Search NASA⌕ Search

SEARCH · Search NASA

Results for “INCOLOY 800H”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Microstructural characterization of dissimilar welds between Incoloy 800H and 321 Austenitic Stainless Steel

In this work, the microstructural character of dissimilar welds between Incoloy 800H and 321 Stainless Steel has been discussed. The microscopic examination of the base metals, fusion zones and interfaces was characterized using an optical microscope and scanning electron microscopy. The results revealed precipitates of Ti (C, N) in the austenitic matrix along the grain boundaries of the base metals. Migration of grain boundaries in the Inconel 82 weld metal was very extensive when compared to Inconel 617 weldment. Epitaxial growth was observed in the 617 weldment which increases the strength and ductility of the weld metal. Unmixed zone near the fusion line between 321 Stainless Steel and Inconel 82 weld metal was identified. From the results, it has been concluded that Inconel 617 filler metal is a preferable choice for the joint between Incoloy 800H and 321 Stainless Steel. - Highlights: • Failure mechanisms produced by dissimilar welding of Incoloy 800H to AISI 321SS • Influence of filler wire on microstructure properties • Contemplative comparisons of metallurgical aspects of these weldments • Microstructure and chemical studies including metallography, SEM–EDS • EDS-line scan study at interface.

36 MATERIALS SCIENCE↗

Hydrogen Permeability of Incoloy 800H, Inconel 617, and Haynes 230 Alloys

A potential issue in the design of the NGNP reactor and high-temperature components is the permeation of fission generated tritium and hydrogen product from downstream hydrogen generation through high-temperature components. Such permeation can result in the loss of fission-generated tritium to the environment and the potential contamination of the helium coolant by permeation of product hydrogen into the coolant system. The issue will be addressed in the engineering design phase, and requires knowledge of permeation characteristics of the candidate alloys. Of three potential candidates for high-temperature components of the NGNP reactor design, the hydrogen permeability has been documented well only for Incoloy 800H, but at relatively high partial pressures of hydrogen. Hydrogen permeability data have been published for Inconel 617, but only in two literature reports and for partial pressures of hydrogen greater than one atmosphere, far higher than anticipated in the NGNP reactor. The hydrogen permeability of Haynes 230 has not been published. To support engineering design of the NGNP reactor components, the hydrogen permeability of Inconel 617 and Haynes 230 were determined using a measurement system designed and fabricated at the Idaho National Laboratory. The performance of the system was validated using Incoloy 800H as reference material, for which the permeability has been published in several journal articles. The permeability of Incoloy 800H, Inconel 617 and Haynes 230 was measured in the temperature range 650 to 950 °C and at hydrogen partial pressures of 10-3 and 10-2 atm, substantially lower pressures than used in the published reports. The measured hydrogen permeability of Incoloy 800H and Inconel 617 were in good agreement with published values obtained at higher partial pressures of hydrogen. The hydrogen permeability of Inconel 617 and Haynes 230 were similar, about 50% greater than for Incoloy 800H and with similar temperature dependence.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Tritium Permeability of Incoloy 800H and Inconel 617

Design of the Next Generation Nuclear Plant (NGNP) reactor and its high-temperature components requires information regarding the permeation of fission generated tritium and hydrogen product through candidate heat exchanger alloys. Release of fission-generated tritium to the environment and the potential contamination of the helium coolant by permeation of product hydrogen into the coolant system represent safety basis and product contamination issues. Of the three potential candidates for high-temperature components of the NGNP reactor design, only permeability for Incoloy 800H has been well documented. Hydrogen permeability data have been published for Inconel 617, but only in two literature reports and for partial pressures of hydrogen greater than one atmosphere, far higher than anticipated in the NGNP reactor. To support engineering design of the NGNP reactor components, the tritium permeability of Inconel 617 and Incoloy 800H was determined using a measurement system designed and fabricated at Idaho National Laboratory. The tritium permeability of Incoloy 800H and Inconel 617, was measured in the temperature range 650 to 950°C and at primary concentrations of 1.5 to 6 parts per million volume tritium in helium. (partial pressures of 10 -6 atm - three orders of magnitude lower partial pressures than used in the hydrogen permeation testing). The measured tritium permeability of Incoloy 800H and Inconel 617 deviated substantially from the values measured for hydrogen. This may be due to instrument offset, system absorption, presence of competing quantities of hydrogen, surface oxides, or other phenomena. Due to the challenge of determining the chemical composition of a mixture with such a low hydrogen isotope concentration, no categorical explanation of this offset has been developed.

08 HYDROGEN↗

Tritium Permeability of Incoloy 800H and Inconel 617

Design of the Next Generation Nuclear Plant (NGNP) reactor and its high-temperature components requires information regarding the permeation of fission generated tritium and hydrogen product through candidate heat exchanger alloys. Release of fission-generated tritium to the environment and the potential contamination of the helium coolant by permeation of product hydrogen into the coolant system represent safety basis and product contamination issues. Of the three potential candidates for high-temperature components of the NGNP reactor design, only permeability for Incoloy 800H has been well documented. Hydrogen permeability data have been published for Inconel 617, but only in two literature reports and for partial pressures of hydrogen greater than one atmosphere, far higher than anticipated in the NGNP reactor. To support engineering design of the NGNP reactor components, the tritium permeability of Inconel 617 and Incoloy 800H was determined using a measurement system designed and fabricated at Idaho National Laboratory. The tritium permeability of Incoloy 800H and Inconel 617, was measured in the temperature range 650 to 950°C and at primary concentrations of 1.5 to 6 parts per million volume tritium in helium. (partial pressures of 10-6 atm)—three orders of magnitude lower partial pressures than used in the hydrogen permeation testing. The measured tritium permeability of Incoloy 800H and Inconel 617 deviated substantially from the values measured for hydrogen. This may be due to instrument offset, system absorption, presence of competing quantities of hydrogen, surface oxides, or other phenomena. Due to the challenge of determining the chemical composition of a mixture with such a low hydrogen isotope concentration, no categorical explanation of this offset has been developed.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Impact of corrosion test container material in molten fluorides

The effects of crucible material choice on alloy corrosion rates in immersion tests in molten LiF–NaF–KF (46.5–11.5-42 mol. %) salt held at 850 °C for 500 hrs are described. Four crucible materials were studied. Molten salt exposures of Incoloy-800H in graphite, Ni, Incoloy-800H, and pyrolytic boron nitride (PyBN) crucibles all led to weight-loss in the Incoloy-800H coupons. Alloy weight loss was ~30 times higher in the graphite and Ni crucibles in comparison to the Incoloy-800H and PyBN crucibles. It is hypothesized galvanic coupling between the alloy coupons and crucible materials contributed to the higher corrosion rates. Alloy salt immersion in graphite and Ni crucibles had similar weight-loss hypothesized to occur due to the rate limiting out diffusion of Cr in the alloys to the surface where it reacts with and dissolves into the molten salt, followed by the reduction of Cr from solution at the molten salt and graphite/Ni interfaces. As a result, both the graphite and the Ni crucibles provided sinks for the Cr, in the formation of a Ni–Cr alloy in the case of the Ni crucible, and Cr carbide in the case of the graphite crucible.

14 SOLAR ENERGY↗

Challenges and successes in establishing a multipurpose fuels and materials irradiation capsule [Slides]

This presentation discusses the challenges and success related to designing and fabricating multipurpose capsules for irradiation experiments for irradiation within the Advanced Test Reactor (ATR) to be presented at tje DEVICE-MTR irradiation experiment design working group meeting hosted by the Japanese Atomic Energy Agency (JAEA). The information herein is limited to the design of the capsules only and no programmatic information from any project supporting the design of the multipurpose capsule is discussed. The intent of the design team was establish a capsule design that could accommodate multiple different irradiation project needs for the irradiation of nuclear fuel and materials of interest in the nuclear field. The main points of the presentation are as follows: use of tin as a molten thermal bond material was selected for the fueled capsule design and was found to be inadequate as it would corrode the stainless steel at high temperatures, this capsule design has high sensitivity to manufacturing of the gas gap and control of the gas mixture, and the fueled capsule has experienced welding challenges with the inner capsule material 800H Incoloy.

42 ENGINEERING↗

Ways of improvement for the materials of sodium cooled fast reactors

The French sodium cooled prototype reactor ASTRID will take into account 'Generation IV' requirements, especially a long operational life-time (60 years) and a high efficiency. The good behavior of austenitic steel AISI316L(N), should be confirmed for a use, in moderately irradiated and unirradiated parts of ASTRID. Parts recovered from dismantled French sodium-cooled reactors will be characterized. Further experiments must be carried out concerning ageing of these components. Other materials will be chosen for fuel wrapping and cladding, in order to reduce creep and swelling under irradiation, (either conventional, or oxide-dispersed strengthened steels (ODSS). Corrosion of ODSS in the presence of sodium needs a serious assessment The lifetime of primary pumps components made of Duplex steels should also be assessed. The disruptions in steam generator tubes should be minimized and controlled; therefore, optimised designs and geometries must be established before defining the corresponding materials. Either Modified 9Cr1Mo or Incoloy 800H, might be candidates;it will be necessary to check whether austenitic steels are compatible with Modified 9Cr1Mo or Incoloy 800H in the same circuit. For all materials, the best manufacturing processes must be combined with thermal, mechanical treatments; calculations of phase diagrams (CALPHAD) might be used to optimise both treatments and chemical compositions. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Next Generation Nuclear Plant Steam Generator and Intermediate Heat Exchanger Materials Research and Development Plan

DOE has selected the High Temperature Gas-cooled Reactor (HTGR) design for the Next Generation Nuclear Plant (NGNP) Project. The NGNP will demonstrate the use of nuclear power for electricity and hydrogen production. It will have an outlet gas temperature in the range of 900°C and a plant design service life of 60 years. The reactor design will be a graphite moderated, helium-cooled, prismatic or pebble-bed reactor and use low-enriched uranium, Tri-Isotopic (TRISO)-coated fuel. The plant size, reactor thermal power, and core configuration will ensure passive decay heat removal without fuel damage or radioactive material releases during accidents. The NGNP Materials Research and Development (R&D) Program is responsible for performing R&D on likely NGNP materials in support of the NGNP design, licensing, and construction activities. Today’s high-temperature alloys and associated ASME Codes for reactor applications are approved up to 760°C. However, some primary system components, such as the Intermediate Heat Exchanger (IHX) for the NGNP will require use of materials that can withstand higher temperatures. The thermal, environmental, and service life conditions of the NGNP will make selection and qualification of some high-temperature materials a significant challenge. Examples include materials for the core barrel and core internals, such as the control rod sleeves. The requirements of the materials for the IHX are among the most demanding. Selection of the technology and design configuration for the NGNP must consider both the cost and risk profiles to ensure that the demonstration plant establishes a sound foundation for future commercial deployments. The NGNP challenge is to achieve a significant advancement in nuclear technology while at the same time setting the stage for an economically viable deployment of the new technology in the commercial sector soon after 2020. A number of solid solution strengthened nickel based alloys have been considered for application in heat exchangers and core internals for the NGNP. The primary candidates are Inconel 617, Haynes 230, Incoloy 800H and Hastelloy XR. Based on the technical maturity, availability in required product forms, experience base, and high temperature mechanical properties all of the vendor pre-conceptual design studies have specified Alloy 617 as the material of choice for heat exchangers. Also a draft code case for Alloy 617 was developed previously. Although action was suspended before the code case was accepted by ASME, this draft code case provides a significant head start for achieving codification of the material. Similarly, Alloy 800H is the material of choice for control rod sleeves. In addition to the above listed considerations, Alloy 800H is already listed in the nuclear section of the ASME Code; although the maximum use temperature and time need to be increased.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Temperature-dependent mechanism on hardening mitigation in thermomechanically processed 800H alloys under neutron irradiation

Irradiation induced hardening is commonly observed in structural materials, and is often associated with the degraded ductility. This study explores the role of thermomechanical processing (TMP) in mitigating irradiation-induced hardening in Incoloy 800H. The radiation response of solution-annealed and TMP-treated samples was systematically investigated to elucidate the underlying mechanisms of hardening reduction. Neutron irradiation was performed on solution-annealed and TMP-treated samples at 359, 431, and 580 °C, revealing consistently lower hardening in TMP samples. Microstructural characterization compared dislocation loops, cavities, clusters, and precipitates to assess their contributions to hardening. The strengthening contributions from individual microstructural features were estimated, and the microstructure-derived yield strength is consistent with the hardness-converted yield strength. The microstructure–properties correlation revealed the temperature-dependent primary hardening mechanism: dislocation loops dominated at lower temperature, whereas Ni3(Al,Ti) γ′ precipitates were predominant at higher temperature. TMP reduced radiation-induced hardening through two mechanisms: (1) increased sink strength from dislocations and Ti(C,N) precipitates limited dislocation loop formation at lower temperatures, and (2) reduced Ti solute within the matrix in TMP samples suppressed γ′ precipitate formation at higher temperatures. These findings identify the mechanisms governing radiation-induced hardening across different temperatures, which lays the foundation for TMP optimization for the development of advanced radiation-tolerant materials.

Zhong, Weicheng [ORNL] (ORCID:0000000231589271)↗

An elastoplastic finite element study of cylindrical plane-strain contact for steel/steel and Inconel 617/Incoloy 800H undergoing unidirectional sliding

The current work employs a two-dimensional plane strain finite element analysis to investigate the unidirectional sliding contact between a deformable half-cylinder and a deformable flat block. The unidirectional sliding is governed by a displacement-controlled action where the materials of the two contacting bodies are first set to identical steels at 20 ℃ and then to Inconel 617 and Incoloy 800H at 800 ℃. First, a normal interference (indentation) is applied, which is followed by unidirectional sliding. The von Mises stress distribution, plastic strain distribution, junction growth, normal force, tangential force, effective coefficient of friction, and scars on the surface of the block are obtained during the sliding motion. The leading edge of the contacting area and the bulk material under the leading edge experience large von Mises stresses. The large plastic strain is found on the surface of the block, and forms a “pocket” shape under the surface. The junction growth is also investigated, showing the direction of the growth is in the same direction of the tangential force that the weaker material experiences. The forces and the effective coefficient of friction are found to stabilize after a certain sliding distance, and the effective coefficient of friction converges to the coefficient of friction used in the model. Pileup is found on the surface of the block after a sufficient unidirectional sliding distance.

Yang, Huaidong↗

Multilayered Coatings for High-Temperature Steam Oxidation: TGA Studies up to 1000 °C

The aim of the study was to obtain a preliminary data focused on the steam oxidation performance of multilayered coatings deposited on 310 stainless steel and 800H Incoloy. The coatings were obtained through the aluminizing thermal diffusion technology with the formation of aluminides; some coating options had an additional top layer of selected composition. In this study, five different coating systems, as well as uncoated metals, were exposed at 1000 °C using thermogravimetric analysis instrumentation simulating an initial stage of steam oxidation corrosion. In this work, along with determination of the mass change of the samples, microanalyses using light optical microscopy, scanning electron microscopy (SEM) equipped with energy x-ray dispersive spectrometry (EDS), as well as surface micro-hardness determination, have been carried out. The designed coating systems demonstrated promising high-temperature steam oxidation performance with no breakaway degradation issues.

36 MATERIALS SCIENCE↗

Corrosion of alloys in a chloride molten salt (NaCl-LiCl) for solar thermal technologies

Next-generation solar power conversion systems in concentrating solar power (CSP) applications require high-temperature advanced fluids in the range of 600–800 °C. Current commercial CSP plants use molten nitrate salt mixtures as the heat transfer fluid and the thermal energy storage (TES) media while operating with multiple hours of energy capacity and at temperatures lower than 565 °C. At higher temperatures, the nitrates cannot be used because they decompose. Molten chloride salts are candidates for CSP applications because of their high decomposition temperatures and good thermal properties; but they can be corrosive to common alloys used in vessels, heat exchangers, and piping at these elevated temperatures. In this article, we present the results of the corrosion evaluations of several alloys in eutectic 34.42 wt% NaCl – 65.58 wt% LiCl at 650–700 °C in nitrogen atmosphere. Electrochemical evaluations were performed using open-circuit potential followed by a potentiodynamic polarization sweep. Corrosion rates were determined using Tafel slopes and Faraday's law. A temperature increase of as little as 50 °C more than doubled the corrosion rate of AISI stainless steel 310 and Incoloy 800H compared to the initial 650 °C test. These alloys exhibited localized corrosion. Inconel 625 was the most corrosion-resistant alloy with a corrosion rate of 2.80±0.38 mm/year. For TES applications, corrosion rates with magnitudes of a few millimeters per year are not acceptable because of economic considerations. Additionally, localized corrosion (intergranular or pitting) can be catastrophic. Furthermore, corrosion-mitigation approaches are required for advanced CSP plants to be commercially viable.

47 OTHER INSTRUMENTATION↗

Corrosion evaluation of alloys and MCrAlX coatings in molten carbonates for thermal solar applications

Here, stainless steels (SS) 310, 321, 347, Incoloy 800H (In800H), alumina-forming austenitic (AFA-OC6), Ni superalloy Inconel 625 (IN625), and MCrAlX (M: Ni, and/or Co; X: Y, Hf, Si, and/or Ta) coatings were corroded in molten carbonates in N 2 and bone-dry CO 2 atmospheres. Electrochemical tests in molten eutectics K 2 CO 3 -Na 2 CO 3 and Na 2 CO 3 -K 2 CO 3 -Li 2 CO 3 at temperatures higher than 600 °C were evaluated using an open-circuit potential followed by a potentiodynamic polarization sweep to determine the corrosion rates. Because the best-performing alloys at 750 °C were In800H followed by SS310, these two alloys were selected as the substrate material for the MCrAlX coatings. The coatings were able to mitigate corrosion in molten carbonates environments. The corrosion of substrates SS310 and In800H was reduced from ~2500 um/year to 34 um/year when coated with high-velocity oxyfuel (HVOF) NiCoCrAlHfSiY and pre-oxidized (air, 900 °C, 24 h, 0.5 °C/min) before molten carbonate exposure at 700 °C in bone-dry CO 2 atmosphere. Metallographic characterization of the corroded surfaces showed that the formation of a uniform alumina scale during the pre-oxidation seems to protect the alloy from the molten carbonate attack.

14 SOLAR ENERGY↗

Corrosion in Supercritical Carbon Dioxide: Materials, Environmental Purity, Surface Treatments, and Flow Issues (Project No. 10-872)

The supercritical CO 2 Brayton cycle is gaining importance for power conversion in the Generation IV fast reactor system because of its high conversion efficiencies. When used in conjunction with a sodium fast reactor, the supercritical CO 2 cycle offers additional safety advantages by eliminating potential sodium-water interactions that may occur in a steam cycle. In power conversion systems for Generation IV fast reactors, supercritical CO 2 temperatures could be in the range of 30°C to 650°C, depending on the specific component in the system. Materials corrosion primarily at high temperatures will be an important issue. Therefore, the corrosion performance limits for materials at various temperatures must be established. The proposed research will have four objectives centered on addressing corrosion issues in a high-temperature supercritical CO 2 environment: Task 1: Evaluation of corrosion performance of candidate alloys in high-purity supercritical CO 2 : The following alloys will be tested: Ferritic-martensitic Steels NF616 and HCM12A, austenitic alloys Incoloy 800H and 347 stainless steel, and two advanced concept alloys, AFA (alumina forming austenitic) steel and MA754. Supercritical CO 2 testing will be performed at 450°C, 550°C, and 650°C at a pressure of 20 MPa, in a test facility that is already in place at the proposing university. High purity CO 2 (99.9998%) will be used for these tests. Task 2: Investigation of the effects of CO, H 2 O, and O 2 impurities in supercritical CO 2 on corrosion: Impurities that will inevitably present in the CO 2 will play a critical role in dictating the extent of corrosion and corrosion mechanisms. These effects must be understood to identify the level of CO 2 chemistry control needed to maintain sufficient levels of purity to manage corrosion. The individual effects of important impurities CO, H 2 O, and O 2 will be investigated by adding them separately to high purity CO 2 . Task 3: Evaluation of surface treatments on the corrosion performance of alloys in supercritical CO 2 : Surface treatments can be very beneficial in improving corrosion resistance. Shot peening and yttrium and aluminum surface treatments will be investigated. Shot peening refines the surface grain sizes and promotes protective Cr-oxide layer formation. Both yttrium and aluminum form highly stable oxide layers (Y 2 O 3 and Al 2 O 3 ), which can get incorporated in the growing Fe-oxide layer to form an impervious complex oxide to enhance corrosion resistance. Task 4: Study of flow-assisted corrosion of select alloys in supercritical CO 2 under a selected set of test conditions: To study the effects of flow-assisted corrosion, tests will be conducted in a supercritical CO 2 flow loop. An existing facility used for supercritical water flow studies at the proposing university will be modified for use in this task. The system is capable of flow velocities up to 10 m/s and can operate at temperatures and pressures of up to 650°C and 20 MPa, respectively. All above tasks will be performed in conjunction with detailed materials characterization and analysis using scanning electron microscopy/energy dispersive spectroscopy (SEM-EDS), x-ray diffraction (XRD), Auger electron spectroscopy (AES) techniques, and weight change measurements. Inlet and outlet gas compositions will be monitored using gas chromatography-mass spectrometry (GCMS).

36 MATERIALS SCIENCE↗

Radiation-Induced Defect Formation Kinetics in Inconel–Cu Multimetallic Layered Composites

This study investigates the stability of Inconel–Cu Multimetallic Layered Composites (MMLCs) in nuclear reactor applications using Molecular Dynamics simulations. The focus is on understanding the underlying mechanisms governing the properties of MMLCs for advanced nuclear reactors, specifically, the mechanochemistry of the interface between Inconel and copper alloys. The selection of Inconel–Cu MMLCs is primarily due to copper’s superior thermal conductivity, enhancing heat management within reactors by preventing hotspots and ensuring uniform temperature distribution. This research examines Incoloy 800H and two Inconel variants (718 and 625), assessing their stability at 1000 K after exposure to 10 keV collision cascades up to 0.12 dpa. Notable findings include defect clustering on the {1 2 0} family of planes of Inconel and Cu, with Stacking Faults and Lomer–Cottrell locks on the Inconel side.

Ramesh, Rajesh↗

Investigation of the hydrochlorination of SiCl4

A research and development program on the hydrochlorination of silicon tetrachloride and metallurgical grade (m.g.) silicon metal to trichlorosilane was carried out as scheduled. Effects of pressure and temperature on this reaction are reported. The presence of HCl in the reaction product mixture was successfully analyzed. Approximately 0.1% to 0.5% HCl based on total chlorosilanes were produced by the hydrochlorination reaction. Experiments on the corrosion study were carried out to evaluate a variety of metals and alloys as the material of construction for the hydrochlorination reactor. Material includes carbon steel, nickel, copper, Alloy 400 (Monel), stainless steel (Type 304), Incoloy 800H and Hastelloy B-2. The corrosion test was carried out at reaction temperature of 500 C, pressure of 300 psig and H2/SiCl4 feed ratio of 2.0 for a total of 87 hours. Results of the corrosion test show that all the test samples achieved a weigh gain.

Mui, J. Y. P.↗

Creep-rupture behavior of iron superalloys in high pressure hydrogen

Two cast alloys (CRM-6D and XF-818) and four sheet alloys (A-26, Incoloy 800H, N-155, and 19-9DL) in the thickness range of 0.79 to 0.99 mm were evaluated for use in the Stirling engine. The creep rupture behavior of these iron base high temperature alloys is being determined in air for 10 hr to 3,00 hr, and in 20.7 MPa (3,000 psi) H2 for 10 to 300 hr at temperatures of 650 deg to 925 deg. Material procurement, preparation and air creep rupture testing are described and existing data is analyzed. Systems for the high pressure hydrogen testing are discussed. Statistical analysis of temperature-compensated rupture data for each alloy is included.

Bhattacharyya, S.↗

Effect of 15 MPa hydrogen on creep-rupture properties of iron-base superalloys

Six wrought alloys (A-286, Incoloy 800H, N-155, 19-9DL, 12RN72, and CG-27) and four cast alloys (XF-813, CRM-6D, HS-31, and SA-F11), candidate materials for use in Stirling engines, were evaluated with reference to creep-rupture characteristics in 15-MPa H2 at 705 and 925 C. An analysis of the test results indicates that hydrogen has no effect on the rupture life and the minimum creep rate of the alloys investigated. Rupture ductility in hydrogen is lower than in air, but the mode of fracture is not significantly affected.

Bhattacharyya, S.↗