Electric field assisted solid-state interfacial joining of TaC-HfC ceramics without filler
Not provided.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Not provided.
Hydrochlorofluorocarbon (HCFC) 141b has been selected as the interim blowing agent for use in urethane insulations on NASA's Space Shuttle External Tank. Due to the expected limited commercial lifetime of this material, research efforts at the NASA Thermal Protection Systems Materials Research Laboratory at the Marshall Space Flight Center are now being devoted to the identification and development of alternatives with zero ozone depletion potential. Physical blowing agents identified to date have included hydrocarbons, fluorocarbons, hydrofluoroethers, and more predominantly, hydrofluorocarbons (HFCs). The majority of the HFC evaluations in industry have focused on the more readily available, low boiling candidates such as HFC 134a. Higher boiling HFC candidates that could be handled at ambient conditions and use current processing equipment would be more desirable. This paper will describe results from a research program of two such candidate HFC's performed as a cooperative effort between Martin Marietta Manned Space Systems, the U.S. Environmental Protection Agency, and Oak Ridge National Laboratories. The purpose of this effort was to perform a cursory evaluation of the developmental HFC's 245ca and 236ea as blowing agents in urethane based insulations. These two materials were selected from screening tests of 37 C2, C3, and C4 isomers based on physical properties, atmospheric lifetime, flammability, estimated toxicity, difficulty of synthesis, suitability for dual use as a refrigerant, and other factors. Solubility of the two materials in typical foam components was tested, pour foaming trials were performed, and preliminary data were gathered regarding foam insulation performance.
U.S. national and regional emissions of HFC-134a are derived for 2008-2012 based on atmospheric observations from ground and aircraft sites across the U.S. and a newly developed regional inverse model. Synthetic data experiments were first conducted to optimize the model assimilation design and to assess model-data mismatch errors and prior flux error covariances computed using a maximumlikelihood estimation technique. The synthetic data experiments also tested the sensitivity of derived national and regional emissions to a range of assumed prior emissions, with the goal of designing a system that was minimally reliant on the prior. We then explored the influence of additional sources of error in inversions with actual observations, such as those associated with background mole fractions and transport uncertainties. Estimated emissions of HFC-134a range from 52 to 61 Gg yr -1 for the contiguous U.S. during 2008-2012 for inversions using air transport from Hybrid Single-Particle Lagrangian Integrated Trajectory (HYSPLIT) model driven by the 12km resolution meteorogical data from North American Mesoscale Forecast System (NAM12) and all tested combinations of prior emissions and background mole fractions. Estimated emissions for 2008-2010 were 20% lower when specifying alternative transport from Stochastic Time-Inverted Lagrangian Transport (STILT) model driven by the Weather Research and Forecasting (WRF) meteorology. Our estimates (for HYSPLIT-NAM12) are consistent with annual emissions reported by U.S. Environmental Protection Agency for the full study interval. The results suggest a 10-20% drop in U.S. national HFC-134a emission in 2009 coincident with a reduction in transportation-related fossil fuel CO 2 emissions, perhaps related to the economic recession. All inversions show seasonal variation in national HFC-134a emissions in all years, with summer emissions greater than winter emissions by 20-50%.
Measurements of rate constants for HFC-134 (CF2HCF2H) relative to CH3CCl3, HFC-125, and HFC-134a are reported. The measurements were made in a slow-flow, temperature controlled photochemical reactor, and were based on relative rates of disappearance of the parent compounds as measured by FTIR spectroscopy. Hydroxyl radicals were generated by 254-nm photolysis of O3 in the presence of water vapor. NASA/JPL rate constants for the reference compounds are used to derive temperature-dependent rate constants of both compounds. Rate constants obtained from the different reference compounds are in excellent agreement. The presently recommended rate constant for HFC-134a is about 25 percent too high.
In this work, a ZrB{sub 2}-SiC-Ta{sub 4}HfC{sub 5}/Ta{sub 4}HfC{sub 5} oxidation-resistant dual-layer coating was fabricated to improve the oxidation resistance of carbon–carbon (C/C) composites. The coating was prepared by pack cementation combined with the slurry paste method. Spark plasma sintering was used in the procedure. The as-prepared dual-layer coating was approximately 110 μm, and no distinct interface was observed between the coating and the matrix. The isothermal oxidation test results showed that the dual coating effectively prevented C/C composites from oxidizing. The weight loss of the coated samples was only 3.3 and 9.5% after oxidation at 1773 K for 20 h and ten thermal shock cycles between 1773 K and room temperature in air, respectively. The pores and microcracks were the main reason for the failure of the coating.
Fusion temperature in refractory carbide systems
Explore the source record for details and available documents.
Solidia/CCSM received funding for further research and development of its Low Temperature Solidification Process (LTS), which is used to create hydrate-free concrete (HFC). LTS/HFC is a technology/materials platform that offers wide applicability in the built infrastructure. Most importantly, it provides a means of making concrete without Portland cement. Cement and concrete production is a major consumer of energy and source of industrial greenhouse gas (GHG) emissions. The primary goal of this project was to develop and commercialize a novel material, HFC, which by replacing traditional concrete and cement, reduces both energy use and GHG emissions in the built infrastructure. Traditional concrete uses Portland Cement (PC) as a binder. PC production involves calcination of limestone at ~1450°C, which releases significant amounts of CO 2 gas to the atmosphere and consumes a large amount of energy due to the high temperature required. In contrast, HFC is a carbonate-based hydrate-free concrete (HFC) that consumes CO 2 gas in its production. HFC is made by reaction of silicate minerals with CO 2 at temperatures below 100°C, more than an order-of-magnitude below the temperature required to make PC. Because of this significant difference in temperature, it is estimated that we will be able to reduce energy use in the cement and concrete industry by up to 30 trillion Btu by 2020. Because of the insulating properties of HFC, we believe we will also be able to significantly reduce energy use in the Building sector, though the extent of this saving is not yet quantified. It is estimated that production of a tonne of PC-based concrete requires about 6.2 million Btu of energy and produces over 1 tonne of CO 2 emissions (Choate, 2003). These can be reduced to 1.9 million Btu and 0.025 tonnes of CO 2 emissions per tonne of HFC (with overall CO 2 -negativity possible by increasing carbonation yield). In this way, by replacing PC-based concrete with HFC in infrastructure we can reduce energy use in concrete production by 70%, and reduce CO 2 emissions by 98%; thus the potential to reduce the impact of building materials on global warming and climate change is highly significant. Low Temperature Solidification (LTS) is a breakthrough technology that enables the densification of inorganic materials via a hydrothermal process. The resulting product exhibits excellent control of chemistry and microstructure, to provide durability and mechanical performance that exceeds that of concrete or natural stone. The technology can be used in a wide range of applications including facade panels, interior tiles, roof tiles, countertops, and pre-cast concrete. Replacing traditional building materials and concrete in these applications will result in significant reduction in both energy consumption and CO 2 emissions.
The purpose of this reasearch effort was to develop high temperature, oxidation resistant thrusters which would lessen the thruster cooling requirements, resulting in increased performance and longer life for onboard propulsion systems for spacecraft. This research effort focussed on developing ceramic matrix composites (CMCs) for this application, and specifically investigated the use of HfC stabilized with TaC. This material composition can potentially operate in a stoichiometric oxygen to hydrogen ratio at a temperature of 5000 deg F (2760 deg C) in a radiatively cooled mode. Various compositions of Hafnium Carbide (HfC) and Tantalum Carbide (TaC) were deposited by chemical vapor deposition (CVD) and tested, in an attempt to identify the composition which offered the best oxidation resistance. Although it was identified that small amounts of TaC appeared to offer improved oxidation resistance over HfC alone, an optimal composition was not identified. A 251bf thruster was fabricated from a novel CMC sandwich construction with a HfC-TaC matrix, and survived two test firings, each of 5 seconds before a failure in the injector caused the run to be aborted. It was not possible to control the relative stoichiometry of the HfC and TaC composition throughout the reactor due to the large difference in the thermodynamics of the HfC and TaC formation from their respective chlorides. This also resulted in an inability to infiltrate TaC into the preform under the experimental conditions investigated. Other material compositions were fabricated and tested and two material systems; HfC-SiC functionally graded to C(sub f)/C and Re functionally graded to C(sub f)/C were selected for further testing. These functionally graded composites have use in a number of propulsion applications presently of interest to NASA and the defense industry. Their ability to withstand extremely hostile thermal environments and the light-weight and high-strength exhibited from the C(sub f)/C composite make these materials particularly suited for these applications. In the Phase III which is presently underway, Re functionally graded to C(sub f)/C is being further developed and tested for application in the thrust cells for the Linear Aerospike Engine for the X33 and RLV.
Future-generation spacecraft components allude discovery of novel materials that can withstand extreme environments (>2000 °C). The combined effect of ultra-high temperature ceramics (UHTCs) and carbon fibers (C f ) can satisfy the demanding requirements of aerospace applications. A novel, hybrid, and flexible hafnium carbide (HfC)-decorated carbon nanofiber (C nf ) mat was fabricated via electrospinning. Enhanced thermal stability of the flexible HfC decorated C nf over C nf can be elucidated from the 20-fold increment in thermal conductivity and the onset of degradation at higher temperatures (840 °C). Successful integration of multi-layered sandwich lattice using in-housed fabricated HfC decorated C nf showed retention of the fibrous structure even after extreme spark plasma sintering (SPS) process at 1850 °C. Fabricating a similar multi-layered structure using procured C f was unsuccessful due to bundled agglomeration and micron-sized fibers. High-load indentation suggests that HfC decorated C nf interlayer is stronger (~2.3 times) than the parent UHTC with no cracking at the interface. Compared with the HfC matrix, the indentation-damaged area at the interface reduced up to ~56% due to toughening mechanisms such as C nf , fiber pull-out and bridging. The synthesized HfC decorated Cnf mat is proposed as an ultra-thin filler material for joining similar or dissimilar UHTCs while maintaining similar chemistry and better mechanical integrity at the interface. Furthermore, the findings insinuate a new paradigm in designing hybrid and flexible ceramic-containing materials for thermal protection systems (TPS) of future-generation spacecraft components that can mitigate failure in extreme environments (>2000 °C).
HfC has shown promise as a material for field emission due to the low work function of the (100) surface and a high melting point. Recently, HfC tips have exhibited unexpected failure after field emission at 2200K. Characterization of the HfC tips identified faceting of the parabolic tip dominated by coexisting (100) and (111) surfaces. To investigate this phenomenon, we used density functional theory (DFT) simulations to identify the role of defects and impurities (Ta, N, O) on HfC surface properties. Carbon vacancies increased the surface energy of the (100) surface from 2.35 J/m 2 to 4.75 J/m 2 and decreased the surface energy of the carbon terminated (111) surface from 8.75 J/m2 to 3.48 J/m 2 . Once 60% of the carbon on the (100) surface have been removed the hafnium terminated (111) surface becomes the lowest energy surface, suggesting that carbon depletion may cause these surfaces to coexist. The addition of Ta and N impurities to the surface are energetically favorable and decrease the work function, making them candidate impurities for improving field emission at high temperatures. Overall, DFT simulations have demonstrated the importance of understanding the role of defects on the surface structure and properties of HfC.
The chemistry of HCFC's and HFC's in the troposphere is controlled by reactions with OH in which a hydrogen atom is abstracted from the halocarbon to form water and a halo-alkyl radical. The halo-alkyl radical subsequently reacts with molecular oxygen to form a peroxy radical. The reactions of HCFC's and HFC's with O(exp1D) atoms are unimportant in the troposphere, but may be important in producing active chlorine of OH in the stratosphere. Here, the rate constants for the reactions of OH and O(exp1D) with many HFC's and HCFC's are evaluated. Recommendations are given for the five HCFC's and three HFC's specified by AFEAS as primary alternatives as well as for all other isomers of C1 and C2 HCFC's and HFC's where rate data exist. In addition, recommendations are included for CH3CCl3, CH2Cl2, and CH4.
Trifluoroacetic acid (TFA), a highly soluble and stable organic acid, is photochemically produced by certain anthropogenically emitted halocarbons such as HFC-134a and HFO-1234yf. Both these halocarbons are used as refrigerants in the automobile industry, and the high global warming potential of HFC-134a has promoted regulation of its use. Industries are transitioning to the use of HFO-1234yf as a more environmentally friendly alternative. In this work, we investigated the environmental effects of this change and found a 33-fold increase in the global burden of TFA from an annual value of 65 tonnes formed from the 2015 emissions of HFC-134a to a value of 2220 tonnes formed from an equivalent emission of HFO-1234yf. The percentage increase in surface TFA concentrations resulting from the switch from HFC-134a to HFO-1234yf remains substantial with an increase of up to 250-fold across Europe. The increase in emissions greater than the current emission scenario of HFO-1234yf is likely to result in significant TFA burden as the atmosphere is not able to disperse and deposit relevant oxidation products. The Criegee intermediate initiated loss process of TFA reduces the surface level atmospheric lifetime of TFA by up to 5 days (from 7 days to 2 days) in tropical forested regions.
Recently it was proposed (Jha et al., 1989; Whittenberger et al., 1990) on the basis of constant velocity testing at 1300 K that dispersion strengthened NiAl composites containing about 4 wt pct HfC possess threshold stresses for creep. Further, 1300 K compression testing has been conducted on NiAl+4HfC, and diametrically opposite behavior has been found: for constant load creep tests a normal power law behavior was observed. However, additional constant velocity testing still indicates that the flow stress is essentially independent of strain rate below 10 exp -6/s. Examination of NiAl+4.3HfC specimens deformed under constant velocity conditions revealed that the original hot extruded small grain structure could be converted to large, elongated grains during testing. Such a transformation appears to be responsible for the apparent threshold stress behavior in HfC dispersed NiAl.
Rapid solidification techniques in combination with HIPing have been used to produce Ti-48Al-2Mn-2Nb and a Ti-48Al-2Mn-2Nb+15 wt% HfC composite. While the composite does contain several second phases within the gamma + alpha(sub 2) matrix, none was identified to be HfC. The elevated-temperature properties were determined by constant velocity compression and constant load tensile testing in air between 1000 and 1173 K. Such testing indicated that the elevated temperature strengths of the HfC-modified aluminide was superior to those of the unreinforced matrix with the best 1100 K temperature slow strain rate properties for both materials being achieved after high-temperature annealing prior to testing. Examination of the microstructures after deformation in combination with the measured stress exponents and activation energies suggest that creep resistance of the HfC-modified form is due to solid-solution strengthening from carbon and hafnium rather than the presence of second phases.
In recent small and medium capacity refrigeration systems, the condenser tubes are provided with micro-fins from inside. The vapour refrigerant at the compressor outlet and the condenser inlet is in superheat state. As it advances in the condenser it is in two phases and at the outlet it is in sub cooled liquid. The heat transfer coefficient (HTC) during condensation of HFC-134a and R-404A in a smooth (8.56 mm ID) and micro-fin tubes (8.96 mm ID) are experimentally investigated. Different from previous studies, the present experiments are performed for various condensing temperatures, with superheating and sub cooling and using hermetically sealed compressor. The test runs are done at average saturated condensing temperatures ranging from 35 C to 60 C. The mass fluxes are between 90 and 800 kg m{sup -2} s{sup -1}. The experimental results indicate that the average HTC increases with mass flux but decreases with increasing condensing temperature for both smooth and micro-fin tubes. The average condensation HTCs of HFC-134a and R-404A for the micro-fin tubes were 1.5-2.5 and 1.3-2 times larger than that in smooth tube respectively. The HTCs for R-404A are less than that of HFC-134a. New correlations based on the data gathered during the experimentation for predicting condensation HTCs are proposed for wide range of operating conditions. (author)
The mechanical properties of swaged rod thermomechanically processed from arc-melted Mo-2Re-Hf-C alloys containing as much as 0.9 mol pct HfC have been evaluated. The low temperature ductilities of these alloys were not influenced by the amount of HfC present but by the amount of Hf in excess of stoichiometry. Maximum ductility occurred at 0.2 to 0.3 at. pct excess Hf. At 0.3 to 0.5 mol pct HfC, alloy strength varied directly with the Mo content of extracted carbide particles, both decreasing as the amount of excess Hf increased. Additions of 2 at. pct Re had little effect on strength or ductility. Tensile and creep strengths of Mo-2Re-0.7Hf-0.5C alloy equaled or exceeded those of other high strength Mo alloys.
The current knowledge of atmospheric degradation of hydrogen containing chlorofluorocarbons (HCFC 22 (CHClF2), HCFC 123 (CHCl2CF3), HCFC 124 (CHClFCF3), HCFC 141b (CFCl2CH3), HCFC 142b (CF2ClCH3)) and fluorocarbons (HFC 125 (CHF2CF3), HFC 134a (CH2FCF3), HFC 152a (CHF2CH3)) is assessed. Except for the initiation reaction by OH radicals, there are virtually no experimental data available concerning the subsequent oxidative breakdown of these molecules. However, from an analogy to the degradation mechanisms of simple alkanes, some useful guidelines as to the expected intermediates and final products can be derived. A noteable exception from this analogy, however, appears for the oxi-radicals. Here, halogen substitution induces new reaction types (C-Cl and C-C bond ruptures) which are unknown to the unsubstituted analogues and which modify the nature of the expected carbonyl products. Based on an evaluation of these processes using estimated bond strength data, the following simplified rules with regards to the chlorine content of the HCFC's may be deduced: (1) HCFC's containing one chlorine atom such as 22 and 142b seem to release their chlorine content essentially instantaneous with the initial attack on the parent by OH radicals, and for HCFC 124, such release is apparently prevented; (2) HCFC's such as 123 and 141b with two chlorine atoms are expected to release only one of these instantaneously; and the second chlorine atom may be stored in potentially long-lived carbonyl compounds such as CF3CClO or CClFO.