Search NASA⌕ Search

SEARCH · Search NASA

Results for “I-V”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

I-V curve analysis of single-nanoparticle Al-doped SrTiO 3

Strontium Titanate (SrTiO 3 or STO) is an oxide-semiconductor material which shows promise for photocatalytic water splitting, but remains poorly understood. To better understand its carrier dynamics, STO nanoparticles deposited onto an Au substrate were placed inside of a Scanning Electron Microscope (SEM) and then contacted with an Au probe. Current-voltage (I-V) measurements were taken with and without electron beam illumination. Fitting to the curves, we estimate the doping density ($N_D \approx 10^{22.1 \pm 1.2}$ cm$^{-3}$) and built-in potential ($\phi_{bi} \approx 0.84 \pm 0.45$ eV). We then used these I-V measurements to estimate the diffusion time ($\tau$) of our samples and observed an exponential dependence of $\tau$ on sample size in the range of 350-550 nm.

36 MATERIALS SCIENCE↗

Power modeling of degraded PV systems: Case studies using a dynamically updated physical model (PV-Pro)

Power modeling, widely applied for health monitoring and power prediction, is crucial for the efficiency and reliability of Photovoltaic (PV) systems. The most common approach for power modeling uses a physical equivalent circuit model, with the core challenge being the estimation of model parameters. Traditional parameter estimation either relies on datasheet information, which does not reflect the system's current health status, especially for degraded PV systems, or requires additional I-V characterization, which is generally unavailable for large-scale PV systems. Thus, we build upon our previously developed tool, PV-Pro (originally proposed for degradation analysis), to enhance its application for power modeling of degraded PV systems. PV-Pro extracts model parameters from production data without requiring I-V characterization. This dynamic model, periodically updated, can closely capture the actual degradation status, enabling precise power modeling. PV-Pro is compared with popular power modeling techniques, including persistence, nominal physical, and various machine learning models. The results indicate that PV-Pro achieves outstanding power modeling performance, with an average nMAE of 1.4 % across four field-degraded PV systems, reducing error by 17.6 % compared to the best alternative technique. Furthermore, PV-Pro demonstrates robustness across different seasons and severities of degradation. The tool is available as a Python package at https://github.com/DuraMAT/pvpro.

14 SOLAR ENERGY↗

BACKFLIP: A Comparison of Market-Benchmark Backsheet Technologies to Novel Non-Fluoro-Based Coextruded Materials and Their Correlation and Impact on PV Module Degradation Rates: Final Results of the Study at 4000 Hours or 2 Years

As the photovoltaic (PV) industry is rapidly expanding around the world, there has been an increasing interest in extending the lifespan of PV modules. Concern has also emerged regarding the recyclability of modules and their component materials, including fluoropolymer-based backsheets. Laminated polyethylene-terephthalate (PET) core backsheets have traditionally been used in the PV industry, but new, co-extruded polyolefin (PO) backsheets show promise as an improved alternative. Mini-module and coupon samples of seven different backsheets (made of layers including contemporary PET and fluoropolymers, novel PO, and polyamide (PA) materials) were run through hygrometric- or UV photolytic-accelerated aging to identify and better understand each material's degradation modes and the backsheets' field reliability. In addition to the artificial aging, the natural weathering methods used in this study are described. The comprehensive set of chemical, mechanical, and structural characterizations at intermittent read points in this study is presented, including: visual appearance and color; gloss; mechanical tensile testing; I-V performance; electroluminescence (EL) imaging; dielectric breakdown; FTIR-chemical structure; X-ray-polymer structure (WAXS); and DSC-crystalline content. After 4000 h of accelerated aging or 2y of outdoor aging, a strong correlation occurs between initial physical characteristics (mechanical tensile test) and operating performance (EL and I-V characteristics).

14 SOLAR ENERGY↗

Ohmic contact formation at the Au/Sr 3 Ir 2 O 7 interface

Here, using X-ray photoelectron spectroscopy (XPS), we show that Au forms an Ohmic contact with the surface of the narrow-bandgap Mott insulator Sr 3 Ir 2 O 7 thin films. XPS reveals no significant binding energy shift with increasing Au overlayer thickness on epitaxial Sr 3 Ir 2 O 7 (001) thin films, consistent with the linear current-voltage (I-V) behavior and indicative of negligible band bending. The absence of Schottky barrier formation at the Au/Sr 3 Ir 2 O 7 interface corroborates the metallic surface character of the Sr 3 Ir 2 O 7 thin film, as observed in angle-resolved photoemission spectroscopy (ARPES) studies, suggesting that the interface behaves effectively as a metal-on-metal contact. Furthermore, XPS points to the presence of distinct surface/interface and bulk electronic states for Sr 3 Ir 2 O 7 . This study provides critical material information for designing iridate-based electronic devices.

36 MATERIALS SCIENCE↗

Sub-1K Cold-Electron Quantum Well Switching at Room Temperature

Quantum states can provide means to systematically manipulate the transport of electrons. Here, in this study, we present electron transport across quasi-bound states of two heterogeneous quantum wells (QWs), where the transport of thermally excited electrons is blocked or enabled depending on the relative positions of the two quasi-bound states, with an abrupt current onset occurring when the two QW states align. The QW switch comprises a source (Cr), QW1 (Cr 2 O 3 ), QW2 (SnO x , x < 2), a tunneling barrier (SiO 2 ), and a drain (Si), where the effective electron mass of QW1 (m* QW1 ) is selected to be larger than QW2 (m* QW2 ). The current-voltage (I-V) measurements of the fabricated devices show abrupt current onsets, with the current transition occurring within 0.25 mV, corresponding to an effective electron temperature of 0.8 K at room temperature. Since transistor power consumption is fundamentally tied to effective electron temperature, this sub-1K cold-electron QW switching holds promise for highly energy-efficient computing.

Fermi−Dirac thermal smearing↗

Inductance meets memory in a quantum magnet

Orbital degrees of freedom offer a largely untapped route to emergent dynamical phenomena in correlated quantum materials. However, it remains unclear whether collective orbital states can intrinsically generate both reactive and memory functionalities in a bulk system. Here we show that in the ferrimagnet Mn₃Si₂Te₆, nonequilibrium reconfiguration of chiral orbital currents produces both emergent inductance and nonvolatile memristance as intrinsic properties of a single crystal. At low frequency and under a magnetic field along the c axis, coherent orbital-current domains generate robust clockwise inductive I-V loops. At higher frequency and low field, current-driven first-order reconfiguration leads to incomplete reversal and metastable trapping, producing an intrinsic electromotive force and a finite remanent voltage at zero current. These results establish orbital currents as a class of quantum state variables that encode both reactive and memory functionalities, opening routes toward intrinsically reconfigurable and energy-efficient electronic systems.

Cao, Tristan [University of Colorado, Boulder]↗

Nm-scale electrical resistance imaging on CdTe by scanning spreading resistance microscopy

Local resistance imaging can provide information on nm-scale carrier distribution in semiconductor devices. Scanning spreading resistance microscopy (SSRM), an atomic force microscopy-based nm-scale resistance mapping technique, has been developed for carrier delineation in Si microdevices. We report on the development and validation of SSRM on CdTe materials, by testing on molecular beam epitaxy (MBE) grown CdTe films. The probe/CdTe contact resistance was suppressed sufficiently below sample's spreading resistance by pressing the probe into the sample with ∼mN contact force and applying a large sample/probe forward bias voltage (V s ), which was understood by analyzing current-voltage (I-V) involving a serially connected insulating top layer with underlying spreading resistance. The carrier concentration as deduced from the resistance measurement, using a single mobility value, is consistent with Hall measurement with a standard deviation of 14% based on a set of MBE films with carrier concentrations in the range of 10 15 –10 16 /cm 3 . The doping polarity was readily identified by flipping V s polarity, where the resistance with reverse V s is orders of magnitude larger than forward V s . While focusing on the SSRM technique validation, we also show an example on an As-doped Cd(Se,Te) polycrystalline thin film of a high-performance CdTe solar cell, which illustrates the local resistance nonuniformity with up to two orders of magnitude differences, indicating if local mobility is roughly constant, local carrier concentration can have significant nonuniformity.

14 SOLAR ENERGY↗

Impact of proton irradiation on 4H-SiC Low Gain Avalanche Detectors (LGADs)

Silicon carbide (SiC) particle detectors have the potential to provide time resolutions and robust performance in extreme environments which exceed that of silicon detectors. In this work 4H-SiC low gain avalanche detectors (LGADs) and complementary PiN diodes were irradiated with 2.5 GeV protons at fluences up to 3.33 × 10 14 p/cm 2 . The electrostatic performance of both irradiated and non-irradiated devices was evaluated using I-V and C-V measurements. Moreover, charge collection measurements using α particles were also conducted. SiC LGADs displayed a loss in rectification, high ON-state resistances >10 10 Ω-cm 2 , and the complete removal of gain when exposed to the highest proton fluence. Additionally, the reductions in capacitance and OFF-state current pointed to compensation of the gain layer as a gain reducing mechanism. The introduction of radiation-induced defects also hinders carrier acceleration, which reduces impact ionization and further gain reduction. LGADs exposed to a fluence of 1 × 10 14 p/cm 2 experienced a partial recovery in gain (originally having a value of ∼ 2) with a value of ∼ 1.65 when applying a bias of 500 V. Charge trapping was also seen in the reduction of charge collection efficiency (CCE) to ∼ 65% for the PiN diode. However, despite the reduction in device performance, the demonstration of a measurable signal after irradiation points to the potential of SiC LGAD detectors for future high energy physics applications.

43 PARTICLE ACCELERATORS↗

Different Damp-Heat-Induced Series Resistance Degradation Behaviors in Fielded Crystalline Silicon Photovoltaic Modules Due to Difference in Bill of Materials

This case study investigates mono-crystalline silicon modules from underperforming portions of a utility-scale photovoltaic power plant. Field-collected I-V curves and electroluminescence imaging suggested that increased series resistance was a primary factor driving module degradation. Selected modules were removed from the field for further analysis, including incremental damp heat accelerated testing, which confirmed a progression in series resistance degradation. Two distinct cell degradation behaviors became apparent during the investigation. Cross-sectional scanning electron microscopy (with elemental analysis) and scanning spreading resistance microscopy identified key differences between the two degradation mechanisms, primarily grid finger width and contact resistance. Additionally, the study highlights the reliability implications of retest requirements in International Electrotechnical Commission 61215 for material changes and how they may have mitigated the degradation observed at this site.

14 SOLAR ENERGY↗

In-Situ Luminescence Imaging of Perovskite Solar Cells Demonstrates Increasing Spatial Nonuniformity Upon Light-Soaking Degradation

In this work we investigate degradation rates of triplecation mixed-halide perovskite p-i-n solar cells. We present an accelerated stress testing procedure using periodic blue light-soaking at elevated temperatures until devices reach ~80% of their initial efficiency. We track light-induced degradation via in-situ: photoluminescence (PL), current-voltage (I-V) curves, and transient photovoltage. Devices underwent 165 hours of light bias at 65degrees C. Results suggest that spatial uniformity in PL intensity decreases as device degradation increases. This investigation lays the groundwork to address the current gap in understanding the interplay between device performance and the evolution of macroscopic features in perovskite solar cells. Thus, we believe spatial characterization techniques will play a crucial role in the commercialization of perovskite solar cells.

imaging↗

Diagnosis of PV Cell Passivation Degradation Resulting from Hot-Humid, High Voltage Potential Aging

Corrosion of the antireflective coating on the cell ("AR c corrosion") was previously observed in studies using hot-humid test conditions with external high voltage (HV) bias. Because AR c corrosion is not well understood, mini-modules (MiMos) were examined in a comparative experiment using PERC and PERT as well as legacy Al-BSF cells. For separate MiMos with the cell circuit electrical at +1500 V, -1500 V, or unbiased "V oc", test conditions in the comparative study included 60degrees C/60% RH for 96 h, as in IEC TS 62804-1; 70degrees C/70%RH for 200 h; and 85degrees C/85% RH for 200 h. Characterizations at each read point included: camera and electroluminescence (EL) imaging, colorimetry, and I-V curve tracing. Characterizations at the final read point included: SunsVoc; spatially mapping external quantum efficiency (EQE); high resolution: photoluminescence (PL), EL, and dark lock-in thermographic (DLIT) imaging. Forensics were performed on extracted cores, including scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS) and scanning Auger microscopy (SAM). Forensics were also conducted on MiMos (stepped HV aging) and full-sized modules (outdoor aging) from previous studies. AR c corrosion was specifically observed for the glass/encapsulant/cell side of +1500 V (HV+) stressed MiMos, where appearance, color, and reflectance were the characteristics most distinguished relative to simultaneously occurring degradation modes. SEM/EDS and SAM identified conversion of silicon nitride to silicon oxide or hydrous silica, preferentially occurring at the edges and tips of the pyramidal textured cell surface.

aging↗

Neuromorphic ionic computing in droplet interface synapses

Ionic devices with memory capabilities can emulate neural functionality, enabling neuromorphic computing and biomedical applications. In this study, we report an ionic spiking synapse based on aqueous droplet interface bilayer assembly. Under stepwise triangular voltages, the device displays coupled memcapacitive-memristive behavior, showing noncrossing pinched hysteretic I-V loops. This hysteretic ion dynamics can be regulated by modifying bilayer components, reconstituting protein channels, or adjusting droplet assembly configuration. Droplet interface synapses (DIS) exhibit fundamental neuromorphic behaviors such as paired-pulse facilitation/depression, spike rate–dependent plasticity, Hebbian learning, and short-term associative learning under classical conditioning. We also used reservoir computing with DIS to implement two learning algorithms: a classification algorithm that recognizes handwritten digits and a reinforcement learning algorithm that learns to play a board game of tic-tac-toe.

Li, Zhongwu [Lawrence Livermore National Laborator↗

Spectral Efficiency and Tandem Performance Calculators [SWR-24-92]

The Spectral Efficiency and Tandem Performance Calculators allow users to test material types for use in tandem photovoltaic devices to better understand if a given material could work well. The Spectral Efficiency (SE) calculator takes a set of current vs voltage (I-V) and quantum efficiency (QE) data along with a spectrum input and plots the spectral efficiency of the cells represented by the datasets for the spectrum provided. The Tandem Performance calculator uses the calculated spectral efficiency of top and bottom cells and the transmission data of the top cell to calculate performance metrics for a tandem device in either a two or four terminal architecture. The SE and Tandem Performance calculators are based on the following publication: Yu, Z., Leilaeioun, M. & Holman, Z. Selecting tandem partners for silicon solar cells. Nat Energy 1, 16137 (2016).

Warren, Emily↗

Cholla Galactic OutfLow Simulations (CGOLS)

These datasets contain full hydro-field snapshots from the galactic outflow simulations in the CGOLS suite, models I-V. The datasets were generated using the Cholla hydrodynamics code (https://github.com/cholla-hydro/cholla); descriptions of the models are in the associated publications (Schneider & Robertson 2018, ApJ; Schneider et al. 2018, ApJ; Schneider et al. 2020, ApJ; and Schneider & Mao, 2024, ApJ). Each hdf5 dataset is numbered according to the simulation time of the snapshot, in Myr. Fields include density, x momentum, y momentum, z momentum, total energy, and thermal energy (for models I - III), as well as a passive scalar field (models IV and V). 2 dimensional density and temperature projections, as well as slices along each midplane are also included if they exist.

79 ASTRONOMY AND ASTROPHYSICS↗

Roles of temperature, materials, and domain inversion in high-performance, low-bias-drift thin film lithium niobate blue light modulators

We demonstrate a thin film lithium niobate electro-optic modulator operating at 456 nm with an RF voltage-length product of 0.38 V-cm and a bandwidth of 6.9 GHz. We test the dielectric relaxation of the modulator with sweeps of temperature and optical input power, and compare equivalent modulators with electrode materials of Cr-Au, Ti-Au and Al in terms of bias stability and current-voltage characteristics. We demonstrate bias stability over at least 8 hours with Al devices, and show relationships between drift, I-V characteristics and ferroelectric domain switching.

Celik, Oguz Tolga (ORCID:0000000264542306)↗

Diagnosis of PV Cell Antireflective Coating Degradation Resulting from Hot-Humid, High Voltage Potential Aging

Corrosion of the antireflective coating on a photovoltaic cell ("ARc corrosion") has previously been observed in studies using hot-humid test conditions with external high-voltage (HV) bias. This study primarily focuses on known vulnerable, legacy aluminum back surface field (Al-BSF) cells in mini-modules (MiMos) put through comparative stepped stress tests. Each cell type had MiMos at +1500 V, -1500 V, or unbiased ("Voc") potential, which were sequentially subjected to test conditions of 60deg C/60% relative humidity (RH) for 96 h, as in International Electrotechnical Commission (IEC) Technical Specification 62804-1; 70 deg C/70% RH for 200 h; and 85 deg C/85% RH for 200 h. Characterizations at each step included visual camera and electroluminescence (EL) imaging, colorimetry, and current-voltage (I-V) curve tracing. Final characterizations included: Suns-Voc; spatial mapping of external quantum efficiency (EQE); high-resolution photoluminescence (PL), EL, and dark lock-in thermography (DLIT) imaging. Forensics were performed on extracted cores, including scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS), X-ray photoelectron spectroscopy (XPS), and scanning Auger microscopy (SAM). Forensics were also conducted on MiMos from previous studies that underwent stepped HV aging and separate outdoor aged full-sized modules. ARc corrosion was specifically seen for the glass/encapsulant/cell side of the +1500V (HV+) stressed MiMos and modules. Appearance, color, and reflectance were the most distinguishing characteristics relative to glass corrosion, gridline-corrosion and -delamination as well as other concurrent degradation modes. SEM/EDS and SAM identified conversion of silicon nitride to hydrated silica, hydrous silica, or hydrated amorphous silica, which preferentially occurred at the edges and tips of the pyramidal textured cell surface.

14 SOLAR ENERGY↗

Fabrication of 4H-SiC Low Gain Avalanche Detectors (LGADs)

Low gain avalanche detectors (LGADs) offer high temporal resolution for high energy particle detection, which is critical for next generation experiments in hadron colliders. While silicon LGADs (Si-LGADs) have rapidly matured in the last decade, research into silicon carbide (SiC) LGADs has only recently begun. By accounting for fundamental differences in material properties and fabrication processes, we present a prototype device design and process flow for 4H-SiC LGADs with etch-based isolation. Critical steps of the process flow and their results are discussed, including plasma etching, passivation, and the formation of low resistivity contacts. Electrical characterization (I-V, C-V) shows sufficient depletion of the device structure to demonstrate low-gain charge carrier multiplication.

High Energy Physics↗

Field Testing of PID-p Susceptible Bifacial PERC Modules: Impact of Light, Voltage and Module History ​

This work investigates the potential induced degradation-polarization (PID-p) of bifacial passivated emitter and rear contact (PERC) modules installed in the field at the Florida Solar Energy Center. 22 modules were stressed over 1 year under various voltage (-1500V, -3500, +1500V) and mounting configurations (close to ground, 2 meters from ground, close to roof). The positively stressed modules were anticipated to have experiences PID-p on their front side. However, no degradation was observed, as the light-induced recovery effect effectively counteracted the degradation. The negatively stressed modules experienced Pmax drops during 2 weeks before stabilizing at 5-6% loss. I-V and EL characteristics suggest a PID-p degradation on the rear side. Lower degradation rates are observed with lower voltage and when the mounting configuration allows more albedo light on the rear side to compensate for the degradation. PID-p is observed to stabilize at similar level for the voltage and mounting configuration tested with slightly lower Pmax in winter. EL imaging reveals that cells are not degrading at the same rate across a module. Some cells get darker and then brighter which corresponds to the silicon/passivation interface going through depletion and then inversion when enough positive charges are accumulated. After full light-recovery, the modules were tested again along with 22 brand-new ones to assess the impact of the module history. Results confirmed the trends observed in the first year with PID-p occurring at voltage as low as -600V and recovered modules degrading faster than brand-new ones.

14 SOLAR ENERGY↗