Search NASA⌕ Search

SEARCH · Search NASA

Results for “Mn4N”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

Materials Data on Mn4N by Materials Project

Mn4N crystallizes in the cubic Pm-3m space group. The structure is three-dimensional. there are two inequivalent Mn sites. In the first Mn site, Mn is bonded to twelve equivalent Mn atoms to form MnMn12 cuboctahedra that share corners with twelve equivalent MnMn12 cuboctahedra, faces with six equivalent MnMn12 cuboctahedra, and faces with eight equivalent NMn6 octahedra. All Mn–Mn bond lengths are 2.66 Å. In the second Mn site, Mn is bonded in a linear geometry to four equivalent Mn and two equivalent N atoms. Both Mn–N bond lengths are 1.88 Å. N is bonded to six equivalent Mn atoms to form NMn6 octahedra that share corners with six equivalent NMn6 octahedra and faces with eight equivalent MnMn12 cuboctahedra. The corner-sharing octahedral tilt angles are 0°.

36 MATERIALS SCIENCE↗

Materials Data on Mn4N by Materials Project

Mn4N crystallizes in the tetragonal P4/mmm space group. The structure is three-dimensional and consists of one ammonia molecule and one Mn framework. In the Mn framework, there are four inequivalent Mn sites. In the first Mn site, Mn is bonded to six Mn atoms to form corner-sharing MnMn6 octahedra. The corner-sharing octahedral tilt angles are 0°. There are four shorter (2.16 Å) and two longer (2.17 Å) Mn–Mn bond lengths. In the second Mn site, Mn is bonded in a linear geometry to two equivalent Mn atoms. In the third Mn site, Mn is bonded in a linear geometry to two equivalent Mn atoms. In the fourth Mn site, Mn is bonded in a linear geometry to two equivalent Mn atoms.

36 MATERIALS SCIENCE↗

The relation of magnetic properties and anomalous Hall behaviors in Mn4N (200) epitaxial films

Highlights: • Ferrimagnetic Mn4N(200) were grown on MgO(100) by plasma assisted molecular beam epitaxy. • We elucidate the relation of nitrogen vacancies and the magnetism by adjusting the growth pressure. • We state the relation of longitudinal resistivity and temperature as ρ{sub xx}∝T{sup 1.9994} (T ≤ 86K) and ρ{sub xx}∝T{sup 0.3068} (T > 86K) by data fitting. • We introduce a method to estimate the Debye temperature of Mn{sub 4}N materials and the residual resistance of 0 K. • We verify the linear relation between anomalou Hall resistivity (ρ{sub AH}) and magnetization at low magnetic field. - Abstract: The Mn{sub 4}N(200) films were grown on MgO(100) substrates by molecular beam epitaxy. The saturated magnetizations are 0.735 μB/f.u. and 0.892 μB/f.u. under pressure of 7.5 × 10{sup −6} mbar–9.5 × 10{sup −6} mbar. Increasing of growth pressure enhances the magnetism of Mn{sub 4}N due to the reduction of nitrogen vacancies. Debye temperature (T{sub D}) of Mn{sub 4}N is estimated to be 86 K. The longitudinal resistivity is linear to T{sup 1.9994} when T D , which coincides with electron-electron scattering of ferromagnetic coupling. The longitudinal resistivity originates from electron-electron scattering below T{sub D} since electron-phonon scattering is frozen. The longitudinal resistivity at 0 K is about 10% lower than 5 K as 7.085 μΩ cm. Mn{sub 4}N films show obvious anomalous Hall Effect in perpendicular magnetic fields. The anomalous Hall resistivity (ρ{sub AH}) of Mn{sub 4}N film is obtained by subtracting the ordinary Hall resistivity from transverse resistivity. The ρ{sub AH} is verified to be linear to magnetization at low magnetic field strength region (0–9 KOe).

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Structural and magnetic properties of ferrimagnetic ε-phase Mn 4 N and antiferromagnetic ζ-phase Mn10N thin films on MgO(001)

Single phase ε-Mn 4 N and ζ-Mn 10 N thin films are grown on MgO(001) using molecular beam epitaxy. The films are identified and characterized using reflection high-energy electron diffraction, x-ray diffraction, back scattered electron scanning electron microscopy, atomic/magnetic force microscopy and Rutherford backscattering spectrometry. These films are found to be highly smooth with root-mean-squared roughnesses 3.39 nm and below. The quality of ε-Mn 4 N grown is strongly dependent on substrate temperature during growth. Epitaxial growth of substantial grains composed of the antiferromagnetic η-phase Mn 3 N 2 side by side with ferrimagnetic ε-phase grains is observed when growth temperature is below 480 °C. Ising domains isolated within areas roughly 0.5 μm across are observed in the ferrimagnetic ε-phase grains of samples consisting of a mix of η- and ε-phase grains. Magnetic domains following semi-continuous paths, which are 0.7–7.2 μm across, are observed in single phase ε-Mn4N. Measurements of the ζ-phase detail the structure and magnetism of the material as high Mn content γ-type ζ-phase with a regular surface corrugation along the [100]-direction and antiferromagnetic.

36 MATERIALS SCIENCE↗

Contribution from Ising domains overlapping out-of-plane to perpendicular magnetic anisotropy in Mn 4 N thin films on MgO(001)

Single phase ε-Mn4N thin and ultrathin films are grown on MgO(001) using molecular beam epitaxy. Reflection high-energy electron diffraction and outof-plane x-ray diffraction measurements are taken for each sample in order to determine the in- and out-of-plane strain for each sample. Vibrating sample magnetometry and superconducting quantum interference device measurements, which are performed on the thin and ultrathin films respectively, are used to plot the magnetization of each sample versus both in- and out-of-plane $\vec H$-fields and to determine the magnitude of perpendicular magnetic anisotropy in these films. Three significant components of perpendicular magnetic anisotropy are observed in these films and are attributed to sample strain (1 component) and shape (2 components). Among these components, the most significant component (0.8 to 4.9 $\frac{Merg}{cm^3}$) is identified as a second term of shape anisotropy, which possesses a negative linear relationship with sample thickness over the range from 9 nm to 310 nm. Atomic (magnetic) force microscopy measurements show the presence of a surface localized magnetic polarization (22% to 82%), which increases with decreasing thickness, when the net magnetization of the films is zero. The second term of shape anisotropy as well as the surface localized polarization, which each depend on sample thickness, are each regarded as a consequence of Ising domains overlapping out-of-plane in these films.

Materials Science↗

“Mn 3 AlN” is Really Mn 4 N

We investigate the synthesis of antiperovskite “Mn 3 AlN” using the published synthesis procedure, as well as several new reaction pathways. In each case, only a combination of antiperovskite Mn 4 N and Mn 5 Al 8 or precursors is obtained. The identity of the obtained antiperovskite phase is unambiguously determined to be Mn4N via synchrotron powder X-ray diffraction (SPXRD), X-ray absorption spectroscopy (XAS), and magnetometry. The experimental results are further supported by thermochemical calculations informed by density functional theory (DFT), which find Mn 3 AlN to be metastable versus decomposition into Mn and AlN. The DFT-based calculations also predict an antiferromagnetic ground state for Mn3AlN. This directly contradicts the previously reported ferromagnetic behavior of "Mn 3 AlN". Instead, the observed magnetic behavior is consistent with ferrimagnetic Mn 4 N. We examine the data in the original publication and conclude that the compound reported to be Mn 3 AlN is in fact Mn 4 N.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗