Search NASA⌕ Search

SEARCH · Search NASA

Results for “Ni coarsening”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Effects of Rhenium Addition on the Temporal Evolution of the Nanostructure and Chemistry of a Model Ni-Cr-Al Superalloy: Analysis of the Coarsening Behavior - 2

The temporal evolution of the nanostructure and chemistry of a model Ni-8.5 at.% Cr-10 at.% Al alloy with the addition of 2 at.% Re was studied using transmission electron microscopy and atom-probe tomography in order to measure the number density and mean radius of the y' (LIZ) precipitates and the chemistry of the y'-precipitates and the y (fcc)-matrix. In this article, the coarsening behavior of the y'-precipitates is discussed in detail and compared with the Umantsev-Olson model for multi-component alloys. In addition, the experimental results are evaluated with PrecipiCalc(TradeMark) simulations. The results show that the diffusivities of the solute elements play a major role in the coarsening behavior of the y'-precipitates and that the addition of Re retards the coarsening kinetics and stabilizes the spheroidal morphology of the precipitates by reducing the interfacial energy.

Yoon, Kevin E.↗

Uses of Computed Tomography for Characterizing Materials Grown Terrestrially and in Microgravity

Tomography (CT) has proved to be of inestimable use in providing a rapid evaluation of a variety of samples from Mechanics of Granular Materials (MGM) to electronic materials (Ge-Si alloys) to space grown materials such as meteorites. The system at Kennedy Space Center (KSC), because of its convenient geographical location, is ideal for examining samples before launch and immediately after returning to Earth. It also has the advantage of the choice of fluxes, and in particular the use of a radioactive cobalt source, which is basically monochromatic. This permits a reasonable measurement of density to be made from which chemical composition can be determined. Due to the current dearth of long duration space grown materials, the CT instrument has been used: (1) to characterize materials in preparation for flight, (2) to determine thermal expansion values, and (3) to examine long duration space grown materials, i.e. meteorites. This work will first describe the establishment of the protocol for obtaining the optimum density readings for any material. Included will be the effects of the hardware or instrumental parameters that can be controlled, and the techniques used to process the CT data. Examples will be given of the compositional variation along a single crystal of Ge-Si alloy. Density variation with temperature has been measured in preparation for future materials science experiments; this involved the fabrication at MSFC and installation of a single zone furnace at KSC incorporating a heat pipe to ensure high temperature uniformity. At the time of writing the thermal expansion of lead (Pb) has been measured from room temperature to 900 C. Three methods are available. Digital radiography enables length changes to be determined. Prior to melting the sample is smaller than the container and the diameter change can be measured. Most critical, however, is the density change in solid, through the melting region, and in the liquid state. These data are needed for engineering purposes to aid in the design of containment cartridges, and for enabling fluid flow calculations. A second sample, with the Pb alloyed with Sb is ready for scanning. This corresponds to the planned composition of Dr. Poirier s flight experiment. Other materials pertinent to NASA programs such as Al-Cu (Trivedi), CdTe (Banish), HgCdTe (Lehoczky) will be examined below and above the melting point. Finally, three-dimensional results will be shown of the structure of a two-phase metallic meteorite of metal and sulfide, in which the Fe-Ni phase has coarsened during slow cooling over hundreds of millions of years.

Source record↗

Thoria stability in TD-NiCr at high temperatures in the presence of chromium in solution.

Study of the influence of chromium in solid solution on the coarsening of ThO2 in TD-NiCr. Comparisons were made of ThO2 coarsening in chromium-free TD-Ni and in TD-NiCr, which is known to be low in Cr2O3 as a contaminant. The results of these comparisons indicate that the presence of 20% Cr in solid solution in a nickel-base alloy does not lead to a more rapid coarsening of ThO2 at temperatures of at least 2462 deg F (1350 deg C).

Dalal, H.↗

Effects of Tantalum on the Temporal Evolution of a Model Ni-Al-Cr Superalloy During Phase Decomposition

The effects of a 2.0 at.% addition of Ta to a model Ni-10.0Al-8.5Cr (at.%) superalloy aged at 1073 K are assessed using scanning electron microscopy and atom-probe tomography. The gamma'(Ll2)-precipitate morphology that develops as a result of gamma-(fcc)matrix phase decomposition is found to evolve from a bimodal distribution of spheroidal precipitates, to {001}-faceted cuboids and parallelepipeds aligned along the elastically soft {001}-type directions. The phase compositions and the widths of the gamma'-precipitate/gamma-matrix heterophase interfaces evolve temporally as the Ni-Al-Cr-Ta alloy undergoes quasi-stationary state coarsening after 1 h of aging. Tantalum is observed to partition preferentially to the gamma'-precipitate phase, and suppresses the mobility of Ni in the gamma-matrix sufficiently to cause an accumulation of Ni on the gamma-matrix side of the gamma'/gamma interface. Additionally, computational modeling, employing Thermo-Calc, Dictra and PrecipiCalc, is employed to elucidate the kinetic pathways that lead to phase decomposition in this concentrated Ni-Al-Cr-Ta alloy.

Booth, Morrison, Christopher↗

The development of directional coarsening of the gamma-prime precipitate in superalloy single crystals

A study has been made of the kinetics of the directional coarsening of the gamma-prime precipitates in Ni-5.8Al-14.6Mo-6.2Ta single crystals during creep at 982 C. In this alloy, which is characterized by a large negative lattice misfit between the gamma-prime precipitate and the gamma matrix, the formation of gamma-prime rafts begins during primary creep, and the rafts grow in length as the deformation proceeds into steady-state creep. After that, the length of the rafts stabilizes. The thickness of the rafts remains constant from primary up to tertiary creep. The directional coarsening behavior of the alloy studied is similar to that of a more conventional single-crystal superalloy having a substantially smaller negative misfit.

Mackay, R. A.↗

The Role of Rhenium on the Temporal Evolution of the Nanostructure of a Model Ni-Al-Cr-Re Superalloy

Rhenium (2 at.%) additions to a model Ni-8.5 at.% Cr-10 at.% Al alloy are studied with respect to its effects on the temporal evolution of the nanostructure and the partitioning behavior of the four elements between the gamma (fcc) and gamma' (L1(sub 2)) phases. Chemical evolution of this quaternary alloy aged at 1073 K from 0.25 to 264 h, is investigated by three-dimensional atom-probe (3DAP) microscopy. The morphology of gamma'-precipitates remains spheroidal, even at an aging time of 264 h. The results demonstrate that Re slows the coarsening of gamma'-precipitates, in comparison to the ternary Ni-10 at.% A1-8.5 at.% Cr alloy at 1073 K.

Yoon, Kevin E.↗

The development of gamma-gamma-prime lamellar structures in a nickel-base superalloy during elevated temperature mechanical testing

The kinetics of the formation and subsequent development of the directional coarsening of the gamma-prime precipitate in model Ni-Al-Mo-Ta superalloy single crystals are examined during tensile creep under various stress levels at 982 and 1038 C. Special attention is given to the gamma and gamma-prime relation to creep time and strain in order to trace the changing gamma-gamma-prime morphology. Directional coarsening of gamma-prime is found to begin during primary creep and its rate is shown to increase with an increase in temperature or stress level. The length of gamma-prime thickness increased linearly with time up to a plateau reached after the onset of steady state creep. The raft thickness, equal to the gamma-prime size, remained constant at this initial value up through the onset of the tertiary creep. The interlaminar spacing indicates the stability of directionally coarsened structure.

Mackay, R. A.↗

The influence of cobalt, tantalum, and tungsten on the microstructure of single crystal nickel-base superalloys

The influence of composition on the microstructure of single crystal nickel-base superalloys was investigated. Co was replaced by Ni, and Ta was replaced by either Ni or W, according to a matrix of compositions based on MAR-M247. Substitution of Ni for Co caused an increase in gamma-prime solvus temperature, an increase in gamma-gamma-prime lattice mismatch, and the precipitation of W-rich phases in the alloys with high refractory metal levels. Substitution of Ni for Ta caused large decreases in gamma-prime solvus temperature, gamma-prime volume fraction, and gamma-gamma-prime lattice mismatch, whereas substitution of W for Ta resulted in smaller decreases in these features. For the alloys with gamma-prime particles that remained coherent, substitution of Ni for Co caused an increase in gamma-prime coarsening rate. The two alloys with the largest magnitude of lattice mismatch possessed gamma-prime particles which lost coherency during unstressed aging and exhibited anomalously low coarsening rates. Creep exposure at 1000 C resulted in the formation of gamma-prime lamellae oriented perpendicular to the applied stress axis in all alloys.

Nathal, M. V.↗

Advanced powder metallurgy aluminum alloys via rapid solidification technology, phase 2

Marko's rapid solidification technology was applied to processing high strength aluminum alloys. Four classes of alloys, namely, Al-Li based (class 1), 2124 type (class 2), high temperature Al-Fe-Mo (class 3), and PM X7091 type (class 4) alloy, were produced as melt-spun ribbons. The ribbons were pulverized, cold compacted, hot-degassed, and consolidated through single or double stage extrusion. The mechanical properties of all four classes of alloys were measured at room and elevated temperatures and their microstructures were investigated optically and through electron microscopy. The microstructure of class 1 Al-Li-Mg alloy was predominantly unrecrystallized due to Zr addition. Yield strengths to the order of 50 Ksi were obtained, but tensile elongation in most cases remained below 2 percent. The class 2 alloys were modified composition of 2124 aluminum alloy, through addition of 0.6 weight percent Zr and 1 weight percent Ni. Nickel addition gave rise to a fine dispersion of intermetallic particles resisting coarsening during elevated temperature exposure. The class 2 alloy showed good combination of tensile strength and ductility and retained high strength after 1000 hour exposure at 177 C. The class 3 Al-Fe-Mo alloy showed high strength and good ductility both at room and high temperatures. The yield and tensile strength of class 4 alloy exceeded those of the commercial 7075 aluminum alloy.

Ray, Ranjan↗

Microstructure Modeling of Third Generation Disk Alloys

The objective of this program was to model, validate, and predict the precipitation microstructure evolution, using PrecipiCalc (QuesTek Innovations LLC) software, for 3rd generation Ni-based gas turbine disc superalloys during processing and service, with a set of logical and consistent experiments and characterizations. Furthermore, within this program, the originally research-oriented microstructure simulation tool was to be further improved and implemented to be a useful and user-friendly engineering tool. In this report, the key accomplishments achieved during the third year (2009) of the program are summarized. The activities of this year included: Further development of multistep precipitation simulation framework for gamma prime microstructure evolution during heat treatment; Calibration and validation of gamma prime microstructure modeling with supersolvus heat treated LSHR; Modeling of the microstructure evolution of the minor phases, particularly carbides, during isothermal aging, representing the long term microstructure stability during thermal exposure; and the implementation of software tools. During the research and development efforts to extend the precipitation microstructure modeling and prediction capability in this 3-year program, we identified a hurdle, related to slow gamma prime coarsening rate, with no satisfactory scientific explanation currently available. It is desirable to raise this issue to the Ni-based superalloys research community, with hope that in future there will be a mechanistic understanding and physics-based treatment to overcome the hurdle. In the mean time, an empirical correction factor was developed in this modeling effort to capture the experimental observations.

Jou, Herng-Jeng↗

Factors which influence directional coarsening of Gamma prime during creep in nickel-base superalloy single crystals

Changes in the morphology of the gamma prime precipitate were examined as a function of time during creep at 982 C in 001 oriented single crystals of a Ni-Al-Mo-Ta superalloy. In this alloy, which has a large negative misfit of -0.80 pct., the gamma prime particles link together during creep to form platelets, or rafts, which are aligned with their broad faces perpendicular to the applied tensile axis. The effects of initial microstructure and alloy composition of raft development and creep properties were investigated. Directional coarsening of gamma prime begins during primary creep and continues well after the onset of second state creep. The thickness of the rafts remains constant up through the onset of tertiary creep a clear indication of the stability of the finely-spaced gamma/gamma prime lamellar structure. The thickness of the rafts which formed was equal to the initial gamma prime size which was present prior to testing. The single crystals with the finest gamma prime size exhibited the longest creep lives, because the resultant rafted structure had a larger number of gamma/gamma prime interfaces per unit volume of material. Reducing the Mo content by only 0.73 wt. pct. increased the creep life by a factor of three, because the precipitation of a third phase was eliminated.

Mackay, R. A.↗

Factors which influence directional coarsening of gamma-prime during creep in nickel-base superalloy single crystals

Changes in the morphology of the gamma prime precipitate were examined as a function of the time during creep at 982 C in 001 oriented single crystals of a Ni-Al-Mo-Ta superalloy. In this alloy, which has a large negative misfit of -0.80 pct., the gamma prime particles link together during creep to form platelets, or rafts, which are aligned with their broad faces perpendicular to the applied tensile axis. The effects of initial microstructure and alloy composition of raft development and creep properties were investigated. Directional coarsening of gamma prime begins during primary creep and continues well after the onset of second state creep. The thickness of the rafts remains constant up through the onset of tertiary creep, a clear indication of the stability of the finely-spaced gamma/gamma prime lamellar structure. The thickness of the rafts which formed was equal to the initial gamma prime size which was present prior to testing. The single crystals with the finest gamma prime size exhibited the longest creep lives, because the resultant rafted structure had a larger number of gamma/gamma prime interfaces per unit volume of material. Reducing the Mo content by only 0.73 wt. pct. increased the creep life by a factor of three, because the precipitation of a third phase was eliminated.

Mackay, R. A.↗

Temporal Evolution of Nanostructures in a Model Nickel-Base Superalloy: Experiments and Simulations

The temporal evolution of the nanostructure of a model Ni-base superalloy (Ni-5.2 at.% Al-14.2 at.% Cr) is studied experimentally employing three-dimensional atom-probe (3DAP) microscopy in conjunction with kinetic Monte Carlo (KMC) simulations at 600 C. It is demonstrated that not only can the mean compositions of individual gamma' (Ni3Al with the Li2 structure) precipitates be measured but the Ni, Al, and Cr concentration profiles within the precipitates can also be determined for precipitates with a mean radius ( ) as small as 0.85 nm. The three asymptotic tinie dependencies of the Lifshitz-Slyzov-Wagner (LSW) theory of coarsening (Ostwald ripening) are measured and found to deviate from its theoretical predictions: possible explanations for these discrepancies are discussed. At 0.25 hr. there is 3DAP microscope evidence for the presence of precipitates of another nickel-rich phase. ="Ni3Cr" (Ni3Cr(1-x)Al(x)), which exhibits short-range order (SRO) and that is metastable with respect to Ni3Al. This metastable phase is also found by KMC simulations and has the composition Ni3Cr(1-x)Al(x), which is Ni-2.91 at.% Al-21.98 at.% Cr at 16 hours. Our results demonstrate that the decomposition of gamma the primary gamma (FCC) phase results in the concurrent formation of an ordered phase and a disordered phase by 0.25 hours.

Sudbrack, Chantal K.↗

Properties of splat-quenched 7075 aluminum type alloys

The 7075 alloy belonging to the Al-Zn-Mg-Cu system, prepared by powder metallurgy techniques, was used in a study of alloys prepared from splat-quenched foils consolidated into bar material by hot extrusion. Ni and Fe were included in one alloy specimen, producing a fine dispersion of FeAl3 type particles which added to the strength of the aged alloy but did not coarsen upon heat treatment. Fine oxide films showing up on air-splatted foils induce finely dispersed oxide stringers (if the foils are not hot-worked subsequently) which in turn promote axial cracking (but longitudinal tensile strength is not seriously impaired). Splatting in a protective atmosphere, or thermomechanical processing, is recommended to compensate for this.

Durand, J. P. H. A.↗

NiAl alloys for structural uses

Alloys based on the intermetallic compound NiAl are of technological interest as high temperature structural alloys. These alloys possess a relatively low density, high melting temperature, good thermal conductivity, and (usually) good oxidation resistance. However, NiAl and NiAl-base alloys suffer from poor fracture resistance at low temperatures as well as inadequate creep strength at elevated temperatures. This research program explored macroalloying additions to NiAl-base alloys in order to identify possible alloying and processing routes which promote both low temperature fracture toughness and high temperature strength. Initial results from the study examined the additions of Fe, Co, and Hf on the microstructure, deformation, and fracture resistance of NiAl-based alloys. Of significance were the observations that the presence of the gamma-prime phase, based on Ni3Al, could enhance the fracture resistance if the gamma-prime were present as a continuous grain boundary film or 'necklace'; and the Ni-35Al-20Fe alloy was ductile in ribbon form despite a microstructure consisting solely of the B2 beta phase based on NiAl. The ductility inherent in the Ni-35Al-20Fe alloy was explored further in subsequent studies. Those results confirm the presence of ductility in the Ni-35Al-20Fe alloy after rapid cooling from 750 - 1000 C. However exposure at 550 C caused embrittlement; this was associated with an age-hardening reaction caused by the formation of Fe-rich precipitates. In contrast, to the Ni-35Al-20Fe alloy, exploratory research indicated that compositions in the range of Ni-35Al-12Fe retain the ordered B2 structure of NiAl, are ductile, and do not age-harden or embrittle after thermal exposure. Thus, our recent efforts have focused on the behavior of the Ni-35Al-12Fe alloy. A second parallel effort initiated in this program was to use an alternate processing technique, mechanical alloying, to improve the properties of NiAl-alloys. Mechanical alloying in the conventional sense requires ductile powder particles which, through a cold welding and fracture process, can be dispersion strengthened by submicron-sized oxide particles. Using both the Ni-35Al-Fe alloys to contain approx. 1 v/o Y2O3. Preliminary results indicate that mechanically alloyed and extruded NiAl-Fe + Y2O3 alloys when heat treated to a grain-coarsened condition, exhibit improved creep resistance at 1000 C when compared to NiAl; oxidation resistance comparable to NiAl; and fracture toughness values a factor of three better than NiAl. As a result of the research initiated on this NASA program, a subsequent project with support from Inco Alloys International is underway.

Koss, D. A.↗

The gravitational effects on liquid phase sintering

The liquid-phase sintering of heavy-metal PM alloys containing 78, 83, 88, 93, or 98 wt pct W plus Ni and Fe in a 7:3 ratio is investigated experimentally. The focus is on the potential role of gravity in phenomena such as specimen slumping and distortion, liquid migration, and microstructural coarsening. The results are presented in extensive graphs and micrographs and discussed in detail, and a preliminary grain-growth model is developed which accounts for the effects of contiguity and the volume fraction of solid.

Kipphut, C. M.↗

Effects of Solute Concentrations on Kinetic Pathways in Ni-Al-Cr Alloys

The kinetic pathways resulting from the formation of coherent gamma'-precipitates from the gamma-matrix are studied for two Ni-Al-Cr alloys with similar gamma'-precipitate volume fractions at 873 K. The details of the phase decompositions of Ni-7.5Al-8.5Cr at.% and Ni-5.2Al-14.2Cr at.% for aging times from 1/6 to 1024 h are investigated by atom-probe tomography, and are found to differ significantly from a mean-field description of coarsening. The morphologies of the gamma'-precipitates of the alloys are similar, though the degrees of gamma'-precipitate coagulation and coalescence differ. Quantification within the framework of classical nucleation theory reveals that differences in the chemical driving forces for phase decomposition result in differences in the nucleation behavior of the two alloys. The temporal evolution of the gamma'-precipitate average radii and the gamma-matrix supersaturations follow the predictions of classical coarsening models. The compositional trajectories of the gamma-matrix phases of the alloys are found to follow approximately the equilibrium tie-lines, while the trajectories of the gamma'-precipitates do not, resulting in significant differences in the partitioning ratios of the solute elements.

Booth-Morrison, Christopher↗

Thermal metamorphism of primitive meteorites. VII - Mineralogy-petrology of heated Murchison /C2/ and alteration of C30 and other chondrites

Alterations caused by week-long heating of Murchison in a low-pressure environment at 400-1400 C are of two types: thermodynamically favored kinetically controlled or thermodynamically controlled rapid processes. Kinetically controlled changes pertinent to chondritic evolution and which vary progressively with temperature in heated Murchison include: chondrule blurring; matrix coarsening; increasing mean Fa and Fs contents of ferromagnesian silicates; equilibration of olivine; increasing Mg/Si, Ca/Si, Al/Si, and Cr/Si and decreasing Fe/Si, Ni/Si, and S/Si in matrix; Cr loss from kamacite; and homogenization and Ni-zoning in taenite at high temperatures. Low-temperature thermodynamically controlled changes include: transformation of high-Ni troilite to low-Ni and formation of Ni- and Co-rich metal from pentlandite. High-temperature changes include formation of Cr-rich magnetite and formation of a Ni-rich sulfide similar to that found in highly altered chondrites. Trends resulting from processes of both kinds in Murchison are consistent with characteristics of a postulated C30 metamorphic suite, while those changes caused by reactions of the second kind are similar to those in heavily shock-heated ordinary chondrites and the heavily metamorphosed C5-6 chondrite, Mulga West. Either the simulations support the metamorphic origin of the C30 suite and other thermally induced changes or the natural alterations support the utility of laboratory simulations in studying meteoritic evolution.

Matza, S. D.↗