Rigid-Rod Sulfonated Polyamide as an Aqueous-Processable Binder for Li-Ion Battery Electrodes

Polymer binders are important components of most battery electrodes, ensuring high performance and long-term durability. Increasing demand for lithium-ion batteries in the automotive, stationary power, and portable electronics industries calls for a greener binder to replace poly(vinylidene difluoride) (PVDF). We evaluate the performance of aqueous solution-processed electrodes prepared with a rigid-rod polymer binder, poly(2,2'-disulfonyl-4,4'-benzidine terephthalamide) (PBDT). The polyamide backbone and double-helical configuration of PBDT give rise to its mechanical strength and rigidity, and its functional nature (H-bonding amides and sulfonates) can provide specific binding with electrode particles. LiFePO 4 electrodes prepared with 3 wt% PBDT show mechanical integrity and cycling stability, achieving over 1000 cycles at 4C rate with negligible capacity decay. These electrodes demonstrate comparable rate performance with their PVDF counterparts while eliminating fluorine from the electrode as well as the organic solvents needed for processing. Furthermore, this study reveals that PBDT holds great potential as a binder for advanced sustainable batteries.

25 ENERGY STORAGE↗

A Polyamide Inhibits Replication of Vesicular Stomatitis Virus by Targeting RNA in the Nucleocapsid

Polyamides have been shown to bind double-stranded DNA by complementing the curvature of the minor groove and forming various hydrogen bonds with DNA. Several polyamide molecules have been found to have potent antiviral activities against papillomavirus, a double-stranded DNA virus. By analogy, we reason that polyamides may also interact with the structured RNA bound in the nucleocapsid of a negative-strand RNA virus. For this work, Vesicular stomatitis virus (VSV) was selected as a prototype virus to test this possibility since its genomic RNA encapsidated in the nucleocapsid forms a structure resembling one strand of an A-form RNA duplex. One polyamide molecule, UMSL1011, was found to inhibit infection of VSV. To confirm that the polyamide targeted the nucleocapsid, a nucleocapsid-like particle (NLP) was incubated with UMSL1011. The encapsidated RNA in the polyamide-treated NLP was protected from thermo-release and digestion by RNase A. UMSL1011 also inhibits viral RNA synthesis in the intracellular activity assay for the viral RNA-dependent RNA polymerase. The crystal structure revealed that UMSL1011 binds the structured RNA in the nucleocapsid. The conclusion of our studies is that the RNA in the nucleocapsid is a viable antiviral target of polyamides. Since the RNA structure in the nucleocapsid is similar in all negative-strand RNA viruses, polyamides may be optimized to target the specific RNA genome of a negative-strand RNA virus, such as respiratory syncytial virus and Ebola virus.

59 BASIC BIOLOGICAL SCIENCES↗

Orientation matters: Measuring the correct surface of polyamide membranes with quartz crystal microbalance

The surface of polyamide reverse osmosis (RO) membranes which regulates interface-dominated phenomena, such as partitioning and fouling, is the one facing the feed during operation. However, the opposite surface of the polyamide selective layer, the one facing the permeate and in contact with the polysulfone porous support, is commonly analyzed in quartz crystal microbalance (QCM) measurements due to limitations of state-of-the-art transfer methodologies. Such measurements on the back surface cannot be generalized because the polyamide layer is chemically and morphologically asymmetric. Herein, we introduce a simple method to coat QCM sensors with polyamide active layers in the correct orientation (i.e., exposing their front surface) and show that interface-dominated phenomena differ significantly between orientations. We start by describing a transfer protocol to coat any surface with a polyamide layer on its front surface orientation. We then systematically analyze the chemical and morphological differences between the two surfaces of the polyamide layer of a commercial RO membrane. Finally, we demonstrate that interface-dominated phenomena depend on the orientation by showing that NaCl partitioning at pH 6 was 1.3 to 2.3-fold higher on the front surface and that organic fouling with humic acid occurred at a lower rate on this surface. The new method presented herein enables measurements on the front surface of polyamide RO membranes, which should be the standard in any future QCM studies.

Fouling behavior↗

Polyamide desalination membrane characterization and surface modification to enhance fouling resistance.

The market for polyamide desalination membranes is expected to continue to grow during the coming decades. Purification of alternative water sources will also be necessary to meet growing water demands. Purification of produced water, a byproduct of oil and gas production, is of interest due to its dual potential to provide water for beneficial use as well as to reduce wastewater disposal costs. However, current polyamide membranes are prone to fouling, which decreases water flux and shortens membrane lifetime. This research explored surface modification using poly(ethylene glycol) diglycidyl ether (PEGDE) to improve the fouling resistance of commercial polyamide membranes. Characterization of commercial polyamide membrane performance was a necessary first step before undertaking surface modification studies. Membrane performance was found to be sensitive to crossflow testing conditions. Concentration polarization and feed pH strongly influenced NaCl rejection, and the use of continuous feed filtration led to higher water flux and lower NaCl rejection than was observed for similar tests performed using unfiltered feed. Two commercial polyamide membranes, including one reverse osmosis and one nanofiltration membrane, were modified by grafting PEGDE to their surfaces. Two different PEG molecular weights (200 and 1000) and treatment concentrations (1% (w/w) and 15% (w/w)) were studied. Water flux decreased and NaCl rejection increased with PEGDE graft density ({micro}g/cm{sup 2}), although the largest changes were observed for low PEGDE graft densities. Surface properties including hydrophilicity, roughness and charge were minimally affected by surface modification. The fouling resistance of modified and unmodified membranes was compared in crossflow filtration studies using model foulant solutions consisting of either a charged surfactant or an oil in water emulsion containing n-decane and a charged surfactant. Several PEGDE-modified membranes demonstrated improved fouling resistance compared to unmodified membranes of similar initial water flux, possibly due to steric hindrance imparted by the PEG chains. Fouling resistance was higher for membranes modified with higher molecular weight PEG. Fouling was more extensive for feeds containing the cationic surfactant, potentially due to electrostatic attraction with the negatively charged membranes. However, fouling was also observed in the presence of the anionic surfactant, indicating hydrodynamic forces are also responsible for fouling.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Determination of the viscosity number of thermoplastics in dilute solution; polyamides (PA)

This West German Standard presents a test used to determine the viscosity number of polyamides and copolyamides which are easily diluted in sulfuric acid, and for other polyamides which are less easily diluted in sulfuric acid, and which are diluted in m-cresol. As formic acid is often used in industry instead of sulfuric acid, this solvent is also presented as an alternative, however, sulfuric acid is preferred because of the thermodynamic solubility characteristics of the polyamides and the handling safety. In addition, it is shown which solvent should be used for each polyamide. Finally, determinations concerning the preparation of the samples are presented. Using the viscosity number, a determination of the molar mass of the polyamides is possible.

Source record↗

Structural characterization and thermal properties of polyamide 6.6/Mg, Al/adipate-LDH nanocomposites obtained by solid state polymerization

A new nanocomposite was obtained by dispersing an adipate-modified layered double hydroxide (Ad-LDH) with adipic acid and hexamethylene diamine. These samples were polymerized in the solid phase under a nitrogen flow for 200 min at 190 {sup o}C. The structural and compositional details of the nanocomposite were determined by powder X-ray diffraction (PXRD), fourier transform infrared (FTIR) spectroscopy, focused ion beam (FIB), thermogravimetric analysis (TGA) and differential thermal analysis (DTA). The PXRD patterns and FIB images show a partially intercalated and partially exfoliated dispersion of layered crystalline materials in the polyamide 6.6 matrix. The best dispersion level is achieved in polyamide 6.6/LDH nanocomposites with low LDH loading. Some residual tactoids and particle agglomerates are also evident at high concentration. The best thermal stability of the nanocomposites is shown by the sample with 0.1% LDH content, for which it is higher than that of pure polyamide. - Graphical abstract: A new nanocomposite was obtained by compounding an adipate-modified layered double hydroxides (LDH) with adipic acid and hexamethylene diamine. These samples were polymerized in the solid phase under a nitrogen flow for 200 min at 190 {sup o}C. The nanodispersion of LDH in polyamide 6.6 may be qualitatively estimated from the analysis and PXRD patterns and FIB images. The decomposition temperature in the nanocomposite with 0.1 % LDH increases significantly compared to that for pristine PA6.6. .

36 MATERIALS SCIENCE↗

Spatial Molecular Layer Deposition of Ultrathin Polyamide To Stabilize Silicon Anodes in Lithium-Ion Batteries

Cycling stability is central to implementing silicon (Si) anodes in next-generation high-energy lithium-ion batteries. However, challenges remain due to the lack of effective strategies to enhance the structural integrity of the anode during electrochemical cycling. Here, we develop a nanoscale polyamide coating, using spatial molecular layer deposition (MLD) of m-phenylenediamine and trimesoyl chloride precursors, to preserve the structural integrity of Si anodes. Poly(acrylic acid) (PAA) has been widely used in Si-based anodes as a binding agent due to its effective binding interactions with Si particles. However, the structural integrity of the anode is compromised by thermochemical decomposition of the poly(acrylic acid) binder, which can occur during electrode drying or during electrochemical cycling. Decomposition causes a 62% decrease in the elastic modulus of the Si anode, as measured by nanoindentation in electrolyte-soaked conditions. This study shows that an ultrathin polyamide coating counteracts this structural degradation, increases the elastic modulus of the degraded anode by 345%, and improves cohesion. Electrochemical analysis of polyamide-coated anodes reveals a film thickness dependence in cycling behavior. High overpotentials and fast capacity fading are observed for Si anodes with a 15 nm coating, whereas Si anodes with a 0.5 nm coating demonstrate stable cycling over 150 cycles with a capacity >1400 mAh g-1. Our findings identify polyamide as an effective electrode coating material to enhance structural integrity, leading to excellent cyclability with higher capacity retention. Furthermore, the use of the spatial MLD approach to deposit the coating enables short deposition time and a facile route to scale-up.

25 ENERGY STORAGE↗

Structural Effects on Solubility and Crystallinity in Polyamide Ionomers

Although polyamides have been an industrial staple for decades, their solubility and processability remain limited due to the strong hydrogen bonding between amide groups. Here, we report a family of polyamides in which aryl rings, alkyl spacers, sulfonate groups, and amide linkages are regularly spaced along the polymer backbone, allowing us to probe the structural elements that affect processability. We accessed these polymers through a synthetic route based on an expanded diamine monomer and characterized them through a range of physical and spectroscopic techniques. Our results show that the combination of sulfonate groups with increased amide content results in highly soluble polymers, which can dissolve in polar solvents such as water, methanol, and N,N-dimethylformamide. Infrared spectroscopy on the solid polymers shows that the aliphatic amides engage in hydrogen bonding with the sulfonate groups, thus inhibiting ion aggregation, crystallization, and microphase separation. These findings expand the avenue to sulfonate-containing polyamide chemistry and provide design rules for the synthesis of more processable ionic polyamides.

amides↗

Thermoset/Thermoplastic Aromatic Polyamides for Composites

Aromatic polyamides are processed at relatively low temperature, then heat-treated to attain high softening temperature required when polyamides are used as matrix resins in structural composites. New polyamides are compatable with organic fibers often used as reinforcing agents in such composites Pendent propargyl groups serve as latent cross-linking agents in new series of polyamide resins.

St. Clair, T. L.↗

Syntheses and thermal stabilities of polyamides from 2,2'-bithiophene-5,5'-dicarbonyl dichloride and diamines

The properties of 12 polymers derived from 2,2'-bithiophene-5,5'-dicarbonyl dichloride are analyzed. The solution and interfacial polymerizations of 2,2'-bithiophene-5,5'-dicarbonyl dichloride are described. It is observed that due to high glass transition temperatures and the lack of flexibility of the polyamide of 2,2'-bithiophene-5,5'-dicarbonyl dichloride most of the polymers failed to fabricate into fibers or films. The data reveal that the polyamides formed from terphenyl ether form a tough, heat-pressed film; the polyamides made from aromatic diamides show great thermal stability; and the polyamides derived from aliphatic or benzylic diamides display no thermal stability.

Barber, Patrick G.↗

Unveiling the microstructural evolution of carbon fibers derived from polyamide-6

Polyacrylonitrile-based carbon fibers have dominated the industry for decades, but the high cost of polyacrylonitrile has prevented the widespread adoption of carbon fiber in high-volume structural applications. As such, a significant amount of research has been dedicated to finding an alternative, low-cost carbon fiber precursor. In this work, carbon fibers were produced from polyamide-6 using metal salt impregnation and a thermo-oxidative stabilization step. To gain further insight into the carbonization process and microstructural transformation, the morphologies, crystallinities, elemental compositions, and thermal stabilities of the fibers were characterized at various stages of processing. The stabilization step resulted in a significant increase in carbon yield, indicating a dramatic increase in thermal stability. This is due to the crosslinking of polyamide-6 chains, which was confirmed by functional group analysis. The crystallinity of the fibers was also significantly altered during processing, as the produced carbon fibers consisted of pseudo-amorphous carbon with two distinct regions of metal salt impregnation. Finally, the findings and microstructural evolution mechanisms provide guidelines for further research into carbon fiber produced from polyamide-6.

36 MATERIALS SCIENCE↗

Wholly Heterocycles-Based Polyamide–Sulfide Containing Pyridine and Thiazole Rings: A Super-Adsorbent Polymer for Lead Removal

Wholly heterocycles-based polyamide-sulfide (PAS) containing pyridine and thiazole rings with thioether linkage was synthesized and used as a novel adsorbent for lead ion removal from water. The polymer adsorbent was fully characterized via FTIR, NMR and scanning electron microscopy (SEM). The thermal properties of the synthesized polyamide were also studied by thermogravimetric analysis and the outcome showed that the polymer has a good to moderate thermal stability. The SEM was used to investigate the morphology of the wholly heterocycles-based polyamide and the outcomes displayed a porous and globular-like morphology, which guarantee effective metal adsorption. Pb(II) ion removal capacity of the synthesized polymer was studied by varying the contact time and the adsorbent concentration. The maximum removal of Pb(II) was obtained as 99%. Equilibrium behavior and kinetic of the adsorption were also investigated using prevalent isotherm and kinetic models. The adsorption capacity was obtained to be around 714 mg g{sup −1}. The Langmuir isotherm and the pseudo-second order kinetic model suggested superior agreement with the equilibrium and kinetic adsorption data, respectively. Generally, the results of this research demonstrated that the synthesized polymer is a super-adsorbent for heavy metal removal from water.

36 MATERIALS SCIENCE↗

Ionization behavior of nanoporous polyamide membranes

Escalating global water scarcity necessitates high-performance desalination membranes, for which fundamental understanding of structure–property–performance relationships is required. In this study, we comprehensively assess the ionization behavior of nanoporous polyamide selective layers in state-of-the-art nanofiltration (NF) membranes. In these films, residual carboxylic acids and amines influence permeability and selectivity by imparting hydrophilicity and ionizable moieties that can exclude coions. We utilize layered interfacial polymerization to prepare physically and chemically similar selective layers of controlled thickness. Additionally, we then demonstrate location-dependent ionization of carboxyl groups in NF polyamide films. Specifically, only surface carboxyl groups ionize under neutral pH, whereas interior carboxyl ionization requires pH >9. Conversely, amine ionization behaves invariably across the film. First-principles simulations reveal that the low permittivity of nanoconfined water drives the anomalous carboxyl ionization behavior. Furthermore, we report that interior carboxyl ionization could improve the water–salt permselectivity of NF membranes over fourfold, suggesting that interior charge density could be an important tool to enhance the selectivity of polyamide membranes. Our findings highlight the influence of nanoconfinement on membrane transport properties and provide enhanced fundamental understanding of ionization that could enable novel membrane design.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Synthesis and Properties of Cross-Linked Polyamide Aerogels

We report the first synthesis of cross-linked polyamide aerogels through step growth polymerization using a combination of diamines, diacid chloride and triacid chloride. Polyamide oligomers endcapped with amines are prepared as stable solutions in N-methylpyrrolidinone from several different diamine precursors and 1,3-benzenedicarbonyl dichloride. Addition of 1,3,5-benzenetricarbonyl trichloride yields gels which form in under five minutes according to the scheme shown. Solvent exchange of the gels into ethanol, followed by drying using supercritical CO2 extraction gives colorless aerogels with densities around 0.1 to 0.2 gcm3. Thicker monolithes of the polyamide aerogels are stiff and strong, while thin films of certain formulations are highly flexible, durable, and even translucent. These materials may have use as insulation for deployable space structures, rovers, habitats or extravehicular activity suits as well as in many terrestrial applications. Strucure property relationships of the aerogels, including surface area, mechanical properties, and thermal conductivity will be discussed.

Aerogel↗

Synthesis of Flexible Polyamide Aerogels Cross-Linked with a Tri-Isocyanate

A new series of flexible polyamide (PA) aerogels was synthesized using terephthaloyl chloride (TPC), 2,2′-dimethylbenzidine (DMBZ) and cross-linked with an inexpensive, commercially available tri-isocyanate (Desmodur N3300A) at polymer concentrations of 6–8 wt.% total solids and repeating units, n, from 30 to 60. The cross-linked DMBZ-based polyamide aerogels obtained, after supercritically drying using liquid CO 2 , had shrinkages of 19–27% with densities ranging from 0.12 g/cm 3 to 0.22 g/cm 3 , porosity and surface areas up to 91% and 309 m 2 /g, respectively, and modulus values ranging from 20.6 to 109 MPa. Evidence suggests that a higher flexibility could be achieved using DMBZ in the polyamide backbone with N3300A as a cross-linker, when compared to previously reported TPC-mPDA-BTC PA aerogels, N3300A-polyimide aerogels, and N3300-reinforced silica aerogels.