Search NASA⌕ Search

SEARCH · Search NASA

Results for “High-steam electrolysis”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

Engineering Thermally Resilient and Kinetically Active Reversible Protonic Ceramic Cells via Interfacial Design

Achieving concurrent fast electrode kinetics and long-term thermo-mechanical durability remains a critical challenge for reversible protonic ceramic electrochemical cells (R-PCECs). Herein, we report an interfacial engineering strategy that integrates a perovs.kite-type PrBaRu0.1Co1.9O5+δ (PBRC) nanoparticle layer onto a PrBa0.5Sr0.5Co1.5Fe0.5O5+δ (PBSCF) substrate (PBRC-PBSCF), together with a modified pellet-assisted sintering approach to fabricate dense BaZr0.4Ce0.4Y0.1Yb0.1O3-δ (BZCYYb4411) electrolytes. The in situ reconstructed heterointerface enhances oxygen reduction/evolution reaction (ORR/OER) kinetics, promotes H2O adsorption/dissociation, and improves steam tolerance, as verified by electrochemical measurements and interfacial microstructural analyses. Density functional theory reveals that Ru-induced electronic modulation at the PBRC-PBSCF interface lowers the energy of oxygen vacancy formation and optimizes the position of the O 2p band center, thereby accelerating oxygen redox kinetics and stabilizing the interface. The resulting R-PCECs deliver an excellent peak power density of 1.112 W cm−2 and an electrolysis current density of −1.257 A cm−2 at 1.3 V in 3% H2O wet air at 600°C, with a reasonable faradaic efficiency. Furthermore, the cells demonstrate excellent stability, sustaining 100 h of thermal cycling (400–600°C, 200°C h−1) in both fuel cell and electrolysis modes, with 600 h of stability in electrolysis mode (600°C, −0.5 to −2 A cm−2).

30 DIRECT ENERGY CONVERSION↗

Sintering protonic zirconate cells with enhanced electrolysis stability and Faradaic efficiency

The emerging applications of steam electrolysis and electrochemical synthesis at 300–600 °C set stringent requirements on the stability of protonic ceramic cells, which cannot be met by Ce-rich electrolytes. A promising candidate is Ce-free BaZr 0.8 Y 0.2 O 3–δ , but its usage has long been hindered due to the high sintering temperatures required for protonic devices. Here we resolved the issue through a co-sintering process, in which the shrinkage stress of a readily sinterable support layer helps to densify the pure BaZr 0.8 Y 0.2 O 3–δ electrolyte membrane at low temperatures. This approach eliminates Ce and harmful sintering aids in the dense zirconate electrolyte membrane, thereby enhancing the Faradaic efficiency and electrochemical stability, especially under harsh operating conditions. Here, the protonic zirconate cells have exceptional performance and demonstrate stable high-steam pressure electrolysis up to 0.7 atm steam pressure, –2 A cm –2 current density and over 800 h of dynamic operation at 600 °C. Our processing breakthrough enables stabilized protonic cells for demanding applications in future energy infrastructure.

25 ENERGY STORAGE↗

Unraveling Grain Boundary Instability in Dense Proton-Conducting Oxides

The long-term stability of protonic ceramic electrolysis cell (PCEC) materials under high-steam operating conditions remains a critical barrier to device commercialization. Here, we investigate the fundamental degradation mechanisms of dense BaCe 0.7 Zr 0.1 Y 0.1 Yb 0.1 O 3-δ (BCZYYb) electrolytes operated at 550 °C, 50% H 2 O in air. Over 1,000 h, the total electrolyte conductivity decreases by 11.1%, driven primarily by a >130% increase in grain-boundary resistivity. Post-mortem analyses reveal that damage is localized to near-surface grain boundaries extending ∼50 μm into the dense electrolyte pellet. This surface localization indicates that degradation is likely to be severe in thin, device-level electrolytes. Degradation is primarily attributed to chemo-mechanical grain-boundary weakening arising from hydration-induced chemical expansion, culminating in the formation of intergranular cracks oriented parallel to the pellet surface. These internal cracks subsequently react with steam and/or CO 2 , leading to the formation of nanoscale insulating phases, including Ba(OH) 2 , nanocrystalline BaCO 3 , and amorphous Ce/Zr/Y/Yb-containing oxides or hydroxycarbonates. After an initial degradation period of approximately 200 h, the overall conductivity stabilizes. Incorporating NiO sintering aids reduces grain-boundary density by an order of magnitude under identical sintering conditions. Although addition of NiO increases the initial resistivity by >160% at 550 °C, it substantially suppresses grain-boundary instability and mitigates chemical degradation. These findings underscore the urgent need for chemical and/or physical stabilization of BCZYYb electrolytes and offer design guidelines to enable durable, high-performance PCECs.

08 HYDROGEN↗