Search NASA⌕ Search

SEARCH · Search NASA

Results for “Li15Si4”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

Electronic Origin For The Phase Transition From Amorphous LixSi To Crystalline Li15Si4

Silicon has been widely explored as an anode material for lithium ion battery. Upon lithiation, silicon transforms to amorphous LixSi (a-LixSi) via electrochemical driven solid state amorphization. With increasing lithium concentration, a-LixSi transforms to crystalline Li15Si4 (c-Li15Si4). The mechanism of this crystallization process is not known. In this paper, we report the fundamental characteristics of the phase transition of a-LixSi to c-Li15Si4 using in-situ scanning transmission electron microscopy (STEM), electron energy loss spectroscopy (EELS), and density function theory (DFT) calculation. We find that when the lithium concentration in a-LixSi reaches a critical value of x = 3.75, the a-Li3.75Si spontaneously and congruently transforms to c-Li15Si4 by a process that is solely controlled by the lithium concentration in the a-LixSi, involving neither large scale atomic migration nor phase separation. DFT calculations indicate that c-Li15Si4 formation is favored over other possible crystalline phases due to the similarity in electronic structure with a-Li3.75Si.

Environmental Molecular Sciences Laboratory↗

Materials Data on Li15Si4 by Materials Project

Li15Si4 crystallizes in the cubic I-43d space group. The structure is three-dimensional. there are two inequivalent Li sites. In the first Li site, Li is bonded in a 3-coordinate geometry to two equivalent Li and three equivalent Si atoms. There are one shorter (2.73 Å) and one longer (2.79 Å) Li–Li bond lengths. There are a spread of Li–Si bond distances ranging from 2.61–2.81 Å. In the second Li site, Li is bonded to eight equivalent Li and four equivalent Si atoms to form LiLi8Si4 cuboctahedra that share corners with eight equivalent SiLi12 cuboctahedra, edges with eight equivalent LiLi8Si4 cuboctahedra, and faces with four equivalent SiLi12 cuboctahedra. All Li–Si bond lengths are 2.86 Å. Si is bonded to twelve Li atoms to form distorted SiLi12 cuboctahedra that share corners with six equivalent LiLi8Si4 cuboctahedra, edges with six equivalent SiLi12 cuboctahedra, faces with three equivalent LiLi8Si4 cuboctahedra, and faces with five equivalent SiLi12 cuboctahedra.

36 MATERIALS SCIENCE↗

First Principles Simulations of the Electrochemical Lithiation and Delithiation of Faceted Crystalline Silicon

Silicon is of significant interest as a next-generation anode material for lithium-ion batteries due to its extremely high capacity. The reaction of lithium with crystalline silicon is known to present a rich range of phenomena, including electrochemical solid state amorphization, crystallization at full lithiation of a Li15Si4 phase, hysteresis in the first lithiation–delithiation cycle, and highly anisotropic lithiation in crystalline samples. Very little is known about these processes at an atomistic level, however. To provide fundamental insights into these issues, we develop and apply a first principles, history-dependent, lithium insertion and removal algorithm to model the process of lithiation and subsequent delithiation of crystalline Si. The simulations give a realistic atomistic picture of lithiation demonstrating, for the first time, the amorphization process and hinting at the formation of the Li15Si4 phase. Voltages obtained from the simulations show that lithiation of the (110) surface is thermodynamically more favorable than lithiation of the (100) or (111) surfaces, providing an explanation for the drastic lithiation anisotropy seen in experiments on Si micro- and nanostructures. Analysis of the delithiation and relithiation processes also provides insights into the underlying physics of the lithiation–delithiation hysteresis, thus providing firm conceptual foundations for future design of improved Si-based anodes for Li ion battery applications.

Environmental Molecular Sciences Laboratory↗

In Situ and Ex Situ TEM Study of Lithiation Behaviours of Porous Silicon Nanostructures

Here in this work, we study the lithiation behaviours of both porous silicon (Si) nanoparticles and porous Si nanowires by in situ and ex situ transmission electron microscopy (TEM) and compare them with solid Si nanoparticles and nanowires. The in situ TEM observation reveals that the critical fracture diameter of porous Si particles reaches up to 1.52 μm, which is much larger than the previously reported 150 nm for crystalline Si nanoparticles and 870 nm for amorphous Si nanoparticles. After full lithiation, solid Si nanoparticles and nanowires transform to crystalline Li 15 Si 4 phase while porous Si nanoparticles and nanowires transform to amorphous Li x Si phase, which is due to the effect of domain size on the stability of Li 15 Si 4 as revealed by the first-principle molecular dynamic simulation. Ex situ TEM characterization is conducted to further investigate the structural evolution of porous and solid Si nanoparticles during the cycling process, which confirms that the porous Si nanoparticles exhibit better capability to suppress pore evolution than solid Si nanoparticles. The investigation of structural evolution and phase transition of porous Si nanoparticles and nanowires during the lithiation process reveal that they are more desirable as lithium-ion battery anode materials than solid Si nanoparticles and nanowires.

25 ENERGY STORAGE↗

In Situ TEM Investigation of Congruent Phase Transition and Structural Evolution of Nanostructured Silicon/Carbon Anode for Lithium Ion Batteries

It is well known that upon lithiation both crystalline and amorphous Si transform to a armorphous LixSi phase, which subsequently crystallizes to a (Li, Si) crystalline compound, either Li15Si or Li22Si5. Up to date, the detailed atomistic mechanism of this phase transformation, and degradation process in nanostructured Si, are not fully understood. Here, we report the microstructural evolution and phase transformation characteristic of a specially designed amorphous silicon (a-Si) coated carbon nanofiber (CNF) composite during charge/discharge process using in-situ TEM and density function theory molecular dynamic (DFT-MD) calculation. We found that the crystallization of Li15Si4 from amorphous LixSi is a spontaneous, congruent phase transition process without phase separation or large scale atomic motion, which is drastically different from what is expected from a classic nucleation and growth process. The a-Si layer is strongly bonded to the CNF and no spallation or cracking is observed during the early stages of cyclic charge/discharge. Reversible volume expansion/contraction upon charge/discharge is fully accommodated along the radial direction. However, with progressive cycling, damage in the form of surface roughness was gradually accumulated on the coating layer, which is believed to be the mechanism for the eventual capacity fade of the composite anode during long term charge/discharge cycling.

25 ENERGY STORAGE↗