Search NASA⌕ Search

SEARCH · Search NASA

Results for “Laser melting”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Ability to Simulate Absorption and Melt Pool Dynamics for Laser Melting of Bare Aluminum Plate: Results and Insights from the 2022 Asynchronous AM-Bench Challenge

The 2022 Asynchronous AM-Bench challenge was designed to test the ability of simulations to accurately predict laser power absorption as well as various melt pool behaviors (width, depth, and solidification) during laser melting of solid metal during stationary and scanned laser illumination. In this challenge, participants were asked to predict a series of experimental outcomes. Experimental data were obtained from a series of experiments performed at the Advanced Photon Source at Argonne National Laboratories in 2019. These experiments combined integrating sphere radiometry with high-speed X-ray imaging, allowing for the simultaneous recording of absolute laser power absorption and two-dimensional, projected images of the melt pool. All challenge problems were based on experiments using bare aluminum solid metal. Participants were provided with pertinent experimental information like laser power, scan speed, laser spot size, and material composition. Additionally, participants were given absorptance and X-ray imaging data from stationary and scanned laser experiments on solid Ti–6Al–4V that could be used for testing their models before attempting challenge problems. In total, this challenge received 56 submissions from eight different research groups for eight individual challenge problems. The data for this challenge, and associated information, are available for download from the NIST Public Data Repository. This paper summarizes the results from the 2022 Asynchronous AM-Bench challenge as well as discusses the lessons learned to help inform future challenges.

36 MATERIALS SCIENCE↗

Statistical Homogenization of Elastic and Fracture Properties of a Sample Selective Laser Melting Material

Selective laser melting (SLM) is an additive manufacturing technique commonly used in the rapid prototyping of components. The complexity of the SLM microstructure poses a unique challenge to deriving effective mechanical properties at different length scales. Representative volume elements (RVEs) are often used to homogenize the material properties of composites. Instead of RVEs, we use statistical volume elements (SVEs) to homogenize the elastic and fracture properties of the material. This relates the inherent variation of a material’s microstructure to the variation in its mechanical properties at different observation scales. The convergence to the RVE limit is examined from two perspectives: the stability of the mean value as the SVE size increases for the mean-based approach, and the tendency of the normalized variation in homogenized properties to zero as the SVE size increases for the variation-based approach. Fracture properties tend to make the RVE limit slower than do elastic properties from both perspectives. There are also differences between vertical (normal to printing plane) and horizontal (in-plane) properties. While the elastic properties tend to make the RVE limit faster for the horizontal direction, i.e., having a smaller variation and more stable mean value, the fracture properties exhibit the opposite effect. We attributed these differences to the geometry of the melt pools.

36 MATERIALS SCIENCE↗

Melting and solidification dynamics during laser melting of reaction-based metal matrix composites uncovered by in-situ synchrotron X-ray diffraction

Laser additive manufacturing (AM) of reaction-based metal matrix composites (MMCs) involves highly complex and non-equilibrium material transformation behavior, including melting, dissolution, precipitation, and solidification. Yet, the dynamics and interplay of these phase transformation processes remain poorly understood, posing substantial challenges in identifying the microstructure formation mechanism, and predicting and controlling the microstructure in the printed parts. Here, in this study, we performed the in-situ X-ray diffraction experiment to characterize the phase evolution dynamics of the 316L + 10 vol.%TiC system during laser melting, which provides direct and quantitative insights of the complex phase reaction and evolution dynamics under rapid heating and cooling conditions relevant to additive manufacturing of reaction-based MMCs. Further in-depth thermodynamic and kinetic calculations revealed that most of the phase evolution behavior observed in the in-situ X-ray diffraction experiment cannot be solely explained by widely used equilibrium thermodynamic models, and diffusion-controlled nonequilibrium dissolution and precipitation kinetics must be considered to elucidate the complex phase evolution behavior, including incomplete TiC dissolution, and three-step TiC precipitation. The three distinct types of precipitates generate unique hierarchical TiC micro- and nanostructures, which enhances the yield strength from 513 MPa to 877 MPa by 71 %, tensile strength from 628 MPa to 1054 MPa by 68 %, and Young's modulus from 193 GPa to 221 GPa by 14 %. The findings of our research provide the knowledge foundation for the design of unique microstructures and advanced MMC materials through laser AM.

36 MATERIALS SCIENCE↗

Effects of an External Magnetic Field on Keyhole Mode Laser Melting of 316 Stainless Steel

Keyhole-mode laser melting is an efficient method for joining or cutting large, thick components, but controlling keyhole depth and fluctuations has remained challenging. Applying an external magnetic field can control melt pool flows and indirectly influence keyhole morphology and dynamics. The induced Lorentz force, comprising Seebeck and damping components, plays a crucial role in the melt pool dynamics, depending on temperature gradient, flow rates, and magnetic field orientation and magnitude. This research investigates the effects of an external magnetic field on keyhole behavior during laser spot melting of 316 stainless steel using synchronized high-speed synchrotron X-ray and thermal imaging. Findings revealed that a longitudinal magnetic field (120 mT) increased keyhole depth but exacerbated lateral fluctuations, resulted in a 20% increase in the melt pool temperature gradient and a 27% decrease in cooling rate. Conversely, a transverse magnetic field (760 mT) reduced keyhole depth and improved porosity formation. The findings suggest that a decrease in keyhole depth correlates with a decrease in fluctuations, and vice versa. These insights enhance understanding of external magnetic fields’ impact on laser melting, with implications for improving part quality.

Alamdari, Aslan Bafahm [The Ohio State Univ., Colu↗

Accelerating laser ray tracing in high fidelity physics simulations of laser melting using squeeze U-net

Laser melting is a core component of the ongoing industrial revolution, dubbed Industry 4.0, as lasers facilitate fast and precise melting and fusion in advanced manufacturing. There is a strong need to optimize the laser process using simulations. However, this has proven challenging as high fidelity simulations are needed for predictive modeling and this is currently prohibitively expensive even when run on hundreds of processors on high performance computers. The challenge is capturing complex physics of laser material interaction, fluid dynamics, thermal physics and material phase transformations at various length and time scales. To close this technological gap, we modified a squeeze U-net to accelerate the laser ray tracing component of such high fidelity models by ~4x–40x while preserving the core physics principle of conservation of energy with 97% accuracy. This approach enables the accurate modeling of global laser energy absorption as a function of local surface temperatures and complex surface topologies, which govern the reflection directions and energy losses of laser rays upon interacting with the material surface.

Computer science↗

Emergence of liquid following laser melting of gold thin films

X-ray structural science is undergoing a revolution driven by the emergence of X-ray Free-electron Laser (XFEL) facilities. The structures of crystalline solids can now be studied on the picosecond time scale relevant to phonons, atomic vibrations which travel at acoustic velocities. In the work presented here, X-ray diffuse scattering is employed to characterize the time dependence of the liquid phase emerging from femtosecond laser-induced melting of polycrystalline gold thin films using an XFEL. In a previous analysis of Bragg peak profiles, we showed the supersonic disappearance of the solid phase and presented a model of pumped hot electrons carrying energy from the gold surface to scatter at internal grain boundaries. This generates melt fronts propagating relatively slowly into the crystal grains. By conversion of diffuse scattering to a partial X-ray pair distribution function, we demonstrate that it has the characteristic shape obtained by Fourier transformation of the measured F ( Q ). The diffuse signal fraction increases with a characteristic rise-time of 13 ps, roughly independent of the incident pump fluence and consequent final liquid fraction. This suggests the role of further melt-front nucleation processes beyond grain boundaries.

36 MATERIALS SCIENCE↗

System and method for large-area pulsed laser melting of metallic powder in a laser powder bed fusion application

The present disclosure relates to systems and methods for performing large area laser powder bed fusion (LBPF) to form a plurality of layers of a 3D part in a layer-by-layer fashion using meltable powder particles. In one implementation the system makes use of a first light source, which may be a diode laser subsystem, for generating a first light pulse of a first duration. The first light is used to preheat a substrate underneath a new layer of powder particles, wherein the substrate is formed from a previously fused quantity of the powder particles. A second light source, which may be a pulse laser, generates a second light pulse subsequent to the first light pulse. The second light pulse has a second duration shorter than the first duration by a factor of at least about 10, and fully melts the new layer of powder particles in addition to the substrate, to achieve a smooth printed layer. The wavelength of the first light pulse also differs from a wavelength of the second light pulse.

Khairallah, Saad A.↗

The effect of blue and infrared laser melting frequency on oxide morphology in 304L

Continuous Wave Laser Beam (LB) melting offers control over the localised heating and cooling of melt pools for welding, brazing, additive manufacturing and solidification. Research into laserliquid metal interactions has primarily focused on the heat and mass transport under large thermal gradients imposed by the localised melting conditions. Recent commercial availability of blue (450 nm) wavelength lasers has enabled the printing of material with poor IR (1064) nm attenuation like Cu. However, little research has been conducted into varying input laser frequency and scan rate at fixed absorption to understand the effects of laser light on surface oxide formation and the underlying liquid metal thermodynamic response. Here, this article conducts laser melting of 304L under Blue (450 nm) and Infrared (IR, 1064 nm) laser frequencies and examines their impact on laser oxide thickness, chemistry and coloration. We find that laser frequencies induce changes in the oxide layer thickness and chemistry that cannot be explained using conventional thermal absorption shifts and fluid dynamics. We suggest that light coupling may have thermodynamic implications for the chemical potential of the liquid metal, which may drive the observed phase behaviour. Identifying mechanisms for the tuning of the chemical potential via laser frequency control could enable the ability to control solidification microstructure and atomic ordering in laser welding and additive manufacturing processes.

304L↗

The Effect of Sulfuric Acid Anodization on the Electrochemical Properties of Aluminum Alloy AlSi 10 Mg Prepared by Selective Laser Melting

Aluminum alloy, AlSi 10 Mg, prepared by selective laser melt (SLM) fabrication was anodized in 9.8% sulfuric acid (Type II) at 15 V for a total of 23 min. Experiments were performed to study the potentiostatic anodization process and its effects on the oxide coating morphology, thickness, and electrochemical properties of the alloy. Prior to anodization, the alloy microstructure is composed of aluminum cells encapsulated in a silicon network. Anodizing the abraded and polished AlSi 10 Mg surface produced a porous oxide layer with a thickness of 5μm. The oxide coating weight was 698 ± 29 mg/ft 2 . The oxide coating forms in the aluminum cells that are isolated from one another by the silicon eutectic phase. In electrochemical tests, the anodic and cathodic potentiodynamic polarization currents were suppressed by factors of 15× and 215×, respectively, as compared to the unanodized controls. The data indicate the anodic oxide coating suppresses the cathodic more than the anodic reaction rate. Linear polarization resistance (R p ) values increased by 279× after anodization. The corrosion current density values (j corr ) decreased by 133× after anodization. Taken together, the electrochemical data indicate the anodic oxide coating (unsealed) increases the corrosion resistance of the SLM alloy by two orders of magnitude.

Electrochemistry↗

In situ synchrotron X-ray diffraction analysis of ultrasonically assisted microstructure refinement during laser melting process

This work investigates the effect of ultrasonic treatment (UST) on the microstructure of AA4043 alloy during laser melting process. Here, the study utilizes in situ synchrotron X-ray diffraction (SXRD) and postmortem electron backscatter diffraction (EBSD) techniques to examine the ultrasonic grain refinement mechanism. The SXRD diffraction patterns exhibit higher continuity of major diffraction rings in the UST-test pattern, indicating a more refined grain structure. The presence of new diffraction spots in the post-test diffraction pattern with UST suggests the breakdown of epitaxial growth of columnar dendrites during solidification. Thermal profiles determined by analyzing the lattice parameter evolution show a faster cooling rate with UST. The inverse pole figures and aspect ratio distribution from EBSD reveal that the UST samples exhibit a refined, more equiaxed grain structure along the weld centerline. UST sample also develops more fine-sized low angle grain boundaries (LAGBs). These features offer better hot-cracking resistance in aluminum alloys.

36 MATERIALS SCIENCE↗

Effect of laser melt schedule on the microstructure of additively manufactured IN718 Superalloy

Laser powder bed fusion (L-PBF) has enabled the fabrication of geometrically complex metallic structures and components that are challenging to producing using conventional manufacturing approaches. The site-specific and far from equilibrium thermal conditions of L-PBF offer the potential to facilitate multi-length scale design of structure and properties across the atomic-through macro-levels. However, L-PBF systems face scalability challenges due to throughput constraints. Laser rotary powder bed fusion (L-RPBF) systems are being investigated as a solution to enhance the deposition rates compared to conventional L-PBF. Rotary systems also offer additional flexibility for controlling the time structure of melting through laser interleaving on alternating layers. Here, in this study, IN718 test samples were printed using single-laser or interleaved dual-laser configuration in a L-RPBF system to investigates the effect of process settings and melt-interleaving on as-fabricated microstructure. The microstructural evolution, such as grain size and crystallographic texture, was assessed by determining variations in the melt-pool shapes. Laser interleaving leads to a reduction in average grain size compared to single laser by ∼ 40 % at high power (400 W) and by ∼36 % at medium power (370 W). Results presented here identify key challenge for obtaining uniform microstructures and barriers for the broader adoption of high-deposition rate L-RPBF.

Dual-laser↗

Transmission electron microscopy of the rapid solidification microstructure evolution and solidification interface velocity determination in hypereutectic Al-20at.%Cu after laser melting

The evolution of rapid solidification (RS) microstructure and solidification interface velocity has been studied experimentally by in-situ transmission electron microscopy and postmortem characterization for hypereutectic Al-20at.%Cu (37 wt.%Cu) after laser melting. Four morphologically distinct regions formed via growth modes changing from θ-Al 2 Cu phase dendrites to eutectic cell growth, possibly α-Al dendrite growth (α-cell), banded growth, and α-Al plane front growth. Tendency for faceting and low capacity for solute trapping limited the θ-phase dendrite growth to solidification interface velocity v < 0.07 m/s. Consequently, formation of pro-eutectic micro-constituent was suppressed, and RS microstructure formation was dominated by eutectic, α-cell, and banded morphology grains for the Al-20at.%Cu alloy. Eutectic growth operated for interface velocity of 0.1 m/s ≤ v < 0.3 m/s, with a transition from regular lamellar, 2-λ and 1-λ mode to a dense irregular morphology dominated by α-phase at v = 0.3 m/s. Interface temperature calculations indicated feasibility of α-cell growth mode for 0.3 m/s ≤ v < 0.7 m/s. Banded growth occurred for 0.7 m/s ≤ v < 1.3 m/s. Plane front α-phase growth was evident for interface velocities v ≥ 1.3 m/s. Previous work on rapid solidification microstructure development in hypereutectic Al-Cu alloys reported a regime of α-cell growth subsequently to eutectic and prior to transition to banded growth for Al-19at.%Cu (36 wt.%Cu), while for Al-22at.%Cu (40 wt.%Cu) eutectic growth transitioned directly to α-plane front growth without emergence of a banded regime. Finally, based on the current study the disappearance of the banded growth regime occurs for a composition larger than 20at.%Cu.

36 MATERIALS SCIENCE↗

Microstructural evolution and phase stability in Nb-containing interstitial Fe-Mn-Co-Cr-C high-entropy alloys: An in-situ synchrotron X-ray diffraction study during laser melting

The influence of Nb on phase stability and microstructural evolution in an interstitial Fe-Mn-Co-Cr-C high-entropy alloy was investigated using in-situ synchrotron X-ray diffraction (SXRD) during laser melting. Scheil-Gulliver simulations predict the formation of σ and γ-f.c.c. phases in all three alloys, along with NbC in Nb-containing compositions. SXRD confirmed the presence of most predicted phases, but the σ phase was absent. Nb promotes crystallite refinement and increases dislocation density, though excessive additions reduce refinement efficiency due to solubility limits and secondary phase formation. Furthermore, Nb addition also enhances ε-h.c.p. phase formation by reducing stacking fault energy through NbC-induced carbon depletion. Analysis of intensity peak evolution reveals that Nb alters preferred grain orientations, reducing {111} γ intensity while enhancing {220} γ , leading to a more isotropic grain distribution. Overall, Nb plays a key role in phase selection, microstructure refinement, and preferred orientation evolution, allowing the tailored microstructure of high-entropy alloys via rapid solidification.

Interstitial high entropy alloys↗

Overcoming the doping limit in GaAs by ion implantation and pulsed laser melting

Most semiconductors exhibit a saturation of free carriers when heavily doped with extrinsic dopants. This carrier saturation or “doping limit” is known to be related to the formation of native compensating defects, which, in turn, depends on the energy positions of their conduction band minimum and valence band maximum. Here, we carried out a systematic study on the n-type doping limit of GaAs via ion implantation and showed that this doping limitation can be alleviated by the transient process of pulsed laser melting (PLM). For n-type doping, both group VI (S) and amphoteric group IV (Si and Ge) dopants were implanted in GaAs. For comparison, p-type doping was also studied using Zn as the acceptor. Implanted dopants were activated by the PLM method, and the results are compared to rapid thermal annealing (RTA). Our results reveal that for all n-type dopants, while implantation followed by the RTA results in a similar saturation electron concentration of 2–3 × 10 18 cm –3 , the transient PLM process is capable of trapping high concentration of dopants in the substitutional site, giving rise to a carrier concentration of >10 19 cm –3 , exceeding the doping limit of GaAs. However, due to scatterings from point defects generated during PLM, the mobility of n-type GaAs after PLM is low (~80–260 cm 2 /V s). Subsequent RTA after PLM (PLM + RTA) is able to remove these point defects and recover the mobility to ~1000–2000 cm2/V s. The carrier concentrations of these PLM + RTA samples are reduced but are still a factor of 3 higher than RTA only GaAs. This can be understood as the dopants are already incorporated in the substitutional site after PLM; they are less likely to be “deactivated” by subsequent RTA. This work is significant to the understanding of doping mechanisms in semiconductors and provides a means for device applications, which require materials with ultra-high doping.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Analytical model for balling defects in laser melting using rivulet theory and solidification

In laser welding and additive manufacturing communities, the balling (humping) defect is primarily attributed to the Plateau–Rayleigh fluid instability (PRI) with a few authors suggesting fluid jetting and volume conservation as alternative mechanisms. As analytical descriptions of these mechanisms are unavailable, combining them into a single formalism is unfeasible. We present a new model of PRI with higher accuracy, accounting for competition with solidification, to compare the expected behavior with known experimental trends when fluid jetting is neglected. We adapt a rivulet instability model from fluid physics to account for the stabilizing effects of the substrate, which the traditional cylindrical-jet geometry does not account for and estimate the instability growth rate. Our model yields a continuous transition from non-balling to balling hitherto lacking in current literature and predicts instability growth at higher wavelengths with strong sensitivity to the solidification front curvature. While the fluid surface is most unstable for shallow melt pools, the absolute magnitude of balling relevant to printing defects scales with melt pool depth and has a maximum for a given melt pool geometry. Synchrotron-based x-ray radiography of thin samples indicates that PRI growth rates and solidification can be comparable in magnitude and thus compete, as we find in this work. We predict that deviations between model predictions and our experimental results demonstrate the importance of fluid flows and heat transport in the balling process. Our experiments further demonstrate at least one mechanism by which the melt pool length and the balling wavelength are not equivalent, as commonly claimed.

Taylor, Z. [Stanford Univ., CA (United States); SL↗

Solidification cracking of laser melted commercial-purity tungsten

The high melting temperature of tungsten (W) makes it an attractive candidate for energy generation applications; however, its use is limited by its poor ductility at low temperatures. This limitation affects even melt-based additive manufacturing (AM) processes such as laser powder bed fusion (PBF-LB), with as-fabricated pure W exhibiting both longitudinal and transverse cracks. Metallurgical and processing factors that affect these cracks are still being explored. This work utilizes powderless single-tracks on pure W plates made over a range of power and velocity combinations in three unique PBF-LB setups: one with flowing argon, one with continuous vacuum, and an in situ high-speed synchrotron X-ray radiography setup. Each had different oxygen activities in their build environments. Longitudinal cracks with oxides appearing to exude from the crack were found for tracks deposited in a build environment with argon shield gas, while no such cracks were observed for builds conducted in vacuum. A calculation showed that direct oxygen ingress into the melt pool from the build environment is negligible when argon shield gas is present. Thus, incorporation of spatter is a likely mechanism for oxygen ingress into the melt pool. Radiography showed extensive keyholing, spatter generation, and crack formation at keyhole porosity. A heat transfer calculation showed the crack formation time was consistent with cooling below its ductile-to-brittle transition (DBT) temperature. This work identifies solidification cracking as a feasible mechanism in pure W beyond the well-known DBT related cracking.

Materials science↗

Influence of Solidification Velocity on Partitioning and Precipitate Evolution in a Multicomponent, Soft Magnetic Alloy Processed by Laser Melting

Multicomponent alloys have recently been shown to overcome the structural-functional barrier associated with soft magnetic materials. Here, single laser tracks have been used to investigate the effects of solidification velocity on the Al 7 Fe 32.6 Co 27.7 Ni 27.7 Ta 5 (at pct) alloy. Ta-rich cell wall partitioning was shown to affect the final distribution and size of the precipitating L1 2 phase, after aging. These findings demonstrate that solidification rate control offers the potential to tailor localized performance in alloys with size-dependent precipitation properties.

Brookins, Jeffrey M. [Oak Ridge National Laborator↗