The anti-perovskite type hydride InPd{sub 3}H{sub 0.89}

Hydrogenation of tetragonal InPd{sub 3} in the ZrAl{sub 3} type structure (four-fold ccp superstructure) yields a hydride with a cubic AuCu{sub 3} type structure (one-fold ccp superstructure). Deuterium can be located by neutron powder diffraction in octahedral voids surrounded exclusively by palladium, [Pd{sub 6}], which are 88.5(6)% occupied in a statistical manner. The resulting deuteride InPd{sub 3}D{sub 0.89} thus crystallizes in a cubic anti-perovskite type structure (space group Pm3-bar m (no. 221), a=402.25(1) pm at 299(2) K). The Pd-D distance of 201.13(1) pm is typical for interstitial hydrides with palladium. Inelastic neutron scattering on the hydride InPd{sub 3}H{sub 0.89}, which shows a spectrum similar to that of binary palladium hydride, confirms the cubic site symmetry of hydrogen in [Pd{sub 6}] interstices. This is also confirmed by the absence of any quadrupole splitting in the {sup 2}D-NMR signal of the deuteride. {sup 1}H NMR spectra of InPd{sub 3}H{sub 0.89} do not show any motional narrowing. Values found for the H jump rate {tau}{sup -1} in InPd{sub 3}H{sub 0.89} remain below 10{sup 6} s{sup -1} in the studied temperature range 28-360 K, indicating a small hydrogen mobility in InPd{sub 3}H{sub 0.8} as compared with binary palladium hydride, PdH{sub {<=}1}. This can be attributed to the large spatial separation of the [Pd{sub 6}] sites. - Graphical abstract: Hydrogen induces a rearrangement in InPd{sub 3} from a ZrAl{sub 3} type structure to a cubic AuCu{sub 3} type structure, thus forming an anti-perovskite type hydride InPd{sub 3}H{sub 0.89}.

36 MATERIALS SCIENCE↗

Solving the “Coloring Problem” in InPd 3– x Ag x ( x = 0–0.7) by Phase Diagrams Modeling and Diffraction Experiments

Here, a series of InPd 3–x Ag x (x = 0–1) compositions were synthesized by conventional high-temperature synthesis, and as-synthesized samples were characterized by powder X-ray diffraction experiments. Up to x = 0.7, InPd 3–x Ag x adopts the ternary substitutional variant of the InPd 3 structure (TiAl 3 -type), when x > 0.7, elemental Ag starts to segregate along with the main phase. Accurate structural characterization in InPd 3–x Ag x faces a critical challenge due to the narrow X-ray scattering contrast among constituents In, Pd, and Ag and nearly identical neutron scattering lengths of Pd and Ag. To overcome this “coloring problem”, a combination of calculation of phase diagrams modeling (CALPHAD) and diffraction techniques (X-ray and neutron) was employed. In the compositional range 0 ≤ x ≤ 0.7, InPd 3–x Ag x presents a ternary variant of the TiAl 3 -type structure, where Ag atoms selectively substitute one (the 2b Wyckoff site) of the two Pd sites in InPd 3 . Notably, in contrast to the isologous InPd 3–x Cu x (x = 0–1) system, Ag substitution does not form an ordered VRh 2 Sn-type structure at the limiting composition. The distinct site preference in InPd 3–x Ag x is elucidated by charge population analysis, electronic structure calculations, and orbital-resolved chemical bonding investigations, and the extent of substitution is supported by formation free energy calculations.

36 MATERIALS SCIENCE↗

The atomic structure of low-index surfaces of the intermetallic compound InPd

The intermetallic compound InPd (CsCl type of crystal structure with a broad compositional range) is considered as a candidate catalyst for the steam reforming of methanol. Single crystals of this phase have been grown to study the structure of its three low-index surfaces under ultra-high vacuum conditions, using low energy electron diffraction (LEED), X-ray photoemission spectroscopy (XPS), and scanning tunneling microscopy (STM). During surface preparation, preferential sputtering leads to a depletion of In within the top few layers for all three surfaces. The near-surface regions remain slightly Pd-rich until annealing to ∼580 K. A transition occurs between 580 and 660 K where In segregates towards the surface and the near-surface regions become slightly In-rich above ∼660 K. This transition is accompanied by a sharpening of LEED patterns and formation of flat step-terrace morphology, as observed by STM. Several superstructures have been identified for the different surfaces associated with this process. Annealing to higher temperatures (≥750 K) leads to faceting via thermal etching as shown for the (110) surface, with a bulk In composition close to the In-rich limit of the existence domain of the cubic phase. The Pd-rich InPd(111) is found to be consistent with a Pd-terminated bulk truncation model as shown by dynamical LEED analysis while, after annealing at higher temperature, the In-rich InPd(111) is consistent with an In-terminated bulk truncation, in agreement with density functional theory (DFT) calculations of the relative surface energies. More complex surface structures are observed for the (100) surface. Additionally, individual grains of a polycrystalline sample are characterized by micro-spot XPS and LEED as well as low-energy electron microscopy. Results from both individual grains and “global” measurements are interpreted based on comparison to our single crystals findings, DFT calculations and previous literature.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Materials Data on InPd by Materials Project

PdIn is Tetraauricupride structured and crystallizes in the cubic Pm-3m space group. The structure is three-dimensional. Pd is bonded in a body-centered cubic geometry to eight equivalent In atoms. All Pd–In bond lengths are 2.87 Å. In is bonded in a body-centered cubic geometry to eight equivalent Pd atoms.

36 MATERIALS SCIENCE↗

Materials Data on Er14(InPd)3 by Materials Project

Er14(PdIn)3 crystallizes in the tetragonal P4_2/nmc space group. The structure is three-dimensional. there are seven inequivalent Er sites. In the first Er site, Er is bonded in a 1-coordinate geometry to one Pd and three In atoms. The Er–Pd bond length is 2.77 Å. There are one shorter (3.25 Å) and two longer (3.55 Å) Er–In bond lengths. In the second Er site, Er is bonded in a 3-coordinate geometry to one Pd and two In atoms. The Er–Pd bond length is 3.43 Å. There are one shorter (3.12 Å) and one longer (3.33 Å) Er–In bond lengths. In the third Er site, Er is bonded in a distorted L-shaped geometry to one Er, two Pd, and two In atoms. The Er–Er bond length is 3.61 Å. There are one shorter (2.83 Å) and one longer (2.89 Å) Er–Pd bond lengths. There are one shorter (3.45 Å) and one longer (3.56 Å) Er–In bond lengths. In the fourth Er site, Er is bonded in a 4-coordinate geometry to ten Er, two equivalent Pd, and two equivalent In atoms. There are a spread of Er–Er bond distances ranging from 3.47–3.63 Å. Both Er–Pd bond lengths are 3.50 Å. Both Er–In bond lengths are 3.38 Å. In the fifth Er site, Er is bonded in a distorted linear geometry to four equivalent Er and two equivalent In atoms. Both Er–In bond lengths are 3.26 Å. In the sixth Er site, Er is bonded in a 3-coordinate geometry to two equivalent Er, three equivalent Pd, and three In atoms. There are one shorter (2.77 Å) and two longer (2.90 Å) Er–Pd bond lengths. There are one shorter (3.12 Å) and two longer (3.37 Å) Er–In bond lengths. In the seventh Er site, Er is bonded in a distorted bent 150 degrees geometry to four equivalent Er, two equivalent Pd, and two equivalent In atoms. Both Er–Pd bond lengths are 2.82 Å. Both Er–In bond lengths are 3.67 Å. There are two inequivalent Pd sites. In the first Pd site, Pd is bonded in a 6-coordinate geometry to eight Er atoms. In the second Pd site, Pd is bonded in a 6-coordinate geometry to eight Er and one In atom. The Pd–In bond length is 3.07 Å. There are two inequivalent In sites. In the first In site, In is bonded to eleven Er and one In atom to form a mixture of corner and face-sharing InEr11In cuboctahedra. The In–In bond length is 3.11 Å. In the second In site, In is bonded in a 12-coordinate geometry to ten Er and two equivalent Pd atoms.

36 MATERIALS SCIENCE↗

Nickel Enhances InPd-Catalyzed Nitrate Reduction Activity and N 2 Selectivity

Palladium–indium (PdIn) is a well-established bimetallic composition for reductively degrading nitrate anions, one of the most ubiquitous contaminants in the groundwater. However, the scarcity and the variable price of these rare-earth and platinum group critical metals may hinder their use for water treatment. Nickel (Ni), a nonprecious metal in the same element group as Pd, could partially replace and lower Pd usage if the resulting trimetallic composition is sufficiently catalytically active. Herein, we report the synthesis and nitrate reduction catalysis of activated carbon-supported “In-on-Pd-on-Ni” catalysts (InPdNi/AC). While bimetallic InPd/AC (0.05 wt % In, 1.3 wt % Pd) was expectedly active, trimetallic InPdNi/AC containing the same In amount, much less Pd (0.1 wt %), and 1 wt % Ni was >17 more active (k cat ≈ 20 vs 349 L min –1 g surface metal –1 ). X-ray photoelectron spectroscopy (XPS) and density functional theory (DFT) calculations showed that Pd gained electron density from Ni, correlating to the increased nitrate reduction activity. Ammonium byproduct selectivity for InPdNi/AC (18% at 50% nitrate conversion) was lower compared to that of InPd/AC (48%), suggestive of the higher surface coverage of NO or its greater reactivity with NO 2 – , which led to more N 2 . Accounting for the catalyst precursor, manufacturing costs, and spent metal recovery, we calculated that Ni incorporation lowered the net catalyst cost significantly (from $\$$1028/kg to $\$$170/kg). The trimetallic composition lowered, by ∼26 times, the catalyst cost of a stirred tank reactor sized to the same treatment capacity as that for the bimetallic case. In conclusion, the results demonstrate that the partial replacement of the precious metal with an earth-abundant one leads to a higher efficiency and lower cost denitrification catalyst, via a material strategy that should be beneficial for other clean-water catalytic systems.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Surface structures of In-Pd intermetallic compounds. I. Experimental study of In thin films on Pd(111) and alloy formation

A combination of experimental methods was used to study the structure of In thin films deposited on the Pd(111) surface and the alloying behavior. X-ray photoelectron spectroscopy (XPS), low-energy electron diffraction (LEED), and scanning tunneling microscopy results indicate that surface alloying takes place at room temperature. Below 2 monolayer equivalents (MLEs), the LEED patterns show the formation of three rotational domains of InPd(110) of poor structural quality on top of the Pd(111) substrate. Both core-levels and valence band XPS spectra show that the surface alloy does not yet exhibit the electronic structure characteristic of the 1:1 intermetallic compound under these conditions. Annealing the 1 MLE thin film up to 690 K yields to a transition from a multilayer InPd near-surface intermetallic phase to a monolayer-like surface alloy exhibiting a well ordered (√(3)×√(3)) R30{sup ∘} superstructure and an estimated composition close to In{sub 2}Pd{sub 3}. Annealing above 690 K leads to further In depletion and a (1 × 1) pattern is recovered. The (√(3)×√(3)) R30{sup ∘} superstructure is not observed for thicker films. Successive annealing of the 2 MLE thin film leads the progressive disappearance of the InPd diffraction spots till a sharp (1 × 1) pattern is recovered above 690 K. In the high coverage regime (from 4 to 35 MLE), the formation of three rotational domains of a bcc-In{sub 7}Pd{sub 3} compound with (110) orientation is observed. This In-rich phase probably grows on top of interfacial InPd(110) domains and is metastable. It transforms into a pure InPd(110) near-surface intermetallic phase in a temperature range between 500 and 600 K depending on the initial coverage. At this stage, the surface alloy exhibits core-level chemical shifts and valence band (VB) spectra identical to those of the 1:1 InPd intermetallic compound and resembling Cu-like density of states. Annealing at higher temperatures yields to a decrease of the In concentration in the near-surface region to about 20 at.% and a (1 × 1) LEED pattern is recovered.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Hydrogenation of palladium rich compounds of aluminium, gallium and indium

Palladium rich intermetallic compounds of aluminium, gallium and indium have been studied before and after hydrogenation by powder X-ray diffraction and during hydrogenation by in situ thermal analysis (DSC) at hydrogen gas pressures up to 39 MPa and temperatures up to 700 K. Very weak DSC signals and small unit cell increases of below 1% for AlPd{sub 2}, AlPd{sub 3}, GaPd{sub 2}, Ga{sub 5}Pd{sub 13}, In{sub 3}Pd{sub 5}, and InPd{sub 2} suggest negligible hydrogen uptake. In contrast, for both tetragonal modifications of InPd{sub 3} (ZrAl{sub 3} and TiAl{sub 3} type), heating to 523 K at 2 MPa hydrogen pressure leads to a rearrangement of the intermetallic structure to a cubic AuCu{sub 3} type with an increase in unit cell volume per formula unit by 3.6-3.9%. Gravimetric analysis suggests a composition InPd{sub 3}H{sub a}pprox{sub 0.8} for the hydrogenation product. Very similar behaviour is found for the deuteration of InPd{sub 3}. - Graphical abstract: In situ differential scanning calorimetry of the hydrogenation of tetragonal InPd{sub 3} (ZrAl{sub 3} type) at 1.3 MPa hydrogen pressure.

36 MATERIALS SCIENCE↗

Surface structures of In-Pd intermetallic compounds. II. A theoretical study

The (110) surface of the InPd intermetallic compound and the In–Pd surface alloy properties are investigated in the framework of the density functional theory, within the projector augmented plane-wave method. Surface segregation is calculated to be energetically unfavorable at stoichiometric InPd(110) surfaces, while indium antisites are shown to segregate to the surface in off-stoichiometric InPd(110) systems. Concerning surface alloys obtained by burying In-doped Pd layers in Pd(111), we demonstrated that the most stable ones are those presenting atomic indium concentrations below 50 at. % (11 at. %, 25 at. %, 33 at. %). According to our calculations, the In-doped Pd layers with concentration above or equal to 50% lead to In-doped Pd multilayers, each presenting an atomic indium concentration below 50 at. %. Alloying and segregation effects in InPd intermetallic compound and In–Pd surface alloys clearly agree with the larger bonding strength of In–Pd (−0.44 eV) compared to In–In (−0.29 eV) and Pd–Pd (−0.31 eV)

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Pd-promoted reduction and restructuring of an In 2 O 3 -based catalyst for CO 2 hydrogenation at room temperature

An unconventional reaction mechanism in an In 2 O 3 /Pd(1 1 1) inverse model catalyst for the CO 2 hydrogenation reaction has been uncovered: In 2 O 3 is partially reduced at room temperature in a reaction atmosphere as a result of its direct contact with Pd(1 1 1), which is an efficient H 2 splitter. The reduction induces changes in surface free energy, leading to a dynamical restructuring at the In 2 O 3 /Pd(1 1 1) interface via formation of InO x and outward diffusion of Pd, as revealed by ambient pressure X-ray photoelectron spectroscopy, X-ray absorption spectroscopy and density functional theory simulations. This dynamical restructuring eventually promotes the growth of 2D InPd y O x nanodomains as the catalytically active phase and the exclusive formation of methanol upon hydrogenation of CO 2 at room temperature. A comparable high selectivity toward CH 3 OH was found in more realistic bulk catalytic systems (2 wt% Pd/In 2 O 3 catalyst and commercial CZA catalyst). Scanning tunneling microscopy under ultrahigh vacuum and ambient pressure reaction atmospheres further reveals the structural dynamics at the InO x /Pd(1 1 1) interface, where we follow in situ the evolution of the InO x particles on Pd(1 1 1) and the mobility of the InPd y O x nanodomains in a CO 2 + H 2 environment. The present findings of the formation of a mixed oxide phase in a dynamically restructuring metal/reducible-oxide interface indicate further implications for other heterogeneous catalytic systems beyond the present CO 2 hydrogenation example and highlight the importance of in situ investigations.

36 MATERIALS SCIENCE↗

Hydrogen reduction and metal-support interaction in a metastable metal-oxide system: Pd on rhombohedral In{sub 2}O{sub 3}

Highlights: • Metal-Support interaction in a metastable Pd/rh-In{sub 2}O{sub 3} material. • No influence of metal-support interaction on phase transformation rh-In{sub 2}O{sub 3}→c-In{sub 2}O{sub 3}. • Sequence of hydride, intermetallic compound formation and phase transformation. • High structural stability of reduced rh-In{sub 2}O{sub 3} and associated oxygen vacancies. • Metastable rh-In{sub 2}O{sub 3} more effective in initial intermetallic formation than c-In{sub 2}O{sub 3}. - Abstract: Structural and chemical consequences of reactive metal-support interaction (RMSI) effects occurring under hydrogen reduction in a metastable metal-oxide system have been exemplified for small PdO particles loaded onto rhombohedral In{sub 2}O{sub 3} (PdO/rh-In{sub 2}O{sub 3}) using synchrotron-based in situ X-ray diffraction experiments at temperatures up to 500 °C. rh-In{sub 2}O{sub 3} is a meta-stable In{sub 2}O{sub 3} polymorph that is prone to gas-phase dependent phase transformation to cubic In{sub 2}O{sub 3} (c-In{sub 2}O{sub 3}). Cross-influence of metal-support interaction and phase transformation can therefore be expected in similar temperature regimes. To separate both effects, comparable experiments have also been conducted on pure rh-In{sub 2}O{sub 3}. Phase transformation of pure rh-In{sub 2}O{sub 3} to cubic In{sub 2}O{sub 3} in hydrogen occurs between 415 °C and 450 °C. On Pd/rh-In{sub 2}O{sub 3}, a sequence of PdO reduction to Pd metal, followed by PdH{sub 0.706} hydride formation and subsequently, InPd and In{sub 3}Pd{sub 2} intermetallic compound formation have been observed between 30 °C and 500 °C. After the intermetallic compound formation is finished at around 400 °C, the phase transformation to c-In{sub 2}O{sub 3} sets in at exactly the same temperature as on pure rh-In{sub 2}O{sub 3} and extends over the same temperature range. This proves that the phase transformation of rh-In{sub 2}O{sub 3} to c-In{sub 2}O{sub 3} is not influenced by the reduction and the intermetallic compound formation. In contrast to Pd on c-In{sub 2}O{sub 3}, In-Pd compound formation from rh-In{sub 2}O{sub 3} occurs at much lower temperatures (230 °C vs. 300 °C), despite finally approaching the same compound stoichiometries (InPd and In{sub 3}Pd{sub 2}). This points to a high structural stability of reduced rh-In{sub 2}O{sub 3}/stability of oxygen vacancies (compared to c-In{sub 2}O{sub 3}) as well as to facilitated diffusion of reduced In(-O) species at low temperatures.

36 MATERIALS SCIENCE↗

Revealing the Synergy between Oxide and Alloy Phases on the Performance of Bimetallic In–Pd Catalysts for CO 2 Hydrogenation to Methanol

In 2 O 3 has recently emerged as a promising catalyst for methanol synthesis from CO2. In this work, we present the promotional effect of Pd on this catalyst and investigate structure–performance relationships using in situ X-ray spectroscopy, ex situ characterization, and microkinetic modeling. Catalysts were synthesized with varying In:Pd ratios (1:0, 2:1, 1:1, 1:2, 0:1) and tested for methanol synthesis from CO 2 /H 2 at 40 bar and 300 °C. In:Pd(2:1)/SiO 2 shows the highest activity (5.1 μmol MeOH/g InPd s) and selectivity toward methanol (61%). While all bimetallic catalysts had enhanced catalytic performance, characterization reveals methanol synthesis was maximized when the catalyst contained both In–Pd intermetallic compounds and an indium oxide phase. Experimental results and density functional theory suggest the active phase arises from a synergy between the indium oxide phase and a bimetallic In–Pd particle with a surface enrichment of indium. We show that the promotion observed in the In–Pd system is extendable to non precious metal containing binary systems, in particular In–Ni, which displayed similar composition–activity trends to the In–Pd system. As a result, both palladium and nickel were found to form bimetallic catalysts with enhanced methanol activity and selectivity relative to that of indium oxide.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗