Direct Visualization of Arsenic Binding on Green Rust Sulfate
Abstract not provided
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Abstract not provided
Explore the source record for details and available documents.
Green rusts (GR) are mixed-valence iron (Fe) hydroxides which form in reducing redox environments like riparian and wetland soils and shallow groundwater. In these environments, silicon (Si) can influence Fe oxides’ chemical and physical properties but its role in GR formation and subsequent oxidative transformation have not been studied starting at initial nucleation. Green rust sulfate [GR(SO 4 )] and green rust carbonate [GR(CO 3 )] were both coprecipitated from salts by base titration in increasing % mol Si (0, 1, 10, and 50). The minerals were characterized before and after rapid (24 h) aqueous air-oxidation by x-ray diffraction (XRD), scanning electron microscopy (SEM), Fe extended x-ray absorption fine structure spectroscopy (EXAFS), and N 2 -BET surface area. Results showed that only GR(SO4) or GR(CO3) was formed at every tested Si concentration. Increasing % mol Si caused decreased plate size and increased surface area in GR(CO3) but not GR(SO4). GR plate basal thickness was not changed at any condition indicating a lack of Si interlayering. Air oxidation of GR(SO4) at all % mol Si contents transformed by dissolution and reprecipitation into lepidocrocite and goethite, favoring ferrihydrite with higher % Si content. Air oxidation of GR(CO3) transformed into magnetite and goethite but increasing Si caused GR to oxidize while retaining its hexagonal plate structure via solid-state oxidation. Our results indicate that Si has the potential to cause GR to form in smaller particles and upon air oxidation, Si can either stabilize the plate structure or alter transformation to ferrihydrite.
Green rusts (GR) are important drivers for trace metal and nutrient cycling in suboxic environments. We investigated whether green rusts would incorporate aluminum (Al) or other elements from naturally-formed clay minerals containing easily-weatherable clay minerals (e.g. mica, interlayered clays). We isolated the clay minerals from a Matapeake silt loam soil by removal of silt and sand, organic matter, and reducible oxides to study mechanisms of interaction between Fe(II) and soil-sourced clay minerals. We conducted batch Fe(II) sorption experiments at multiple near-neutral pHs (6.5–7.5) and reaction times (2h–365 days). Mineral transformations were characterized by selective extractions, X-ray diffraction (XRD), and Fe X-ray absorption spectroscopy (XAS) analyzed by shell-fitting and linear combination fitting (LCF) with natural and synthetic standards. Clay mineral fraction contained a mixture of quartz, kaolinite, interlayered vermiculite, mica, and chlorite with significant structural Fe (2.6% wt). Uptake of Fe(II) increased with pH and kinetics were rapid until 5 days, followed by slow continuous Fe(II) uptake. Citrate-bicarbonate desorption kinetics from Fe(II) sorbed clay released more Al and silicon (Si) compared with unreacted soil clay fraction whereas magnesium (Mg) and potassium (K) were unaffected. Citrate-bicarbonate extracted Fe contained more Fe(II) than an ideal GR with an Fe(II)/Fe(III) molar ratio of 5.50. Analysis of the Fe EXAFS by both LCF and shell fitting was best modeled as a combination of Fe(III)-clay reduction to Fe(II) and precipitation of GR and Fe(II)-Al LDH. After 7 days of Fe(II) sorption, LCF identified 55.2% total Fe in clay, 33.4% GR(Cl) and 11.4% Fe(II)-Al LDH. Further, these results provide novel evidence of Fe(II)-Al LDHs precipitating on naturally-formed soil clay minerals as a minor phase to GR. The geochemical implications are that GRs formed in soils and sediments should be considered to have Al and Si as well as Mg substitutions affecting their structure and reactivity.
Abstract Ionic liquids are green solvents that have wide applications in material synthesis, catalysis, and separation. A model switchable ionic liquid (SWIL) consisting of 1,8‐diazabicycloundec‐7‐ene (DBU) and 1‐hexanol with carbon dioxide (CO 2 ) as the trigger gas is chosen to synthesize nanocrystalline green rust. Under anoxic conditions, by adding iron (II) acetate (Fe(C 2 H 3 O 2 ) 2 ) and methanol to the degassed SWIL, a nanoparticulate green rust with carbonate (nano‐GR) is synthesized. More importantly, the molecular structural change of the ionic liquid resulting in green rust crystallines is first characterized using in situ liquid using time‐of‐flight secondary ion mass spectrometry (ToF‐SIMS) coupled with the system for analysis at the liquid vacuum interface (SALVI), a vacuum compatible microfluidic reactor in this work. Dimers and ionic clusters consisting ferric and ferrous ions are identified in liquid ToF‐SIMS spectra. Spectral principal component analysis is used to confirm that these ion pairs including dimers and cluster ions are different from nonionic liquids. The results show that liquid ToF‐SIMS can be a useful tool to study complex liquids at the molecular level providing insights into predicative synthesis of nanomaterials using environmentally friendly green solvents and giving unique visualization of the evolving material interface due to nucleation.
Chlorinated ethenes have been used extensively as solvents, degreasers, and dry-cleaning agents in a range of commercial and industrial applications. This has created a legacy of contaminated soils and groundwater, particularly with respect to perchloroethylene (PCE; a.k.a. tetrachloroethene—C 2 Cl 4 ), and trichloroethylene (TCE; a.k.a. trichloroethene—C 2 HCl 3 ), prompting the development of a wide array of treatment technologies for remediation of chlorinated ethene-contaminated environments. Green rusts are highly redox-active layered Fe(II)-Fe(III) hydroxides that have been shown to be facile reductants for a wide range of organic and inorganic pollutants. The reduction of chlorinated ethenes [vinyl chloride (VC); 1,1-dichloroethene(11DCE), cis-1,2-dichloroethene (c12DCE), trans-1,2-dichloroethene (t12DCE), TCE, and PCE] was examined in aqueous suspensions of green rust, alone as well as with the addition of Ag(I) (AgGR) or Cu(II) (CuGR). Green rust alone was ineffective as a reductant for the reductive dechlorination for all of the chlorinated ethenes. Near-complete removal of PCE was observed in the presence of AgGR, but all other chlorinated ethenes were essentially non-reactive. Partial removal of chlorinated ethenes was observed in the presence of CuGR, particularly 11DCE (34%), t12DCE (51%), and VC (66%). Significant differences were observed in the product distributions of chlorinated ethene reduction by AgGR and CuGR. The effectiveness of Ag(I)- and Cu(II)-amended green rusts for removal of chlorinated ethenes may be improved under different conditions (e.g., pH and interlayer anion) and warrants further investigation.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Banded iron formation (BIF) deposition in the Archean ocean is thought to have been initiated by the oxidation of dissolved iron into ferric primary precursor phases that descended through the water column and were deposited on the seafloor. Effective interpretation of the trace element and isotopic composition of BIFs in the geologic record requires an understanding of the identity and longevity of those precursor phases. Temporal and spatial variation in oxidant concentration and ocean chemistry may have driven precursor mineralogy. Furthermore, precursor phases may undergo transitions during descent and burial. This experimental study follows the evolution of iron mineralogy, speciation, and redox state during the precipitation of iron under variable oxygen fluxes and in fluids containing different iron-complexing anions (chloride, sulfate, and phosphate). Additionally, suspensions collected after incomplete oxidation were anoxically aged to simulate changes to precursor mineralogy during descent below the seawater redoxcline. Results from X-ray diffraction, sequential dissolution, colorimetric determination of Fe redox state, and Fe K-edge X-ray absorption fine structure spectroscopy showed that under all experimental conditions, intermediate precipitates collected before complete iron uptake contained mineralized ferrous iron. Purely ferric mineral assemblages were not observed until iron was removed from solution. In low-oxygen experiments, intermediate precipitates contained phases with stoichiometric Fe 2+ , including magnetite, vivianite, and green rust (GR). Chloride green rust (GR1) had more ferric iron than sulfate green rust (GR2) and more readily transitioned to magnetite via disproportionation. GR2 was stable over a broader range of iron uptake; magnetite appeared mainly as an additional oxidation product in sulfate solution. In high oxygen experiments, mineralized ferrous iron occurred in amorphous phases or as a non-stoichiometric component in ferric oxides; final ferric assemblages were less crystalline than in low-oxygen equivalents. Low concentrations of phosphate increased the total iron oxidation rate, but also increased the ferrous content of intermediate precipitates. The incorporation of phosphate stabilized GR2 and facilitated GR2 precipitation over a larger range of iron uptake. In higher concentrations of phosphate, vivianite and poorly crystalline ferric hydroxides formed in place of GR. Here, these findings suggest that over a range of possible ocean chemistries, mixed-valence phases may have been short lived but relevant precursors to BIF. Additionally, anionic chemistry and oxidant concentration are shown to influence the crystallinity and chemical resistivity of final ferric assemblages, affecting their reactivity during later anoxic burial.
The bioreduction of Fe(III) oxides by dissimilatory iron-reducing bacteria may result in the formation of a suite of Fe(II)-bearing secondary minerals, including magnetite (a mixed Fe(II)/Fe(III) oxide), siderite (Fe(II) carbonate), vivianite (Fe(II) phosphate), chukanovite (ferrous hydroxy carbonate), and green rusts (mixed Fe(II)/Fe(III) hydroxides). In an effort to better understand the factors controlling the formation of specific Fe(II)-bearing secondary minerals, we examined the effects of Fe(III) oxide mineralogy, phosphate concentration, and the availability of an electron shuttle (9,10-anthraquinone-2,6-disulfonate, AQDS) on the bioreduction of a series of Fe(III) oxides (akaganeite, feroxyhyte, ferric green rust, ferrihydrite, goethite, hematite, and lepidocrocite) by Shewanella putrefaciens CN32, and the resulting formation of secondary minerals, as determined by X-ray diffraction, Mössbauer spectroscopy, and scanning electron microscopy. The overall extent of Fe(II) production was highly dependent on the type of Fe(III) oxide provided. With the exception of hematite, AQDS enhanced the rate of Fe(II) production; however, the presence of AQDS did not always lead to an increase in the overall extent of Fe(II) production and did not affect the types of Fe(II)-bearing secondary minerals that formed. The effects of the presence of phosphate on the rate and extent of Fe(II) production were variable among the Fe(III) oxides, but in general, the highest loadings of phosphate resulted in decreased rates of Fe(II) production, but ultimately higher levels of Fe(II) than in the absence of phosphate. In addition, phosphate concentration had a pronounced effect on the types of secondary minerals that formed; magnetite and chukanovite formed at phosphate concentrations of ≤1 mM (ferrihydrite), <~100 µM (lepidocrocite), 500 µM (feroxyhyte and ferric green rust), while green rust, or green rust and vivianite, formed at phosphate concentrations of 10 mM (ferrihydrite), ≥100 µM (lepidocrocite), and 5 mM (feroxyhyte and ferric green rust). These results further demonstrate that the bioreduction of Fe(III) oxides, and accompanying Fe(II)-bearing secondary mineral formation, is controlled by a complex interplay of mineralogical, geochemical, and microbiological factors.
Rhenium (Re) is an extremely rare element, with a crustal abundance of approximately 0.4 parts per billion (ppb) and a sea water concentration of 8.3 parts per trillion (ppt). However, Re concentrations in anoxic marine sediments range from 2 to 184 ppb, which is attributed to reduction of the highly soluble perrhenate ion (Re(VII)O 4 - ) to insoluble Re(IV) species. Anoxic sediments typically contain Fe(II) and sulfide species, which could potentially reduce Re(VII) to Re(IV). In this study, we examined the interactions of KReO 4 with magnetite (Fe 3 O 4 ), siderite (FeCO 3 ), vivianite (Fe 3 (PO 4 ) 2 •8H 2 O), green rust (mixed Fe(II)/Fe(III) layered double hydroxide), mackinawite (FeS), and chemically reduced nontronite (NAu-1) using X-ray absorption near-edge structure (XANES) and extended X-ray absorption fine structure (EXAFS) spectroscopy to determine the valence state and speciation of Re. Uptake of Re by green rust was rapid, with ~50% associated with the solids within 2 days. In contrast, there was <10% uptake by the other Fe(II) phases over 48 days. Reduction of Re(VII) to Re(IV) was only observed in the presence of green rust, producing clusters of bidentate-coordinated Re(IV)O 6 octahedra.. These results suggest that except for green rust, the potential for other Fe(II)-bearing minerals to act as reductants for ReO 4 - in sedimentary environments requires further investigation.
Fe(II)-bearing minerals (magnetite, siderite, green rust, etc.) are common products of microbial Fe(III) reduction, and they provide a reservoir of reducing capacity in many subsurface environments that may contribute to the reduction of redox active elements such as vanadium; which can exist as V(V), V(IV), and V(III) under conditions typical of near-surface aquatic and terrestrial environments. To better understand the redox behavior of V under ferrugenic/sulfidogenic conditions, we examined the interactions of V(V) (1 mM) in aqueous suspensions containing 50 mM Fe(II) as magnetite, siderite, vivianite, green rust, or mackinawite, using X-ray absorption spectroscopy at the V K-edge to determine the valence state of V. Two additional systems of increased complexity were also examined, containing either 60 mM Fe(II) as biogenic green rust (BioGR) or 40 mM Fe(II) as a mixture of biogenic siderite, mackinawite, and magnetite (BioSMM). Within 48 h, total solution-phase V concentrations decreased to <20 µM in all but the vivianite and the biogenic BiSMM systems; however, >99.5% of V was removed from solution in the BioSMM and vivianite systems within 7 and 20 months, respectively. The most rapid reduction was observed in the mackinawite system, where V(V) was reduced to V(III) within 48 h. Complete reduction of V(V) to V(III) occurred within 4 months in the green rust system, 7 months in the siderite system, and 20 months in the BioGR system. Vanadium(V) was only partially reduced in the magnetite, vivianite, and BioSMM systems, where within 7 months the average V valence state stabilized at 3.7, 3.7, and 3.4, respectively. The reduction of V(V) in soils and sediments has been largely attributed to microbial activity, presumably involving direct enzymatic reduction of V(V); however the reduction of V(V) by Fe(II)-bearing minerals suggests that abiotic or coupled biotic–abiotic processes may also play a critical role in V redox chemistry, and thus need to be considered in modeling the global biogeochemical cycling of V.
A method and apparatus are provided for removing EPA regulated chemical species from industrial wastewater using green rust. The apparatus includes a green rust generator having an iron anode and a carbon cathode.
Compared to more abundant metalloids (e.g., As, Se, and Sb), little is known regarding the biogeochemistry of tellurium (Te), a critical metal whose use in CdTe photovoltaic solar cells is driving increasing global demand for this element. In this study, to understand the redox behavior of Te under ferrugenic/sulfidogenic conditions, we examined the potential for reduction of Te(VI) and Te(IV) in aqueous suspensions containing Fe(II) as siderite, vivianite, green rust, magnetite, or mackinawite; Fe(II)-bearing minerals which are often formed during microbial reduction of Fe(III) oxides. In the mackinawite systems, complete reduction of Te(VI) or Te(IV) to Te(0) was observed within 12 h, and near complete reduction (>90% Te(0)) was observed within 2.5 days in the green rust systems. In the presence of siderite, complete reduction of Te(VI) or Te(IV) to Te(0) occurred within 60 days. We observed >60% reduction of Te(VI) to Te(IV) within 2.5 days in the magnetite system, but Te(0) did not form until 120 days; however, complete reduction to Te(0) was observed within 120 days when starting with Te(IV). With vivianite there was >80% reduction of Te(VI) to Te(IV) within 12 h, without further reduction to Te(0) over the duration of the experiment (120 days); in the Te(IV)-vivianite system, there was no evidence of Te(IV) reduction within 120 days. The reduction of Te(VI) and Te(IV) in soils and sediments has been largely attributed to direct reduction by microbes; however, the reduction of Te(VI) and Te(IV) by Fe(II)-bearing minerals suggests that abiotic or coupled biotic-abiotic processes may also play a critical role in Te redox chemistry in natural and engineered environments.
The construction of an underground facility can dramatically change the quality, flow direction, and level of groundwater. It may also impact subsurface microbial composition and activity. Groundwater quality was monitored over eight years in two observational wells near an underground disposal facility on the east coast of South Korea. The results showed dramatic increases in dissolved ions such as O 2 , Na, Ca, Mg, and SO 4 during facility construction. Seepage water samples downgradient from the silos and tunnels, and precipitates deposited along the seepage water flow path were collected to determine the impact inside the disposal facility. X-ray analysis (powder X-ray diffraction (pXRD) and X-ray absorption fine structure (XAFS)) were used to characterize the mineral precipitates. Microbial community composition was determined by 16S rRNA gene sequencing. The seepage water composition was of two types: Ca-Cl and Ca-Na-HCO 3 . The ratio of Cl and δ 18 O showed that the Ca-Cl type seepage water was influenced by groundwater mixed with seawater ranging from 2.7% to 15.1%. Various sulfate-reducing bacteria were identified in the Ca-Cl type seepage water, exhibiting relatively high sulfate content from seawater intrusion. Samples from the Ca-Na-HCO 3 type seepage water had an extremely high pH (>10) and abundance of Hydrogenophaga. The precipitates observed along the flow path of the seepage water included calcite, ferrihydrite, green rust, and siderite, depending on seepage water chemistry and microbial activity. This study suggests that the construction of underground structures creates distinct, localized geochemical conditions (e.g., high alkalinity, high salinity, and oxic conditions), which may impact microbial communities. These biogeochemical changes may have undesirable large-scale impacts such as water pump clogging. Overall, an understanding of the process and long-term monitoring are essential to assess the safety of underground facilities.
Electrocoagulation of zero-valent iron has been widely applied to the removal of dissolved arsenic, but the solid-liquid separation of arsenic-containing precipitates remains technically challenging. In this work, zero-valent iron was electrochemically oxidized to magnetic iron oxides for the removal of As(V) from simulated and actual mining wastewaters. The results indicated that lepidocrocite was formed when zero-valent iron was oxidized by dissolved oxygen, but ferrihydrite and green rust were first formed and then transformed to magnetic iron oxides (mainly magnetite and maghemite) in the electrochemical oxidation from 0 to 0.9 V (vs. SCE), which facilitates the adsorption of As(V) and subsequent solid-liquid separation under a magnetic field. In simulated As(V)-containing solution with initial pH 7.0, zero-valent iron was electrochemically oxidized to magnetite and maghemite at 0.6 V (vs. SCE) for 2 h. The As(V) concentration first decreased from 5127.5 to 26.8 μg L -1 with a removal ratio of 99.5%. In actual mining wastewaters, zero-valent iron was electrochemically oxidized to maghemite at 0.6 V (vs. SCE) for 24 h, and the As(V) concentration decreased from 5486.4 to 3.6 μg L -1 with a removal ratio of 99.9%. The removal ratio of As(V) increased slightly with increasing potential, and increased first and then decreased with increasing initial pH. Compared with that of SO 4 2- and NO 3 - , the presence of Cl - significantly enhanced the removal of As(V). This work provides a highly efficient, facile and low-cost technique for the treatment of arsenic-containing wastewaters.