A New Grain Refiner for Ferritic Steels
A new grain refiner, LaB{sub 6}, was identified for ferritic steels based on the crystallographic calculation using the edge-to-edge matching model. Addition of 0.5 wt pct LaB{sub 6} led to a reduction of the average grain size from 765 to 92 μm and the proportion of the columnar structure from 35 to 8 pct in an as-cast Fe-4Si ferritic alloy. Although LaB{sub 6} was supposed to act as an active inoculant for δ-ferrite, thermodynamic calculation indicated that LaB{sub 6} is not thermodynamically stable in the melt of the Fe-4Si alloy. It was subject to decompose into La and B solutes. Consequently, both La and B reacted with Fe, O and S, forming different compounds. Microstructural examination at room temperature observed La{sub 2}SO{sub 2} and La{sub 2}O{sub 3} particles within the ferrite grains and Fe{sub 2}B along the grain boundaries in the samples. Through EBSD analysis, a reproducible orientation relationship between ferrite and La{sub 2}SO{sub 2} was identified. In addition, the edge-to-edge matching calculation also predicted the high potency for La{sub 2}SO{sub 2} to be an effective nucleant for δ-ferrite. It was considered that the grain refinement of LaB{sub 6} was attributed to the enhanced heterogeneous nucleation of δ-ferrite by La{sub 2}SO{sub 2}, and the solute effect of B due to the high Q-value in ferrite.