Materials Data on Lu(CuS)3 by Materials Project

Lu(CuS)3 crystallizes in the trigonal P-3m1 space group. The structure is two-dimensional and consists of one Lu(CuS)3 sheet oriented in the (0, 0, 1) direction. Lu3+ is bonded to six S2- atoms to form LuS6 octahedra that share corners with nine CuS4 tetrahedra, edges with six equivalent LuS6 octahedra, and edges with six CuS4 tetrahedra. There are three shorter (2.64 Å) and three longer (2.77 Å) Lu–S bond lengths. There are three inequivalent Cu1+ sites. In the first Cu1+ site, Cu1+ is bonded to four equivalent S2- atoms to form CuS4 tetrahedra that share corners with six equivalent LuS6 octahedra, corners with six equivalent CuS4 tetrahedra, edges with three equivalent LuS6 octahedra, and edges with three equivalent CuS4 tetrahedra. The corner-sharing octahedra tilt angles range from 19–53°. There are three shorter (2.33 Å) and one longer (2.46 Å) Cu–S bond lengths. In the second Cu1+ site, Cu1+ is bonded in a trigonal planar geometry to three equivalent S2- atoms. All Cu–S bond lengths are 2.21 Å. In the third Cu1+ site, Cu1+ is bonded to four S2- atoms to form CuS4 tetrahedra that share corners with three equivalent LuS6 octahedra, corners with six equivalent CuS4 tetrahedra, and edges with three equivalent LuS6 octahedra. The corner-sharing octahedral tilt angles are 9°. There are one shorter (2.22 Å) and three longer (2.43 Å) Cu–S bond lengths. There are three inequivalent S2- sites. In the first S2- site, S2- is bonded to three equivalent Lu3+ and four equivalent Cu1+ atoms to form distorted SLu3Cu4 pentagonal bipyramids that share corners with three equivalent SLu3Cu3 octahedra, edges with three equivalent SLu3Cu3 octahedra, and edges with nine equivalent SLu3Cu4 pentagonal bipyramids. The corner-sharing octahedral tilt angles are 4°. In the second S2- site, S2- is bonded to three equivalent Lu3+ and three equivalent Cu1+ atoms to form distorted SLu3Cu3 octahedra that share corners with three equivalent SLu3Cu4 pentagonal bipyramids, corners with three equivalent SCu4 trigonal pyramids, edges with six equivalent SLu3Cu3 octahedra, and edges with three equivalent SLu3Cu4 pentagonal bipyramids. In the third S2- site, S2- is bonded to four Cu1+ atoms to form SCu4 trigonal pyramids that share corners with three equivalent SLu3Cu3 octahedra and corners with six equivalent SCu4 trigonal pyramids. The corner-sharing octahedral tilt angles are 65°.

36 MATERIALS SCIENCE↗

Materials Data on Lu(CuS)3 by Materials Project

Lu(CuS)3 crystallizes in the trigonal R-3 space group. The structure is three-dimensional. Lu3+ is bonded to six equivalent S2- atoms to form LuS6 octahedra that share corners with twelve equivalent CuS4 tetrahedra, edges with three equivalent LuS6 octahedra, and edges with six equivalent CuS4 tetrahedra. All Lu–S bond lengths are 2.69 Å. Cu1+ is bonded to four equivalent S2- atoms to form CuS4 tetrahedra that share corners with four equivalent LuS6 octahedra, corners with six equivalent CuS4 tetrahedra, edges with two equivalent LuS6 octahedra, and edges with three equivalent CuS4 tetrahedra. The corner-sharing octahedra tilt angles range from 15–56°. There are a spread of Cu–S bond distances ranging from 2.33–2.41 Å. S2- is bonded to two equivalent Lu3+ and four equivalent Cu1+ atoms to form a mixture of distorted corner and edge-sharing SLu2Cu4 octahedra. The corner-sharing octahedra tilt angles range from 0–90°.

36 MATERIALS SCIENCE↗

Ionic liquids-modulated two-phase thermal synthesis of three-dimensional CuS nanostructures

A novel method was proposed for successful fabrication of CuS nanostructures with various morphologies. At the ionic liquids (ILs)-modulated CHCl{sub 3}-H{sub 2}O interface, copper cupferronate [Cu(cup){sub 2}] in CHCl{sub 3} reacted with thiourea in water to generate CuS nanostructures via a solvothermal reaction process. The effects of alkyl chain length of imidazolium cations and nature of anions of the ILs, molar ratio of Cu(cup){sub 2} to thiourea, the reaction temperature and time on the morphology of the products were studied systematically. It was shown that by changing alkyl chain length of imidazolium cations and nature of anions of the ILs, CuS nanostructures with various morphologies, including flowers, urchins, large nanodisks and nanoparticles, could be obtained at the liquid-liquid interface, and the ILs played important template roles in directing the formation of CuS nanostructures. Furthermore, the as-prepared CuS samples exhibited high catalytic activity for photodegradation of methyl orange and thermal decomposition of ammonium perchlorate. - Graphical abstract: At the ionic liquids-modulated CHCl{sub 3}-H{sub 2}O interface, the CuS nanostructures with the various morphologies of flowers, urchins, large nanodisks and nanoparticles have been successfully prepared via a solvothermal reaction process. Highlights: Black-Right-Pointing-Pointer The properties of oil-H{sub 2}O interface can be modulated by employing different ILs. Black-Right-Pointing-Pointer The modulated interface has been used to prepare CuS nanostructures with various morphologies. Black-Right-Pointing-Pointer The CuS samples exhibited high catalytic activity for the photodegradation of methyl orange.

36 MATERIALS SCIENCE↗

Polysulfides capture-copper additive for long cycle life lithium sulfur batteries

Copper powder was introduced into the lithium sulfur battery system to capture intermediate polysulfides and Cu x S (x = 1 or 2) species was generated depending on the chain length of polysulfides. This phenomenon was verified by X-ray absorption near edge structure technique. The results indicated that copper can be oxidized to CuS by Li 2 S x (x ≥ 6), and a mixture of Cu 2 S and CuS was obtained when x ranges from 3 to 6. While Cu 2 S is eventually formed in the presence of Li 2 S 3 . After several cycles activation, the polysulfide-shuttle effect and self-discharge phenomenon which hinder the application of lithium sulfur batteries are found nearly eliminated Further experiments demonstrated that in the case of Cu 2 S generation, a high specific sulfur capacity of 1300 mAh g –1 could be delivered, corresponding to 77.6% sulfur utilization, while the Coulombic efficiency approximates around 100%. As a result, self-discharge experiment further demonstrated that polysulfides almost disappear in the electrolyte, which verified the polysulfide-capture capability of copper.