Search NASA⌕ Search

SEARCH · Search NASA

Results for “Ni-rich NMC”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Interphasial engineering for Ni-rich NMC cathode materials

Ni-rich LiNi 1-x-y Mn x CoyO 2 , (NMC: 1-x-y ≥ 0.6) are promising cathode materials for lithium-ion batteries (LIBs) due to high reversible capacity and low cost. However, the fast capacity decay and voltage fading caused by interphasial instability requires improvement. The unstable cathodeelectrolyte interphase (CEI) and transition metal (TM) dissolution at higher voltages can lead to the drastic deterioration of electrochemical performance. In this review, recent approaches to novel electrolyte and additive design, cathode engineering including artificial CEI, and doping/coating on the surface of particles or the whole electrode are comprehensively summarized. In conclusion, the importance of multi-model and multi-scale characterization methods in understanding the effects of interphasial chemistry on battery performance is highlighted.

25 ENERGY STORAGE↗

First-principles study of the structures and redox mechanisms of Ni-rich lithium nickel manganese cobalt oxides

To reduce the cobalt (Co) content in lithium-ion batteries, Ni-rich (high-Ni) lithium nickel manganese cobalt oxides (NMC) are pursued as one of the next-generation cathode materials. However, there is still debate on the crystal and electronic structures of the baseline, LiNiO 2 . Density Functional Theory (DFT) calculations were performed to provide a theoretical understanding of Ni-rich NMC. First, it was found that the commonly used $R\bar{3}m$ structure for LiNiO 2 is metallic, contrary to the experimentally reported mix-conducting behavior. Among the four different space groups, $R\bar{3}m$, C2/m, P2 1 /c, and P2/c, P2/c with charge disproportionation of Ni 2+ and Ni 4+ is the most energetically stable and semiconducting structure of LiNiO 2 . Therefore, the atomic structures of representative Ni-rich NMC were built by partially replacing Ni with Co or Mn in the P2/c LiNiO 2 to form Li x Ni y Mn z Co 1-y-z O 2 . In the fully lithiated (x=1.0) high Ni content NMC (y>0.5), the oxidation state of all Mn ions becomes 4+, while Co ions still maintain 3+, and part of the Ni ions become 3+ to compensate for the charge. Upon delithiation, the local environment shows more variation of the charge states on the transition metal (TM) ions. The average oxidation on each TM follows a sequence of losing electrons that starts from Ni 2+ to Ni 3+ , then oxidizing Ni 3+ and Co 3+ , while Mn 4+ remains electrochemically inactive till x=0. Finally, a general relationship for the oxidation state change in each TM as a function of x is derived and shows agreement with both modeling and experimental data.

25 ENERGY STORAGE↗

In-Situ FTIR Detection of Transition Metal (TM)-Ion Dissolution From Cathodes in Li-Ion Batteries

Transition metal (TM) ions, commonly Ni and Mn, play a crucial role in Li-ion battery cathodes as the reaction centers for rapid redox reactions. A major challenge with TM-based cathodes is capacity degradation, particularly at higher operating voltages. This degradation is closely linked to the dissolution of TMs from the cathode materials and their subsequent deposition on the anode. This process not only modifies the surface structure of the cathode but, more significantly, alters the SEI composition on the anode [1-2]. The dissolution of TMs cations into a liquid electrolyte from cathode materials, such as Mn-ion dissolution from Mn-rich cathode (LMR), is detrimental to the cycling performance of Li-ion batteries [3-4]. Much attention has been paid to this issue but there remains a lack of characterization techniques which can detect the TM-ion dissolution from the cathode during electrochemical measurements. In our study, we use in-situ ATR-FTIR as an effective technique to probe the TM-ion dissolution from the cathode. We have first demonstrated the detrimental effects of TM ions on the electrochemical performance of Li-ion batteries by adding a small amount of TM salt (50 mM Mn(PF6)) to the electrolyte of a Li-ion coin cell with LFP and graphite electrode. We observed a rapid capacity fade after the first delithiation cycle. To investigate TM ion dissolution, we established a baseline IR spectrum for various TM solvation states (such as Mn and Ni) by measuring concentration-dependent IR spectra. This baseline spectrum helps us detect TM ion dissolution during battery cycling. In this work, we discuss in detail the effect of TM ions on the electrochemical performance of Li-ion batteries and the detection of TM ions during battery cycling using in-situ FTIR spectroscopy. We will compare TM dissolution between coated and uncoated cathodes to examine the effect of cathode coatings to mitigate degradation due to TM dissolution and cross-over from cathode to anode. References: (1) Zhan, C.; Wu, T.; Lu, J.; Amine, K. Dissolution, migration, anddeposition of transition metal ions in Li-ion batteries exemplified byMn-based cathodes - a critical review. Energy Environ. Sci. 2018, 11,243-257. (2) Jung, R.; Linsenmann, F.; Thomas, R.; Wandt, J.; Solchenbach,S.; Maglia, F.; Stinner, C.; Tromp, M.; Gasteiger, H. A. Nickel,Manganese, and Cobalt Dissolution from Ni-Rich NMC and TheirEffects on NMC622-Graphite Cells. J. Electrochem. Soc. 2019, 166,A378-A389. (3) Zhao, L.; Chenard, E.; Capraz, O. O.; Sottos, N. R.; White, S.R. Direct Detection of Manganese Ions in Organic Electrolyte by UV-Vis Spectroscopy. J. Electrochem. Soc. 2018, 165, A345-A348 (4) Zhang, Y.; Hu, A.; Xia, D.; Hwang, S.; Sainio, S.; Nordlund, D.;Michel, F. M.; Moore, R. B.; Li, L.; Lin, F. Operando characterization and regulation of metal dissolution and redeposition dynamics nearbattery electrode surface. Nat. Nanotechnol. 2023, 18, 790.

25 ENERGY STORAGE↗

Conformal PEDOT Coating Enables Ultra-High-Voltage and High-Temperature Operation for Single-Crystal Ni-Rich Cathodes

Single-crystal Ni-rich Li[Ni x Mn y Co 1-x-y ]O 2 (SC-NMC) cathodes represent a promising approach to mitigate the cracking issue of conventional polycrystalline cathodes. However, many reported SC-NMC cathodes still suffer from unsatisfactory cycling stability, particularly under high charge cutoff voltage and/or elevated temperature. Herein, we report an ultraconformal and durable poly(3,4-ethylenedioxythiophene) (PEDOT) coating for SC-NMC cathodes using an oxidative chemical vapor deposition (oCVD) technique, which significantly improves their high-voltage (4.6 V) and high-temperature operation resiliency. The PEDOT coated SC LiNi 0.83 Mn 0.1 Co 0.07 O 2 (SC-NMC83) delivers an impressive capacity retention rate of 96.7% and 89.5% after 100 and 200 cycles, respectively. Significantly, even after calendar aging at 45 degrees C and 4.6 V, the coated cathode can still retain 85.3% (in comparison with 59.6% for the bare one) of the initial capacity after 100 cycles at a 0.5 C rate. Synchrotron X-ray experiments and interface characterization collectively reveal that the conformal PEDOT coating not only effectively stabilizes the crystallographic structure and maintains the integrity of the particles but also significantly suppresses the electrolyte's corrosion, resulting in improved electrochemical/thermal stability. Our findings highlight the promise of an oCVD PEDOT coating for single-crystal Ni-rich cathodes to meet the grand challenge of high-energy batteries under extreme conditions.

25 ENERGY STORAGE↗

Extreme fast charge aging: Effect of electrode loading and NMC composition on inhomogeneous degradation in graphite bulk and electrode/electrolyte interface

Empowering extreme fast charging (XFC) requires a comprehensive understanding of its application with advanced anode and cathode materials in lithium-ion batteries. No report exists for the full extent of limitations for the anode with crosstalk effect from paired cathode as well as Li plating due to electrode loading under XFC. In this study, a combination of cell testing and multiple length characterization is used to investigate XFC aging mechanism in cells with a low loading of 1.5 mAh cm -2 and high loading of 2.5 mAh cm -2 for graphite (Gr)/Ni-rich LiNi x Mn y Co 1-x-y O 2 (NMCs). Operando XRD mappings show 1.5 mAh cm -2 loadings result in higher strain in graphite for all three cathode types. Among the three NMC cathodes, the graphite from NMC532 and NMC811 cells show comparable strain. Scanning electron microscopy (SEM) images show distinct differences between 6-C-charged anodes in two loadings. Significantly increased electrode thickness can be seen due to more damage in the graphite bulk and accumulation of the electrolyte decomposition products in electrode pores. X-ray photoelectron spectroscopy (XPS) reveals both cathode chemistry and Li plating influence the non-uniform SEI composition on graphite surface. We report higher Ni content in NMC811 promotes the higher levels of salt decomposition on the SEI and formation of higher mass of electrolyte aging products.

25 ENERGY STORAGE↗

Computational Elucidation of Mechanical Degradation in NMC Cathodes: Impact on Cell Performance

Next-generation lithium ion batteries are expected to demonstrate superior energy and power density with longer cycle life for successful electrification of the automobile, aviation, and marine industries. Adoption of lithium metal anodes with solid electrolytes can help to achieve that goal given that the dendrite-related issues are solved eventually. Another possibility is to use Ni-rich high-capacity NMC cathode materials with liquid and/or solid electrolytes, which presently experiences rapid capacity fade while charged to higher voltages. Several mechanical and chemical degradation mechanisms are active within these NMC-based cathode particles. Recent experimental research activities attempted to correlate the mechanical damage with the capacity fade experienced by Ni-rich LiNi x Mn y Co z O 2 (x+y+z = 1) (NMC) cathodes. Here, a computational framework is developed in this study capable of quantifying the evolution of inter primary particle and cathode/electrolyte interfacial fracture experienced by the poly- and single-crystalline NMC cathodes during charge/discharge operation. Influences of mechanical degradation on the overall cell capacity, while operating with liquid and/or solid electrolytes, are successfully characterized. Decreasing the size of the cathode primary particles, or the size of the single-crystalline cathodes, can mitigate the overall mechanical degradation, and subsequent capacity fade, experienced by NMC cathodes. The developed theoretical methodology can help the engineers and scientists to better understand the mechanical degradation mechanism prevalent in Ni-rich NMC cathodes and build superior lithium ion-based energy storage devices for the application in next-generation devices.

25 ENERGY STORAGE↗

Stability Enhancement and Microstructural Modification of Ni-Rich Cathodes via Halide Doping

In this study, elemental doping is an effective strategy to modify surface and bulk chemistry in NMC cathode materials. By adding small amounts of lithium halide salts during the calcination process, the Ni-rich NMC811 cathode is doped with Br, Cl, or F halogens. The dopant type has a significant impact on the lithiation process and heavily influences the final cathode porosity and surface morphology. Utilizing a variety of electrochemical, surface, and bulk characterization techniques, it is demonstrated that an initial content of 5 mol % LiBr or LiCl in the lithium source is effective in improving capacity retention while also providing excellent rate performance. The improvements are attributed to a substantial increase in specific surface area, the formation of a stable cathode electrolyte interface (CEI) layer, and suppressed surface reconstruction. In addition, the particle microstructure is better equipped to handle cyclic volume changes with increased values of critical crack lengths. Overall, it is demonstrated that anion doping via the addition of lithium halide salts is a facile approach toward Ni-rich NMC modification for enhanced cathode performance.

25 ENERGY STORAGE↗

Ni-Rich Li[Ni x MnyCo 1– x – y ]O 2 Single Crystals as Superior Fast Charge Cathodes for Lithium-Ion Batteries

The utilization of single-crystal (SC) Li[Ni x MnyCo 1-x-y ]O 2 (NMC) cathodes has facilitated unparalleled performance in commercial high-energy lithium-ion batteries (LIBs). In the current study, we evaluate the application of SC cathodes in fast charge (FC)-LIBs where particle cracking is a predominant failure mechanism. Ni-rich SC-NMC samples with various compositions, sizes, and shapes are synthesized and investigated for their influence on FC performance. We reveal the necessity of utilizing smaller SCs (<1 μm) as larger sizes (>2 μm) experience significant particle-level lithium concentration gradients under FC conditions. To improve lithium transport and minimize side reactivities, we strategically expose the (104) crystal facets on the surface. Exceptional performance was observed on an optimized SC-LiNi 0.80 Mn 0.05 Co 0.15 O 2 , delivering a discharge capacity of 165 mAh/g even after 150 cycles at 6C charge. Our study not only demonstrates the promise of SC-NMC but also provides the key insights for the design and optimization of advanced cathodes for FC-LIBs.

25 ENERGY STORAGE↗

Understanding Structural and Compositional Evolution during NMC Cathode Direct Recycling via Solid-State NMR

Recycling end-of-life lithium-ion batteries (LIBs) to recover high-value cathode materials such as LiNixMnyCozO2 (NMC) is driven by economical, geopolitical, and sustainability needs. There has been recent interest in direct recycling methods to improve efficiency and recovery of materials, including ionothermal, hydothermal, solid-state, or redox mediator methods. In conjunction with recycling process development, detailed structural characterization is necessary in order to understand the mechanisms and efficacy of cathode recycling steps. Solid-state nuclear magnetic resonance (NMR) spectroscopy is a unique tool that can probe Li coordination, bulk and surface environments, and transition metal ordering in recycled and upcycled NMC cathodes. Here, 6,7Li, 1H, and 19F NMR spectroscopy to probe structural and compositional changes as well as surface impurities that may form during each step in NMC direct recycling is utilized. During relithiation, Li reinsertion into the NMC lattice is observed. During upcycling, where the goal is to increase the Ni content in the NMC, incorporation of Ni-rich phases into the bulk Li environment is observed. Surface impurities formed during processing were also identified. These studies provide valuable information for optimizing recycling processes to reach targeted cathode composition and structure that can enable electrochemical performance comparable to or better than pristine materials.

36 MATERIALS SCIENCE↗

Stabilizing Ni-rich layered cathode for high-voltage operation through hierarchically heterogeneous doping with concentration gradient

High-nickel LiNi x Mn y Co 1-x-y O 2 (NMC) cathodes have demonstrated superior energy density, yet their stability is compromised under high voltage conditions. To address this, here we propose a strategy of heterogeneous doping with a concentration gradient, specifically through Sr–Zr co-modification. We synthesized Ni-rich NMC particles featuring several micron-sized secondary particles composed of micron-sized primary grains. This design aims to harness the structural robustness of single-crystalline grains and the favorable diffusion kinetics of polycrystalline secondary particles. Systematic characterization using a combination of electrochemical measurements and synchrotron analytics reveals an intriguing pattern of hierarchically heterogeneous Sr–Zr co-doping. It demonstrates a depth-dependent concentration gradient at the secondary particle level and competing dopant segregation over the buried grain boundaries. This unique characteristic creates opportunities for enhancing battery performance, particularly by optimizing precursors and implementing advanced modulation techniques. We also investigate the dissolution and precipitation of the cathode's transition metal cations upon high-voltage cycling. These insights suggest that a tailored compositional variation can be a viable approach to effectively design the next-generation high-Ni NMC cathode materials for high-voltage lithium batteries.

36 MATERIALS SCIENCE↗

Nanoscopic strain evolution in single-crystal battery positive electrodes

Single-crystal Ni-rich layered oxides (SC-NMC) with a grain-boundary-free configuration have effectively addressed the long-standing cracking issue of conventional polycrystalline Ni-rich materials (PC-NMC) in lithium-ion batteries, prompting a shift in optimization strategies. However, continued reliance on anisotropic lattice volume change—a well-established failure indicator in PC-NMC—as a metric for understanding strain and guiding compositional design for SC-NMC becomes controversial. Here, in this study, by leveraging multiscale diagnostic techniques, we unravelled the distinct nanoscopic strain evolution in SC-NMC during battery operation, challenging the conventional composition-driven strategies and mechanical degradation indicators used for PC-NMC. Through particle-level chemomechanical analysis, we reveal a decoupling between mechanical stability and lattice volume change in SC-NMC, identifying that structural instability in SC materials is primarily driven by multidimensional lattice distortions induced by kinetics-driven reaction heterogeneity and progressively deactivating chemical phases. Using this mechanical failure mode, we redefine the roles of cobalt and manganese in maintaining mechanical stability. Unlike cobalt’s detrimental role in PC-NMC, we find cobalt to be critical in enhancing the longevity of SC-NMC by mitigating localized strain along the extended diffusion pathway, whereas manganese exacerbates mechanical degradation.

36 MATERIALS SCIENCE↗

Room-Temperature Eutectic Synthesis for Upcycling of Cathode Materials

Ni-rich LiNixMnyCo1−x−yO2 (NMC) materials have been adopted in a range of applications, including electric vehicles. The recycled NMC material from a spent cell would be much more valuable if it could be upgraded to a Ni-rich, more energy-dense version of the material. This work demonstrates a simple, inexpensive, and facile method to upcycle LiNi1/3Mn1/3Co1/3O2 (NMC111, 160 mAh∙g−1), a cathode used in early generations of electric vehicle batteries, to LiNi0.8Mn0.1Co0.1O2 (NMC811, 190 mAh∙g−1), a more energy-dense cathode material. In this study, a preliminary investigation into a room-temperature eutectic synthesis of NMC811 is performed using NMC111, LiOH, and nickel nitrate as precursors. The synthesized material showed the desired crystal structure and stoichiometry, though the cycle life and Li diffusion coefficient need improvement when compared to commercially available NMC811. This study demonstrates an interesting proof of concept of the room-temperature eutectic synthesis process for LIB cathodes and could be improved by tuning the synthesis conditions.

lithium-ion battery↗

Direct recycling of spent nickel-rich cathodes in reciprocal ternary molten salts

Lithium-ion batteries (LIBs) have revolutionized portable electronics and electric vehicles (EVs), but the growing accumulation of end-of-life (EOL) batteries poses environmental challenges. Recycling high-value cathodes from EOL LIBs can minimize waste and reduce the need for mining critical minerals. Here, this study focuses on the direct recycling of Ni-rich cathodes, particularly lithium-manganese-cobalt-oxide (NMC) 622 in a “reciprocal ternary molten salts (RTMS)" system. The ionothermal relithiation in the RTMS system successfully restores the layered structure, lithium content, and electrochemical performance of the NMC 622 cathode, comparable to the pristine material. The cost analysis reveals that cathode regeneration through ionothermal relithiation is more economical than virgin production or conventional recycling methods.

25 ENERGY STORAGE↗

Underlying limitations behind impedance rise and capacity fade of single crystalline Ni-rich cathodes synthesized via a molten-salt route

Layered oxide LiNi x Mn y Co z O 2 (NMC) cathodes are often synthesized as polycrystalline secondary particles. Due to intergranular fracture stemming from volume changes of randomly oriented primary particles during charge/discharge, the synthesis of larger single-crystalline cathodes is of high interest. In this work, molten salt assisted growth of micron-sized Ni-rich crystals is achieved with excellent crystallinity, low cation mixing, and negligible impurities. However, electrochemical performance is compromised by high surface reactivity resulting in decomposition of electrolyte and subsequent formation of a thick CEI layer. While intergranular fracture is eliminated, planar gliding and severe intragranular fracture along the (003) plane occurs in the high voltage region within the first few cycles and is associated primarily with H2 to H3 structural transitions. In addition, H2 to H3 transitions are highly irreversible with cyclic voltammograms revealing polarization growth within <5 cycles. Subsequently, the single-crystalline material exhibited markedly reduced available capacity and enhanced capacity fade from sharp impedance growth compared to its polycrystalline counterpart. Here, this work furthers a fundamental understanding into the limitations of single-crystalline Ni-rich cathodes, and the obstacles limiting the advantages offered by the single-crystalline morphology.

25 ENERGY STORAGE↗

Degradation in Ni-Rich LiNi 1– x – y Mn x Co y O 2 /Graphite Batteries: Impact of Charge Voltage and Ni Content

Ni-rich LiNi 1– x–y Mn x CoyO 2 (NMC) materials are attractive as cathodes for Li-ion batteries due to their high energy density and low Co content. However, these materials may display poor electrochemical reversibility relating to structural and interfacial instabilities. The influence of Ni content and level of delithiation during charge on degradation mechanisms and relevance to electrochemical cycling behavior are probed for LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) and LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathode materials in a full cell configuration under two upper voltage limits (4.1 and 4.3 V). The combined use of dQ/dV analysis of electrochemical voltage profiles, operando XRD, and postcycling scanning electron microscopy (SEM) measurements indicates that a major contributor to capacity fade is the large anisotropic volume change from an H2 $\leftrightarrows$ H3 phase transition and associated mechanical degradation particularly for NMC811. Notably, transition metal dissolution and deposition on the negative electrode are found to correlate with the structural changes occurring in the cathode under high voltage charge. X-ray photoelectron spectroscopy (XPS) analyses of the cycled cathodes reveal a more organic-rich cathode–electrolyte interphase (CEI) when cycling to 4.3 V with lower relative amounts of LiF. Surface reconstruction is not a significant factor under these cycling conditions as determined by soft X-ray absorption spectroscopy (sXAS) analysis. The results emphasize the opportunity to match the electrochemical test parameters with the specific NMC active material to mitigate degradation and extend cycle life.

36 MATERIALS SCIENCE↗

Single-Crystalline Ni-Rich LiNi x Mn y Co 1– x – y O 2 Cathode Materials: A Perspective

To drive electrical vehicles for long-range, the energy density of Li-ion batteries must be further enhanced, which requires high-energy cathode materials. Among them, Ni-rich LiNi x Mn y Co 1–x–y O 2 (x > 0.5, NMC) is one of the most promising candidates. However, traditional poly-crystal (PC) NMC materials, whose particles are secondary clusters consisting of many primary crystalline particles, are susceptible to pulverization along the inter grain/particle boundaries, resulting in poor cycle stability. Recently, single crystal (SC)-NMC cathodes are proposed as they are believed to have several merits such as high structural integrity, lower interface with electrolyte, and potentially better energy storage performance. Nevertheless, several queries, such as the merits of SC structure and the mechanism for their structure degradation, are still controversial and required to be addressed. Here, in this study, the synthesis parameters, properties, energy storage as well as safety of SC- and PC-NMC cathodes with various Ni contents are critically reviewed, for clarifying the merits and drawbacks of SC. Furthermore, the study focuses on the recent advances of insight mechanisms and strategies for stabilizing the structure/interface by doping, morphology engineering, surface coating, and composition tailoring. The remaining challenges, safety concerns, and perspectives to enhance the electrochemical performance of SC-NMC cathodes for electric vehicle application are followed.

25 ENERGY STORAGE↗

Reviving the rock-salt phases in Ni-rich layered cathodes by mechano-electrochemistry in all-solid-state batteries

The rock-salt phase (RSP) formed on the surface of Ni-rich layered cathodes in liquid-electrolyte lithium-ion batteries is conceived to be electrochemically "dead". Here we show massive RSP forms in the interior of LiNi x Mn y Co (1–x-y) O 2 (NMC) crystals in sulfide based all solid state batteries (ASSBs), but the RSP remains electrochemically active even after long cycles. The RSP and the layered structure constitute a two-phase mixture, a material architecture that is distinctly different from the RSP in liquid electrolytes. The tensioned layered phase affords an effective percolation channel into which lithium is squeezed out of the RSPs by compressive stress, rendering the RSPs electrochemically active. Consequently, the ASSBs with predominant RSP in the NMC cathode deliver remarkable long cycle life of 4000 cycles at high areal capacity of 4.3 mAh/cm 2 . Our study unveils distinct mechano-electrochemistry of RSPs in ASSBs that can be harnessed to enable high energy density and durable ASSBs.

25 ENERGY STORAGE↗