Photoinduced and thermal reactions involving hydrogen in high-germania-core optical fibres
We report a Raman scattering study of photoinduced and thermal reactions between H{sub 2} and germanosilicate optical fibres with 22 mol % and 97 mol % GeO{sub 2} in the core (F1 and F2, respectively) after H{sub 2} loading at 150 MPa (1500 atm). The mechanisms of photoreactions are investigated in a wide range of incident laser wavelengths (244, 333, 354, 361 and 514 nm). Thermal reactions are studied at 500 {sup 0}C. The results indicate that the main mechanism behind the formation of hydrogen-containing defects with Raman bands at 700, 750, 2190, 3600 and 3680 cm{sup -1} involves {identical_to}Ge-O-Ge{identical_to} or {identical_to}Ge-O-Si{identical_to} bond breaking and formation of hydride and hydroxyl species: =GeH{sub 2} (700, 750 cm{sup -1}), {identical_to}Ge-H (2190 cm{sup -1}), {identical_to}GeO-H (3600 cm{sup -1}) and {identical_to}SiO-H (3680 cm{sup -1}). The key features of the reactions in the F1 and F2 fibres are analysed. In particular, photoinduced reactions give {identical_to}Si-OH groups only in the F1 fibres, whereas the formation of germanium nanoclusters at a relatively low temperature ({approx}500 {sup 0}C) or {identical_to}GeO-H and {identical_to}Ge-H defects under 514-nm irradiation has only been observed in the F2 fibres. (optical fibres)