Hot Cracking Behavior and Beam-Induced Grain Refinement in Electron Beam Freeform Fabricated Al 7075
Electron beam freeform fabrication (EBF 3 ) is a high deposition rate, wire-based directed energy deposition (DED) additive manufacturing (AM) process used to print metallic parts in a vacuum environment. While high specific strength 7xxx-series Al alloys are of interest in the aerospace and automotive industries, these alloys suffer from hot cracking issues during fusion welding and AM. In this work, linear deposits of Al 7075 were fabricated with EBF 3 to study the effects of baseplate thickness, preheat temperature, and beam focus on hot cracking behavior. Solidification cracks were observed in the first deposition layer, and by the third layer coalesced into large “macrocracks” running vertically through the build height. Fine, intergranular liquation “microcracks” appeared between macrocracks below the root of the final deposit layer fusion zone. Increasing the substrate preheat temperature from 165°C to 320°C deepened the partially melted zone and resulted in a more than twofold increase in the liquation microcrack density. Analysis of Scheil solidification diagrams revealed that fugitive losses of Zn and Mg during deposition increased the susceptibility to solidification cracking and promoted substrate liquation cracking. Focused electron beam (EB) conditions combined with a high aspect ratio elliptical raster pattern resulted in bands of refined, equiaxed grains. The refined microstructure suppressed solidification macrocracking and caused a nearly fivefold reduction in liquation crack density, demonstrating that beam-induced grain refinement may be a promising low-cost method for reducing hot cracking during AM.