Search NASA⌕ Search

SEARCH · Search NASA

Results for “NICKEL 52”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Gamow-Teller Transitions in Proton Rich Exotic pf-shell Nuclei Deduced from Mirror Transitions

The rp-process nucleosynthesis proceeds through nuclei near the proton drip-line, in which Gamow-Teller (GT) transitions starting from unstable pf-shell nuclei play important roles. In the {beta}-decay study of these nuclei, half-lives can be measured rather accurately. On the other hand, in the high-resolution ({sup 3}He, t) charge-exchange reactions on mirror nuclei, individual GT transitions can be studied up to high excitations. For the accurate study of the GT transition strengths in the A = 52, T = 2, system, we compare and combine the {beta}-decay study of the proton-rich nucleus {sup 52}Ni and the {sup 52}Cr({sup 3}He, t) measurement assuming the isospin symmetry of the T{sub z} = {+-}2{yields}{+-}1 transitions.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Nuclear Data Sheets for A = 52

The nuclear structure data belonging to all nuclei with mass number A=52 have been compiled and evaluated using experimental nuclear reaction data and decay data available before July 10, 2015. This evaluaton supersedes the previous publication for this msss chain (2007Hu08, Nuclear Data Sheets 108, 773 (2007)). The data for the ε decay of {sup 52}Co (104 ms) and the ε decay of {sup 52}Ni (40.8 ms) are both incomplete, so new studies would be useful.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

LATERALLY PROPAGATING DETONATIONS IN THIN HELIUM LAYERS ON ACCRETING WHITE DWARFS

Theoretical work has shown that intermediate mass (0.01 M{sub Sun} < M{sub He} < 0.1 M{sub Sun }) helium shells will unstably ignite on the accreting white dwarf (WD) in an AM CVn binary. For more massive (M > 0.8 M{sub Sun }) WDs, these helium shells can be dense enough (>5 Multiplication-Sign 10{sup 5} g cm{sup -3}) that the convectively burning region runs away on a timescale comparable to the sound travel time across the shell, raising the possibility for an explosive outcome rather than an Eddington limited helium novae. The nature of the explosion (i.e., deflagration or detonation) remains ambiguous, is certainly density dependent, and likely breaks spherical symmetry. In the case of detonation, this causes a laterally propagating front whose properties in these geometrically thin and low-density shells we begin to study here. Our calculations show that the radial expansion time of <0.1 s leads to incomplete helium burning, in agreement with recent work by Sim and collaborators, but that the nuclear energy released is still adequate to realize a self-sustaining laterally propagating detonation. These detonations are slower than the Chapman-Jouguet speed of 1.5 Multiplication-Sign 10{sup 9} cm s{sup -1}, but still fast enough at 0.9 Multiplication-Sign 10{sup 9} cm s{sup -1} to go around the star prior to the transit through the star of the inwardly propagating weak shock. Our simulations resolve the subsonic region behind the reaction front in the detonation wave. The two-dimensional nucleosynthesis is shown to be consistent with a truncated one-dimensional Zeldovich-von Neumann-Doering calculation at the slower detonation speed. The ashes from the lateral detonation are typically He rich, and consist of predominantly {sup 44}Ti, {sup 48}Cr, along with a small amount of {sup 52}Fe, with very little {sup 56}Ni and with significant {sup 40}Ca in carbon-enriched layers. If this helium detonation results in a Type Ia supernova, its spectral signatures would appear for the first few days after explosion.

79 ASTRONOMY AND ASTROPHYSICS↗

THE EFFECTS OF CURVATURE AND EXPANSION ON HELIUM DETONATIONS ON WHITE DWARF SURFACES

Accreted helium layers on white dwarfs have been highlighted for many decades as a possible site for a detonation triggered by a thermonuclear runaway. In this paper, we find the minimum helium layer thickness that will sustain a steady laterally propagating detonation and show that it depends on the density and composition of the helium layer, specifically {sup 12}C and {sup 16}O. Detonations in these thin helium layers have speeds slower than the Chapman-Jouget (CJ) speed from complete helium burning, v{sub CJ} = 1.5 × 10{sup 9} cm s{sup –1}. Though gravitationally unbound, the ashes still have unburned helium (≈80% in the thinnest cases) and only reach up to heavy elements such as {sup 40}Ca, {sup 44}Ti, {sup 48}Cr, and {sup 52}Fe. It is rare for these thin shells to generate large amounts of {sup 56}Ni. We also find a new set of solutions that can propagate in even thinner helium layers when {sup 16}O is present at a minimum mass fraction of ≈0.07. Driven by energy release from α captures on {sup 16}O and subsequent elements, these slow detonations only create ashes up to {sup 28}Si in the outer detonated He shell. We close by discussing how the unbound helium burning ashes may create faint and fast 'Ia' supernovae as well as events with virtually no radioactivity, and speculate on how the slower helium detonation velocities impact the off-center ignition of a carbon detonation that could cause a Type Ia supernova in the double detonation scenario.

79 ASTRONOMY AND ASTROPHYSICS↗

Special features of single-particle proton spectra of nickel, zinc, and germanium isotopes in the vicinity of the proton drip line

The single-particle proton spectra of the neutron-deficient isotopes {sup 50,52}Ni, {sup 56,58,60,62}Zn, and {sup 60,62,64}Ge were calculated on the basis of the dispersive optical model whose parameters were extrapolated from the region of stable isotopes. The resulting parameter values lead to agreement between the total number of protons in bound states and the charge number Z of the respective nucleus. The results of the calculations are indicative of a weakly magic character of the {sup 58}Zn nucleus, which has a traditional magic number of N = 28 and a nearly magic number of Z = 30, and the {sup 64}Ge nucleus, for which N = Z = 32.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Grain boundary velocity and curvature are not correlated in Ni polycrystals

Grain boundary velocity has been believed to be correlated to curvature, and this is an important relationship for modeling how polycrystalline materials coarsen during annealing. We determined the velocities and curvatures of approximately 52,000 grain boundaries in a nickel polycrystal using three-dimensional orientation maps measured by high-energy diffraction microscopy before and after annealing at 800°C. Unexpectedly, the grain boundary velocities and curvatures were uncorrelated. Instead, we found strong correlations between the boundary velocity and the five macroscopic parameters that specify grain boundary crystallography. The sensitivity of the velocity to grain boundary crystallography might be the result of defect-mediated grain boundary migration or the anisotropy of the grain boundary energy. The absence of a correlation between velocity and curvature likely results from the constraints imposed by the grain boundary network and implies the need for a new model for grain boundary migration.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Study of Volumetrically Heated Ultra-High Energy Density Plasmas

Heating dense matter to millions of degrees is important for applications, but requires complex and expensive methods. The major goal of the project was to demonstrate using a compact laser the creation of a new ultra-high energy density plasma regime characterized by simultaneous extremely high temperature and high density, and to study it combining experimental measurements and advanced simulations. We have demonstrated that trapping of intense femtosecond laser pulses deep within ordered nanowire arrays can heat near solid density matter into a new ultra hot plasma regime. Extreme electron densities, and temperatures of several tens of million degrees were achieved using laser pulses of only 0.5 J energy from a compact laser. Our x-ray spectra and simulations showed that extremely highly ionized plasma volumes several micrometers in depth are generated by irradiation of gold and Nickel nanowire arrays with femtosecond laser pulses of relativistic intensities. We obtained extraordinarily high degrees of ionization (e.g. we peeled 52 electrons from gold atoms, and up to 26 electrons from nickel atoms). In the process we generated Gigabar pressures only exceeded in the central hot spot of highly compressed thermonuclear fusion plasmas.. The plasma created after the dissolved wires expand, collide, and thermalize, is computed to have a thermal energy density of 0.3 GJ cm -3 and a pressure of 1-2 Gigabar. These are pressures only exceeded in highly compressed thermonuclear fusion plasmas. Scaling these results to higher laser intensities promises to create plasmas with temperatures and pressures exceeding those in the center of the sun.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of thermal aging and irradiation on microstructure and crack growth response of Alloy 690

Nickel-base Alloy 690 and the associated weld Alloys 52 and 152 are typically used for nozzle penetrations in replacement heads for pressurized water reactor (PWR) vessels, because of their excellent overall resistance to general corrosion and environmental degradation, primarily stress corrosion cracking (SCC). However, many of the existing PWRs reactors are expected to operate for 40-80 years. Likewise, advanced water-cooled small modular reactors (SMRs) will use Ni-Cr alloys and are expected to receive initial operating licenses for 60 years. Hence, the thermal stability of Ni-Cr alloys is a potential concern for the long-term performance of both existing and advanced nuclear plants, and possibly spent fuel storage containers. The objective of this research is to understand the microstructural changes occurring in high-Cr, Ni-based Alloy 690 during long time exposure to the reactor operating temperatures, and the effect of these changes on the service performance. One area of particular concern is the potential for long range ordering (LRO), i.e. formation of the intermetallic Ni 2 Cr phase under prolonged exposure to reactor temperatures and/or irradiation, which can increase strength, decrease ductility, and cause dimensional changes or lead to in-service embrittlement of components made with these alloys. Hence, this research focused on the microstructural evolution and the SCC response of Alloy 690 under accelerated thermal aging and irradiation conditions. The materials studied involved Alloy 690 from two sources: (i) Alloy 690 plate from an Alloy 152 dissimilar metal weld (DMW) joining the Alloy 690 plate to Alloy 533 LAS, aged at three different temperatures (370°C, 400°C and 450°C) for up to 75,000h (equivalent to 60 years of service), and (ii) specimens neutron-irradiated in the BOR-60 reactor up to 40 dpa. For aged Alloy 690 specimens, hardness was found to increase with aging time, however, the microstructural characterization by means of synchrotron X-ray did not find evidence of LRO. The microstructural characterization of neutron-irradiated specimens by TEM found no evidence of LRO either. Testing in a primary water environment of Alloy 690 specimens aged to a 60-year service equivalent revealed a fatigue and corrosion fatigue crack growth responses similar to those measured on the un-aged alloy. The SCC CGR response was also low. Overall, the two Alloy 690 heats investigated in this work, aged up to 60-year service equivalents or exposed to neutron irradiation up to 40 dpa, did not exhibit a deterioration in microstructure or performance.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Effect of thermal aging on microstructure and crack growth response of Alloy 152 weld

Nickel-based Alloy 690 and the associated weld Alloys 52 and 152 are typically used for nozzle penetrations in replacement heads for pressurized water reactor (PWR) vessels, because of their excellent overall resistance to general corrosion and environmental degradation, primarily stress corrosion cracking (SCC). However, many of the existing PWRs are expected to operate for 40-80 years. Likewise, advanced water-cooled small modular reactors (SMRs) will use Ni-Cr alloys and are expected to receive initial operating licenses for 60 years. Hence, the thermal stability of Ni-Cr alloys is a potential concern for the long-term performance of both existing and advanced nuclear power plants, and possibly spent fuel storage containers. The objective of this research is to understand the microstructural changes occurring in high-Cr, Ni-based Alloy 152 weldments during long time exposure to the reactor operating temperatures, and the effect of these changes on the service performance. One area of particular concern is the potential for long range ordering (LRO), i.e. formation of the intermetallic Ni2Cr phase under prolonged exposure to reactor temperatures and/or irradiation, which can increase strength, decrease ductility, and cause dimensional changes or lead to in-service embrittlement of components made with these alloys. Hence, this research focused on the microstructural evolution and the SCC response of Alloy 152 under accelerated thermal aging. The materials studied involved three heats of Alloy 152 used to produce a dissimilar metal weld (DMW) joining an Alloy 690 plate to an Alloy 533 low alloy steel (LAS) plate, thermally aged at three different temperatures (370°C, 400°C and 450°C) for up to 75,000h (equivalent to 60 years of service). The microstructural characterization by means of synchrotron X-ray did not find evidence of LRO in any of the three heats aged to an equivalent of 60 years of service. Testing in a primary water environment of a heat of Alloy 152 aged at 370°C to a 60-year service equivalent revealed a fatigue and corrosion fatigue crack growth responses similar to those measured on the un-aged alloy. However, the SCC CGR response of the aged sample appears to show a deterioration in performance.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Effect of thermal aging on microstructure and stress corrosion cracking behavior of Alloy 152 weldment

Nickel-based Alloy 690 and the associated weld Alloys 52 and 152 are typically used for nozzle penetrations in replacement heads for pressurized water reactor (PWR) vessels, because of their excellent overall resistance to general corrosion and environmental degradation, primarily stress corrosion cracking (SCC). However, many of the existing PWRs are expected to operate for 40-80 years. Likewise, water-cooled small modular reactors (SMRs) will use Ni-Cr alloys and are expected to receive initial operating licenses for 60 years. Hence, the thermal stability of Ni-Cr alloys is a potential concern for the long-term performance of both existing and advanced nuclear power plants, and possibly spent fuel storage containers. The objective of this research is to understand the microstructural changes occurring in high-Cr, Ni-based Alloy 152 weldments during long time exposure to the reactor operating temperatures, and the effect of these changes on the service performance. One area of particular concern is the potential for long range ordering (LRO), i.e. formation of the intermetallic Ni2Cr phase under prolonged exposure to reactor temperatures and/or irradiation, which can increase strength, decrease ductility, and cause dimensional changes or lead to in-service embrittlement of components made with these alloys. Hence, this research focused on the microstructural evolution and the SCC response of Alloy 152 under accelerated thermal aging. The materials studied involved three heats of Alloy 152 used to produce a dissimilar metal weld (DMW) joining an Alloy 690 plate to an Alloy 533 low alloy steel (LAS) plate, thermally aged at three different temperatures (370°C, 400°C and 450°C) for up to 75,000h (equivalent to 60 years of service). The microstructural characterization by means of synchrotron X-ray conducted in small, 0.2 mm - step line scans in the high-deformation regions of the weld root – covering areas spanning from the weld heat affected zone (HAZ) in Alloy 690 to the weld and weld butter on LAS - did not show evidence of LRO in any of the three Alloy 152 heats aged to an equivalent of 60 years of service. Testing in a primary water environment of two heats of Alloy 152 aged at 370°C to a 60-year service equivalent revealed a fatigue and corrosion fatigue crack growth responses similar to those measured on the un-aged alloys. However, the SCC CGR response of the aged samples appears to show a deterioration in performance, confirming our previous observation.

36 MATERIALS SCIENCE↗

Effect of Thermal Aging on Microstructure and Stress Corrosion Cracking Behavior of an Alloy 152 1st Layer Butter Weldment

Nickel-based Alloy 690 and the associated weld Alloys 52 and 152 are typically used for nozzle penetrations in replacement heads for pressurized water reactor (PWR) vessels, because of their excellent overall resistance to general corrosion and environmental degradation, primarily stress corrosion cracking (SCC). However, many of the existing PWRs are expected to operate for 40- 80 years. Likewise, water-cooled small modular reactors (SMRs) will use Ni-Cr alloys and are expected to receive initial operating licenses for 60 years. Hence, the thermal stability of Ni-Cr alloys is critical for the long-term performance of both existing and advanced nuclear power plants, and possibly spent fuel storage containers. The objective of this research is to understand the microstructural changes occurring in high-Cr, Ni-based Alloy 152 weldments during long time exposure to the reactor operating temperatures, and the effect of these changes on the service performance. One area of particular concern is the potential for long range ordering (LRO), i.e. formation of the intermetallic Ni2Cr phase under prolonged exposure to reactor temperatures and/or irradiation, which can increase strength, decrease ductility, and cause dimensional changes or lead to in-service embrittlement of components made with these alloys. Hence, this research focused on the microstructural evolution and the SCC response of Alloy 152 under accelerated thermal aging. The materials studied involved three heats of Alloy 152 used to produce a dissimilar metal weld (DMW) joining an Alloy 690 plate to an Alloy 533 low alloy steel (LAS) plate, thermally aged at three different temperatures (370°C, 400°C and 450°C) for different durations up to 75,000h (equivalent to 60 years of reactor service). The microstructural characterization by means of synchrotron X-ray conducted in small, 0.2 mm - step line scans in the high-deformation regions of the weld root – covering areas spanning from the weld heat affected zone (HAZ) in Alloy 690 to the weld and weld butter on LAS - did not show evidence of LRO in any of the three Alloy 152 heats aged at 370°C and 450°C to an equivalent of 60 years of service. However, the first weld butter layer has high levels of deformation and is highly susceptible to SCC even in its non-aged condition. Nanohardness testing confirmed the extreme hardening with aging (ΔHV ≅ 100) at two locations within this weldment. In absence of LRO, hardening is suspected to be due to thermally-induced Cr carbide precipitation and coarsening. Testing in a primary water environment of the 1st layer of Alloy 152 weld butter aged at 370°C to a 60-year service equivalent revealed a fatigue and corrosion fatigue crack growth responses similar to those measured on the un-aged alloys. Similarly, the SCC CGR response of the aged weld butter does not appear to show a deterioration in performance, however, the difficult-to-test weldment geometry may affect the test results.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

The Effect of Thermal Aging on the Performance of High-Cr Ni-based Alloys in Primary Water Environment

Nickel-based Alloy 690, and the associated weld Alloys 52 and 152, are used for nozzle penetrations in replacement heads for pressurized water reactor (PWR) vessels. They are chosen for their excellent overall resistance to general corrosion and environmental degradation, primarily stress corrosion cracking (SCC). However, many of the existing PWRs are expected to operate beyond their first or second license renewal (e.g., 40 to 60 years or beyond 60 years). Hence, the thermal stability of Ni-Cr alloys is a potential concern for the long-term performance of both existing and advanced nuclear power plants. Moreover, Ni-Cr alloys are being considered for high-level radioactive waste disposal containers that will be required to contain the waste for at least 10,000 years.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

XRF 100316D/SN 2010bh AND THE NATURE OF GAMMA-RAY BURST SUPERNOVAE

We present ground-based and Hubble Space Telescope optical and infrared observations of Swift XRF 100316D/SN 2010bh. It is seen that the optical light curves of SN 2010bh evolve at a faster rate than the archetype gamma-ray burst supernova (GRB-SN) 1998bw, but at a similar rate to SN 2006aj, an SN that was spectroscopically linked with XRF 060218, and at a similar rate to the non-GRB associated Type Ic SN 1994I. We estimate the rest-frame extinction of this event from our optical data to be E(B - V) = 0.18 {+-} 0.08 mag. We find the V-band absolute magnitude of SN 2010bh to be M{sub V} = -18.62 {+-} 0.08, which is the faintest peak V-band magnitude observed to date for spectroscopically confirmed GRB-SNe. When we investigate the origin of the flux at t - t{sub 0} = 0.598 days, it is shown that the light is not synchrotron in origin, but is likely coming from the SN shock breakout. We then use our optical and infrared data to create a quasi-bolometric light curve of SN 2010bh, which we model with a simple analytical formula. The results of our modeling imply that SN 2010bh synthesized a nickel mass of M{sub Ni} {approx} 0.1 M{sub sun}, ejected M{sub ej} {approx} 2.2 M{sub sun}, and has an explosion energy of E{sub k} {approx} 1.4 x 10{sup 52} erg. Thus, while SN 2010bh is an energetic explosion, the amount of nickel created during the explosion is much less than that of SN 1998bw and only marginally more than SN 1994I. Finally, for a sample of 22 GRB-SNe we check for a correlation between the stretch factors and luminosity factors in the R band and conclude that no statistically significant correlation exists.

79 ASTRONOMY AND ASTROPHYSICS↗

Dehydrogenation of 1-Phenylethanol Catalyzed by Nickel(II)diphosphine Complexes

Catalytic efficacy of the nickel(II)-diphosphine systems in the dehydrogenation of 1-phenylethanol to acetophenone under acceptorless conditions was investigated. Steric and electronic factors of the phosphine ligands were found to play an important role in the catalysis, while the nature of the base used and the reaction conditions, viz. time, temperature, and stoichiometry, have also shown major influence. Based on the preliminary analysis, a homogeneous pathway, perhaps involving nickel hydride species, was proposed. Due to the gradual disintegration of the catalytic species, deterioration of catalytic activity was observed resulting into low to moderate conversions. Among the series of catalysts examined, the highest conversion of 52% was exhibited by the catalyst C4, dichloro(1,2-bis(diphenylphosphino)ethane)nickel(II) (5 mol%), when loaded with 50 mol% of sodium ethoxide in toluene at 120 °C.

1,2 bis(alkyl/arylphosphino) alkane. homogeneous c↗

THE PROPAGATION OF NEUTRINO-DRIVEN JETS IN WOLF-RAYET STARS

We numerically investigate the jet propagation through a rotating collapsing Wolf-Rayet star with detailed central engine physics constructed based on the neutrino-driven collapsar model. The collapsing star determines the evolution of the mass accretion rate, black hole mass, and spin, all of which are important ingredients for determining the jet luminosity. We reveal that neutrino-driven jets in rapidly spinning Wolf-Rayet stars are capable of breaking out from the stellar envelope, while those propagating in slower rotating progenitors fail to break out due to insufficient kinetic power. For progenitor models with successful jet breakouts, the kinetic energy accumulated in the cocoon could be as large as {approx}10{sup 51} erg and might significantly contribute to the luminosity of the afterglow emission or to the kinetic energy of the accompanying supernova if nickel production takes place. We further analyze the post-breakout phase using a simple analytical prescription and conclude that the relativistic jet component could produce events with an isotropic luminosity L {sub p(iso)} {approx} 10{sup 52} erg s{sup -1} and isotropic energy E {sub j(iso)} {approx} 10{sup 54} erg. Our findings support the idea of rapidly rotating Wolf-Rayet stars as plausible progenitors of GRBs, while slowly rotational ones could be responsible for low-luminosity or failed GRBs.

79 ASTRONOMY AND ASTROPHYSICS↗

Neutron cross section covariances in the resonance region: 52Cr, 56Fe, 58Ni

We evaluated covariances for neutron capture and elastic scattering cross sections on major structural materials, {sup 52}Cr, {sup 56}Fe and {sup 58}Ni, in the resonance region which extends beyond 800 keV for each of them. Use was made of the recently developed covariance formalism based on kernel approximation along with data in the Atlas of Neutron Resonances. The data of most interest for AFCI applications, elastic scattering cross section uncertainties at energies above about few hundred keV, are on the level of about 12% for {sup 52}Cr, 7-8% for {sup 56}Fe and 5-6% for {sup 58}Ni.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Characterization of stress corrosion cracks in Ni-based weld alloys 52, 52M and 152 grown in high-temperature water

Ni-based weld alloys 52, 52M and 152 are extensively used in repair and mitigation of primary water stress corrosion cracking (SCC) in nuclear power plants. In the present study, a series of microstructure and microchemistry at the SCC tips of these alloys were examined with scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), transmission electron microscopy (TEM), energy-dispersive X-ray spectroscopy (EDS), scanning transmission electron microscopy (STEM) and energy filtered transmission electron microscopy (EFTEM). The specimens have similar chemical compositions and testing conditions. Intergranular (IG) and transgranular (TG) SCC was observed in all of them. The cracks were filled with nickel-oxides and partial precipitations of chrome carbides (CrCs), niobium carbides (NbCs), titanium nitrides (TiNs) and silicon carbides (SiCs), while iron (Fe) was largely dissolved into the solution. However, the crack densities, lengths and distributions were different for all three specimens. - Highlights: • Microstructure and microchemistry at the SCC tips of Ni-based weld alloys 52, 52M and 152 were examined. • The crack densities, lengths and distributions were found to be different for different alloys. • IGSCC and TGSCC were observed on alloy 52, only TGSCC was observed on alloy 52M and 152. • The cracks were filled by Ni-oxides and precipitated CrCs, NbCs, TiNs and SiCs.

36 MATERIALS SCIENCE↗

A Cobalt– and Manganese–Free High–Nickel Layered Oxide Cathode for Long–Life, Safer Lithium–Ion Batteries

High-nickel LiNi 1–x–y Mn x Co y O 2 and LiNi 1–x–y Co x Al y O 2 cathodes are receiving growing attention due to the burgeoning demands on high-energy-density lithium-ion batteries. The presence of both cobalt and manganese in them, however, triggers multiple issues, including high cost, high toxicity, rapid surface deterioration, and severe transition-metal dissolution. Herein, a Co- and Mn-free ultrahigh-nickel LiNi 0.93 Al 0.05 Ti 0.01 Mg 0.01 O 2 (NATM) cathode that exhibits 82% capacity retention over 800 deep cycles in full cells, outperforming two representative high-Ni cathodes LiNi 0.94 Co 0.06 O 2 (NC, 52%) and LiNi 0.90 Mn 0.05 Co 0.05 O 2 (NMC, 60%) is presented. It is demonstrated that a titanium-enriched surface along with aluminum and magnesium as the stabilizing ions in NATM not only ameliorates unwanted side reactions with the electrolyte and structural disintegrity, but also mitigates transition-metal dissolution and active lithium loss on the graphite anode. As a result, the graphite anode paired with NATM displays an ultrathin (≈8 nm), monolayer anode-electrolyte interphase architecture after extensive cycling. Furthermore, NATM displays considerably enhanced thermal stability with an elevated exothermic temperature (213 °C for NATM vs 180 and 190 °C for NC and NMC, respectively) and remarkably reduced heat release. This work sheds light on rational compositional design to adopt ultrahigh-Ni cathodes in lithium-based batteries with low cost, long service life, and improved thermal stability.

25 ENERGY STORAGE↗