Strain effects and microstructural evolution in Ge-Si system materials prepared by ion implantation and by ultrahigh vacuum chemical vapor deposition

Appropriately utilizing some microstructures may be very helpful to acquire desirable Ge-Si system materials. In this work, the Ge-Si system materials have been prepared either by ion implantation or ultrahigh vacuum chemical vapor deposition (UHVCVD). The interesting microstructures including half-loop dislocations, SiGe nanoclusters, and dislocation dipoles have been found in these two kinds of Ge-Si system materials. It is demonstrated that the evident surface strain state and adequate surface layer quality have been realized by employing these microstructures. Compared with the dipole dislocations in the Ge-Si systems deposited by UHVCVD on the compliant silicon on insulator, the half-loop dislocations and the SiGe nanoclusters induced by Ge ion implantation and subsequent annealing can relax the SiGe layer more effectively and lead to relatively large strain in the surface silicon. It may provide some new approaches to the control of misfit strains for fabricating desirable Ge-Si system materials.

36 MATERIALS SCIENCE↗

The distribution of Ga and Sb impurities in Ge-Si crystals grown by the Bridgman method using a feeding rod

Gallium- and antimony-doped Ge{sub 1-x}Si{sub x} crystals (0 {<=} x {<=} 0.25) have been grown by the improved Bridgman method using a silicon seed and a macrohomogeneous feeding Ge-Si rod of the corresponding composition. The impurity concentration profiles along the grown crystals were determined from Hall measurements. The mathematical problem of impurity distribution along two-component mixed crystals grown from a melt with uniform and graded composition is solved in the Pfann approximation and within the virtual-crystal model for the solid solution. It is shown that the experimental impurity distributions in Ge{sub 1-x}Si{sub x} crystals are described well by the data calculated on the assumption of linear change in the impurity segregation coefficient with the crystal composition.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Concerning the energy levels of silver in Ge-Si alloys

The emission from impurity states of silver (an element of the IB subgroup) in a Ge-Si alloy, containing 18 at % Si, has been studied. The donor level of silver has been found in crystals doubly doped with gallium and silver, while its first acceptor level has been revealed in crystals doped with only silver. Single crystals were grown by pulling from a melt using a feeding rod. Doping with gallium was performed by introducing this element into the feeding rod, and silver was introduced into the crystals via diffusion. The positions of the donor and first acceptor Ag levels with respect to the top of the valence band were found by analyzing the temperature dependence of the Hall coefficient and the electroneutrality equation for the crystal: 0.06 and 0.29 eV, respectively.

36 MATERIALS SCIENCE↗

Band engineered epitaxial Ge-Si{sub x}Ge{sub 1-x} core-shell nanowire heterostructures

We report the growth of germanium (Ge)-silicon-germanium (Si{sub x}Ge{sub 1-x}) epitaxial core-shell nanowire (NW) heterostructures, with tunable Si and Ge shell content. The Ge NWs are grown using the vapor-liquid-solid growth mechanism, and the Si{sub x}Ge{sub 1-x} shells are grown in situ, conformally on the Ge NWs using ultrahigh vacuum chemical vapor deposition. We use transmission electron microscopy to demonstrate epitaxial shell growth, and scanning energy dispersive x-ray spectroscopy to determine the shell thickness and content. The Si and Ge shell content can be tuned depending on the SiH{sub 4} and GeH{sub 4} partial pressures during the shell growth, enabling band engineered core-shell NW heterostructures.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Electroactive complex in thermally treated Ge-Si crystals

It is shown by Hall measurements that quenching complexly doped Ge{sub 1-x}Si{sub x} (0 {<=} x {<=} 0.20) crystals from 1050-1080 K leads to the formation of additional electroactive acceptor centers in them. The activation energy of these centers increases linearly with an increase in the silicon content in the crystal and is described by the relation E{sub k}{sup x} = (52 + 320x) meV. Annealing these crystals at 550-570 K removes the additional acceptor levels. It is established that the most likely model for the additional electroactive centers is a pair composed of substituent copper and aluminum atoms (Cu{sub s}Al{sub s}) or interstitial copper and substituent aluminum atoms (Cu{sub i}Al{sub s}). It is shown that the generation of additional deep acceptor levels must be taken into account when using the method of precise doping of Ge{sub 1-x}Si{sub x} crystals with copper.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Controlling Axial p-n Heterojunction Abruptness Through Catalyst Alloying in Vapor-Liquid-Solid Grown Semiconductor Nanowires

The p-n junction can be regarded as the most important electronic structure that is responsible for the ubiquity of semiconductor microelectronics today. Efforts to continually scale down the size of electronic components is guiding research to explore the use of nanomaterials synthesized from a bottom-up approach - group-IV semiconductor nanowires being one such material. However, Au-catalyzed synthesis of Si/Si1-x-Gex semiconductor nanowire heterojunctions using the commonly-used vapor-liquid-solid (VLS) growth technique results in diffuse heterojunction interfaces [1], leading to doubts of producing compositionally-sharp p-n junctions using this approach. However, we have recently reported the ability to increase Ge-Si nanowire heterojunction abruptness by VLS synthesis from a Au(1-x)Ga(x) catalyst alloy as shown by EDX analysis in an SEM [2]. In this work, we have extended the use of a AuGa catalyst alloy to produce more compositionally abrupt p-n junction interfaces compared to using pure Au as directly measured by atom probe tomography. As shown in Figure 1(a-b), individual Ge-Si heterostructured nanowires were grown vertically atop Ge(111) microposts. Direct growth on the microposts provides a facile approach to nanowire analysis which circumvents the need to use FIB-based sample preparation techniques. Both nanowires grown from pure Au and a AuGa catalyst alloy were analyzed. The corresponding 3D APT reconstruction of an individual heterostructured nanowire is shown in Figure 1(c) with the corresponding materials labeled. A 1-dimensional composition profile along the analysis direction in Figure 1(d) confirms an increase in heterojunction abruptness for nanowires grown from AuGa (~10nm) compared to nanowires grown from pure Au (~65nm). Analysis of the P distribution within the Si region (Figure 1(e)) indicates that P reaches a constant distribution over approximately 10nm when incorporated through the AuGa catalyst, whereas it continually increases over 100’s of nanometers when incorporated through pure Au. The apparent lower overall P concentration within the nanowire grown from the AuGa alloy suggests that the solubility of P in the alloy is lower compared to pure Au. The ability to controllably increase nanowire p-n junction abruptness is important for nanowire applications as solar cells and tunneling field effect transistors where an increase in device performance is expected from shaper p-n junction interfaces. [1] T.E. Clark et al., Nano Lett. 8 (2008) 1246. [2] D.E. Perea et al., Nano Lett. 11 (2011) 3117. [3] The research was supported through the user program at both the Center for Integrated Nanotechnologies at Los Alamos National Laboratory and the Environmental Molecular Sciences Laboratory at Pacific Northwest National Laboratory.

Environmental Molecular Sciences Laboratory↗

Catalyst Composition and Impurity-dependent Kinetics of Nanowire Heteroepitaxy

The mechanisms and kinetics of axial Ge-Si nanowire heteroepitaxial growth based on the tailoring of the Au catalyst composition via Ga alloying are studied by environmental transmission electron microscopy combined with systematic ex-situ CVD calibrations. The morphology of the Ge-Si heterojunction, in particular the extent of a local, asymmetric increase in nanowire diameter, is found to depend on the Ga composition of the catalyst, on the TMGa precursor exposure temperature, and on the presence of dopants. To rationalize the findings, a general nucleation-based model for nanowire heteroepitaxy is established which is anticipated to be relevant to a wide range of material systems and device-enabling heterostructures.

Environmental Molecular Sciences Laboratory↗

Oxide-Free Three-Dimensional Germanium/Silicon Core–Shell Metalattice Made by High-Pressure Confined Chemical Vapor Deposition

Metalattices are crystalline arrays of uniform particles in which the period of the crystal is close to some characteristic physical length scale of the material. In this work, we explore the synthesis and properties of a germanium metalattice in which the similar to 70 nm periodicity of a silica colloidal crystal template is close to the similar to 24 nm Bohr exciton radius of the nanocrystalline Ge replica. The problem of Ge surface oxidation can be significant when exploring quantum confinement effects or designing electronically coupled nanostructures because of the high surface area to volume ratio at the nanoscale. To eliminate surface oxidation, we developed a coreshell synthesis in which the Ge metalattice is protected by an oxide-free Si interfacial layer, and we explore its properties by transmission electron microscopy (TEM), Raman spectroscopy, and electron energy loss spectroscopy (EELS). The interstices of a colloidal crystal film grown from 69 nm diameter spherical silica particles were filled with polycrystalline Ge by high-pressure confined chemical vapor deposition (HPcCVD) from GeH4. After the SiO2 template was etched away with aqueous HF, the Ge replica was uniformly coated with an amorphous Si shell by HPcCVD as confirmed by TEM-EDS (energy-dispersive X-ray spectroscopy) and Raman spectroscopy. Formation of the shell prevents oxidation of the Ge core within the detection limit of XPS. The electronic properties of the core-shell structure were studied by accessing the Ge 3d edge onset using STEM-EELS. A blue shift in the edge onset with decreasing size of Ge sites in the metalattices suggests quantum confinement of the Ge core. The degree of quantum confinement of the Ge core depends on the void sizes in the template, which is tunable by using silica particles of varying size. The edge onset also shows a shift to higher energy near the shell in comparison with the Ge core. This shift along with the observation of Ge-Si vibrational modes in the Raman spectrum indicate interdiffusion of Ge and Si. Both the size of the voids in the template and core-shell interdiffusion of Si and Ge can in principle be tuned to modify the electronic properties of the Ge metalattice.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of Si interlayers on the magnetic and mechanical properties of Fe/Ge neutron polarizing multilayer mirrors

The neutron polarizing supermirror is one of the most important optical devices for polarizing neutron beams. To meet a variety of research demands, neutron polarizing supermirrors need to display high polarization efficiencies at low external magnetic fields. Fe/Si and Fe/Ge multilayers are typically used in neutron polarizing supermirrors because the contrast in scattering length densities almost vanishes for spin-down neutrons. The Fe/Si/Ge/Si multilayer, obtained by adding thin interlayers of Si to an Fe/Ge multilayer, is effective in reducing the external field strength necessary to achieve efficient neutron polarization. To gain insight into the mechanism that controls the required external field strength for a neutron polarizing supermirror, we investigated the magnetic and mechanical properties of Fe/Si, Fe/Ge, and Fe/Si/Ge/Si multilayers. The external field strength required to achieve efficient neutron polarization was found to be proportional to the compressive film stress. The compressive stress of the Fe/Si/Ge/Si multilayer was smaller by a factor of 4.4 and 2.7 than that of Fe/Si and Fe/Ge multilayers, respectively. These measurements and analyses showed that a reduction in the compressive film stress in the Fe/Si/Ge/Si multilayer permits the use of lower external field strength to achieve efficient neutron polarization. X-ray photoelectron spectroscopic studies showed that the formation of a Ge-Si solid solution in the Ge layer may explain the marked reduction in compressive stress in the case of the Fe/Si/Ge/Si multilayer. This study confirmed that a reduction in compressive film stress is very important for a high-performance neutron polarizing supermirror.

36 MATERIALS SCIENCE↗

Engineering Heteromaterials to Control Lithium Ion Transport Pathways

Safe and efficient operation of lithium ion batteries requires precisely directed flow of lithium ions and electrons to control the first directional volume changes in anode and cathode materials. Understanding and controlling the lithium ion transport in battery electrodes becomes crucial to the design of high performance and durable batteries. Recent work revealed that the chemical potential barriers encountered at the surfaces of heteromaterials play an important role in directing lithium ion transport at nanoscale. Here, we utilize in situ transmission electron microscopy to demonstrate that we can switch lithiation pathways from radial to axial to grain-by-grain lithiation through the systematic creation of heteromaterial combinations in the Si-Ge nanowire system. Lastly, our systematic studies show that engineered materials at nanoscale can overcome the intrinsic orientation-dependent lithiation, and open new pathways to aid in the development of compact, safe, and efficient batteries.

36 MATERIALS SCIENCE↗

Materials Data on Si3Ge by Materials Project

GeSi3 is alpha bismuth trifluoride structured and crystallizes in the cubic Fm-3m space group. The structure is three-dimensional. Ge4+ is bonded in a body-centered cubic geometry to eight equivalent Si+1.33- atoms. All Ge–Si bond lengths are 2.74 Å. There are two inequivalent Si+1.33- sites. In the first Si+1.33- site, Si+1.33- is bonded in a body-centered cubic geometry to four equivalent Ge4+ and four equivalent Si+1.33- atoms. All Si–Si bond lengths are 2.74 Å. In the second Si+1.33- site, Si+1.33- is bonded in a body-centered cubic geometry to eight equivalent Si+1.33- atoms.

36 MATERIALS SCIENCE↗

Materials Data on SiGe3 by Materials Project

Ge3Si crystallizes in the tetragonal I4/mmm space group. The structure is three-dimensional. there are two inequivalent Ge sites. In the first Ge site, Ge is bonded to eight Ge and four equivalent Si atoms to form a mixture of distorted corner, edge, and face-sharing GeSi4Ge8 cuboctahedra. There are four shorter (2.81 Å) and four longer (3.08 Å) Ge–Ge bond lengths. All Ge–Si bond lengths are 3.08 Å. In the second Ge site, Ge is bonded in a square co-planar geometry to eight equivalent Ge and four equivalent Si atoms. All Ge–Si bond lengths are 2.81 Å. Si is bonded in a square co-planar geometry to twelve Ge atoms.

36 MATERIALS SCIENCE↗

Materials Data on Si7Ge by Materials Project

GeSi7 is Moissanite 9R-like structured and crystallizes in the cubic P-43m space group. The structure is three-dimensional. Ge4+ is bonded to four equivalent Si+0.57- atoms to form GeSi4 tetrahedra that share corners with twelve equivalent SiSi4 tetrahedra. All Ge–Si bond lengths are 2.41 Å. There are two inequivalent Si+0.57- sites. In the first Si+0.57- site, Si+0.57- is bonded to one Ge4+ and three equivalent Si+0.57- atoms to form corner-sharing SiSi3Ge tetrahedra. All Si–Si bond lengths are 2.37 Å. In the second Si+0.57- site, Si+0.57- is bonded to four equivalent Si+0.57- atoms to form SiSi4 tetrahedra that share corners with four equivalent GeSi4 tetrahedra and corners with eight equivalent SiSi4 tetrahedra.

36 MATERIALS SCIENCE↗

Materials Data on SiGe by Materials Project

SiGe is Zincblende, Sphalerite structured and crystallizes in the cubic F-43m space group. The structure is three-dimensional. Ge4+ is bonded to four equivalent Si4- atoms to form corner-sharing GeSi4 tetrahedra. All Ge–Si bond lengths are 2.42 Å. Si4- is bonded to four equivalent Ge4+ atoms to form corner-sharing SiGe4 tetrahedra.

36 MATERIALS SCIENCE↗

Materials Data on SiGe by Materials Project

SiGe crystallizes in the monoclinic P2_1 space group. The structure is three-dimensional. there are eight inequivalent Ge4+ sites. In the first Ge4+ site, Ge4+ is bonded in a single-bond geometry to one Si4- atom. The Ge–Si bond length is 2.41 Å. In the second Ge4+ site, Ge4+ is bonded in a trigonal non-coplanar geometry to three Si4- atoms. All Ge–Si bond lengths are 2.42 Å. In the third Ge4+ site, Ge4+ is bonded in a single-bond geometry to one Si4- atom. The Ge–Si bond length is 2.42 Å. In the fourth Ge4+ site, Ge4+ is bonded in a trigonal non-coplanar geometry to three Si4- atoms. There are a spread of Ge–Si bond distances ranging from 2.42–2.44 Å. In the fifth Ge4+ site, Ge4+ is bonded in a single-bond geometry to one Si4- atom. The Ge–Si bond length is 2.43 Å. In the sixth Ge4+ site, Ge4+ is bonded in a trigonal non-coplanar geometry to three Si4- atoms. There are one shorter (2.42 Å) and two longer (2.43 Å) Ge–Si bond lengths. In the seventh Ge4+ site, Ge4+ is bonded in a trigonal non-coplanar geometry to three Si4- atoms. There are a spread of Ge–Si bond distances ranging from 2.42–2.44 Å. In the eighth Ge4+ site, Ge4+ is bonded in a single-bond geometry to one Si4- atom. The Ge–Si bond length is 2.41 Å. There are eight inequivalent Si4- sites. In the first Si4- site, Si4- is bonded to one Ge4+ and three Si4- atoms to form corner-sharing SiSi3Ge tetrahedra. There are one shorter (2.38 Å) and two longer (2.39 Å) Si–Si bond lengths. In the second Si4- site, Si4- is bonded to three Ge4+ and one Si4- atom to form corner-sharing SiSiGe3 tetrahedra. The Si–Si bond length is 2.38 Å. In the third Si4- site, Si4- is bonded to one Ge4+ and three Si4- atoms to form corner-sharing SiSi3Ge tetrahedra. There are one shorter (2.37 Å) and two longer (2.38 Å) Si–Si bond lengths. In the fourth Si4- site, Si4- is bonded to three Ge4+ and one Si4- atom to form corner-sharing SiSiGe3 tetrahedra. The Si–Si bond length is 2.36 Å. In the fifth Si4- site, Si4- is bonded to one Ge4+ and three Si4- atoms to form corner-sharing SiSi3Ge tetrahedra. In the sixth Si4- site, Si4- is bonded to three Ge4+ and one Si4- atom to form corner-sharing SiSiGe3 tetrahedra. In the seventh Si4- site, Si4- is bonded to three Ge4+ and one Si4- atom to form corner-sharing SiSiGe3 tetrahedra. In the eighth Si4- site, Si4- is bonded to one Ge4+ and three Si4- atoms to form corner-sharing SiSi3Ge tetrahedra.

36 MATERIALS SCIENCE↗