Thermo-Poro-Mechanical Modeling of RTV Intumescence

Room temperature vulcanizing (RTV) silicone is a high-temperature adhesive used as a gap-filler between heatshield tiles in numerous entry missions. Its propensity to intumesce, or swell upon exposure to heat, is a well-known effect that needs to be carefully quantified during design. At tile interfaces of charring ablators, intumescence, combined with differential recession, could cause the gap filler to protrude past the ablator outer mold line, forming a “fence”. Fencing can in turn cause transition to turbulence of the flow wetting the heat shield, leading to augmented surface heating. Recent experiments conducted at the Plasmatron X facility, the high enthalpy wind tunnel of the Center for Hypersonics and Entry Systems Studies, have shown prominent fencing of RTV gap fillers in PICA, under both nitrogen and air plasmas. Similar observations are well known in the arcjet literature. Further experiments under controlled environment, performed using in situ X-ray micro-computed tomography (micro-CT) at the Advanced Light Source (ALS), have shown heating rate-dependent swelling and shrinkage of RTV during pyrolysis. To simulate RTV intumescence, a novel model was introduced in the Porous Materials Analysis Toolbox based on OpenFOAM, PATO, to account for pore-pressure buildup within both closed- and open-pores. The governing equation for the thermo-poro-mechanical response were developed, assuming linear elasticity for the charring silicone. A new multi-pyrolysis model that tracks non-monotonic advancement of material properties with pyrolysis was proposed. This model addresses the limitations of state-of-the-art ablator models to capture the different stages of thermal degradation and coupled thermomechanics. Swelling of RTV was simulated using the new thermo-poro-mechanical model and compared against in situ micro-CT data. Results showed good agreement in intumescence height and temperature profiles at all heating rates, indicating that the key factor contributing to RTV swelling is the internal pressure build-up within closed- and open-pores. As RTV is cured into a soft (rubbery) compound with low-porosity and permeability, initial temperature increase and pyrolysis gas production cause a significant increase of internal pressure, causing a pronounced volume growth. As thermal degradation progresses, rigidization of the silicone occurs due to char hardening which counteract volume shrinkage after gas pressure relief. Overall, our model shows that accounting for changes in properties such porosity, permeability and key thermomechanical coefficients is crucial for capturing the RTV volume change during ablation and enable a predictive capability for heatshield tile interface response. A plan for future calibration of thermomechanical properties evolution during degradation is discussed, as a key next step to close the new model.

RTV

Thermo-Poro-Mechanical Modeling of RTV Intumescence

Room temperature vulcanizing (RTV) silicone is a high-temperature adhesive used as a gap-filler between heatshield tiles in numerous entry missions. Its propensity to intumesce, or swell upon exposure to heat, is a well-known effect that needs to be carefully quantified during design. At tile interfaces of charring ablators, intumescence, combined with differential recession, could cause the gap filler to protrude past the ablator outer mold line, forming a “fence”. Fencing can in turn cause transition to turbulence of the flow wetting the heat shield, leading to augmented surface heating. Recent experiments conducted at the Plasmatron X facility, the high enthalpy wind tunnel of the Center for Hypersonics and Entry Systems Studies, have shown prominent fencing of RTV gap fillers in PICA, under both nitrogen and air plasmas. Similar observations are well known in the arcjet literature. Further experiments under controlled environment, performed using in situ X-ray micro-computed tomography (micro-CT) at the Advanced Light Source (ALS), have shown heating rate-dependent swelling and shrinkage of RTV during pyrolysis. To simulate RTV intumescence, a novel model was introduced in the Porous Materials Analysis Toolbox based on OpenFOAM, PATO, to account for pore-pressure buildup within both closed- and open-pores. The governing equation for the thermo-poro-mechanical response were developed, assuming linear elasticity for the charring silicone. A new multi-pyrolysis model that tracks non-monotonic advancement of material properties with pyrolysis was proposed. This model addresses the limitations of state-of-the-art ablator models to capture the different stages of thermal degradation and coupled thermomechanics. Swelling of RTV was simulated using the new thermo-poro-mechanical model and compared against in situ micro-CT data. Results showed good agreement in intumescence height and temperature profiles at all heating rates, indicating that the key factor contributing to RTV swelling is the internal pressure build-up within closed- and open-pores. As RTV is cured into a soft (rubbery) compound with low-porosity and permeability, initial temperature increase and pyrolysis gas production cause a significant increase of internal pressure, causing a pronounced volume growth. As thermal degradation progresses, rigidization of the silicone occurs due to char hardening which counteract volume shrinkage after gas pressure relief. Overall, our model shows that accounting for changes in properties such porosity, permeability and key thermomechanical coefficients is crucial for capturing the RTV volume change during ablation and enable a predictive capability for heatshield tile interface response. A plan for future calibration of thermomechanical properties evolution during degradation is discussed, as a key next step to close the new model.

silicone intumescence

Optical properties of morphologically complex black carbon aerosols: Effects of coatings

Optical properties are computed for fractal-like aggregate black carbon (BC) aerosols coated with different substances. Two models are used for these aerosols: (i) the coated aggregate model (model I), where coating is added to the voids and surroundings of BC fractal-like aggregates; and (ii) the closed-cell aggregate model (model II), where coating is added concentrically to each monomer of BC fractal-like aggregates. Our results favor choosing the coated aggregate model (model I) to simulate scattering and absorption by coated BC aerosols because this model is morphologically more realistic, and because this model yields mass absorption cross section (MAC) and backscattering linear depolarization ratio (LDR) values that are consistent with field measurements. Moreover the corresponding computed degree of linear polarization (DoLP) and LDR values are very sensitive to changes in the coating volume fraction (fvol) and the coating refractive index (m). With the same absorbing BC core, the MAC value increases steadily with increasing fvol and m values. For example, using a density of 1.8 g/cm 3 and BC refractive index 1.95 + i0.79, the calculated MAC values for uncoated BC aggregates range from 6.2 to 6.8 m 2 /g at 0.55 µm. When coating material is applied to the BC aggregates, the calculated MAC values for model I particles increase to between 9.8 and 13.2 m 2 /g (depending on m) when fvol = 87.5%. The backscattering LDR values also tend to increase with the increasing m values for the shapes and sizes considered in our study. For model I particles, the backscattering LDR values span a wide range of 4.2–27.8% at a wavelength of 0.35 µm at fvol = 87.5% when m increases from 1.33 to 1.55. Our results are relevant to analyses of polarimetric and lidar observations of smoke particles, especially when these particles undergo hygroscopic growth.

Black carbon aerosols

Material Properties and Modeling of Room Temperature Vulcanizing Silicone

Room Temperature Vulcanizing silicone (RTV) is a high-temperature adhesive that has successfully been used as a gap-filler between Thermal Protection System (TPS) tiles for heatshields on numerous missions. It is also used to bond instrumentation plugs such as temperature and pressure sensors into the heatshields. While RTV has been traditionally assumed to be a non-porous and non-ablating material, numerous experiments have shown that RTV pyrolyzes and becomes highly porous as it is heated. Heating RTV has also shown swelling, or intumescence, which can pose unique problems that lead to roughness induced boundary-layer transition, surface oxide formation and contamination of heat shield sensors. Therefore, it is crucial to understand and model the intumescence phenomenon of RTV. As data for RTV material properties is limited, the first step in modeling RTV is to collect material properties such as pyrolysis mass-loss, microstructure change, virgin and char porosity, etc. which was performed in our initial study. Additionally, thermomechanical properties such as Young’s modulus and Poisson ratio are required for modeling the intumescence of RTV, which were taken from literature and the coefficient of thermal expansion was collected using in-situ heating and Micro Computed Tomography (µ-CT) in previous studies. Finally, numerous other properties such as pyrolysis gas properties, virgin and char thermal conductivity and specific heat were compiled from previous experiments and literature into a material database that can be used for simulations. In Porous Material Analysis Toolbox based on OpenFOAM (PATO) [4], structural mechanics coupled with material response was used for simulating the intumescence of RTV as it is heated. However, since the permeability of the material is very low, the pyrolysis gas creates an internal pressure build-up as the material is being heated, significantly contributing to the deformation of the material. To correctly characterize this phenomenon, additional physics models were implemented into PATO's stress analysis solver, and results were compared with RTV dilatometry test data as a preliminary verification case. Future work will include experiments of RTV at the Plasmatron X facility and the in-situ heating cell with µ-CT, and improvement of simulation tools to more accurately model RTV intumescence.

PATO