Evidence that Surface-Segregated Sr Phases Can Be Removed in LSCF via Ceria Pre-Infiltration, Are Less Apt to Form in SSC

Here Ce 0.9 Gd 0.1 O 1.95−x (GDC) pre-infiltration was performed on 12 vol.% La 0.6 Sr 0.4 Co 0.8 Fe 0.2 O 3−x (LSCF) or Sm 0.5 Sr 0.5 CoO 3−x (SSC) infiltrated GDC Solid Oxide Fuel Cell cathodes. The addition of 7.5 vol.% of ∼40 nm diameter GDC nanoparticles into a ∼30 μ m thick porous scaffold of partially-sintered, sub-micron GDC particles before LSCF infiltration 1) lowered the temperature needed to produce a LSCF-GDC polarization resistance ( R P ) of 0.1 Ohm*cm 2 by ∼50 °C, and 2) reduced the amount of 500 h, 650 °C open-circuit LSCF-GDC R P degradation from ∼37% to ∼6%. In contrast, GDC pre-infiltration had no effect on the initial SSC-GDC R P or the 19% in R P degradation observed during 500 h of 650 °C open-circuit aging. X-Ray Photoelectron Spectroscopy showed that GDC pre-infiltration lowered the concentration of strontium species on the surface of the initial and 650 °C-aged LSCF-GDC, but had no effect on the initial or aged SSC-GDC Sr concentrations. Similarly, Electrochemical Impedance Spectroscopy showed that for both the initial and aged LSCF-GDC, GDC pre-infiltration improved oxygen exchange at the infiltrate-backbone and infiltrate-gas interfaces, but had no effect on the SSC-GDC. Hence, GDC pre-infiltration was concluded to improve LSCF-GDC performance and durability by scavenging exsolved Sr-rich secondary phases that form on the interfaces of LSCF, but not SSC.

36 MATERIALS SCIENCE↗

The Impact of Sintering Atmosphere and Temperature on the Phase Evolution of High Surface Area LSCF Prepared by In Situ Carbon Templating

The thermochemical stability of lanthanum strontium cobalt ferrite (LSCF) processed between 1000 °C–1200 °C via the in situ carbon templating method was studied. This method generates high surface area ceramics at traditional solid oxide fuel cell (SOFC) sintering temperatures by generating a carbon template in situ and subsequently removing the template by oxidation at 700 °C. Argon processed samples produced an amorphous carbon template, whereas nitrogen tended to form graphitic carbon. Prior to the oxidation step, nitrogen samples comprised larger La 2 O 3 crystallites (22–40 nm) compared to argon (9–17 nm). Upon oxidation, argon samples resulted in a pure LSCF phase with surface areas in the 21–29 m 2 ·g −1 range, whereas nitrogen samples contained significant impurities. This demonstrates that the size of La 2 O 3 crystallites formed during inert processing limited the ability to produce a pure LSCF phase. Symmetrical cells comprising nano-LSCF electrodes generated by the templating method were compared to cells sintered directly in air. Impedance results suggest that nano-LSCF cells and cells processed in air were dominated by interfacial charge transfer resistance and gas diffusion, respectively. The results map out conditions for preparing and integrating high surface area, nanostructured LSCF into SOFC electrodes at traditional sintering temperatures. Strategies for improving the interfacial resistance of nano-LSCF electrodes are discussed.

Muhoza, Sixbert P. (ORCID:0000000299864241)↗

Sulfur poisoning mechanism of LSCF cathode material in the presence of SO 2 : a computational and experimental study

Aiming at the comprehensive understanding of the single sulfur poisoning effect and, eventually, the multiple impurities poisoning phenomena on the SOFC (Solid Oxide Fuel Cell) cathode materials, the sulfur poisoning effect on the (La 0.6 Sr 0.4 ) 0.95 Co 0.2 Fe 0.8 O 3 (LSCF-6428) has been investigated in the presence of 10 ppm SO 2 at 800, 900, and 1000°C, respectively, with a combined computational and experimental approach. The good agreement between the CALPHAD (Computer Coupling of Phase Diagrams and Thermochemistry) simulations and the XRD (X-Ray Diffraction), SEM (Scanning Electron Microscopy), and TEM (Transmission Electron Microscopy) characterization results support the reliability of the CALPHAD approach in the SOFC field. Furthermore, comprehensive simulations were made to understand the impact of temperature, P(SO 2 ), P(O 2 ), and Sr concentration on the threshold of SrSO 4 stability. Results showed that the formation of SrSO4 is thermodynamically favored at lower temperatures, higher P(SO 2 ), higher P(O 2 ), and higher Sr concentration. Finally, comparisons were also made between LSCF-6428 and LSM20 (La 0.8 Sr 0.2 MnO 3 ) using simulations, which confirmed that LSCF-6428 is a poor sulfur-tolerant cathode, in agreement with the literature.

36 MATERIALS SCIENCE↗

Sr and Co Vapor-Phase Transport from LSCF Cathodes

A series of tests were performed to differentiate between surface diffusion and vapor-phase diffusion of chemical species from LSCF cathode material at typical sintering temperatures (up to 1100°C) in SOFC production. A GDC source substrate was printed with LSCF and separated by an air gap from a YSZ target substrate. Various geometries with long surface paths were employed to reduce the possibility of surface transport. Sr and Co were detected on the target substrates via energy dispersive spectroscopy (EDS) and x-ray photoelectron spectroscopy (XPS), including spatially resolved XPS. These results support a vapor-phase transport mechanism for Sr and Co. Sintering conditions and barrier layer requirements may need to be revisited to prevent the formation of undesired strontium zirconate at cathode/electrolyte interface due to vapor-phase transport.

vapor phase transport, SOFC cathode, Sr transport↗

Electrically Conductive and Protective Coating Compatibility with LSCF Cathodes

Ferritic stainless-steel interconnect materials are used in intermediate or high-temperature SOFCs because of their oxidation resistance, high formability, and low cost. Their corrosion resistance is due to the formation of a protective chromium oxide scale during operation. However, the protective oxide layer produces Cr-containing volatile species at SOFC operating temperatures and conditions, which can cause cathode poisoning. Spinel coatings have been developed to prevent cathode poisoning while maintaining an electrically conductive pathway through SOFC stacks. Generally, Mn-Co-O spinel has been the material of choice, but PNNL has developed an Mn-Cu-O spinel protective coating to remove the costly Co and enhance the electrical conductivity. This paper will focus on the electrically conductive coating’s compatibility with LSCF in high-temperature operating environments.

Choi, Jung-Pyung↗

Fabrication and accelerated long-term stability test of asymmetrical hollow fiber-supported thin film oxygen separation membrane

Asymmetrical hollow fiber-supported thin film membrane may provide microstructural advantages for air separation and oxygen production. The fabrication of such a membrane is usually very difficult, particularly the sintering behaviors and thermal expansion coefficient (TEC) mismatch among multiple layers. This directly affects the reliability and long-term stability of the membrane. Here, in this research, the sintering behaviors of a set of simple oxides are systematically studied and ZnO is identified as a material component for composite substrate La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3-δ (LSCF)-ZnO. The LSCF-ZnO ratios are further optimized by trading off several factors, e.g., matching the sintering behaviors and TECs of the LSCF-ZnO composite with those of LSCF thin film separation layer while enhancing the substrate strength. With the identified LSCF-ZnO ratio, the LSCF-ZnO composite hollow fiber substrate precursor is formed through slurry spinning process with porous microstructure being formed via phase inversion process. The thin film LSCF dense separation layer is then dip-coated on the substrate followed by co-sintering process. A thin, porous PrBaCo(Fe 0.6 Zr 0.2 Y 0.2 )O 5+δ (PBCFZY) catalyst layer is fabricated on the dense LSCF separation layer with dip-coating and sintering process, forming an asymmetrical membrane device LSCF-ZnO/LSCF/PBCFZY. Oxygen permeation test of the device is systematically conducted, and the fundamental mechanisms are analyzed. An accelerated long-term stability test of the membrane is also conducted (~550h, 46 thermal cycling loads), demonstrating excellent robustness and durability. The device is characterized and analyzed before and after the test. By replacing a considerable amount of high cost LSCF with low cost ZnO in the substrate, it not only enhances the stability but also reduces the capital cost of the membrane for practical applications.

42 ENGINEERING↗

Surface enhanced performance of La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3-δ cathodes by infiltration Pr-Ni-Mn-O progress

Herein the present study reports the enhancement of electrochemical oxygen reduction activity of porous La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3–δ (LSCF) cathodes by coating a thin film of Pr-Ni-Mn oxide (PNM5) using a multi-step infiltration process. XRD examination reveals that PNM5 mainly contains a multiphase mixture of Pr 6 O 11 , PrNiO 3 , MnO and NiO. SEM morphology shows a thin PNM5 film and small particles are formed on the surface of LSCF backbone particles. Impedance spectrum analysis indicates that PNM5 infiltrated LSCF exhibits dramatically reduced polarization resistance (R p ), reaching R p of 0.244 Ω cm 2 at 973 K, which is one-half of the baseline LSCF cathode. The activation energy of LSCF cathodes infiltrated with PNM5 is 1.45 eV, slightly lower than the baseline LSCF cathode (1.77 eV). Distribution of relaxation time (DRT) function analysis shows PNM5 infiltration layer significantly promotes the oxygen reduction reaction (ORR) of cathode surface. With the increase in firing temperature, the total resistance increases and R p changes from ion transport to oxygen reduction reaction. Degradation rate of the PNM5-infiltrated LSCF is also lower, 0.02168% vs 0.07093% for the baseline LSCF over a 200-h period. A single cell testing indicated that the peak power density of the PNM5-infiltrated cell was increased by 140.66%. Overall, PNM5 could be a potential catalyst for boosting the performance of a commercial LSCF cathode for solid oxide fuel cells (SOFC).

36 MATERIALS SCIENCE↗

On-Demand Designing of Cathode Internal Surface Architecture for Dramatic Enhancement of SOFC Performance and Durability

This project is aimed to design and modify the internal surfaces of porous composite cathode from currently commercially viable Solid Oxide Fuel Cells (SOFCs), using additive manufacturing process of Atomic Layer Deposition (ALD). The material systems being investigated are commercial composite electrodes complex three-dimensional topographies. In term of the chemistry of the ALD layer applied on the internal surface of the porous cathode, this project has employed commercially relevant electrolyte, electrocatalyst and noble metal materials set. Such materials are fully compatible with the commercial fuel cells, and this project has developed special nanostructure on the surface of the commercial composite cathodes. The formation of the designed nanoarchitecture on the surface of SOFC cathode has been achieved through precise control of ALD parameters and their effect on overall cell performance and resultant electrochemical reaction mechanism of cathodes has been investigated through full cell electrochemical performance testing and nanostructure characterization by transmission electron microscopy (TEM). Under the support of this award, following has been achieved: (1). For cathode materials in solid oxide fuel cells (SOFCs), such as perovskite mixed conductor La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3-x (LSCF), cation surface segregation and consequently losing conductivity and active sites for the oxygen reduction reaction (ORR) are problematic. To mitigate the cation segregation and enhance SOFC durability, further decorating the internal backbone surface using the desired electrocatalysts could be a promoting approach. Commonly, the cation segregation such as Sr is very volatile, so the effective surface decoration is ideally conformal. Nevertheless, the conformal surface coating would inevitably alter the ORR pathways that initially take place on the surface of the backbone. To reveal the impact of the conformal coating on both the catalytic activity and the conductivity of the cathode, the unary electrocatalyst of Pt or CoO x , was applied to the LSCF/SDC composite electrode of inherently functional SOFCs, respectively. Both ALD coating layers evolve strong interaction with the LSCF composite cathode. Upon operations, the Pt coating layer remains conformal on LSCF grain surfaces but turns into discrete particles on SDC grain surfaces. Meanwhile, CoO x conformal coating grows to be the discrete nanograins on both the LSCF and SDC grains. ALD coating of the cathode alone reduces the ohmic resistance up to 28 % for the entire cells. The increased conductivity induced by the ALD coating of Pt or CoO x is ascribed to different mechanisms. For the inherent functional SOFCs, the present study presents a novel and feasible approach to apply a conformal, dense coating layer on the surface of a mixed conductor, simultaneously increasing the conductivity and durability of the SOFC cathode. (2). High resistance of the oxygen electrode still significantly hinders the state-of-the-art Solid Oxide Fuel Cells (SOFCs). In particular, for an oxygen electrode consisting of mixed electronic and ionic conductors, such as perovskite lanthanum strontium cobalt ferrite (LSCF), it deteriorates due to its low chemical stability of the grain surface. Such degradation is often associated with the segregation of cations. To prevent the cation surface segregation and its resultant perovskite phase decomposition, we demonstrate a conformal ultra-thin (7-10 nm) surface heterogeneous coating layer consisting of subjacent discrete Pt nanoparticles capped with a superjacent fully dense conformal CoO x layer. The performance studies indicate the ALD coating reduces the cell series resistance by up to 40 %. The conformal CoO x layer consists of randomly orientated but single-layered nanograins, with high-density intergranular and surface grain boundaries serving as the electrochemical reaction sites and facilitating mass transport. The conformal coating layer appears to have successfully suppressed the Sr outward diffusion and confined the Sr enriched layer to a ~ 2 nm interface perovskite phase between the coating layer and the LSCF grain surface. Moreover, this ultra-thin Sr enriched perovskite layer presumably possesses high oxygen vacancy and high ionic conductivity and further imposes tensile strain to the LSCF grain surfaces. With the combination of a conformal CoO x nanoionics, Sr enriched layer, and its strained interface, the ALD coating induced surface layer is estimated to have a conductivity of ~ 1.27x10 4 S/cm, which is over two orders magnitude of that from LSCF at 750 ºC.

30 DIRECT ENERGY CONVERSION↗

Enhancing Oxygen Reduction Activity and Cr Tolerance of Solid Oxide Fuel Cell Cathodes by a Multiphase Catalyst Coating

Intermediate temperature solid oxide fuel cells (IT-SOFCs) are cost-effective and efficient energy conversion systems. Here, the sluggish oxygen reduction reaction (ORR) and the degradation of cathodes are critical challenges to the commercialization of IT-SOFCs. Here, a highly efficient multiphase (MP) catalyst coating, consisting of Ba 1–x Co 0.7 Fe 0.2 Nb 0.1 O 3–δ (BCFN) and BaCO 3 , to enhance the ORR activity and durability of the state-of-the-art lanthanum strontium cobalt ferrite (La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3–δ , LSCF) cathode is reported. The conformal MP catalyst-coated LSCF cathode shows a polarization resistance (R p ) of 0.048 Ω cm 2 at 650 °C, about one order of magnitude smaller than that of the bare LSCF. In an accelerated Cr-poisoning test, the degradation rate of the catalyst-coated LSCF electrode is 10 –3 Ω cm 2 h –1 (0.59% h –1 ) over 200 h, only one fifth of the degradation rate of the bare LSCF electrode at 750 °C. In addition, anode-supported single cells with the MP catalyst-coated LSCF cathode show a dramatically enhanced peak power density (1.4 W cm –2 vs 0.67 W cm –2 at 750 °C) and increased durability against Cr and H 2 O. Both experimental results and density functional theory-based calculations indicate that the BCFN phase improves the ORR activity while the BaCO 3 phase enhances the stability of the LSCF cathode.

solid oxide fuel cells↗

Combined Cr and S poisoning behaviors of La 1-x Sr x MnO 3±δ and La 1-x Sr x Co 1-y FeyO 3-δ cathodes in solid oxide fuel cells

Although the individual effects of airborne Cr and S contaminants on SOFC cathode performance degradation have been extensively studied, the combined effects of Cr and S contaminants remain largely unexplored. Under the real SOFC operating condition where the Cr and S species coexist, their effects may compete, affecting the poisoning behavior. Here, our investigation reveals that the combined Cr and S poisoning behavior of LSCF remains different from those of individual Cr and S poisonings, while the combined poisoning mechanism of LSM is equivalent to the sum of those of individual Cr and S effects. For LSCF electrode, gaseous Cr species are deposited mainly at the LSCF/GDC interface by electrochemical reduction, rather than forming SrCrO 4 on LSCF surfaces (as in the case of Cr-only poisoning), indicating no reaction between Cr vapors and SrO on the LSCF surface. Thermodynamic analysis demonstrates that the SrO on LSCF surface absorbs SO 2 (g) and thereby loses the Cr-gettering effect, allowing Cr vapors to flow through LSCF and to reach the LSCF/GDC interface where the Cr deposition occurs. Unlike LSCF, LSM electrode shows cumulative effects of Cr and S, as Cr accumulation occurs at the triple-phase boundary and S absorption takes place at localized Sr-rich regions.

36 MATERIALS SCIENCE↗

Sm 0.5 Sr 0.5 CoO 3-δ Surface Modification of La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3-δ -Ce 0.9 Gd0.1 2-δ Composite Oxygen Electrodes for Solid Oxide Electrochemical Cells

La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3- δ -Ce 0.9 Gd 0.1 O 2- δ (LSCF-GDC) composite oxygen electrodes have been widely used in intermediate temperature (<700 °C) solid oxide cells, with composite usually providing better electrochemical performance than single-phase LSCF. However, LSCF-based electrodes are often observed to degrade over time due to Sr segregation. Here we present an impedance spectroscopy study comparing the degradation behaviors of LSCF-GDC and Sm 0.5 Sr 0.5 CoO 3- δ (SSC) infiltrated LSCF-GDC electrodes. The LSCF-GDC polarization resistance increases by ~5 times over ~1000 h at 650 °C. In contrast, the SSC-infiltrated electrode shows similar initial polarization resistance but much more stable performance. The impedance modeling results show that the improved stability is associated with the low frequency oxygen dissociative adsorption/desorption process. The results suggest that this adsorption/desorption process slows due to increased Sr segregation on LSCF over time, and that SSC does not degrade significantly due to Sr surface segregation.

Electrochemistry↗

In-situ exsolution of bimetallic CoFe nanoparticles on (La,Sr)FeO 3 perovskite: Its effect on electrocatalytic oxidative coupling of methane

This study presents in-situ reduction of lanthanum strontium cobalt ferrite (LSCF) perovskite as an effective method for modifying its surface properties and enhancing its electrocatalytic reactivity for oxidative coupling of methane (OCM). The evolution of hetero-phases during the reduction of LSCF resulted in CoFe nanoparticles being formed at the surface. The in-situ reduced LSCF cell for OCM could be operated in either an ion pump or a fuel cell mode. High selectivity of 63% and 10.2% were reported for C 2+ hydrocarbons and C 3 H 6 , respectively. DFT calculations on LSCF and CoFe revealed that the high selectivity of C 2+ hydrocarbons on the LSCF primarily stems from the presence of CoFe nanoparticles. In-situ DRIFTS conducted under CH 4 proved that complete oxidation of CH 4 can be effectively inhibited by reducing LSCF, and control of oxygen supply is an important parameter for selective conversion of CH 4 to higher order hydrocarbon.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

LaCrO 3 -Coated La 0.6 Sr 0.4 Co 0.2 Fe0.8O3–δ Core–Shell Structured Cathode with Enhanced Cr Tolerance for Intermediate-Temperature Solid Oxide Fuel Cells

La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3-δ (LSCF) is a common cathode material for intermediate temperature solid oxide fuel cells due to its excellent oxygen reduction reaction catalytic activity. However, the Cr-poisoning effect is a severe issue causing its electrochemical performance degrada-tion. To develop a LSCF-based cathode with excellent Cr-tolerance, LaCrO 3 -coated LSCF core-shell structured (LCr@LSCF) cathode was prepared via solution infiltration method. After coated by LCr shell, the long-term stability and Cr-tolerance were obviously improved, at the price of sacrificing some electrochemical performance. As a result, the development of LCr@LSCF cathode with eye-catching Cr-tolerance is of great significance to the commercialization of LSCF.

36 MATERIALS SCIENCE↗

Advanced sorbents for modular oxygen production for REMS gasifiers

Under a DOE funded effort, Thermosolv LLC has been developing a sorbent-based oxygen production technology for gasification and oxy-combustion applications. The sorbents utilize oxygen-storage properties of certain perovskites to (1) selectively adsorb oxygen at moderate temperature from compressed air and (2) release the adsorbed oxygen into a vacuum or a sweep gas such as CO2 and/or steam. Through cyclic operations of multiple sorbent beds such a process can be made continuous. Pressure drop across the sorbent bed and other similar design considerations dictate that the sorbent be in the form of a high surface-area-to-volume pellet and yet still possess sufficient crush strength and integrity. Process efficiency is determined by the sorption and desorption kinetics and sorbent capacity. Typical process involves cycle times in the order of 100 seconds, a time too short to fully utilize the full volume of the sorbent and the sorption capacity of the sorbent pellets. As a part of this project, Thermosolv LLC undertook the development of oxygen sorbents as a high-surface area supported sorbent on a light-weight inert support to (1) reduce the cost, (2) increase the productivity, and (3) reduce the overall weight of the reactor. Using a previously developed perovskite (LSCF 1991) with its well-characterized performance, composite sorbent pellets each consisting of an inert core coated by a thin layer of the functional perovskite material were produced. Several low-density, inexpensive inert solids supports in the 1/8”-1/4” size were selected to keep the pressure drop across the sorbent bed in the acceptable range. A number of commercial technologies including spray coating, dip coating, incipient impregnation of porous substrate followed by thermal annealing at various temperatures and duration were employed and tested to produce robust composite supported sorbent pellets. A sense of optimum coating thickness was developed by testing sorbent pellets of various increasing diameter pellets. LSCF-1991extrudates ranging in size from 1/32” to 3/16” were tested in a TGA and in a fixed-bed pressure swing test set-up for sorption/desorption cycles of interest. The data show that for the operational conditions of interest the coating thickness for a supported sorbent pellet needs to be approximately 1/32” (about 0.8 mm). Subsequent work thereby concentrated on developing composite pellets of various substrates, shapes and sizes with coating layer of about this size range. Candidate support materials were chosen based on cost, inertness, mechanical strength, thermal expansion and chemical stability with sorbent material, and in a size range to give an acceptable pressure drop in fixed-bad reactor configurations. Coating application methods used for application of the sorbent onto the support included precipitation, spray coating and dip coating from sorbent slurries and sol gels. For all coated supports where we could successfully apply a uniform coating of desired thickness with an acceptable handling performance in terms of exfoliation, TGA-based cyclic sorption/desorption testing was performed to determine cycling capacity of oxygen. Among nearly twenty different support materials tested, best adhesion performance was obtained from stainless saddle supports. In the bench-scale fixed-bad tests stainless steel saddle support composite pellets with a coating thickness in the 0.6 mm or so range, the composite sorbent pellet performance approached up to 95% of that of the 2 mm parent material pellets. In a parallel approach to reducing the cost of the sorbent, alternate sorbent formulations replacing/reducing the amount of cobalt in the LSCF family were also investigated. Successful formulations that could match the performance of LSCF 1991 were identified based on TGA cyclic tests as LSCF 1919 and LSF 1910. In the range of operational envelop of cycle times and other relevant process operating conditions, the reduced Co formulations showed comparable performance in the bench-scale fixed-bad cyclic operations. As a part of this project, we also attempted substitution of La and Sr with Ca and Ba, and Co with Mn, Ni and Cu with little success, but the overall project goal of reducing sorbent cost in terms of raw material and manufacturing expenses was successful.

01 COAL, LIGNITE, AND PEAT↗

An improved oxygen reduction reaction activity and CO 2 -tolerance of La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3-δ achieved by a surface modification with barium cobaltite coatings

Solid oxide fuel cells (SOFCs) cathode often suffers from the poisoning effect of the contaminants commonly encountered in air such as CO 2 . Here we report an effective approach to enhancing the activity and CO 2 tolerance of the state-of-the-art La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3-δ (LSCF) cathode enabled by a coating of BaCoO 3-δ (BCO), as verified by the electrochemical testings, Raman analyses, and density functional theory calculations. When surface modified with a thin-film BCO coating, LSCF displays a much enhanced ORR activity and an improved durability against CO 2 . For example, anode supported SOFCs with the LSCF cathode coated with BCO coatings show a remarkable peak power density (Pmax) of 0.41 Wcm -2 and a significantly reduced degradation rate in current density of ~0.08% h -1 at 0.8 V and 700 °C for a period of 300 hs when humidified H2 (with 3 vol%H2O) was used as fuel and air with 8 vol% CO 2 as oxidant. The demonstrated performance is improved when compared with those of the cells with a blank LSCF electrode (a Pmax of ~0.36 Wcm -2 and a degradation rate of ~0.15% h -1 ) under the same conditions. Furthermore, the adsorption energy calculations suggests that BCO coating makes CO 2 adsorption much weaker than LSCF (-0.54 eV versus -1.07 eV).

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗