At least 19 records

Co-sputter deposition of Nb₃Sn layer into SRF cavity using Nb-Sn composite target

Nb₃Sn, with its superior superconducting critical temperature (Tc ~18.3 K) and superheating field (Hsh ~400 mT), is considered a promising material for superconducting radiofrequency (SRF) cavities, offering enhanced cryogenic performance compared to bulk niobium cavities. A Nb₃Sn coating technique has been developed for Nb SRF cavities using co-sputtering of Nb-Sn composite target in a DC cylindrical magnetron sputtering system. The composite target configuration and discharge conditions for co-sputtering were optimized to deposit Nb-Sn films on flat Nb substrates, followed by annealing to form Nb₃Sn. Multiple strategies have been explored to improve the surface homogeneity of the Nb₃Sn coating, including optimizing a two-step annealing process, annealing in Sn vapor, and a light Sn recoating process. A 1.5 µm Nb-Sn co-sputtered film was deposited on the interior of a 2.6 GHz Nb SRF cavity and annealed at 600 °C for 6 h, followed by 950 °C for 1 h. Cryogenic RF testing of the annealed cavity demonstrated a Tc of 17.8 K, confirming the formation of Nb₃Sn. Then, the annealed cavity underwent a light recoating treatment and attained a quality factor (Q0) of 8.5E+08 at 2.0 K.

Accelerator Physics↗

Commissioning of a two-target DC cylindrical magnetron sputter coater for depositing Nb 3 Sn film on Nb superconducting radiofrequency cavities

A DC cylindrical magnetron sputter coater was commissioned and used to coat Nb 2.6 GHz superconducting radiofrequency (SRF) cavity with Nb 3 Sn. The sputter coater has two identical cylindrical magnetrons that can move, with a controlled speed, along the axis of the SRF cavity to coat the inside surface of the cavity. The design of the sputter coater is discussed, along with its performance. Initially, a sample holder that allows coating on flat substrates at positions similar to the equator and beam tubes of a 2.6 GHz SRF cavity was used to test conditions for fabricating Nb 3 Sn layers. Multilayers of Nb and Sn were sequentially sputtered on flat Nb and sapphire substrates mounted on the equivalent positions of the cavity's beam tubes and the equator using the two identical cylindrical magnetrons. Then, the Nb/Sn multilayers were annealed at 950 °C for 3 h. Here, the ~1.2 μm thick Nb 3 Sn film did not show any other Nb–Sn compounds and had a superconducting transition temperature of 17.61–17.76 K. The 2.6 GHz SRF cavity was coated using similar conditions as flat samples. Cryogenic RF testing of the Nb 3 Sn-coated cavity demonstrated a quality factor of 3.2 × 10 8 at an accelerating gradient of 5 MV/m at 4.4 K.

43 PARTICLE ACCELERATORS↗

Neutron yields from 435 MeV/nucleon Nb stopping in Nb and 272 MeV/nucleon Nb stopping in Nb and Al

Neutron fluences were measured from 435 MeV/nucleon Nb ions stopping in a Nb target and 272 MeV/nucleon Nb ions stopping in targets of Nb and Al for neutrons above 20 MeV and at laboratory angles between 3 degrees and 80 degrees. The resultant spectra were integrated over angles to produce neutron energy distributions and over energy to produce neutron angular distributions. The total neutron yields for each system were obtained by integrating over the angular distributions. The angular distributions from all three systems are peaked forward, and the energy distributions from all three systems show an appreciable yield of neutrons with velocities greater than the beam velocity. Comparison of the total neutron yields from the two Nb + Nb systems suggests that the average neutron multiplicity decreases with decreasing projectile energy. Comparison of the total yields from the two 272 MeV/nucleon systems suggests that the total yields show the same dependence on projectile and target mass number as do total inclusive neutron cross sections. The data are compared with Boltzmann-Uehling-Uhlenbeck model calculations.

NASA Discipline Radiation Health↗

Influence of Nb alloying on Nb recrystallization and the upper critical field of Nb 3 ⁢Sn

Nb 3 Sn conductors are important candidates for high-field magnets for particle accelerators, and they continue to be widely used for many laboratory and NMR magnets. However, the critical current density, J c , of present Nb 3 Sn conductors declines swiftly above 12-15 T. State-of-the-art Ta- and Ti-doped strands exhibit upper critical field, H c2 , values of ~ 24-26.5 T (4.2 K) and do not reach the FCC target J c , which serves as the present stretch target for Nb 3 Sn development. As recently demonstrated, to meet this goal requires enhanced vortex pinning but an independent and supplementary approach is to significantly enhance H c2 . In this study, we have arc-melted multiple Nb alloys with added Hf, Zr, Ta and Ti and drawn them successfully into monofilament wires to investigate the possibilities of H c2 enhancement through alloying. H c2 (T) was measured for all samples in fields up to 16 T and some up to 31 T. We have found that all alloys show good agreement with the standard Werthamer, Helfand, and Hohenberg (WHH) fitting procedure without the need to adjust the paramagnetic limitation parameter (α) and spin-orbit scattering parameter (λ so ). The evaluation of dH c2 /dT near T c , which is proportional to the electronic specific heat coefficient γ and the normal state resistivity ρn, allows a better understanding of the induced disorder introduced by alloying in the A15 phase. So far, we have observed that Hf alloying of pure Nb can enhance H c2 (0) by 3-4 T to ~28 T, while adding just 1 at. %Hf or Zr into a Nb4Ta base alloy can raise H c2 (0) to ~31 T. Very importantly we find that Hf and Zr raise the alloy recrystallization temperature above the usual A15 reaction temperature range of 650°C – 750°C, thus ensuring denser A15 phase nucleation in the Nb alloy grain boundaries, possibly leading to a more homogeneous A15 phase Sn content and refined A15 grain size. Furthermore, the potential for further advancements in Nb 3 Sn properties is explored in relation to the recrystallization of the Nb alloy and the factors controlling the upper critical field.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Selective thermal evolution of native oxide layer in Nb and Nb$_3$Sn-coated SRF grade Nb: An in-situ angular XPS study

This contribution discusses the results of an in-situ angular XPS study on the thermal evolution of the native oxide layer on Nb3Sn and pure Nb. XPS data were recorded with conventional spectrometers using an AlK(alpha) X-ray source for spectra collected up to 600 C, and an MgK(Alpha) X-rays source for temperatures above 600 C. The effect of the thickness, composition, and thermal stability of that oxide layer is relevant to understanding the functional properties of superconducting radiofrequency (SRF) cavities used in particle accelerators. There is a consensus that oxide plays a role in surface resistance (Rs). The focus of this study is Nb3Sn, which is a promising material that is used in the manufacturing of superconducting radiofrequency (SRF) cavities as well as in quantum sensing, and pure Nb, which was included in the study for comparison. The thermal evolution of the oxide layer in these two materials is found to be quite different, which is ascribed to the influence of the Sn atom on the reactivity of the Nb atom in Nb3Sn films. Nb and Sn atoms in this intermetallic solid have different electronegativity, and the Sn atom can reduce electron density around neighbouring Nb atoms in the solid, thus reducing their reactivity for oxygen. This is shown in the thickness, composition, and thermal stability of the oxide layer formed on Nb3Sn. The XPS spectra were complemented by grazing incident XRD patterns collected using the ESRF synchrotron radiation facility. The results discussed herein shed light on oxide evolution in the Nb3Sn compound and guide its processing for potential applications of the Nb3Sn-based SRF cavities in accelerators and other superconducting devices.

Cano, Arely↗

Sputter coating of Nb₃Sn into SRF cavity using stoichiometric target

Nb₃Sn has emerged as a leading alternative material due to its higher superconducting critical temperature (Tc) and superheating field (Hsh), promising a viable solution to the intrinsic performance limit currently faced by Nb superconducting radiofrequency (SRF) cavities. We sputter-coated Nb₃Sn inside Nb SRF cavity using a stoichiometric Nb₃Sn tube target in a DC cylindrical magnetron sputter coater. The target was fabricated by growing an estimated >20 μm thick Nb₃Sn layer on a Nb tube via Sn vapor diffusion using Jefferson Lab’s coating system. Approximately 150 nm thick Nb-Sn films were sputter-deposited onto flat Nb samples at positions representing the beam tubes and equator of a 2.6 GHz Nb cavity. Post-deposition annealing at 950 °C for 3 h resulted in the formation of Nb₃Sn. Microstructural analysis of the annealed films was carried out to investigate the morphology and structure of the Nb₃Sn films. Later, a 2.6 GHz Nb SRF cavity was coated with a ~1.2 μm thick sputtered Nb-Sn film using a stoichiometric Nb₃Sn target, followed by annealing. Cryogenic RF testing of the annealed cavity demonstrated a Tc of 17.8 K, indicating the formation of Nb₃Sn. After a light Sn recoating treatment, the cavity achieved a quality factor (Q0) of 6.7E+08 at lower field at 2.0 K.

Accelerator Physics↗

Nb₃Sn Coating of a 2.6 GHz SRF Cavity by Sputter Deposition Technique

Nb₃Sn is of interest as a coating for SRF cavities due to its higher transition temperature Tc ~18.3 K and superheating field Hsh ~400 mT, both are twice that of Nb. Nb₃Sn coated cavities can achieve high-quality factors at 4 K and can replace the bulk Nb cavities operated at 2 K. A cylindrical magnetron sputtering system was built, commissioned, and used to deposit Nb₃Sn on the inner surface of a 2.6 GHz single-cell Nb cavity. With two identical cylindrical magnetrons, this system can coat a cavity with high symmetry and uniform thickness. Using Nb-Sn multilayer sequential sputtering followed by annealing at 950°C for 3 hours, polycrystalline Nb₃Sn films were first deposited at the equivalent positions of the cavity’s beam tubes and equator. The film’s composition, crystal structure, and morphology were characterized by energy dispersive spectroscopy, X-ray diffraction, and atomic force microscopy. The Tc of the films was measured by the four-point probe method and was 17.61 to 17.76 K. Based on these studies, ~1.2 micron thick Nb₃Sn was deposited inside a 2.6 GHz Nb cavity. We will discuss first results from samples and cavity coatings, and the status of the coating system.

43 PARTICLE ACCELERATORS↗

Oxygen Distribution and Segregation at Grain Boundaries in Nb and Ta-Encapsulated Nb Thin Films for Superconducting Qubits

We report on atomic-scale analyses of oxygen distribution and segregation at grain boundaries (GBs) of Nb and Ta-encapsulated Nb (Ta/Nb) thin films for superconducting qubits using atom probe tomography (APT) and transmission electron microscopy (TEM). We observe oxygen segregation at grain boundaries (GBs) relative to the oxygen concentration within the grains for both Nb and Ta-capped Nb thin films and find that a higher oxygen concentration in the interior of Nb grains leads to greater oxygen segregation levels at GBs. This finding reveals that the formation of a local equilibrium of oxygen concentration between GBs and grain interiors of Nb is the primary driving force of the oxygen segregation behaviors in Nb and Ta-capped Nb. The enrichment factors (CGB/Cgrain) for oxygen segregation at GBs in Nb and Ta-capped Nb range from 2.4 ± 0.3 to 2.7 ± 0.4. The current results also highlight that controlling oxygen impurities in Nb during film deposition and fabrication processing is important to concomitantly reducing the level of oxygen segregation at GBs in Nb. Finally, we find that increases in the oxygen concentration in both Nb grains and GBs correlate with a suppression in the critical temperature for superconductivity (Tc). Together, our comparative chemical and charge transport property analyses provide atomic-scale insights into a potential mechanism, contributing to the decoherence in superconducting qubits.

Lee, Jaeyel [Fermilab] (ORCID:0000000185429612)↗

Rapid Nb 3 Sn film growth by sputtering Nb on hot bronze

Nb deposited by magnetron sputtering onto hot Cu-15 wt.%Sn bronze substrates at temperatures above 700 °C achieved Nb 3 Sn film growth at a rate of 33 nm min -1 , which was an order of magnitude faster than that achieved for deposition of Nb on bronze at low temperature followed by in situ post reaction at the same high temperatures. Tin content in the Nb 3 Sn films made on hot bronze was ~26.3%, which is significantly higher than ~24.5% obtained by post-reaction as well as for typical bulk reactions between Nb and α -bronze. The Nb 3 Sn lattice parameter was consistent with measured tin content and predicted elastic strain for both routes. Critical temperatures of 14 K–16 K, instead of 18 K, were consistent with elastic strain due to coefficient of thermal expansion mismatch between the Nb 3 Sn and bronze substrate and, for the hot-bronze samples, stress related to the growth mechanism. Films were fully coalesced and had surface roughness values <20 nm over a 100 μ m 2 scan. Grain structure of the Nb 3 Sn films produced by Nb sputtering on hot bronze resembles zone 2 in the Thornton structure-zone diagram, in contrast to the equiaxed grain structure reminiscent of microstructure observed in reacted Nb 3 Sn wires exhibited by the post-reaction route.

Physics↗

Lower Temperature Annealing of Vapor Diffused Nb₃Sn for Accelerator Cavities

Nb₃Sn is a next-generation superconducting material for the accelerator cavities with higher critical temperature and superheating field, both twice compared to Nb. It promises superior performance and higher operating temperature than Nb, resulting in significant cost reduction. So far, the Sn vapor diffusion method is the most preferred and successful technique to coat niobium cavities with Nb₃Sn. Although several post-coating techniques (chemical, electrochemical, mechanical) have been explored to improve the surface quality of the coated surface, an effective process has yet to be found. Since there are only a few studies on the post-coating heat treatment at lower temperatures, we annealed Nb₃Sn-coated samples at 800 C - 1000 C to study the effect of heat treatments on surface properties, primarily aimed at removing surface Sn residues. This paper discusses the systematic surface analysis of coated samples after annealing at temperatures between 850 C and 950 C.

43 PARTICLE ACCELERATORS↗

Unveiling a high capacity multi-redox (Nb 5+ /Nb 4+ /Nb 3+ ) NASICON-Nb 2 (PO 4 ) 3 anode for Li- and Na-ion batteries

Sodium superionic conductor (NASICON)-type materials are widely explored as Li- and Na-ion cathodes and solid-state electrolytes but are largely ignored as anodes due to their lower capacities and higher intercalation voltages, which reduce the overall energy densities of Li- and Na-ion batteries (LIBs and SIBs). Herein, we unveil high capacity multi-redox empty NASICON-Nb 2 (PO 4 ) 3 as a potential anode material for LIBs and SIBs, which reversibly delivers 167 and 150 mA h g -1 at the average voltages of 1.86 V vs. Li + /Li 0 and 1.46 V vs. Na + /Na 0 , respectively. The Li and Na intercalation reactions proceed via multiple phase transitions, leading to short-range ordered Li 3 Nb 2 (PO 4 ) 3 and triclinic (P$\overline{1}$ with combining macron]) Na 3 Nb 2 (PO 4 ) 3 , as revealed by in situ X-ray diffraction studies. Our density functional theory calculations are also in agreement with the in situ measurements in predicting a stable Na 3 Nb 2 (PO 4 ) 3 composition in the Na–Nb 2 (PO 4 ) 3 pseudo-binary system. X-ray absorption spectroscopy confirms the participation of multi-redox Nb 5+ /Nb 4+ /Nb 3+ couples. The Nb 2 (PO 4 ) 3 anode delivers capacities greater than 124 and 106 mA h g -1 at 1C rate in Li and Na cells, respectively. In conclusion, pairing Nb 2 (PO 4 ) 3 with suitable cathodes and electrolytes can lead to high energy density batteries.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

APC Nb 3 Sn superconductors based on internal oxidation of Nb–Ta–Hf alloys

In the last few years, a new type of Nb 3 Sn superconducting composite, containing a high density of artificial pinning centers (APC) generated via an internal oxidation approach, has demonstrated a significantly superior performance relative to present, state-of-the-art commercial Nb3Sn conductors. This was achieved via the internal oxidation of Nb-4at.%Ta-1at.%Zr alloy. On the other hand, our recent studies have shown that internal oxidation of Nb–Ta–Hf alloys can also lead to dramatic improvements in Nb 3 Sn performance. Here in this work we follow up on this latter approach, fabricating a 61-stack APC wire based on the internal oxidation of Nb-4at.%Ta-1at.%Hf alloy, and compare its critical current density (J c ) and irreversibility field with APC wires made using Nb-4at.%Ta-1at.%Zr. A second goal of this work was to improve the filamentary design of APC wires in order to improve their wire quality and electromagnetic stability. Our new modifications have led to significantly improved residual resistivity ratio and stability in the conductors, while still keeping non-Cu J c at or above the conductor J c specification required by the proposed Future Circular Collider. Further improvement via optimization of the wire recipe and design is ongoing. Finally, additional work needed to make APC conductors ready for applications in magnets is discussed.

43 PARTICLE ACCELERATORS↗

Undercooling studies on Nb-Pt and Nb-Si alloys using the 105 meter drop tube

Niobium-platinum samples of compositions ranging from 16 to 32 at. pct have been undercooled to as much as 540 K in the low gravity, containerless environment of a 105 meter drop tube. Undercooling was terminated in the Nb-Pt samples by the nucleation and growth of the Nb3Pt phase. In the 16-18 at. pct Pt samples, this resulted in samples which are completely Nb3Pt, in contrast to both the equilibrium phase diagram and the nonundercooled samples which formed with Nb dendrites and interdendritic Nb3Pt. Undercoolings for the Nb-Si samples were up to 670 K, which corresponds to 27 percent of the liquidus temperature or 80 percent of the estimated hypercooling limit. In the Nb-Si system, a coupled zone was identified as well as a metastable extension of the solubility limit of Si in Nb due to deep undercooling.

Robinson, M. B.↗

Topographic Evolution of Nb Surfaces Subjected to Electropolishing

Surface quality plays an important role in the performance of SRF cavities. We report the topographic evolution of H degassed, N and O doped Nb surfaces subjected to electropolishing using atomic force microscopy. N doped Nb shows a substantial increase in roughness due to formation of niobium nitrides into the surface. Implications of the topography on magnetic field enhancement and vortex entry are discussed.

Lechner, E.M.↗

Thermal Stability and Lattice Strain Evolution of High-Nb-Containing TiAl Alloy under Low-Cycle-Fatigue Loading

The micromechanical behavior and the effect of temperature on the micromechanical mechanism of high-Nb-containing TiAl alloy during low-cycle fatigue still remain uncertain. Herein, in situ and ex situ synchrotron-based high-energy X-ray (HEXRD) experiment results reveal that the gamma and omega(o) phases suffer compressive lattice strains but the lattice strain in the alpha(2) phase evolves from tensile to compressive during low-cycle fatigue at 900 degrees C. In addition, the three phases suffer compressive lattice strains during cooling to room temperature, which could result in larger compressive lattice strains in gamma and omega(o) phases and the change of the lattice strain state in the alpha(2) phase. The peak-broadening results show gamma recrystallization is dominant in the interrupted low-cycle-fatigue samples, whereas inhomogeneous deformation occurs in the failed low-cycle-fatigue samples. The performed synchrotron diffraction experiments offer a deeper insight into the phase transformations and micromechanism of TiAl alloy during low-cycle fatigue.