Temperature dependence of irradiation-induced nanocrystallization in amorphous silicon carbide

Ion irradiation induced nucleation and growth in amorphous SiC at elevated temperatures are investigated in this study. Both as-deposited amorphous and Kr ion irradiation-amorphized SiC films are used for the investigation. Similar behavior of particle precipitation in the two types of the films is observed. It is found that the threshold temperature for nucleation is between 550 and 700 K, which is considerably higher than the critical temperature for full amorphization in SiC irradiated with Kr ions. There is a temperature regime up to at least 900 K, where the growth rates are only weakly dependent of the irradiation temperature. This temperature regime is potentially useful to tailor the size and density of nanocrystalline SiC precipitates by optimizing the ion irradiation conditions.

Ion irradiation, Nucleation and Growth, Silicon Ca↗

Radio-Frequency Rapid Thermal Processing Enabling Spatial Phase Transformation and Nanocrystallization of Soft Magnetic Amorphous Alloys

Thermal processing of soft magnetic amorphous and nanocrystalline alloys is explored under the influence of radio-frequency induction-heating techniques. Direct induction-heating concepts based on longitudinal and transverse flux heating are examined and the details of electromagnetic fields interaction with metallic strips are discussed by analytical calculations as well as finite element analysis. Initial experimental results confirming spatial control of phase transformations and nanocrystallization within a single strip of Finemet Fe-based amorphous ribbons are reported. Here, the degree to which primary and secondary crystallization temperature are achieved depends on the spacing between the ribbon relative to the induction coil as well as the coil design and configuration. For transverse coil configurations, the local temperature and therefore microstructural evolution is different across the lateral dimension of processed ribbons, with reduced gap sizes producing enhanced peak temperatures and larger temperature distributions with greater spatial variation in microstructure. In addition, indirect susceptor-based induction heating under tension is performed and the impact of microstructure is demonstrated. Herein, potential for exploiting spatially optimized phase transformations is illustrated through electromagnetic field–assisted processing in a scalable manufacturing process with amorphous and nanocrystalline soft magnetic alloys.

36 MATERIALS SCIENCE↗

Unravel unusual hardening behavior of a Pd–Ni–P metallic glass in its supercooled liquid region

Monolithic metallic glasses often exhibit work softening induced by high atom mobility in the supercooled liquid region in tension. In this work, we report an unusual viscous flow of the Pd 42.5 Ni 42.5 P 15 metallic glass in its supercooled liquid region, which is characterized by a remarkable hardening behavior with decent plasticity during tension. To unravel the causes of this unusual hardening, we conducted structural and thermodynamic analyses by employing several experiments, including dynamic mechanical analysis, differential scanning calorimetry, high-resolution transmission electron microscopy, and in situ heating synchrotron high-energy x-ray diffraction. It was found that the unusual hardening behavior was attributed to structural ordering during deformation, rather than nanocrystallization or structural relaxation observed, sometimes, in metallic glasses deformed in supercooled liquid region. We also incorporated an additional work hardening region in the modified deformation map for metallic glasses.

36 MATERIALS SCIENCE↗

Induced Anisotropy in FeCo-Based Nanocrystalline Ferromagnetic Alloys (HITPERM) by Very High Field Annealing

Very high magnetic field annealing is shown to affect the magnetic anisotropy in FeCo-base nanocrystalline soft ferromagnetic alloys. Alloys of composition Fe(44.5)Co(44.5)Zr(7)B(4) were prepared by melt spinning into amorphous ribbons, then wound to form toroidal bobbin cores. One set of cores was crystallized in a zero field at 600 deg. C for 1 h, then, field annealed at 17 tesla (T) at 480 deg. C for 1 h. Another set was crystallized in a 17-T field at 480 deg. C for 1 h. Field orientation was transverse to the magnetic path of the toroidal cores. An induced anisotropy is indicated by a sheared hysteresis loop. Sensitive torque magnetometry measurements with a Si cantilever sensor indicated a strong, uniaxial, longitudinal easy axis in the zero-field-crystallized sample. The source is most likely magnetoelastic anisotropy, caused by the residual stress from nanocrystallization and the nonzero magnetostriction coefficient for this material. The magnetostrictive coefficient lambda(5) is measured to be 36 ppm by a strain gage technique. Field annealing reduces the magnitude of the induced anisotropy. Core loss measurements were made in the zero-field-crystallized, zero-field-crystallized- than-field-annealed, and field-crystallized states. Core loss is reduced 30%-50% (depending on frequency) by field annealing. X-ray diffraction reveals no evidence of crystalline texture or orientation that would cause the induced anisotropy. Diffusional pair ordering is thought to be the cause of the induced anisotropy. However, reannealing the samples in the absence of a magnetic field at 480 deg. C does not completely remove the induced anisotropy.

FERROMAGNETIC ALLOYS↗

Nanostructure refinement and phase formation of flash annealed FeNi-based soft magnetic alloys

In this work, the resulting nanocomposite microstructures of FeNi nanocrystallites under different heating and cooling rates (5 °C/min vs 400-500 °C/s) is investigated. Conventional furnace annealing under low heating rates and slow cooling resulted in both BCC α-FeNi and FCC γ-FeNi nanocrystallites with an average grain size on the order of 25-27 nm whereas high heating rates achieved via flash annealing techniques have enabled a dramatically refined microstructure consisting of 5-7 nm grains with FCC γ-FeNi phase and found to be the dominant phase following primary crystallization. Grain size refinement and phase identity optimization yielded low values of coercivities-17 A/m and high permeability similar to 11 x 10 3 measured at 400 Hz/1 kA/m in flash annealed samples at 450 °C for 5 s. The magnetic behavior and the underlying mechanism of optimal soft magnetic properties are discussed in terms of the critical role of the grain size in domain wall pinning and coercivity.

36 MATERIALS SCIENCE↗

Size- and Phase-Controlled Nanometer-Thick ß-Ga2O3 Films with Green Photoluminescence for Optoelectronic Applications

Realization and optimization of the tunable/enhanced optical properties is critical to further advance the field of optoelectronics, photonics, and nano-electronics. In this context, here, we demonstrate green-emission characteristics with a ~30 fold enhancement in selectively engineered nanocrystalline Ga2O3 with a control over size, phase and interface nanostructure. Pulsed-laser-deposited ß-phase Ga2O3 films with an average crystallite size of ~9 nm along with a highly dense, close-compact nano-columnar structure with lowest possible defect density facilitates the thirty-fold enhancement in the photoluminescence (PL) intensity in green-region. Enhanced PL-emission in the optimized, engineered nano-architecture sheds light in designing Ga2O3-materials for promising future optoelectronic/photocatalytic applications.

Ga2O3, Nanocrystalline Films, Pulsed-Laser Deposit↗

Amorphous and Nanocomposite Magnets for High Efficiency, High Speed Motor Designs

This project developed metal amorphous nanocomposite (MANC) soft magnetic materials (SMMs) for a rare earth (RE)-free 2.5 kW motor with 4% increased efficiency. The Project modeled RE-free motor topologies. The project outcomes addressed: (a) metal to alloy processing & magnet core production; (b) soft magnetic laminate & core post-processing; and (c) producing a 2.5 kW motor extending to TRL-5.

30 DIRECT ENERGY CONVERSION↗

Laser Patterning Assisted Devitrification and Domain Engineering of Amorphous and Nanocrystalline Alloys

We have investigated laser-patterning and devitrification as a novel method to realize emergent properties in modified regions at the ribbon surface consisting of periodic localized laser spots thermally treated under rapid heating and cooling conditions. Fe-based amorphous ribbons were annealed for systematically varied laser power. Extremely high heating and cooling rates on the order of 10(exp 8)-10(exp 10)K/s have been estimated by finite element analysis simulations. Observations suggest surface melting followed by rapid solidification fast enough to quench and form an amorphous structure upon cooling. Diffusion of heat occurs from the laser irradiated surface region so that a finite volume of material surrounding this region rises in temperature above the crystallization temperature relevant for conventional isothermal annealing experiments. The underlying mechanism of laser annealing and consequences of heat transients involved are discussed in terms of impacts upon micro/nanostructure, residual stresses, and magnetic domain structure surrounding the laser irradiated region. The study illustrates the potential to exploit spatially optimized phase transformations in a scalable manufacturing process of amorphous and nanocrystalline alloys to locally access otherwise inaccessible extreme heating and cooling rates.

Amorphous ribbons↗