Quantifying the Glide Resistance to Dislocations in Proton-Irradiated FeCrAl Alloy
Not provided.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Not provided.
The determination of Critical Resolved Shear Stress (CRSS) in titanium for basal, prismatic, and pyramidal slip-planes without empirical constants is presented by combining Density Functional Theory (DFT) and anisotropic elasticity. A new mechanism leading to tension-compression (T-C) asymmetry in the CRSS levels has been revealed for the first time. The conditions for this asymmetry are established, involving a complex interplay between the dislocation core-structure and core-advance behavior. The three conditions for T-C asymmetry that need to be simultaneously satisfied can be summarized as: (1) a medium stacking fault width, d, (3 < d/b F < 10, where b F is the magnitude of the Burgers vector of the full dislocation), (2) an asymmetric core-structure of the extended dislocation (ξ 1 ≠ ξ 2 , where ξ 1 and ξ 2 are the core-widths of the first and second partials, respectively), and (3) intermittent motion of the partials (Δd/b F ≠ 0, where Δd is the magnitude of fluctuation in stacking fault width during intermittent motion). Pyramidal-slip in titanium satisfies all three conditions, resulting in significant T-C asymmetry. The CRSS theory considers a Wigner-Seitz (W-S) cell based domain area assigned to each lattice site for the calculations of core-energies accurately capturing the slip-plane lattice. The W-S based approach is essential due to the lower symmetry of the HCP crystal circumventing potential errors associated with the one-dimensional atomic-row approximation. Dislocation core structures are obtained for all the slip-systems in titanium showing significant distortion of the disregistry profile governing the core-advance behavior. The CRSS values predicted from the theory show agreement with the experimental CRSS levels reported in the literature.
The resistance to dislocation glide associated with slip systems {110}<111> and {112}<111> in single phase FeCrAl alloy is measured via micromechanical testing in a scanning electronic microscopy at room temperature. Two important factors, the shape and orientation of a pillar, are discussed with respect to the glide resistance and stress-strain response. Maximizing Schmid factor of one specific slip system while minimizing others is recommended in order to diminish obvious dislocations-induced hardening during in-situ testing. Apparent Schmid factor analysis is conducted to select grains with preferred orientations. Two types of pillars with conventional cylindrical shape or dog-bone shape are tested under compression to estimate the resistance to dislocation glide and evaluate the effect of pillar shape on the compression stress-strain response. One dog-bone pillar is tested under tension to check the tension-compression isotropy of dislocation slip. We discover that the shape of a pillar to a smaller extent affects the measured resistance but strongly influences the stress strain response. Cylindrical pillars exhibit apparent hardening associated with early yielding due to stress or strain concentration at contact region, while dog-bone pillars show an obvious yielding and continuous shearing without hardening. The resistance is 220 MPa for slip system {110}<111> and 230 MPa for slip system {112}<111>. Finite element analysis is performed to account for the influence of pillar shape and contact condition on mechanical response.
Refractory multiprincipal element alloys (MPEAs) are promising material candidates for high-temperature, high-strength applications. However, their deformation mechanisms, particularly at the dislocation scale, are unusual compared to those of conventional alloys, making it challenging to understand the origin of their high strength. Here, using an atomistically informed phase-field dislocation dynamics model, we study transitions in the morphology and critical stresses of long gliding screw dislocations over extended distances in a refractory MPEA. The model MPEA crystal accounts for the atomic-scale fluctuations in chemical composition across the glide planes via spatially correlated lattice energies and for the differences in glide resistances between screw and edge dislocations of unit length. Here, we show that the dislocation moves in a stop-start motion, alternating between wavy morphology in free flight and nearly recovered straight screw orientation in full arrest. The periods of wavy glide are due to variable kink-pair formation and migration rates along the length, where portions with higher rates glide more quickly. The critical stress to initiate motion corresponds to the stress required to form and migrate a kink pair at the weakest region along the length of the dislocation. Heterogeneity in lattice energy leads to variability in the local stress-strain response and to a strain hardening-like response, in which the critical stress to reactivate glide increases with glide distance. Statistical assessment of hundreds of realizations of dislocations indicates that the amount of hardening directly scales with the dispersion in underlying lattice energy.
In this work, we investigate the operation of Frank-Read (FR) sources in a refractory multi-principal element alloy (MPEA). Simulations of discrete dislocation motion in MPEAs is enabled by the development of a phase field dislocation dynamics model that treats the atomic-scale fluctuations in lattice energies across the glide plane, present due to local ordering in the chemical composition within the nominally random MPEA atomic structure. We consider, through simulation, a range of length scales over which ordering occurs, varying from short-range lengths, a few times dislocation core width, to long-range lengths, an order of magnitude longer than the core. Characteristic of this body-centered cubic MPEA, the simulations also include screw/edge character dependence in glide resistance, as informed by atomic scale simulation. The critical stresses to activate the source for the same source size are found to be statistically distributed, as a direct consequence of the underlying variation in lattice energy. Furthermore, analysis of critical state for activating edge and screw FR sources in the MPEA reveals that FR source operation occurs via a two-step mechanism, involving athermal kink-pair formation, unlike the conventional FR source operation in a material with no composition fluctuations. This mechanism lowers the average critical stress required to activate the FR source and causes the statistical dispersion in critical stress to depend on the range of composition ordering. More importantly, it leads to a more severe dependence of source strength on FR source length than predicted by line tension alone.
The Peierls barrier measures the lattice resistance to dislocation glide in crystalline solids. We use the nudged elastic band (NEB) method to calculate the Peierls barriers for screw and edge dislocation glide in a face-centered cubic (FCC) metal of Ni. The minimum energy paths (MEPs) across single or sequential Peierls barriers are determined under shear loading. The NEB results show the decreasing Peierls barrier with increasing shear stress, giving the Peierls stress at which the Peierls barrier vanishes. The effects of boundary condition and system size on Peierls barriers are studied by comparing strain- and stress-controlled NEB results. Furthermore, the free-end NEB methods are applied to determine MEPs with improved computational efficiency. The NEB results are also used to evaluate the energetic driving force of dislocation glide, which is consistent with that determined from the Peach-Koehler force. The accuracy of the present NEB results based on an empirical interatomic potential is assessed by comparison with a machine-learning potential. This work demonstrates the robust and efficient quantification of Peierls barriers to dislocation glide in an FCC metal, and it lays a solid foundation for the atomistic determination of Peierls barriers in compositionally complex alloys with the FCC structure in future studies.
An integrated in-situ neutron diffraction and elastic plastic self-consistent crystal plasticity (EPSC-CP) modeling scheme is performed on a binary Al–12Ce alloy and a ternary Al–12Ce–0.4Mg alloys. Using this scheme, the constitutive parameters, i.e. elastic constants and slip system parameters of individual phases can be calibrated which can be used in microstructure-based CP models to predict materials performance. From this study, it is shown that the elastic constants of Al 11 Ce 3 intermetallics calculated from density function theory calculation in the literature are rather accurate. When applied to the EPSC-CP model, the lattice strains of both the binary and ternary alloys are correctly predicted as compared with experiments, and large lattice strain differences between Al (100) plane and Al 11 Ce 3 (010) plane are demonstrated. The slip system parameters calibrated by the scheme shows that the addition of 0.4 wt% Mg in the alloy has little influence on the critical resolved shear stress of initial dislocation glide in the Al matrix which caused plastic yield in the material. This can be explained by the very dilute Mg solute content in the Al solid solution, causing large spacing of Al–Mg lattice misfit sites and little impact on resistance of dislocation glide at initial yield. The 0.4 wt% Mg addition, on the other hand, has a large influence on the hardening term in the slip system parameters, indicating those Al–Mg misfit sites do help dislocation accumulation during the deformation. The impact of dilute Mg addition on the Al slip system parameters is also reflected in the flow behavior of the ternary alloy: little impact on the yield stress, but a large impact on working hardening and tensile strength of the materials which is consistent with the literature.
Al-Si cast alloys are usually composed of α-Al and Al-Si eutectic. Si flakes and Al matrix generally hold cube-on-cube orientation relationship with the primary interface (111) Al ∥(111) Si . Extensive experimental studies demonstrated that Si flakes cannot significantly improve mechanical properties of Al-Si cast alloys. We hypothesize that the weak strengthening effect associated with Si flakes might be attributed to thermomechanical properties of Al-Si interfaces besides their morphologies. To characterize Al-Si interfaces with a large lattice mismatch (> 30%), we proposed the quasi-coincident site lattice (Q-CSL) as reference lattice, and demonstrated that the Q-CSL Al-Si coherent interface has three characteristic coherent structures, one stable and low energy structure and two metastable and high energy structures. The translation vectors for the same type of coherent Q-CSL structures are consistent with three displacement shift complete (DSC) vectors. The two metastable structures can be obtained by shifting the low energy structure with three partial DSC vectors. Semi-coherent interface is composed of the low energy Q-CSL patches and three sets of interface misfit dislocations with Burgers vectors same as the DSC vectors. Atomistic simulations revealed that Al-Si interface exhibits low shear resistance. Ideal shear strength of the Q-CSL coherent interface is 110 MPa and semi-coherent interface is 20 MPa. The low shear resistance is attributed to the glide of interface misfit dislocations. Al-Si interface also exhibits low formation and migration energies of point defects. Owing to low shear strength and low formation and migration energies of point defects, interface sliding or shear readily happen under mechanical loading or during dislocation-interface interactions. Lattice dislocations can cross slip onto or climb along Al-Si interfaces. These reactions decrease the number of accumulated dislocation loops around Si flakes and promote nucleation and emission of lattice dislocations from Al-Si interfaces to matrix, consequently reduce the repulsive force on approaching dislocations and weaken Si flakes strengthening effect. In situ tension and compression tests in a scanning electron microscope reveal relatively weak strengthening effect due to Si flakes, consistent with the computed dislocation interaction with interfaces and shear behavior of interfaces.
Refractory complex concentrated alloys (RCCAs) have emerged as promising candidates for high-temperature structural applications due to their high melting points and potential for exceptional strength, whereas their creep properties remain relatively underexplored. Here, we investigate the tensile creep behavior of NbTaTi and NbTaTiV in high vacuum to elucidate the influence of alloying on creep mechanisms. NbTaTiV exhibits higher creep resistance than NbTaTi, which is attributed to V-induced edge-dislocation-glide-controlled deformation. Microstructural analysis reveals the formation of Ti- and interstitial impurity-rich secondary phases during creep, which enhances the creep resistance without significant embrittlement. Stress exponents (∼3) and activation energies (∼those for vacancy diffusion) align with thermally activated dislocation glide-controlled creep. Despite NbTaTiV surpassing Ni-based superalloys in yield strength at elevated temperatures, its single-phase BCC structure limits creep resistance under engineering-relevant conditions, highlighting the necessity of deliberate secondary phase design to achieve competitive high-temperature performance.
Medium- and high-entropy alloys based on the CrCoNi-system have been shown to display outstanding strength, tensile ductility and fracture toughness (damage-tolerance properties), especially at cryogenic temperatures. Here we examine the J Ic and (back-calculated) K JIc fracture toughness values of the face-centered cubic, equiatomic CrCoNi and CrMnFeCoNi alloys at 20 K. At flow stress values of ~1.5 GPa, crack-initiation K JIc toughnesses were found to be exceptionally high, respectively 235 and 415 MPa√m for CrMnFeCoNi and CrCoNi, with the latter displaying a crack-growth toughness K ss exceeding 540 MPa√m after 2.25 mm of stable cracking, which to our knowledge is the highest such value ever reported. Characterization of the crack-tip regions in CrCoNi by scanning electron and transmission electron microscopy reveal deformation structures at 20 K that are quite distinct from those at higher temperatures and involve heterogeneous nucleation, but restricted growth, of stacking faults and fine nanotwins, together with transformation to the hexagonal closed-packed phase. The coherent interfaces of these features can promote both the arrest and transmission of dislocations to generate respectively strength and ductility which strongly contributes to sustained strain hardening. Indeed, we believe that these nominally single-phase, concentrated solid-solution alloys develop their fracture resistance through a progressive synergy of deformation mechanisms, including dislocation glide, stacking-fault formation, nano-twinning and eventually in situ phase transformation, all of which serve to extend continuous strain hardening which simultaneously elevates strength and ductility (by delaying plastic instability), leading to truly exceptional resistance to fracture.
Helical edge states in quantum spin Hall (QSH) materials are central building blocks of topological matter design and engineering. Despite their principal topological protection against elastic backscattering, the level of operational stability depends on manifold parameters such as the band gap of the given semiconductor system in the “inverted” regime, temperature, disorder, and crystal orientation. Here, we theoretically investigate electronic and transport properties of QSH edge states in large gap 1-T' WTe 2 monolayers. We explore the impact of edge termination, disorder, temperature, and interactions on experimentally addressable edge state observables, such as local density of states and conductance. We show that conductance quantization can remain surprisingly robust even for heavily disordered samples because of an anomalously small edge state decay length and additional protection related to the large direct gap allowed by glide symmetry. From the simulation of temperature-dependent resistance, we find that moderate disorder enhances the stability of conductance by localizing bulk states. We evaluate the edge state velocity and Luttinger liquid parameter as functions of the chemical potential, finding prospects for physics beyond linear helical Luttinger liquids in samples with ultraclean and well-defined edges.
The creep behavior of single crystals of gamma-prime and gamma alloys were investigated and compared to the response of two-phase superalloys tested previously. High temperature deformation in the gamma alloys was characteristic of a climb-controlled mechanism, whereas the gamma-prime based materials exhibited glide-controlled creep behavior. The superalloys were much more creep resistant than their constituent phases, which indicates the importance of the gamma/gamma-prime interface as a barrier for dislocation motion during creep.
Iridates have attracted much interest in the last decade for their novel magnetism emerging in the limit of strong spin-orbit coupling and possible unconventional superconductivity. A standard for growing iridate single crystals has been the flux method using platinum crucibles. Here, in this work, we show that this widely used method compromises the sample quality by inclusion of platinum impurities. We find that Sr 2 IrO 4 single crystals grown in iridium crucibles show remarkable differences from those grown in platinum crucibles in their sample characterizations using Raman spectroscopy, resistivity, magnetization, optical third harmonic generation, resonant x-ray diffraction, and resonant inelastic x-ray scattering measurements. In particular, we show that several peaks of sizable intensities disappear in the Raman spectra of samples free of platinum impurities, and a significantly larger activation energy is extracted from the resistivity data compared to previously reported values. Furthermore, we find no evidence of the previously reported glide-symmetry-breaking structural distortions and confirm the I 4 1 / acd space group of the lattice symmetry. Although the platinum impurities are not apparent in the magnetic properties and thus went unnoticed in the stoichiometric insulating phase for a long time, their effects can be much more detrimental to transport properties in chemically doped compounds. Therefore, our result suggests using growth methods that avoid platinum impurities for an investigation of the intrinsic physical properties of iridates, and possible superconducting phases.
Here, in this work, we report a novel approach to reduce the channel resistance by inducing a phase transition behavior from 2H to 1T in a monolayer MoS 2 (1L-MoS 2 ) by a synchrotron X-ray monochromatic beam (mono-beam) radiation. The effects of the biphase structure by the mono-beam on the 1L-MoS2 film were investigated using Raman spectra, photoluminescence (PL) spectra, scanning tunneling microscopy, and scanning tunneling spectroscopy, respectively. Through material characterization, we identified that the lateral sliding of S-vacancies along the S-plane in the 1L-MoS 2 is the key reason for the origin of unidirectional phase transition. The precise phase engineering triggered by the mono-beam radiation process allows the realization of field-effect transistors (FET) with 2X improvement in mobility toward a high on/off ratio (~10 8 ) and a near-ideal subthreshold swing of ~88 mV per decade. The validity of the phase engineering could be further extended for its application as a memory device, exhibiting a gate tunable conduction modulation behavior and a high resistance ratio of ~10 2 at a gate bias of 5 V with endurance of ~100 cycles. Furthermore, an artificial neural network using the synaptic weight update with accuracy of ~93 % was achieved.
Environmental regulations have driven the development of refrigerants with low global warming potential (GWP). To design heat exchangers using these new refrigerants, data are needed concerning the heat transfer coefficient and pressure drop in two-phase flow. Another change is the increasing use of aluminum tubes rather than copper tubes to reduce heat exchanger cost. Hence, this study presents an experimental investigation of flow condensation using an expanded axial micro-fin aluminum tube with a fin-tip diameter of 5.96 mm. Here, the experiments included single compounds R-32, R-1234yf, and R-1234ze(E), zeotropic mixtures with low glide (R-454B), and zeotropic mixtures with high-glide (R-454C and R-455A). Experiments were conducted at condensation temperatures ranging from 40 °C to 50 °C, reduced pressures ranging from 0.21 to 0.55, and mass fluxes ranging from 150 to 350 kg/(m 2 s). Data obtained for these refrigerants constitute one of the first reports for high-glide refrigerants using axial micro-fin aluminum tubes. An evaluation of heat transfer degradation of zeotropic mixtures due to mass transfer resistance at the liquid/vapor interface is presented. This information can be used to design heat exchangers for next generation air conditioning and refrigeration systems.
Flat-flexible circuits or ‘flex circuits’ have varied applications in electronics and in explosive detonation systems. They pose advantages over conventional coaxial cables in their ability to fit into small mechanical envelopes and routings. A typical flex circuit is composed of a laminated assembly of multiple layers of conductor and dielectric materials. Copper, because of its high electrical conductivity, is one of the primary materials used in flex circuit conductors. The conductor must maintain structural integrity and electrical continuity when the flexible circuit is bent during processing or to fit an application envelope. Under some strain conditions a cable may have degraded electrical performance even though visible damage may not be evident. Dislocation density can increase by mechanisms such as dislocation forest hardening, where gliding dislocations in primary slip planes get pinned at obstacles and form Frank-Read sources. Dislocation density increases within the conductor layers may impact electrical resistivity but would not necessarily result in visible mechanical failure. In some detonation applications, such as for building implosion for demolition, the time for signal transmission and voltage used for firing detonators can be critical. If the resistance in a single flex cable within a building demolition array is too high, the resultant demolition shape may be asymmetric, leading to unplanned damage to nearby structures and potential hazards to public safety. This study will apply non-destructive evaluation techniques to evaluate the detectability of damage accumulation in flat, flexible copper-conductor cables and discuss potential implications to their practical use.
Impurities acting as traps, reduce the self-interstitial atom (SIA) cluster mobility, thereby increasing recombination and in turn enhancing radiation-resistance of polycrystalline materials. However, at elevated temperatures, depending on SIA-trap (impurity) binding energy, SIA clusters may trap and detrap (detach) numerous times. In tungsten, SIA clusters of all sizes glide one-dimensionally (1D) along their Burgers vector direction. Hence, detrapped SIAs would retrace their path, confining their 1D-glide between traps. However, small SIA clusters can change the direction of their 1D-glide by overcoming a rotation barrier. In addition, impurities or solutes are known to reduce this barrier. A lower rotation barrier can result in detrapped SIA clusters that diffuse in a random 1D direction, effectively leading to 3D (net-3D) diffusion. Here we investigate the effect of two cases of SIA diffusion, namely confined-1D diffusion and net-3D diffusion, on the damage accumulation in polycrystalline tungsten under 14 MeV neutron irradiation using the object kinetic Monte Carlo method. Simulations were performed using cascade debris obtained from molecular dynamics simulations with primary knock-on atom (PKA) energies corresponding to 14 MeV neutrons. In the simulations with net-3D diffusion, SIA clusters of all sizes diffuse in a random 1D direction after the clusters detrap. While for the confined 1D diffusion case, SIA clusters larger than size 5 retain their original direction of 1D-glide. In both types of simulations, trapped vacancies are assumed to be permanently immobilized. Unexpectedly, the damage accumulation was lower with confined 1D diffusion than that with net-3D. We present a systematic comparison of the influence of the two cases of SIA diffusion on the radiation damage accumulation as a function of dose rate, detrapping barrier, and impurity concentration at 1025 K.
The experiment was aimed at checking compatibility of the aluminum conductors with conventional conductors and contacts under different conditions of manufacturing (mechanical or magnetostrictive crimping) and storage in laboratory or in long-duration space environment. The electrical characteristics of connections built from nickel-plated conductors and glided copper contacts were noted to vary over the duration of the experiment. These variations are unrelated with the crimping or storage conditions or with metal pairing (nickel-plated aluminum/tinned or silver copper). Such evolutions, even slight, are detrimental to connection quality. The same observations hold for some like connections subjected to long-duration thermal cycles. Therefore, work on aluminum technology was reoriented toward a silver aluminum conductor/ golded aluminum contact solution. The first evaluation test performed according to this definition have yielded satisfactory results.