Search NASA⌕ Search

SEARCH · Search NASA

Results for “MODULE ENCAPSULATION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Metal Halide Perovskite Solar Module Encapsulation Using Polyolefin Elastomers: The Role of Morphology in Preventing Delamination

The development of perovskite solar cells (PSCs) has ushered in a new era of solar technology, characterized by its exceptional efficiency and cost-effective production. However, the soft and fragile nature of perovskites makes module encapsulation challenging. Polyolefin elastomers (POEs) have been reported to be promising encapsulants for perovskite modules. However, little research exists on identifying criteria among different types of POEs as encapsulants. Here, two POEs with different morphologies were compared as encapsulants. The first POE crystallizes during encapsulation (crystal content ∼40%), and the resulting shrinkage or warpage leads to delamination, causing minimodule failure. In contrast, perovskite minimodules encapsulated with a mostly amorphous POE exhibited better reliability and reproducibility. The best perovskite minimodules passed the thermal cycling test for 240 cycles between −40 and 85 °C and the damp heat test for 1419 h, according to the IEC 61215 standard. This study highlights the importance of the morphology of encapsulants in achieving high-quality encapsulation. Published by the American Physical Society 2024

14 SOLAR ENERGY↗

Testing Protocol for Module Encapsulant Creep (Presentation)

Recently there has been an interest in the use of thermoplastic encapsulant materials in photovoltaic modules to replace chemically crosslinked materials, e.g., ethylene-vinyl acetate. The related motivations include the desire to: reduce lamination time or temperature; use less moisture-permeable materials; or use materials with better corrosion characteristics. However, the use of anythermoplastic material in a high-temperature environment raises safety and performance concerns, as the standardized tests currently do not expose the modules to temperatures in excess of 85C, yet modules may experience temperatures above 100C in operation. Here we constructed eight pairs of crystalline-silicon modules and eight pairs of glass/encapsulation/glass mock modules using differentencapsulation materials of which only two were designed to chemically crosslink. One module set was exposed outdoors with insulation on the back side in Arizona in the summer, and an identical set was exposed in environmental chambers. High precision creep measurements and performance measurements indicate that despite many of these polymeric materials being in the melt state at some of thehighest outdoor temperatures achievable, very little creep was seen because of their high viscosity, temperature heterogeneity across the modules, and in the case of the crystalline-silicon modules, the physical restraint of the backsheet. These findings have very important implications for the development of IEC and UL qualification and safety standards, and in regards to the necessary level ofcure during the processing of crosslinking encapsulants.

14 SOLAR ENERGY↗

Field-Aged Glass/Backsheet and Glass/Glass PV Modules: Encapsulant Degradation Comparison

Ethylene vinyl acetate (EVA) is the predominant encapsulant in crystalline-silicon photovoltaic (PV) modules; however, its degradation is a subject of major concern, which causes significant power loss under field conditions. This article presents a comparison of EVA degradation in field-aged PV modules with glass/backsheet (G/B) and glass/glass (G/G) architectures. Modulelevel characterization included UV fluorescence imaging and I-V measurements. Material analytical techniques, including colorimetry, differential scanning calorimetry, thermogravimetric analysis, Fourier transform infrared spectroscopy, and Raman spectroscopy, were performed to correlate the module performance parameters with EVA material properties. An intense EVA discoloration in G/G modules was observed, which was corroborated by higher module Isc and Pmax degradation rates compared with its counterpart G/B modules. Higher power degradation was accompanied by a significant increase in EVA crosslinking, vinyl acetate content, yellowness index, and presence of functional groups containing unsaturated moieties that are linked to degradation products of photothermal reaction, and a higher decrease in the degree of crystallinity. The absence of a polymeric backsheet in hermetically sealed G/G modules, which restricts photobleaching and enhances the entrapment of volatile acetic acid and other degradation by-products, plays a major role in causing higher EVA degradation in G/G modules. This article concludes that EVA might have been a good choice of an encapsulant for the G/B modules over the decades, but it may prove to be an inappropriate choice for the G/G modules because of potential degassing, corrosion, and/or discoloration issues. Ionomers or polyester-based encapsulants like polyolefins could be best suited for G/G modules as it appears to be a current trend in the industry.

14 SOLAR ENERGY↗

What Is a Polyolefin? A Critical Overview of Ethylene Copolymers Used as Solar Photovoltaic Module Encapsulants

In recent years, photovoltaic (PV) encapsulant films marketed as polyolefins (POs), more specifically as PO elastomers (POEs) and thermoplastic POs (TPOs), have gained significant market share and are projected to become the dominant encapsulation films by 2030. Relative to other industries, there are significant misconceptions about the term PO in the PV industry. Both in the scientific literature as well as in sales and advertising, the terms PO, POE, and TPO are often misused to describe the same type of material with comparable properties, while in reality these may each consist of separate material classes. This paper provides a comprehensive literature and market review, to showcase a broad range of PO and other ethylene copolymer encapsulants from recent studies, and discusses the materials' properties to clarify what constitutes a “polyolefin.” In addition, to promote a clearer comparison of encapsulant properties, we propose a two‐dimensional taxonomy to categorize polymers used in module manufacturing, including POs. In terms of improving the reliability of solar PV modules, PO‐based encapsulants have several advantages (including lower water uptake and ion diffusion), but might come with disadvantages too, such as a more complex processing and a higher sensitivity to the storage conditions and shelf life. All this might prospectively impact adhesion properties of the encapsulant to other materials' interfaces (glass, cells etc.) and end‐product quality. Because the track record of field‐deployed PV modules containing PO encapsulants is also limited, we hope to contribute to better material understanding and precision in communication in PV to secure quality.

14 SOLAR ENERGY↗

Nanomechanical and Fluorescence Characterizations of Weathered PV Module Encapsulation

Nanoindentation and fluorescence spectroscopy provide spatially resolved mechanical and chemical characterization for degradation of poly (ethylene-co-vinyl acetate) (EVA) encapsulants aged under accelerated weathering and in field deployed photovoltaic (PV) modules. For the accelerated weathering tests, two different EVA formulations in the glass/EVA/glass-laminated coupons were exposed to ultraviolet (UV) light for 180 days at three different temperatures (40, 60, and 80 °C) and UV intensities (0.4, 2.2, and 2.9 W/m2/nm at 340 nm). The fluorescence spectra and moduli were uniform through the cross section of both EVA formulations at the lowest temperature and UV intensity; however, under the highest temperature and UV intensity, the UV irradiated sides showed lower moduli and higher fluorescence compared to the opposite sides. For EVA obtained from PV modules deployed 27 years in Sacramento, CA, USA, changes in fluorescence intensity across the thickness were relatively greater than changes in modulus. On the other hand, for EVA obtained from the same type of module stored in the shed for 27 years, no fluorescence was observed, and a uniform modulus was seen through the EVA layer, but with substantially higher values than those obtained from the field-deployed modules. The different extent of changes between laboratory and field exposures suggests the importance of considering effects of temperature and UV intensity for designing a reliable accelerated testing. This study uniquely demonstrates the capability of microscale characterization using nanoindentation and fluorescence microscopy to monitor mechanical and chemical degradation of EVA encapsulants in PV modules.

14 SOLAR ENERGY↗

Evaluation of the PID-s Susceptibility of Modules Encapsulated in Materials of Varying Resistivity

A common mechanism of potential-induced degradation is by shunting (PID-s) in PV modules, usually associated with the transport of sodium ions (Na+) through the encapsulant and penetrating the front junction of solar cells under voltage stress. Encapsulants with high volume resistivity have been suggested as a potentially cost-effective solution to this degradation mechanism. In this work, we examine three polyolefin elastomer (POE) encapsulants with volume resistivity varying over two orders of magnitude (ranging from 9 x 10^13 to 1 x 10^16 ..omega.. cm) that show equivalent and complete resistance to PID at the damp heat stress test level of 85 degrees C and 85% relative humidity and -1000 V system voltage stress. Performance is compared with a PID-susceptible ethylene vinyl acetate (EVA) encapsulant with resistivity 1 x 10^13 ..omega.. cm. The independence of PID susceptibility with respect to the resistivity of the polyolefin is attributed to the impermeability of POEs to Na + ions. Specific ions (i.e. Na + ), rather than charge-carrying species in general, are responsible for this degradation mechanism.

14 SOLAR ENERGY↗

Value Proposition of UV-Absorbers in PV Module Encapsulation

Various common crystalline silicon cell technologies were exposed to UVA radiation (1.24 Wm-2 nm-1 at 340 nm peak) on the front and back faces at 45 degrees Celsius for periods up to 3000 h, representing about 3 y of solar exposure in Phoenix, Arizona, USA. The resulting degradation of the open-circuit voltage and short-circuit current is presented. Of the various cell types examined, significant levels of degradation were seen in all cases. Less degradation was generally found after UV irradiation of cell fronts and older cell types, whereas a bifacial PERC type exposed on the rear showed about 25% degradation in short circuit current, attributable to lack of a diffused surface field. Selected cells were exposed to UV irradiation with the addition of long pass UV filters to replicate UV-absorbers in encapsulants. Modern cell designs are sensitive to UV-ID because of reduced or eliminated front and back surface field and increased dependence on high quality surface passivation. Single transformation of the independent variable (t, kW h/m^2) could be used to achieve a linear model of the data to extrapolate to 50 y. Solar Advisor Model (SAM) shows appropriate filtering of UV-irradiation can improve LCOE and net present value of plant. Some advanced cell types are seen to be UV-resistant (cell level solutions also exist). Solutions therefore exist on the cell, glass, and encapsulant level. Changes over time in each of these would also need to be considered (solarization, encapsulant browning...).

ENGINEERING,SOLAR ENERGY↗

Chapter 10.2: Encapsulant Materials for PV Modules

Encapsulant materials used in photovoltaic (PV) modules serve multiple purposes; it provides optical coupling of PV cells and protection against environmental stress. Polymers must perform these functions under prolonged periods of high temperature, humidity, and UV radiation. When PV panels were first developed in the 1960s and the 1970s, the dominant encapsulants were based on polydimethyl siloxane (PDMS). Ethylene-co-vinyl acetate (EVA) is currently the dominant encapsulant chosen for PV applications, not because it has the best combination of properties, but because it is an economical option with an established history of acceptable durability. Getting new products onto the market is challenging because there is no room for dramatic improvements, and one must balance the initial cost and performance with the unknowns of long-term service life. Recently, there has been renewed interest in using alternative encapsulant materials with some significant manufacturers switching from EVA to polyolefin elastomer-based (POE) alternatives.

14 SOLAR ENERGY↗

Durability of ionomer encapsulants in photovoltaic modules

Ethylene vinyl acetate (EVA) has for decades been the preferred material for photovoltaic (PV) module encapsulation. However, while it is relatively inexpensive and initially adheres well to module components, EVA discolors with age and - as interfacial adhesion degrades - becomes susceptible to delamination, ultimately resulting in reduced module efficiency and shortened service lifetimes. As potential replacements for EVA, ionomer thermoplastic materials cure faster, are more resistant to discoloration and potential induced degradation, and do not evolve corrosive acetic acid, making them compatible with new device materials such as perovskites. Since there is limited information on ionomer durability for PV module applications, a series of field and accelerated laboratory aging studies were conducted to assess ionomer interface stability in the presence of terrestrial environmental stressors. It is shown that adhesion to the glass and cell interfaces of PV modules is inferior to EVA, both before and after aging, rendering ionomers particularly susceptible to delamination after short timeframes. Potential solutions to improve ionomer adhesion are discussed.

14 SOLAR ENERGY↗

Hybrid chip-on-board LED module with patterned encapsulation

Light modules and methods of forming light modules are disclosed. A light module includes a first plurality and a second plurality of light emitting elements configured to emit, respectively, a first light and a second light, and both arranged on a substrate. An encapsulation layer is disposed over the first and second plurality of the light emitting elements, and a wavelength converting element is dispersed in the encapsulation layer. A concentration of the wavelength converting element in the encapsulation layer varies, is larger over the first plurality of light emitting elements and is smaller over the second plurality of light emitting elements.

Soer, Wouter Anthon↗

Nondestructive Characterization and Accelerated UV Testing of Browned Field-Aged PV Modules

Encapsulant browning is one of the most common degradation modes found in crystalline silicon field-aged photovoltaic modules. Browning, usually undetected unless severe, reduces the short-circuit current (Isc) produced by a module. Therefore, field-aged browned modules have been subjected to accelerated UV testing to obtain true end-of-life activation energy for the encapsulant browning mechanism. A novel time- and resource-saving accelerated UV exposure testing method simultaneously allowing multiple module temperatures to be maintained in a single chamber run is presented. Six field-aged crystalline silicon modules of glass/backsheet construction (three each from BP Solar/Solarex MSX 60 and Siemens M55) with similar glass and encapsulant formulation were exposed to a UV dosage of 450 kWh/m2 . Through passive heating, the average module temperatures for the BP Solar/Solarex modules were 60 degrees C, 77 degrees C, and 85 degrees C and those of Siemens M55 were 75 degrees C, 80 degrees C, and 837 degrees C. To study UV browning, the modules were intermittently characterized through visual imaging, UV fluorescence imaging, electroluminescence imaging, quantum efficiency measurements, module, and cell-level light I-V measurements. An Isc decrease corroborated the increased extent of browning with increased module temperature. For the BP Solar/Solarex modules, the Low T, Mid T, and the High T modules showed a 1.37%, 2.48%, and 3.26% Isc drop, respectively. The Siemens modules showed a 4.11%, 5.65%, and 6.95% Isc drop. The multiple cell-level Isc data points obtained for each module temperature increased provided statistical significance. Activation energy for encapsulant browning was calculated as 0.44 and 0.72 eV for MSX 60 and M55 modules, respectively.

14 SOLAR ENERGY↗

High voltage photo-switch package module having encapsulation with profiled metallized concavities

A photo-conductive switch package module having a photo-conductive substrate or wafer with opposing electrode-interface surfaces metalized with first metallic layers formed thereon, and encapsulated with a dielectric encapsulation material such as for example epoxy. The first metallic layers are exposed through the encapsulation via encapsulation concavities which have a known contour profile, such as a Rogowski edge profile. Second metallic layers are then formed to line the concavities and come in contact with the first metal layer, to form profiled and metalized encapsulation concavities which mitigate enhancement points at the edges of electrodes matingly seated in the concavities. One or more optical waveguides may also be bonded to the substrate for coupling light into the photo-conductive wafer, with the encapsulation also encapsulating the waveguides.

36 MATERIALS SCIENCE↗

Water reflection analysis of encapsulated photovoltaic modules

A method for moisture testing of a fully assembled photovoltaic (PV) module. An assembled PV module is probed with short wave IR probe energy in the range of 1700-2000 nm. Energy reflected from the assembled PV module is collected and directed to a sensor. Noise is removed from a signal of the sensor with reference to the probe energy. Absorption is of the probe energy is determined. The absorption is correlated to moisture in the PV module. A preferred system that carries out the method provides a signal-to-noise ratio (as defined by standard deviation/mean of measured reflectance) of at least 3800.

Fenning, David↗