Materials Data on Li2SiO3 by Materials Project

Li2SiO3 crystallizes in the orthorhombic Cmc2_1 space group. The structure is three-dimensional. Li1+ is bonded to four O2- atoms to form distorted LiO4 tetrahedra that share corners with five equivalent SiO4 tetrahedra and corners with seven equivalent LiO4 tetrahedra. There are a spread of Li–O bond distances ranging from 1.96–2.19 Å. Si4+ is bonded to four O2- atoms to form SiO4 tetrahedra that share corners with two equivalent SiO4 tetrahedra and corners with ten equivalent LiO4 tetrahedra. There is two shorter (1.61 Å) and two longer (1.70 Å) Si–O bond length. There are two inequivalent O2- sites. In the first O2- site, O2- is bonded to two equivalent Li1+ and two equivalent Si4+ atoms to form distorted corner-sharing OLi2Si2 tetrahedra. In the second O2- site, O2- is bonded to three equivalent Li1+ and one Si4+ atom to form distorted corner-sharing OLi3Si tetrahedra.

36 MATERIALS SCIENCE↗

Tritium trapping in silicon carbide in contact with solid breeder under high flux isotope reactor irradiation

The trapping of tritium in silicon carbide (SiC) injected from ceramic breeding materials was examined via tritium measurements using imaging plate (IP) techniques. Monolithic SiC in contact with ternary lithium oxide (lithium titanate and lithium aluminate) as a ceramic breeder was irradiated in the High Flux Isotope Reactor (HFIR) in Oak Ridge, Tennessee, USA. The distribution of photo-stimulated luminescence (PSL) of tritium in SiC was successfully obtained, which separated the contribution of 14C ß-rays to the PSL. The tritium incident from ceramic breeders was retained in the vicinity of the SiC surface even after irradiation at 1073 K over the duration of ~3000 h, while trapping of tritium was not observed in the bulk region. The PSL intensity near the SiC surface in contact with lithium titanate was higher than that obtained with lithium aluminate. The amount of the incident tritium and/or the formation of a Li2SiO3 phase on SiC due to the reaction with lithium aluminate under irradiation likely were responsible for this observation.

99 GENERAL AND MISCELLANEOUS↗

Efficacy of a Solution-Based Approach for Making Sodalite Waste Forms for an Oxide Reduction Salt Utilized in the Reprocessing of Used Uranium Oxide Fuel

This paper describes various approaches for making sodalite with a LiCl-Li2O oxide reduction salt used to recover uranium from used oxide fuel. The approaches include sol-gel and solution-based synthesis processes. As-made products were mixed with 5 and 10 mass% of a Na2O-B2O3-SiO2 glass binder and these, along with product without a binder, were heated using either a cold-press-and-sinter method or hot uniaxial pressing. The results demonstrate the limitation of sodalite yield due to the fast intermediate reactions between Na+ and Cl- to form halite in solution and Li2O and SiO2 to form lithium silicates (e.g., Li2SiO3 or Li2Si2O5) in the calcined and sintered pellets. The results show that pellets can be made with high sodalite fractions (~92 mass%) and low porosities using a solution-based approach and this LiCl-Li2O salt.

electrochemical↗

Investigating the Chemical Reactivity of Lithium Silicate Model SEI Layers

Silicon anodes suffer from an unstable solid electrolyte interphase (SEI) layer that contributes to undesirable capacity fade with cycling. A key part to addressing this unstable SEI formation is to examine how certain components of the SEI react with the electrolyte over time. One SEI component that has not been thoroughly studied in the context of the chemical reactivity against the electrolyte is lithiated silicate. Four model silicate thin films with increasing lithium content were deposited by radio frequency (RF) magnetron sputtering to study how the lithiation of the native oxide on a silicon anode affects the chemical stability of the anode surface. SiO2, Li2Si2O5, Li2SiO3, and Li3SiOx films were exposed to 1.2 M LiPF6 in the 3:7 wt% ethylene carbonate/ethyl methyl carbonate (EC/EMC) electrolyte for periods of time that are representative of the amount of time it takes to undergo cell formations. Soaked samples were rinsed, dried, and characterized by a combination of attenuated total reflectance-infrared spectroscopy (ATR-IR), focused ion beam-secondary electron microscopy (FIB-SEM), and X-ray photoelectron spectroscopy (XPS) depth profiling. It was found that the rate of the decrease in film thickness of the silicates exposed to the electrolyte over time increases as a function of the lithium content in the thin film. This reaction involves HF etching and LiPF6 salt degradation leading to silicate loss and fluorination throughout the bulk. Understanding this chemical instability is critical to determining the overall mechanism of SEI degradation over time.

ADVANCED PROPULSION SYSTEMS,ENERGY STORAGE↗

Crystallization of a Li2O2SiO2 Glass under High Hydrostatic Pressures

The crystallization behavior of a Li2O.2SiO2 (LS2) glass subjected to a uniform hydrostatic pressure of 4.5 or 6 GPa was investigated between 550 and 800 C using XRD, IR, Raman, TEM, NMR, and DTA. The density of the glass subjected to 6 GPa was between 2.52 plus or minus 0.01 and 2.57 plus or minus 0.01 grams per cubic centimeters, depending upon the processing temperatures, and was higher than that of the stoichiometric LS2 crystals, 2.46 plus or minus 0.01 grams per cubic centimeter. Thus, crystallization in 6 GPa glass occurred in a condition of negative volume dilatation, deltaV = V(sub glass) - V(sub crystal), while that for the 4.5 GPa glass occurred in the condition deltaV greater than 0. For deltaV greater than 0, which also includes the control glass at ambient (one atmosphere) pressure, the glasses always crystallize Li2Si2O5 (orthorhombic, Ccc2) crystals, but for deltaV less than 0 (6 GPa), the glasses crystallize Li2SiO3 crystals with a slightly deformed structure. The crystal growth rate vs. temperature curve moved to higher temperature with increasing pressure, and was independent of the sign of deltaV. These results for the effect of hydrostatic pressure on the crystallization of LS2 glass were discussed from thermodynamic considerations.

Fuss, T.↗

A Novel Theoretical Method to Search Good Candidates of Solid Sorbents for CO2 Capture

The increasing atmospheric CO2 concentration is the most important environmental issue of global warming that the world faces today. During past few decades, many technologies have been developing to separate and capture CO2 from coal gasifier. As high temperature CO2 absorbents, solid materials are potential candidates. Lithium silicate(Li4SiO4) and zirconate(Li2ZrO3) have been studying for CO2 capture by researchers at Toshiba and found that they absorb CO2 at 773K and release CO2 around 973K. Based on these well-known experimental exploring results on these lithium salts, we have been developing a novel theoretical methodology to search better solid materials for CO2 capture: (1) Based on the crystal structures of solids, the density functional calculations are performed to obtain their electronic structural properties and their binding energies. The energy change(ΔE) for the reaction solid_sorbent+CO2 ↔ sorbent_CO2+ solid are evaluated. (2) For a vast of data-bank of solid materials, as our first filter if |ΔE|<|ΔGLi2SiO4|, where ΔG is the free energy change for reaction of Li2SiO4+CO2↔ Li2CO3 +Li2SiO3, we select this solid as a potential good candidate for CO2 capture. (3) For these possible candidates, we further perform phonon calculations and obtain their vibration frequencies. With them, partition functions of solids(Z) can be calculated out. With Z, the thermal dynamical properties (zero point energy, entropy, enthalpy, free energy, etc.) under different conditions (temperature(T), pressure(P)) can be readily calculated. With them, the chemical potentials(Δμ)(functional of T and P) for the sorption/desorption reaction are evaluated. (4) Using Δμ as our second filter, we can reduce the number of our selected good candidates to a small number of better candidates. (5) The last step is to make the fine tune (the 3rd filter) the better candidates to a small set of the best candidates by considering the operating conditions(T, P, etc.), absorbing CO2 weight percentage, stabilities, and the associated costs, etc.

01 COAL, LIGNITE, AND PEAT↗

Constructing stable interface layer for boosting high-voltage cycling performance of single-crystal Ni-rich cathodes

Increasing demand for electric vehicles (EVs) worldwide and the requirements for environmental protection have greatly promoted the development of low-Co, Ni-rich layered cathodes due to their high energy density, reasonable cost, and less environmental pollution. Nevertheless, serious performance degradation and safety concerns resulting from structural/interfacial instability under high operating voltages (≥4.3 V) have greatly hindered its commercialization. Herein, we propose a feasible surface modification strategy by introducing a multifunctional Li 2 SiO 3 (LSO) coating layer onto the surface of Co less single-crystalline LiNi 0.63 Co 0.07 Mn 0.3 O 2 (NCM) to solve the above challenges. Additionally, the uniform Li 2 SiO 3 coating layer has a unique three-dimensional (3D) ion diffusion channel, which greatly promotes the transmission of Li + and alleviates interfacial stress accumulation. Equally important, the electrochemically inert Li 2 SiO 3 coating layer has a stable structure framework with strong Si-O bonds, which inhibit anisotropic particle volume expansion and the occurrence of side reactions during long-term cycling. As a consequence, LSO modified NCM exhibits greatly improved electrochemical properties even at harsh testing conditions and achieves capacity retention of 79.1% after 200 cycles at 25°C within 2.95-4.5 V in half cells. Furthermore, it provides an outstanding capacity retention of 94.7% after 300 cycles at 25°C within 2.95-4.4 V when tested in pouch full cells.

25 ENERGY STORAGE↗