Search NASA⌕ Search

SEARCH · Search NASA

Results for “Mixed polymer fractional composition”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

In-situ Lunar Launch and Landing Pad Construction with Regolith-Thermoset Polymer Composite Materials

Lunar launch and landing pads are necessary to mitigate risks to lander/ascent vehicles and surrounding surface assets from rocket plume ejected regolith. The current state of the art of landing and launching from the lunar surface is to land/launch on unprepared regolith surfaces. Though this has been a relatively successful approach, significant risks exist for the Artemis Program due to higher thrust levels leading to increased ejecta and cratering, presence of co-located assets in the ejecta path, and potential strict surface levelness requirements. Regolith-thermoset polymer composite materials were developed and evaluated for off Earth launch and landing pad applications. Performance under hot fire conditions was assessed for two simulated Starship lunar launch/landing environments, one targeting thermal conditions and the second targeting pressure conditions. Paver test articles were prepared at 20% and 11% polymer mass fractions. Sintered paver test articles were prepared with 20% polymer grouting filling the seams between pavers. Though significant erosion was experienced during the more extreme thermal testing conditions, all test articles successfully mitigated regolith ejecta from plume effects. A concept for preparing and emplacing the materials was developed and tested in laboratory conditions. The testing evaluated the feasibility of using twin and single screw extruder technology to mix, convey and deposit materials. Both the twin and single screw extruders were capable of processing and extruding the composite with a maximum of 90% mass fraction of regolith achieved by the twin screw extruder.A primary risk for application of regolith-thermoset polymer composites as lunar launch/landingpad is the mass of polymer required to be landed on the moon. Calculations were performed that show that a 100 m diameter, 0.025 m thick pad with polymer mass fraction of 15% will require a payload mass of 72 mt to the Lunar surface. This is below the planned Starship payload capacity to the lunar surface of 100 mt. The regolith-thermoset polymer composite based construction approach proved feasibility in three critical areas: performance under launch/landing conditions, demonstration of a mixing and depositing strategy, and fitting within the planned lunar payload capacity. It is recommended that materials and systems be developed to TRL 6 for a small-scale lunar demonstration of emplacement of a launch/landing pad via a CLPS mission to support Artemis Program roadmap gap closure activities.

ISRU↗

Phase relationship in three-phase composites which include a void phase

The paper shows the relationship among polymer, particles, and voids in a three-phase composite and how some of the properties of a composite may be changed by changing the proportions of the phases. The three-phase composite is an aggregate of microspheres bonded together with a small amount of polymer which may not form a continuous matrix. The void space (third phase) is obtained by limiting the amount of polymer which is mixed with the microspheres. A ternary phase diagram is used to show the proportional relationship among the three phases, with each apex representing a volume fraction of unity for a constituent while the side opposite the apex represents a volume fraction of zero for that constituent. The vertical dimension represents some composite property such as density or strength. The effect of composition on composite properties is shown by plotting them on a binary phase diagram which represents a perpendicular plane coincident with the 0.60 volume fraction microsphere line.

Price, H. L.↗

Propellant development for the Advanced Solid Rocket Motor

The properties of a propellant developed for the NASA Advanced Solid Rocket Motor (ASRM) are described in terms of its composition, performance, and compliance to NASA specifications. The class 1.3 HTPB/AP/A1 propellant employs an ester plasticizer and the content of ballistic solids is set at 88 percent. Ammonia evolution is prevented by the utilization of a neutral bonding agent which allows continuous mixing. The propellant also comprises a bimodal AP blend with one ground fraction, ground AP of at least 20 microns, and ferric oxide to control the burning rate. The propellant's characteristics are discussed in terms of tradeoffs in AP particle size and the types of Al powder, bonding agent, and HTPB polymer. The size and shape of the ballistic solids affect the processability, ballistic properties, and structural properties of the propellant. The revised baseline composition is based on maximizing the robustness of in-process viscosity, structural integrity, and burning-rate tailoring range.

Landers, L. C.↗

Polymer precursors for ceramic matrix composites

The synthesis and characterization of a polycyclohexasilane is reported. Because of its cyclic structure, it is anticipated that this polymer might serve as a precursor to SIC having a high char yield with little rearrangement to form small, volatile cyclic silanes, and, as such, would be of interest as a precursor to SiC composite matrices and fibers, or as a binder in ceramic processing. Several approaches to the synthesis of a bifunctional cyclic monomer were attempted; the most successful of these was metal coupling of PhMeSiCl2 and Me2SiCl2. The procedure gives six-membered ring compounds with all degrees of phenyl substitution, from none to hexaphenyl. The compounds with from 0-2 groups were isolated and characterized. The fraction with degree of phenyl substitution equal to 2, a mixture of cis and trans 1,2-; 1,3-; and 1,4 isomers, was isolated in 32 percent yield. Pure 1,4 diphenyldecamethylcyclohexasilane was isolated from the mixed diphenyl compounds and characterized. Diphenyldecamethylcyclohexasilanes were dephenylated to dichlorodecamethylcyclohexasilanes by treating with H2SO4.NH4Cl in benzene. The latter were purified and polymerized by reacting with sodium in toluene. The polymers were characterized by HPGPC, elemental analysis, proton NMR, and IR. Thermogravimetric analyses were carried out on the polymers. As the yield of residual SiC was low, polymers were heat treated to increase the residual char yield. As high as 51.52 percent residual char yield was obtained in one case.

Litt, M. H.↗

Effect of Architecture on the Resistivity of Carbon Fiber Polymer Composites

The electrical resistivity of carbon fiber laminar composites can be tailored by weave direction, fiber composition, resin composition, applied pressure, and fiber fraction. Although the weave direction was only found to be important in the case of high aspect ratio composites, the other factors were found to influence the resistivity generally. Most intriguing, the resistivity of composites with lamina of different fiber compositions follows a parallel resistor model. This opens the door for higher performance, lower cost composites to be fabricated from these mixed fiber composites.

Gaier, James R.↗