Search NASA⌕ Search

SEARCH · Search NASA

Results for “NiAl”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

NiAl-based Polyphase in situ Composites in the NiAl-Ta-X (X = Cr, Mo, or V) Systems

Polyphase in situ composites were generated by directional solidification of ternary eutectics. This work was performed to discover if a balance of properties could be produced by combining the NiAl-Laves phase and the NiAl-refractory metal phase eutectics. The systems investigated were the Ni-Al-Ta-X (X = Cr, Mo, or V) alloys. Ternary eutectics were found in each of these systems and the eutectic composition, temperature, and morphology were determined. The ternary eutectic systems examined were the NiAl-NiAlTa-(Mo, Ta), NiAl-(Cr, Al) NiTa-Cr, and the NiAl-NiAlTa-V systems. Each eutectic consists of NiAl, a C14 Laves phase, and a refractory metal phase. Directional solidification was performed by containerless processing techniques in a levitation zone refiner to minimize alloy contamination. Room temperature fracture toughness of these materials was determined by a four-point bend test. Preliminary creep behavior was determined by compression tests at elevated temperatures, 1100-l400 K. Of the ternary eutectics, the one in the NiAl-Ta-Cr system was found to be the most promising. The fracture toughness of the NiAl-(Cr, Al)NiTa-Cr eutectic was intermediate between the values of the NiAl-NiAlTa eutectic and the NiAl-Cr eutectic. The creep strength of this ternary eutectic was similar to or greater than that of the NiAl-Cr eutectic.

Johnson, D. R.↗

Nial and Nial-Based Composites Directionally Solidified by a Containerless Zone Process

A containerless electromagnetically levitated zone (CELZ) process has been used to directionally solidify NiAl and NiAl-based composites. The CELZ processing results in single crystal NiAl (HP-NiAl) having higher purity than commercially pure NiAl grown by a modified Bridgman process (CP-NiAl). The mechanical properties, specifically fracture toughness and creep strength, of the HP-NiAl are superior to binary CP-NiAl and are used as a base-line for comparison with the composite materials subsequently studied. Two-phase composite materials (NiAl-based eutectic alloys) show improvement in room temperature fracture toughness and 1200 to 1400 K creep strength over that of binary HP-NiAl. Metallic phase reinforcements produce the greatest improvement in fracture toughness, while intermetallic reinforcement produces the largest improvement in high temperature strength. Three-phase eutectic alloys and composite materials were identified and directionally solidified with the intent to combine the improvements observed in the two-phase alloys into one alloy. The room temperature fracture toughness and high temperature strength (in air) serve as the basis for comparison between all of the alloys. Finally, the composite materials are discussed in terms of dominant fracture mechanism observed by fractography.

Joslin, Steven M.↗

Elevated temperature compressive properties of reaction milled NiAl-AlN and Zr-doped NiAl-AlN composites

Previous studies of a single lot of NiAl powder which had been ground under high intensity conditions in liquid nitrogen (cryomilling) indicated that this processing leads to a high strength, elevated temperature NiAl-AlN composite. Because this was the first known example of the use of the reaction milling process to produce a high temperature composite, the reproducibility of this technique was unknown. Two additional lots of NIAl powder and a lot of a Zr-doped NiAl powder have been cryomilled, and analyses indicate that AlN was formed within a NiAl matrix in all three cases. Compression testing between 1200 K and 1400 K has shown that the deformation resistance of these heats is similar to that of the first lot of NiAl-AlN; thus cryomilling can improve the creep resistance of NiAl by a factor of six. Based on this work, it is concluded that cryomilling of NiAl powder to form high temperature, high strength NiAl-AlN composites is a reproducible process.

Whittenberger, J. D.↗

Processing, physical metallurgy and creep of NiAl + Ta and NiAl + Nb alloys

Powder processed NiAl + Ta alloys containing 1, 2, and 4.5 at percent tantalum and NiAl + Nb alloys containing 1 and 2 at percent niobium were developed for improved creep properties. In addition, a cast alloy with 5 at percent tantalum was also studied. Hot extrusion parameters for processing alloys with 1 and 2 at percent of tantalum or niobium were designed. The NiAl + 4.5 at percent Ta alloy could be vacuum hot pressed successfully, even though it could not be extruded. All the phases in the multiphase alloys were identified and the phase transformations studied. The Ni2AlTa in NiAl + 4.5 at percent Ta alloy transforms into a liquid phase above 1700 K. Solutionizing and annealing below this temperature gives rise to a uniform distribution of fine second phase precipitates. Compressive creep properties were evaluated at 1300 K using constant load and constant velocity tests. In the higher strain rate region single phase NiAl + 1 at percent Ta and NiAl + 1 at percent Nb alloys exhibit a stress exponent of 5 characteristic of climb controlled dislocation creep. In slower strain rate regime diffusional creep becomes important. The two phase alloys containing 2 to 5 at percent Ta and 2 at percent Nb show considerable improvement over binary NiAl and single phase alloys. Loose dislocation networks and tangles stabilized by the precipitates were found in the as crept microstructure. The cast alloy which has larger grains and a distribution of fine precipitates shows the maximum improvement over binary NiAl.

Pathare, Viren M.↗

Removal of iodine (I- and IO3-) from aqueous solutions using CoAl and NiAl layered double hydroxides

The treatment of radioactive iodine released from nuclear power plants and radiological waste disposal sites is of great concern due to its high mobility and toxicity. In particular, iodide (I-) and iodate (IO3-) are the major iodine species of concern under various pHs and groundwater conditions. Herein, CoAl and NiAl layered double hydroxides (LDHs) were synthesized by a hydrothermal method and investigated to identify the removal mechanisms and efficiencies of both I- and IO3-. Both CoAl and NiAl LDHs exhibited rapid iodine removal processes within 20 min, following the pseudo-second-order model via ion-exchange with parent NO3- anion in the LDHs. The CoAl LDH’s maximum sorption capacities for I- and IO3- were about 1.67 and 2.16 mmol g-1, respectively, whereas for the NiAl LDH, these were about 2.10 and 2.26 mmol g-1, and they followed the Langmuir isotherm model. Interestingly, both the CoAl and NiAl LDHs showed a preferential ion-exchange affinity for IO3- over I-, which was attributed to the structural similarity of the IO3- and NO3- as well as new formation of secondary Co(or Ni)(IO3)2·2H2O phases. In addition, a desorption study indicated that the selectivity order was SO42- = IO3- = OH- > HCO3- > Cl- > NO3- = I- and demonstrated the higher retention of the IO3- than I- anion. This study provides insights into promising iodine sorbents and the different removal mechanisms of I- and IO3- using CoAl and NiAl LDHs.

Kang, Jaehyuk↗

Correlation of deformation mechanisms with the tensile and compressive behavior of NiAl and NiAl(Zr) intermetallic alloys

To identify the mechanisms controlling strength and ductility in powder-extruded NiAl and NiAl + 0.05 at. pct Zr, tensile and compressive testing was performed from 300 to 1300 K for several grain sizes. Grain size refinement significantly increased yield stress in both alloys and, in some cases, slightly lowered the ductile-to-brittle transition temperature (DBTT), although no room-temperature tensile ductility was observed even in the finest grain size specimens. The small Zr addition increased the DBTT and changed the low-temperature fracture mode from intergranular in NiAl to a combination of intergranular and transgranular in the Zr-doped alloy. Scanning electron microscopy of compression specimens deformed at room temperature revealed the presence of grain-boundary cracks in both alloys. These cracks were due to the incompatibility of strain in the polycrystalline material, owing to the lack of five independent slip systems. The tendency to form grain-boundary cracks, in addition to the low fracture stress of these alloys, contributed to the lack of tensile ductility at low temperatures.

Bowman, R. R.↗

Formation of β-NiAl Phase During Casting of a Ni-Based Superalloy

A high-refractory Ni-based superalloy prototype was melted on a research scale while simulating industry practices. Ingots were vacuum induction melted and subjected to a computationally optimized homogenization heat treatment prior to fabrication which consisted of forging and hot rolling. Failure of one of the ingots at the early stage of the forging process was attributed to the precipitation of the β-NiAl phase during melting which stabilized the eutectic constituent.

36 MATERIALS SCIENCE↗

Room temperature ductility of NiAl-strengthened ferritic steels: Effects of precipitate microstructure

The effects of precipitate microstructure on the room temperature ductility of a series of carefully designed Fe-Al-Ni-Cr-Mo steels were investigated. Transmission electron microscopy (TEM), ultra small angle X-ray scattering (USAXS), and atom probe tomography (APT) were conducted to quantify the nano-scaled precipitates. The accuracy of the characterization results was verified by a numerical analysis. Three point bending tests results demonstrated that ductility was a function of the precipitate volume fraction and the Al and Ni concentrations in the Fe matrix, these relationships were discussed in terms of possible mechanisms. The ductility was also found to be independent of the precipitate size and inter-particle spacing in the studied range, which was validated by a theoretical model.

36 MATERIALS SCIENCE↗

Processing and Mechanical Properties of NiAl-Based In-Situ Composites

In-situ composites based on the NiAl-Cr eutectic system were successfully produced by containerless processing and evaluated. The NiAl-Cr alloys had a fibrous microstructure while the NiAl-(Cr,Mo) alloys containing 1 at. percent or more molybdenum exhibited a lamellar structure. The NiAl-28Cr-6Mo eutectic displays promising high temperature strength while still maintaining a reasonable room temperature fracture toughness when compared to other NiAl-based materials. The Laves phase NiAlTa was used to strengthen NiAl and very promising creep strengths were found for the directionally solidified NiAl-NiAlTa eutectic. The eutectic composition was found to be near NiAl-15.5Ta (at. percent) and well aligned microstructures were produced at this composition. An off-eutectic composition of NiAl-14.5Ta was also processed, consisting of NiAl dendrites surrounded by aligned eutectic regions. The room temperature toughness of these two phase alloys was similar to that of polycrystalline NiAl even with the presence of the brittle Laves phase NiAlTa. Polyphase in-situ composites were generated by directional solidification of ternary eutectics. The systems investigated were the Ni-Al-Ta-X (X=Cr, Mo, or V) alloys. Ternary eutectics were found in each of these systems and both the eutectic composition and temperature were determined. Of these ternary eutectics, the one in the NiAl-Ta-Cr system was found to be the most promising. The fracture toughness of the NiAl-(Cr,Al)NiTa-Cr eutectic was intermediate between those of the NiAl-NiAlTa eutectic and the NiAl-Cr eutectic. The creep strength of this ternary eutectic was similar to or greater than that of the NiAl-Cr eutectic.

Johnson, David Ray↗

NiAl alloys for structural uses

Alloys based on the intermetallic compound NiAl are of technological interest as high temperature structural alloys. These alloys possess a relatively low density, high melting temperature, good thermal conductivity, and (usually) good oxidation resistance. However, NiAl and NiAl-base alloys suffer from poor fracture resistance at low temperatures as well as inadequate creep strength at elevated temperatures. This research program explored macroalloying additions to NiAl-base alloys in order to identify possible alloying and processing routes which promote both low temperature fracture toughness and high temperature strength. Initial results from the study examined the additions of Fe, Co, and Hf on the microstructure, deformation, and fracture resistance of NiAl-based alloys. Of significance were the observations that the presence of the gamma-prime phase, based on Ni3Al, could enhance the fracture resistance if the gamma-prime were present as a continuous grain boundary film or 'necklace'; and the Ni-35Al-20Fe alloy was ductile in ribbon form despite a microstructure consisting solely of the B2 beta phase based on NiAl. The ductility inherent in the Ni-35Al-20Fe alloy was explored further in subsequent studies. Those results confirm the presence of ductility in the Ni-35Al-20Fe alloy after rapid cooling from 750 - 1000 C. However exposure at 550 C caused embrittlement; this was associated with an age-hardening reaction caused by the formation of Fe-rich precipitates. In contrast, to the Ni-35Al-20Fe alloy, exploratory research indicated that compositions in the range of Ni-35Al-12Fe retain the ordered B2 structure of NiAl, are ductile, and do not age-harden or embrittle after thermal exposure. Thus, our recent efforts have focused on the behavior of the Ni-35Al-12Fe alloy. A second parallel effort initiated in this program was to use an alternate processing technique, mechanical alloying, to improve the properties of NiAl-alloys. Mechanical alloying in the conventional sense requires ductile powder particles which, through a cold welding and fracture process, can be dispersion strengthened by submicron-sized oxide particles. Using both the Ni-35Al-Fe alloys to contain approx. 1 v/o Y2O3. Preliminary results indicate that mechanically alloyed and extruded NiAl-Fe + Y2O3 alloys when heat treated to a grain-coarsened condition, exhibit improved creep resistance at 1000 C when compared to NiAl; oxidation resistance comparable to NiAl; and fracture toughness values a factor of three better than NiAl. As a result of the research initiated on this NASA program, a subsequent project with support from Inco Alloys International is underway.

Koss, D. A.↗

Low-index surface energies, cleavage energies, and surface relaxations for crystalline NiAl from first-principles calculations

NiAl surfaces frequently serve as a platform for studying a broad range of physical and chemical phenomena including chemisorption, catalysis, oxidation, alloy growth, and surface nanostructure formation. Knowledge of precise values for low-index surface energies of NiAl, the most fundamental quantities characterizing surface thermodynamics, is often invaluable for understanding of these phenomena. In all previous analyses for NiAl(100) and NiAl(111), Ni- and Al-terminations are not distinguished, and half of the cleavage energy (or equivalently, the average of the surface energies of two differently terminated surfaces) is always identified as the “surface energy”. No values are available for individual surface energies of Ni- or Al-terminated NiAl(100) or NiAl(111) surfaces, whereas knowledge of only cleavage energy is often insufficient for analyzing surface-associated behavior. As such, in this work we perform extensive first-principles density-functional-theory (DFT) calculations for surface energies and cleavage energies of NiAl(110), NiAl(100) and NiAl(111) by considering the chemical-potential-based formulations to clarify the ambiguity in their surface energies and cleavage energies. We obtain a surface-energy phase diagram for these three low-index surfaces versus the relevant chemical potential, as well as the chemical-potential-dependent Wulff plots for NiAl crystal equilibrium shapes. We also provide the surface-relaxation information from our DFT calculations for comparison with previous experimental data.

42 ENGINEERING↗

Influence of Cr and W alloying on the fiber-matrix interfacial shear strength in cast and directionally solidified sapphire NiAl composites

Sapphire-reinforced NiAl matrix composites with chromium or tungsten as alloying additions were synthesized using casting and zone directional solidification (DS) techniques and characterized by a fiber pushout test as well as by microhardness measurements. The sapphire-NiAl(Cr) specimens exhibited an interlayer of Cr rich eutectic at the fiber-matrix interface and a higher interfacial shear strength compared to unalloyed sapphire-NiAl specimens processed under identical conditions. In contrast, the sapphire-NiAl(W) specimens did not show interfacial excess of tungsten rich phases, although the interfacial shear strength was high and comparable to that of sapphire-NiAl(Cr). The postdebond sliding stress was higher in sapphire-NiAl(Cr) than in sapphire-NiAl(W) due to interface enrichment with chromium particles. The matrix microhardness progressively decreased with increasing distance from the interface in both DS NiAl and NiAl(Cr) specimens. The study highlights the potential of casting and DS techniques to improve the toughness and strength of NiAl by designing dual-phase microstructures in NiAl alloys reinforced with sapphire fibers.

Asthana, R.↗

Creep Properties of NiAl-1Hf Single Crystals Re-Investigated

NiAl-1Hf single crystals have been shown to be quite strong at 1027 C, with strength levels approaching those of advanced Ni-based superalloys. Initial testing, however, indicated that the properties might not be reproducible. Study of the 1027 C creep behavior of four different NiAl-1Hf single-crystal ingots subjected to several different heat treatments indicated that strength lies in a narrow band. Thus, we concluded that the mechanical properties are reproducible. Recent investigations of the intermetallic NiAl have confirmed that minor alloying additions combined with single-crystal growth technology can produce elevated temperature strength levels approaching those of Ni-based superalloys. For example, General Electric alloy AFN 12 {Ni-48.5(at.%) Al-0.5Hf-1Ti-0.05Ga} has a creep rupture strength equivalent to Rene 80 combined with a approximately 30-percent lower density, a fourfold improvement in thermal conductivity, and the ability to form a self-protective alumina scale in aggressive environments. Although the compositions of strong NiAl single crystals are relatively simple, the microstructures are complex and vary with the heat treatment and with small ingot-toingot variations in the alloy chemistry. In addition, initial testing suggested a strong dependence between microstructure and creep strength. If these observations were true, the ability to utilize NiAl single-crystal rotating components in turbine machinery could be severely limited. To investigate the possible limitations in the creep response of high-strength NiAl single crystals, the NASA Glenn Research Center at Lewis Field initiated an in depth investigation of the effect of heat treatment on the microstructure and subsequent 1027 C creep behavior of [001]-oriented NiAl-1Hf with a nominal chemistry of Ni-47.5Al-1Hf-0.5Si. This alloy was selected since four ingots, grown over a number of years and possessing slightly different compositions, were available for study. Specimens taken from the ingots were subjected to several heat treatment schedules, examined by transmission electron microscopy, and tested in both compression and tension. An example of the microstructure found in a [001]-oriented NiAl-1Hf specimen after a solution treatment at 1317 C for 50 hr followed by air cooling is illustrated in the image on the left, where the NiAl matrix contains a uniform distribution of nanometer-scale Gphase (Ni16Hf6Si7) precipitates. Other heat treating schedules produced microstructures with nanometer-sized G-phase cubes and plates or, in an extreme case, produced a microstructure with all the G-phase converted to Heusler (Ni2AlHf) particles. The results of 1027 C creep strength and strain rate testing are illustrated which summarizes data from tensile and compressive testing of samples cut from all four NiAl-1Hf ingots and subjected to a variety of heat treatment schedules. With one exception, all the strength values lie in a narrow band that spans six orders of magnitude in strain rate. The only factor that produced results outside of this band was the heat treatment schedule that dissolved all the G-phase and replaced it with Heusler precipitates. The results portrayed in this figure lead to the important practical conclusion that the elevated-temperature creep properties of NiAl-1Hf single crystals are reproducible and are not affected by small variations in alloy chemistry from ingot to ingot or by different initial distributions of G-phase in the heat-treated alloy. The only variable in this study that produced a significant and delerious effect on mechanical strength was a post-solution heat treatment that lead to the complete disappearance of the G-phase in favor of Heusler precipitates.

Whittenberger, J. Daniel↗

Improving the phase stability and oxidation resistance of β-NiAl

High temperature alloys are essential to many industries that require a stable material to perform in harsh oxidative environments. Many of these alloys are suited for specific applications such as jet engine turbine blades where most other materials would either melt or oxidize and crumble (1). These alloys must have a high melting temperature, excellent oxidation resistance, good creep resistance, and decent fracture toughness to be successfully used in such environments. The discovery of Ni based superalloys in the 1940s revolutionized the high temperature alloy industry and there has been continued development of these alloys since their advent (2). These materials are capable of operating in oxidative environments in the presence of combustion gases, water vapor and at temperatures around 1050 C. Demands for increased f uel efficiency, however, has highlighted the need for materials that can be used under similar atmospheres and at temperatures in excess of 1200 C. The current Ni based superalloys are restricted to lower temperatures due to the presence of a number of low melting phases that result in softening of the alloys above 1000 C. Therefore, recent research has been aimed at exploring and developing newer alloy systems that can meet the escalating requirements. This thesis comprises a part of such an effort. The motivation of this work is to develop a novel high temperature alloy system that shows improved performance at higher temperatures than the currently employed alloys. The desired alloy should be in accordance with the requirements established in the National Energy Technology Laboratory (NETL) FutureGen program having an operating temperature around 1300 C. Alloys based on NiAl offer significant potential payoffs as structural materials in gas turbine applications due to a unique range of physical and mechanical properties. Alloying additions to NiAl could be used to further improve the pertinent properties that currently limit this system from replacing Ni based superalloys. Modifications to NiAl were explored to increase the phase stability and oxidation resistance which would allow these alloys to be used at even higher temperatures yielding greater efficiencies. The extended Miedema model was an effective tool that screened all of the potential phase space for ternary substitutions to NiAl and found the few potential systems worth further investigation. After production of the alloys it was determined that Ir, Rh, and Pd were the top candidates for substitution on Ni site up to 12 at%. The melting temperature of NiAl could be increased as much as 150 C with 12 at% Ir and 130 C with 12 at% Rh substitution. Pall adium on the other hand decreased the melting temperature by 50 C at the 12 at% substitution level. The grain size was found to have a profound influence on the oxidation resistance. Both Ir and Rh substitutions resulted in finer grain sizes compared to Pd substitutions or base NiAl. The grain size increased drastically during high temperature annealing with the PGM substitutions hindering grain growth only slightly. However, the addition of 0.05 at% Hf limited the grain growth dramatically during high temperature annealing. NiAl inherently has respectable oxidation resistance up to 1100 C. It was found through experimental testing that both Ir and Rh substitutions improve the oxidation resistance of NiAl at ultra-high temperatures with Ir performing the best. Both PGM substitutions decreased the growth rate as well as forming a more adherent oxide scale. Pd substitutions appeared to have a negligible effect to the oxidation resistance of NiAl. Hafnium addition of 0.05 at% was found to decrease the oxidation rate as well as increase the scale adherence. The combination of both Ir substitution (6-9 at%) and Hf addition (0.05 at%) produced the alloy with the best oxidation resistance. Although improvements in phase stability and oxidation resistance have been made to the NiAl system, more development and testing are still needed. Two major issues yet to be resolved are the low fracture toughness at ambient temperatures and low creep resistance at elevated temperatures. Efforts are underway to improve both of these properties by adding a second phase refractory metal, namely molybdenum.

36 MATERIALS SCIENCE↗