SEARCH · Search NASA
Results for “Intermetallic phase”
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Microwave Heating of Nanocrystals for Rapid, Low-Aggregation Intermetallic Phase Transformations
The use of intermetallic Pt–Co nanocrystals (NCs) for the electrocatalytic oxygen reduction reaction is quickly gaining interest thanks to the higher electrochemical stability of the intermetallic L1 o phase compared to a random alloy A1 phase. However, the thermal treatment that enables the intermetallic phase transformation also causes considerable NC aggregation, resulting in a significant loss of electrochemically active surface area. Herein, we report the use of microwave radiation to induce the intermetallic phase transformation in Cu-doped Pt–Co NCs. We demonstrate that microwave radiation reduces NC aggregation while allowing for a complete phase transformation in only 30 s. Furthermore, these microwave-treated NCs demonstrate higher mass activity for the oxygen reduction reaction while maintaining electrochemical stability similar to the thermally annealed samples.
Increased thermal conductivity and decreased electron–phonon coupling factor of the aluminum scandium intermetallic phase (Al 3 Sc) compared to solid solutions
Aluminum scandium alloys and their intermetallic phases have arisen as potential candidates for the next generation of electrical interconnects. Here, in this work, we measure the in-plane thermal conductivity and electron–phonon coupling factor of aluminum scandium alloy thin films deposited at different temperatures, where the temperature is used to control the grain size and volume fraction of the Al 3 Sc intermetallic phase. As the Al 3 Sc intermetallic formation increases with higher deposition temperature, we measure increasing in-plane thermal conductivity and a decrease in the electron–phonon coupling factor, which corresponds to an increase in grain size. Our findings demonstrate the role that chemical ordering from the formation of the intermetallic phase has on thermal transport.
Strontium Effects on the Formation of Iron-Intermetallic Phases in Secondary Al–9Si–0.6Fe Alloys
The presence and morphology of Fe-containing intermetallic phases affect the mechanical properties of aluminum alloys, especially in secondary Al–Si-based cast alloys. Although strontium (Sr) addition of 50 to 500 ppm is known to refine the needle-type eutectic silicon structure, the influence of Sr on the formation of Fe-intermetallic phases remains unclear. The present work investigates the combined additions of Sr and Mn to Al–9Si–0.6Fe–0.35Mg (All compositions are in wt pct except otherwise stated.) alloys on the formation of Fe-intermetallic phases at different solidification rates from ~ 1.5 to ~ 60 °C/s. Long and branched-type AlFeSi phase with size ranging from 50 to 120 µm are more common when solidified at the rate of 1.5 °C/s regardless of Sr and Mn additions. However, at the fast solidification rate of 60 °C/s, a 60 ppm Sr addition significantly reduced the average length of needle-shaped AlFeSi phase to less than 3 to 5 µm. Thermodynamic simulations have been performed using CALculation of PHAse Diagrams (CALPHAD) models to predict the formation of various phases and their possible interactions during solidification. The results indicated that the combination of a high solidification rate and about 60 ppm of Sr is beneficial to refining the δ-Al 3 FeSi 2 phase in Al–Si–Mg alloys containing 0.6 pctFe. As a result, this unexpected finding of Fe-intermetallic refinement by low Sr addition (~60 ppm) provides an important guide in designing secondary alloys for sustainable casting applications.
Evolution of intermetallic phases in an Al–Si–Ti alloy during solution treatment
A cast Al–Si–Ti alloy was solution treated at 540 °C for different periods between 0 and 72 h to understand the evolution of intermetallic phases. Only an (Al,Si) 3 Ti intermetallic phase with a low Si content was found in the as-cast alloy. The (Al,Si) 3 Ti particles were converted partly into a lamellar structure, a eutectoid phase, consisting of a Si-rich phase and an Al phase during solution treatment. The amount of the lamellar structure increased with the solution treatment time, but the composition of either constitute was kept almost unchanged regardless of the solution treatment times. The lamellar Si-rich phase is (Al,Si) 2 Ti (τ 2 ) with a TiSi 2 (C49-type) structure based on thermodynamic calculations and high-resolution TEM analyses. FCC Al phase is the product residing between the τ 2 lamellae after the completion of transformation from (Al,Si) 3 Ti to τ 2 phase. A near-rational orientation relationship (OR) between the Al and τ 2 phases is determined as Al [110]//τ 2 [100], Al ()//τ 2 [060]. The phase transformation from (Al,Si) 3 Ti to τ 2 being a result of the diffusion of Ti and Si within the original (Al,Si) 3 Ti particulates as well as the Si diffusion from the Al matrix during solution treatment is proposed. The formation of the lamellar structure in the microstructure is attributed mainly to the limited diffusivity of Ti element.
Numerical investigation of micro-galvanic corrosion in Mg alloys: Role of the cathodic intermetallic phase size and spatial distributions
Magnesium alloys are of increasing interest in structural applications due to their low-density, moderate specific strength and stiffness, recyclability, and high damping among other properties. However, the wide-scale applicability of magnesium alloys in structural applications has been limited due to many factors including its poor corrosion resistance. In this work, a numerical investigation to simulate the micro-galvanic corrosion behavior was performed to examine the influence of size and distribution of cathodic intermetallic phase (ß-Mg17Al12) in a Mg matrix. The ratio of cathodic to anodic surface area was kept constant in each simulation condition to understand the effect of size and spacing distributions. In general, fragmentation of a larger intermetallic particle into smaller ones was found to enhance the localized current density. However, the uniform distribution of this small intermetallic phase throughout the matrix was found to reduce the overall dissolution current density and hence, pitting corrosion severity.
The initial formation and growth of intermetallic phases in the Cu-Zn system
Diffusion kinetics of beta, gamma, and epsilon intermetallic phases in copper-zinc system
Helium-bubble-enhanced disordering of intermetallic phase under irradiation
Understanding and controlling phase transformations in metals and alloys under irradiation is vital to the design of irradiation-tolerant materials. The L1 2 -ordered intermetallic phase in nickel-based superalloys provides superior high-temperature mechanical properties and corrosion resistance. Here, we studied the order-disorder transformation kinetics of an L1 2 -structured gamma-prime phase in nickel-based superalloy Rene N4 under krypton ion irradiation and the effect of pre-implanted helium gas bubbles on the kinetics of phase transformation. Furthermore, the presence of pre-implanted helium gas bubbles significantly enhances the order-disorder transformation of L1 2 -structured gamma-prime phase under irradiation at 300 °C. The evolution of pre-implanted helium gas bubbles under irradiation implies that helium gas bubbles could effectively trap irradiation-induced vacancies and impede the reordering process of anti-site defects in gamma-prime phase.
Method for imparting strength to intermetallic phases
A method for achieving both improved high strength and improved ductility ·in intermediate phases is provided. The method, briefly stated, comprises the steps of providing a melt whose composition substantially corresponds to that of a preselected intermetallic phase having a crystal structure of the L1 2 type, such as nickel. aluminide, modified with from about 0.01 to 2.5 atomic percent boron, and rapidly solidifying the melt at a cooling rate of at least about 10 3 ° C./second to form a solid body, the principal phase of which is of the L1 2 type crystal structure in either its ordered or disordered state.
Intermetallic phase formation in Al-Si-Zr alloys during hot isostatic pressing revealed by experiments and molecular dynamics
Understanding phase transformations at alloy interfaces is critical for the design of advanced structural materials. Here, in this study, we investigate the formation mechanisms of the Al 2 SiZr intermetallic phase in the Al-Si-Zr system under hot isostatic pressing (HIP) using molecular dynamics (MD) simulations and thermodynamic analysis. A unique aspect of our approach in MD involves the replacement of a disordered Al 2 SiZr stoichiometry with an ordered phase at the Al-Zr interface once HIP results in the desired Al 2 SiZr stoichiometry, allowing us to compute the total energetic cost of transformation by accounting for both formation energies and diffusion barriers. Diffusion coefficients and activation energies, extracted across a range of temperatures, reveal that HIP substantially enhances atomic mobility, creating favorable stoichiometry for phase evolution. Our results show that Al 2 SiZr phase formation is kinetically unfavorable at lower temperatures but becomes feasible when the thermodynamic driving energy surpass a critical energy threshold.
Controlling the Fe-intermetallic phases and mechanical properties of secondary Al-9Si-1Fe alloy with Cr and Mn additions
Not Available
Electrochemical Characteristics of Intermetallic Phases in Al–Cu–Li Alloys
This study provides a comprehensive overview of the electrochemical characteristics of intermetallic compounds (IMCs) commonly encountered in the 3rd generation Al–Cu–Li alloys. The electrochemical measurements were carried out on a AA2070-T8 alloy and surrogate alloys that have the compositions of select IMCs, typically found in AA2070-T8. The effects of environmental variables such as [Cl − ] and pH on the corrosion potential, pitting potential, repassivation potential, corrosion rate, and galvanic current of these IMCs were thoroughly evaluated utilizing the electrochemical microcell method. An electrochemical database was documented that covers eight groups of common IMCs in various Al alloys. The findings improve the understanding of interactions between matrix and IMCs in Al alloys, with implications for corrosion mitigation and new materials design.
Aluminum-fiber composites containing intermetallic phase at the matrix-fiber interface
A solid aluminum-fiber composite comprising: (i) an aluminum-containing matrix comprising elemental aluminum; (ii) coated or uncoated fibers embedded within said aluminum-containing matrix, wherein said fibers have a different composition than said aluminum-containing matrix and impart additional strength to said aluminum-containing matrix as compared to said aluminum-containing matrix in the absence of said fibers embedded therein; and (iii) an intermetallic layer present as an interface between each of said fibers and the aluminum-containing matrix, wherein said intermetallic layer has a composition different from said aluminum-containing matrix and said fibers, and said intermetallic layer contains at least one element that is also present in the aluminum-containing matrix and at least one element present in the fibers, whether from the coated or interior portion of the fibers. Methods of producing the above-described composite are also described.
High strength ultrafine eutectic composites with metastable intermetallic phases
Not Available
Design of an additively manufactured functionally graded material of 316 stainless steel and Ti-6Al-4V with Ni-20Cr, Cr, and V intermediate compositions
This study presents a method for designing a computationally informed gradient pathway to fabricate a functionally graded material (FGM) with terminal alloys of 316 stainless steel (SS316) and Ti-6Al-4V via directed energy deposition additive manufacturing with powder feedstock. In this work, the grading is accomplished through the introduction of intermediate elements and alloys (Ni-20Cr, Cr, and V) to avoid the brittle Fe-Ti intermetallic phases that form in the direct liquid phase joining of Ti-alloys and stainless steels. Using a combination of equilibrium calculations and Scheil-Gulliver simulations, a compositional pathway was designed to avoid deleterious phases. FGM samples were fabricated and experimentally characterized to determine the viability of the pathway. A change in phases from fcc to bcc was predicted to occur within the Ni-20Cr/Cr gradient region, and this was validated through experimental characterization. No detrimental phases (intermetallic, Laves, or σ phases) formed along the gradient path, demonstrating a successful computationally-informed design and fabrication of an FGM from SS316 to Ti-6Al-4V.
Systematic discovery of new nano-scale metastable intermetallic eutectic phases in laser rapid solidified Aluminum-Germanium alloy
Laser surface remelting of as-cast Al-Ge eutectic alloy is shown to produce ultrafine lamellar eutectic morphology with interlamellar spacing refined up to ∼60 nm and composed of FCC Al solid solution and unusual Al x Ge y intermetallic phases that do not form during near-equilibrium solidification. The microstructures are characterized and analyzed using a combination of selected area electron diffraction, high-resolution scanning transmission electron microscopy, energy dispersive X-ray spectroscopy to obtain high-resolution elemental maps, and atomistic modeling using density functional theory followed by atomic-scale image simulation. Depending on the local solidification conditions, the crystallography of the Al x Ge y intermetallic phases in the eutectic microstructure is either monoclinic (C 2/c) or monoclinic (P 2 1 ), with high densities of defects in both cases. This is in sharp contrast to the as-cast alloys that showed nominally pure Al and Ge phases with significant solute partitioning and equilibrium FCC and diamond cubic crystal structures, respectively. Corresponding kinetic phase diagrams are proposed to interpret the evolution of nano-lamellar eutectic morphologies with equilibrium Al and metastable Al x Ge y phases, and to explain increased solid solubility in the Al phases manifested by precipitation of ultrafine clusters of Ge. Furthermore, the reasons for the formation of these metastable eutectics under laser rapid solidification are discussed from the perspective of the competitive growth criterion.
Effect of Mg Content in Melt-Spun Mn–Bi–Mg–Sb–In Alloys on the Structure and Properties of Field-Annealed Magnets
Mn-Bi alloys modified with Mg and other elements were recently developed into promising rare-earth-free permanent magnets through successive melt-spinning, warm compaction, and short magnetic-field annealing. This letter reports herein on the crystal structures, texture, and magnetic properties observed in Mn 50 Bi 49-x Mg x Sb 0.5 In 0.5 alloys (x = 0, 1.5, 3.0, 4.5) throughout these processing steps. The Mg substitution favors MnBi-based intermetallic phases over the Bi- and Mn-based solid solutions and the stable α intermetallic phase over the metastable β' intermetallic phase. Magnesium increases the c/a ratio of the α phase lattice parameters for all studied x values and it increases the degree of the field-annealing-induced texture for x ≤ 3. The effect of Mg on coercivity is explained as combination of a positive one via the α phase magnetocrystalline anisotropy and a negative one via the development of texture. The effect of the substitution on the maximum energy product additionally involves the decreasing density of the alloys; the optimum x is found to be ≈3. Additionally reported are the thermal properties of selected alloys. The mechanism of field-annealing effect on the coercivity is briefly discussed.
Phase stability and magnetic and electronic properties of a spark plasma sintered CoFe – P soft magnetic alloy
More efficient power conversion devices are able to transmit greater electrical power across larger distances to satisfy growing global electrical needs. A critical requirement to achieve more efficient power conversion are the soft magnetic materials used as core materials in transformers, inductors, and motors. To that effect it is well known that the use of non-equilibrium microstructures, which are, for example, nanocrystalline or consist of single phase solid solutions, can yield high saturation magnetic polarization and high electrical resistivity necessary for more efficient soft magnetic materials. In this work, we synthesized CoFe – P soft magnetic alloys containing nanocrystalline, single phase solid solution microstructures and studied the effect of a secondary intermetallic phase on the saturation magnetic polarization and electrical resistivity of the consolidated alloy. Single phase solid solution CoFe – P alloys were prepared through mechanically alloying metal powders and phase decomposition was observed after subsequent consolidation via spark plasma sintering (SPS) at various temperatures. The secondary intermetallic phase was identified as the orthorhombic (Co x Fe 1-x ) 2 P phase and the magnetic properties of the (Co x Fe 1-x ) 2 P intermetallic phase were found to be detrimental to the soft magnetic properties of the targeted CoFe – P alloy.