identified. This analysis informs evaluations for crack extension and the potential for pellet debris loss from the fuel rod for cases of pellet oxidation in dry storage canisters where inadvertent residual water may undergo radiolysis causing oxidizing conditions to pellets exposed to the canister environment through breached cladding.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Crack Stability in Breached Fuel

This report describes the fracture mechanics formalism to evaluate the stability of cracks in a fuel cladding. Recognized consensus-body linear elastic fracture mechanics (LEFM) was applied to identify the crack instability length, or the length at which unstable mechanical crack extension would occur, as a function of pellet swelling loading (radial strain and fraction conversion from UO 2 to U 3 O 8 ) at the local cracked cladding region for two postulated fracture toughness (K IC ) values of the cladding. The crack opening displacement (COD) and the crack opening area (COA) were also identified. This analysis informs evaluations for crack extension and the potential for pellet debris loss from the fuel rod for cases of pellet oxidation in dry storage canisters where inadvertent residual water may undergo radiolysis causing oxidizing conditions to pellets exposed to the canister environment through breached cladding.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Simulating Fracture Sealing by Granular LCM Particles in Geothermal Drilling

Lost circulation occurs when the returned fluid is less than what is pumped into the well due to loss of fluid to pores or fractures. A lost-circulation event is a common occurrence in a geothermal well. Typical geothermal reservoirs are often under-pressured and have larger fracture apertures. A severe lost-circulation event is costly and may lead to stuck pipe, well instability, and well abandonment. One typical treatment is adding lost-circulation materials (LCMs) to seal fractures. Conventional LCMs fail to properly seal fractures because their mechanical limit is exceeded at elevated temperatures. In this paper, parametric studies in numerical simulations are conducted to better understand different thermal effects on the sealing mechanisms of LCMs. The computational fluid dynamics (CFDs) and the discrete element method (DEM) are coupled to accurately capture the true physics of sealing by granular materials. Due to computational limits, the traditional Eulerian–Eulerian approach treats solid particles as a group of continuum matter. With the advance of modern computational power, particle bridging is achievable with DEM to track individual particles by modeling their interactive forces between each other. Particle–fluid interactions can be modeled by coupling CFD algorithms. Fracture sealing capability is investigated by studying the effect of four individual properties including fluid viscosity, particle size, friction coefficient, and Young’s modulus. It is found that thermally degraded properties lead to inefficient fracture sealing.

15 GEOTHERMAL ENERGY↗

Measurement of Deformation Heterogeneity During Shale Swelling Using Digital Image Correlation

Abstract Rock-fluid interactions in shale formations are one of the main sources of wellbore instability issues and inadequate stimulation performance. For better planning of fracturing operations and optimizing production from these reservoirs, it is important to understand the mechanisms behind these interactions. These issues are especially prevalent in clay-rich shales, such as Tuscaloosa Marine Shale, which is the subject of this study. Conventional techniques to quantify these shale-fluid interactions comprise of measuring swelling in powdered rock grains or measurement of deformation in the whole pieces of the core using a linear variable differential transformer and strain gages. However, the contribution from individual laminae to overall deformation cannot be evaluated using these methods. In this study, we developed an experimental setup to evaluate the spatial deformation in shale during interaction with water using digital image correlation (DIC). Deformation of two shale samples, with 34 wt% to 51 wt% clay content, was studied. White paint was used to generate a random speckle pattern on the specimen and then immersed in deionized water. The deformation process was captured using a digital camera and images were analyzed using DIC to quantify the deformation. The implementation of the DIC technique enables the visualization and quantification of spatial deformation in the specimen during interacting with water. The results show the localization of large strains in select laminations. The results provide a better understanding of shale deformation when interacting with water in comparison to traditional measurements that can provide only an average strain value.

Energy & Fuels↗

Phenomenological Model of Nonlinear Dynamics and Deterministic Chaotic Gas Migration in Bentonite: Experimental Evidence and Diagnostic Parameters

Understanding gas migration in compacted clay materials, e.g., bentonite and claystone, is important for the design and performance assessment of an engineered barrier system of a radioactive waste repository system, as well as many practical applications. Existing field and laboratory data on gas migration processes in low-permeability clay materials demonstrate the complexity of flow and transport processes, including various types of instabilities, caused by nonlinear dynamics of coupled processes of liquid–gas exchange, dilation, fracturing, fracture healing, etc., which cannot be described by classical models of fluid dynamics in porous media. We here show that the complexity of gas migration processes can be explained using a phenomenological concept of nonlinear dynamics and deterministic chaos theory. To do so, we analyzed gas pressure and gas influx (i.e., input) and outflux (i.e., output), recorded during the gas injection experiment in the compact Mx80-D bentonite sample, and calculated a set of the diagnostic parameters of nonlinear dynamics and chaos, such a global embedding dimension, a correlation dimension, an information dimension, and a spectrum of Lyapunov exponents, as well as plotted 2D and 3D pseudo-phase-space strange attractors, based on the univariate influx and outflux time series data. These results indicate the presence of phenomena of low-dimensional deterministic chaotic behavior of gas migration in bentonite. In particular, during the onset of gas influx in the bentonite core, before the breakthrough, the development of gas flow pathways is characterized by the process of chaotic gas diffusion. After the breakthrough, with inlet-to-outlet movement of gas, the prevailing process is chaotic advection. During the final phase of the experiment, with no influx to the sample, the relaxation pattern of gas outflux is resumed back to a process of chaotic diffusion. The types of data analysis and a proposed phenomenological model can be used to establish the basic principles of experimental data-gathering, modeling predictions, and a research design.

36 MATERIALS SCIENCE↗

Fifth-degree elastic energy for predictive continuum stress–strain relations and elastic instabilities under large strain and complex loading in silicon

Materials under complex loading develop large strains and often phase transformation via an elastic instability, as observed in both simple and complex systems. Here, we represent a material (exemplified for Si I) under large Lagrangian strains within a continuum description by a 5th-order elastic energy found by minimizing error relative to density functional theory (DFT) results. The Cauchy stress—Lagrangian strain curves for arbitrary complex loadings are in excellent correspondence with DFT results, including the elastic instability driving the Si I → II phase transformation (PT) and the shear instabilities. PT conditions for Si I → II under action of cubic axial stresses are linear in Cauchy stresses in agreement with DFT predictions. Such continuum elastic energy permits study of elastic instabilities and orientational dependence leading to different PTs, slip, twinning, or fracture, providing a fundamental basis for continuum physics simulations of crystal behavior under extreme loading.

36 MATERIALS SCIENCE↗

Fifth-degree elastic energy for predictive continuum stress-strain relations and elastic instabilities under large strain and complex loading in silicon

Materials under complex loading develop large strains and often phase transformation via an elastic instability, as observed in both simple and complex systems. Here, we represent a material (exemplified for Si I) under large Lagrangian strains within a continuum description by a 5th-order elastic energy found by minimizing error relative to density functional theory (DFT) results. The Cauchy stress—Lagrangian strain curves for arbitrary complex loadings are in excellent correspondence with DFT results, including the elastic instability driving the Si I → II phase transformation (PT) and the shear instabilities. PT conditions for Si I → II under action of cubic axial stresses are linear in Cauchy stresses in agreement with DFT predictions. Such continuum elastic energy permits study of elastic instabilities and orientational dependence leading to different PTs, slip, twinning, or fracture, providing a fundamental basis for continuum physics simulations of crystal behavior under extreme loading.

Levitas, Valery↗

Linking constituent phase properties to ductility and edge stretchability of two DP 980 steels

Two DP 980 steels were characterized with multiple methods to determine its microstructure characteristics, tensile properties and edge stretchability. The first (DP980-B) is a commercial grade DP980 steel produced by AK Steel, while the second (DP980-T) is a modification of the first one by a tempering process. Both contain two individual phases: ferrite and martensite with body centered cubic (BCC) and tetragonal (BCT) crystal structure respectively. ASTM standard tensile tests were performed for both materials, revealing that DP980-B has higher work hardening and larger total elongation than DP980-T. Standard hole piercing and subsequent hole expansion and extrusion tests were also performed. The critical hole expansion ratio (HER) of hole pierced sheet at different nominal clearances, on the other hand, show an opposite trend: the HER of DP980-T almost doubles that of DP980-B. This indicates the tensile ductility and edge stretchability are determined by different mechanisms due to different deformation modes. The ductility of sheet metal during uniaxial tension is determined by deformation instability, i.e. necking, due to less constraint at the region of deformation and fracture will occur quickly after necking. The contribution of post-necking deformation to the total elongation is insignificant for the high strength grades such as DP980 steels. The ductility during hole-expansion, however, is mainly determined by material fracture behavior that is dependent on phase property disparity and material intrinsic fracture parameters. With the individual phase properties for both DP steels determined by in situ tensile tests under high energy X-ray diffraction, the results show that DP980-T steel has lower property disparities between the two phases than DP980-B steel, due to the tempering process. This explains why the DP980-T steel has higher HER than DP980-B steel: lower phase disparity will lead to less local deformation during loading. The higher work hardening rate for DP980-B steel contributes to its higher uniform elongation compared with DP980-T steel based on the maximum load condition of deformation instability. An integrated finite element simulation framework for studying hole expansion is also presented here, based on the calculated individual phase properties from the combined high energy x-ray diffraction (HEXRD) and elastic plastic self-consistent modeling. The simulation results correlate well with the experimental results on the HER difference between the two materials.

36 MATERIALS SCIENCE↗