Search NASA⌕ Search

SEARCH · Search NASA

Results for “PORTLAND CEMENT”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Influence of curing temperature on belite cement hydration: A comparative study with Portland cement

Belite cements (BCs) could be a more sustainable binder than Portland cements (PCs) but adequate knowledge of the hydration features has still to be built. In particular, the mild curing hydration temperature effects have been extensively studied for PCs but not for BCs. This research was triggered by a previous work reporting improved mechanical strengths of BCs at higher curing temperatures. Here, we report the hydration characteristics of a BC at 20, 40 and 60 °C and compared to those of a typical PC. We have corroborated previous findings and used a multi-technique approach including Rietveld phase analysis, thermal analysis, calorimetry, silicon MAS-NMR, mercury intrusion porosimetry and chiefly synchrotron X-ray microtomography, to thoroughly understand the different behavior. In a nutshell, the improved mechanical performances at mild curing temperatures for BCs are mainly due to a much larger belite degree of reaction, with lower porosity coarsening of belite cements also playing a role.

36 MATERIALS SCIENCE↗

Graphene nanoplatelets reinforced cement as a solution to leaky wellbores reinforcing weak points in hydrated Portland cement with graphene nanoparticles improves mechanical and chemical durability of wellbore cements

In this work, to improve the performance of wellbore cement under subsurface environments, graphene nanoplatelets (GNPs) were added in various percentages to Class-H cement slurry. Microstructural characterization of cement slurries cured at 90 °C and 95% RH indicates that GNP modifies the microstructure of hydrated cement by reinforcing pore spaces. As a result, the mechanical properties, such as Young's modulus and axial peak stress, obtained from high temperature triaxial compression tests are significantly improved based on different percentages of added GNPs. Furthermore, the hydrated 1 × 2 inch GNP- Portland cement cores tested under simulated deep wellbore conditions of high-temperature and high pressure (HTHP), appear to have a ductile-like behavior, when compared to a typical brittle nature of Portland cement pastes. From our observations and published data on graphene resistance to fracture, GNP addition to cement is evidently enhancing the flexibility of cement. These improvements would reduce the risks associated with wellbore cement deterioration and a consequent leakage in fossil fuel production, geothermal energy production, CO 2 storage as well as long-term sealing materials in plugging and abandonment of all wellbores at the end of their service life.

36 MATERIALS SCIENCE↗

Comparison on the properties of ITZs in fly ash-based geopolymer and Portland cement concretes with equivalent flowability

Highlights: • Modelled ITZs can effectively avoid the effects caused by different factors and test locations of ITZ. • ITZ properties of PC and geopolymer concretes are compared based on equivalent flowability of binders. • Geopolymer ITZ exhibits stronger bonding than that of PC, and higher mechanical properties than geopolymer paste. • Strong ITZs in geopolymer concrete are attributed to the layer of gel-rich paste with dense microstructures. • Elastic modulus and hardness properties of ITZs in PC concrete are increased due to the CH crystals. This paper aims to compare the properties of interfacial transition zones (ITZs) in Portland cement (PC) concrete and geopolymer concrete. Portland cement and geopolymer pastes were designed with the equivalent flowability to provide similar mix and casting condition of ITZs. Two types of modelled ITZs were prepared to facilitate the nanoindentations across ITZs, microstructural characterization, and comparison on the properties of ITZs with less influential factors. The results showed that the interfacial bonding of ITZs between geopolymer matrix and aggregate is relatively stronger than the counterpart in the PC concrete. There is a high amount of crystalline hydration products in the ITZs of PC concrete, but a layer gel-rich paste with denser microstructures in the ITZs of geopolymer concrete. Additionally, the interface morphology and nanoindentation analysis indicate that the property of ITZs in the modelled geopolymer concrete is not poorer than that of the corresponding geopolymer paste.

36 MATERIALS SCIENCE↗

Initial hydration process of calcium silicates in Portland cement: A comprehensive comparison from molecular dynamics simulations

As the main components of Portland cement, calcium silicates show substantial differences in their hydration reactivity which have not been fully explained. A comprehensive comparison of the initial hydration process of calcium silicates, namely dicalcium silicate (C{sub 2}S) and tricalcium silicate (C{sub 3}S), was conducted using molecular dynamics simulations. The initial hydration process was divided into three stages using cut-off times of 0.001 ns and 3 ns. The hydration of M{sub 3}-C{sub 3}S (010) was more evident than that of β-C{sub 2}S (100), supported by the hydroxylation degree, radial distribution function, atomic density profile, etc. The coordination number of the surface Ca atoms might be the underlying reason for such a difference. Interactions between cement surfaces and water molecules were mainly characterised by solid OH bonding and Ca-water O bonding. Dissolution of Ca atoms was observed, although quite scarce, while no dissolution of Si atoms was observed.

36 MATERIALS SCIENCE↗

Sulfate Promotes Compact CaCO 3 Formation and Protects Portland Cement from Supercritical CO 2 Attack

Supercritical (sc) CO 2 in geologic carbon sequestration (GCS) can chemically and mechanically deteriorate wellbore cement, raising concerns for long-term operations. In contrast to the conventional view of “sulfate attack” on cement, we found that adding 0.15 M sulfate to the acidic brine can significantly reduce the impact of scCO 2 attack on Portland cement, resulting in stronger cement than that found in a sulfate-free system. Scanning electron microscopy revealed a decreased total attack depth in reacted cement in the presence of sulfate. With a newly defined minimum porosity term in reactive transport modeling, our model suggests that sulfate caused CaCO 3 to fill more nanopore spaces in the cement. Small angle X-ray scattering experiments also showed that sulfate can decrease the pore sizes of the carbonate layer. The results suggest that the interactions between sulfate and cement can generate a less porous CaCO 3 layer, which better resists acidic brine. Using this mechanism as a proof-of-concept, we tested the incorporation of sodium sulfate into Portland cement and synthesized new cement composites that show stronger resistance against scCO 2 attacks. Finally, these newly discovered interfacial interactions between CaCO 3 and sulfate provide new insights into engineering mechanically strong and green materials for safer GCS.

54 ENVIRONMENTAL SCIENCES↗

Combined effect of NaAlO2 and NaOH on the early age hydration of Portland cement with a high concentration of borate solution

The early age hydration of ordinary Portland cement in 5 M borate solution, with or without the addition of NaAlO{sub 2} and/or NaOH, was investigated. Hydration was measured using calorimetry, X-ray diffraction, thermogravimetric analysis, {sup 11}B and {sup 27}Al magic angle spinning NMR analysis, and scanning transmission electron microscopy. The purpose of this study was to reveal the mechanisms behind the retardation caused by a high concentration borate solution and the restoration of hydration through the combined addition of NaOH and NaAlO{sub 2}. Amorphous ulexite, which formed on the surface of the cement particles and prevented the further dissolution of anhydrous phases, was identified as the retardation product. The mechanism of the combined addition of NaAlO{sub 2} and NaOH in overcoming retardation was to transform amorphous ulexite into B-AFt and gowerite (CaB{sub 6}O{sub 10}·5H{sub 2}O). Formation of gowerite is favorable because of the much higher boron immobilization capacity in weight percentage, comparing to usual boron-containing phases reported previously.

36 MATERIALS SCIENCE↗

Effect of ZnO on the whiteness of white Portland cement clinker

The addition of ZnO to significantly improve the Hunter whiteness of white Portland cement (WPC) clinkers is introduced in this paper. The effects of ZnO on the whiteness of WPC were studied by chroma analysis, X-ray diffraction (XRD), the Rietveld method, hydration heat measurements and SEM-EDS. The results showed that adding ZnO increased the visible light reflectance, increased the brightness (L{sup ⁎}), and reduced the yellowness (b{sup ⁎}) of WPC clinker with high Fe{sub 2}O{sub 3}. Therefore, ZnO can increase the whiteness of WPC clinker. Zn was mainly distributed in the amorphous phase and unquantifiable crystalline phase (ACn), and then dissolved in the silicate phase. ZnO stabilized R-C{sub 3}S, reduced the crystallization of C{sub 3}A, and increased the ACn content. ZnO increased the amount of Fe in the ACn and minerals, thereby reducing the formation of C{sub 4}AF and improving whiteness. ZnO increased the accumulated heat of hydration but prolonged the induction period. This method provides a new approach for the WPC industry to broaden sources of raw materials and improve product quality.

36 MATERIALS SCIENCE↗

Comparison of liquid absorption-release of superabsorbent polymers in alkali-activated slag and Portland cement systems: An NMR study combined with additional methods

In this study, {sup 1}H low-field NMR was used to compare the liquid absorption-release behaviour of superabsorbent polymers (SAPs) in Portland cement (PC) paste, NaOH-activated slag (SH-AAS) paste, and water glass-activated slag (WG-AAS) paste. The liquid absorption of SAPs in the PC paste was lower than that in the SH-AAS paste and the WG-AAS paste. The liquid release was also faster, which was mainly due to the higher Ca{sup 2+} concentration in the pore fluid of the PC system. In the AAS system, although the Ca{sup 2+} concentration in the pore fluid was low, the Na{sup +} concentration was much higher than that in the PC system due to the activator. The Ca{sup 2+} in the PC system is an important factor affecting the swelling of SAPs, while in the AAS system, the swelling limitation of SAPs is the result of the combined effects of Ca{sup 2+} and Na{sup +}, with Na{sup +} being dominant.

36 MATERIALS SCIENCE↗

Supercritical, liquid, and gas CO 2 reactive transport and carbonate formation in portland cement mortar

In this paper, we investigate carbonate formation and reactive transport rate in variably saturated portland cement mortars when high concentrations of gas, liquid, or supercritical CO 2 flow through their pore network. Xray computed tomography completed during CO 2 flow is used to quantify the microstructural evolution as the mortar carbonates. After in situ tests, higher resolution scans, thermogravimetric analysis, and desorption isotherm analysis are performed to further quantify microstructural changes. We found that at dry conditions supercritical CO 2 moves more rapidly through the pore space and precipitates more carbonates than liquid or gas CO 2 . However, at 50% degree of saturation (DOS) the CO 2 state did not affect the rate of transport in that each specimen exposed to a different CO 2 state carbonated within the first hour of CO 2 exposure. When the pore space is at 50 or 100% DOS, supercritical CO 2 did not react with hydration products more rapidly nor did it result in more carbonate formation during exposure compared to gas or liquid CO 2 . The amount of Ca(OH) 2 that contributes to CaCO 3 formation is correlated to the DOS. For the mortar composition analyzed, Ca(OH) 2 contributes to approximately 40% of the carbonates formed in the 50% DOS specimens and 15% in the 100% DOS specimens. In other words, as the amount of moisture in the pore space increases, phases other than Ca(OH) 2 contribute to more than 50% of the total CaCO 3 formed.

42 ENGINEERING↗

Probing the exact form and doping preference of magnesium in ordinary Portland cement clinker phases: A study from experiments and DFT simulations

Highlights: • The doping behaviors of Mg in OPC clinker phases were systematically studied. • About 1.3 wt% MgO enter OPC clinker phases by forming substitutional solid solutions. • In the 4 composed minerals, C{sub 3}S, C{sub 3}A and C{sub 4}AF can host more Mg ions than C{sub 2}S. • Mg ions prefer to replace Ca in C{sub 3}S, C{sub 2}S and C{sub 3}A while replace Fe and Ca in C{sub 4}AF. • Both the large structure distortions and formation energies governs the low solubility. A systematic study was performed to learn the exact existence form and doping behaviors of magnesium in ordinary Portland cement (OPC) clinker. Our results show that about 1.3 wt% MgO incorporates into OPC clinker phases by forming substitutional solid solutions while excess Mg accumulate and exist as periclase. Results from Rietveld refinement present a substitution preference in C{sub 3}S and C{sub 3}A over C{sub 2}S. More in-depth analyses from density function theoretical simulations show that in C{sub 3}S, C{sub 2}S and C{sub 3}A, the substitution occurs by replacing Ca while in C{sub 4}AF, it probably occurs by substituting Fe and Ca ions. The large structure distortions and sharp increase in formation energies with increasing MgO determines its low solubility. This work provides a clear understanding of the existence states and the intrinsic mechanism governing doping behaviors of Mg, thus should be very important in guiding the synthesis of OPC clinker by utilizing high-Mg limestone.

36 MATERIALS SCIENCE↗

Natural carbonation of portland cement with synthetic zeolite Y as a supplementary cementitious material

Risks associated with carbonation are a key limitation to greater replacement levels of ordinary portland cement (OPC) by supplementary cementitious materials (SCMs). The addition of pozzolanic SCMs in OPC alters the hydrate assemblage by forming phases like calcium-(alumina)-silicate-hydrate (C-(A)-S-H). The objective of the present study was to elucidate how such changes in hydrate assemblage influence the chemical mechanisms of carbonation in a realistic OPC system. Here, in this paper, we show that synthetic zeolite Y (faujasite) is a highly reactive pozzolan in OPC that reduces the calcium content of hydration products via prompt consumption of calcium hydroxide from the evolving phase assemblage prior to CO 2 exposure. Suppression of portlandite at moderate to high zeolite Y content led to a more damaging mechanism of carbonation by disrupting the formation of a passivating carbonate layer. Without this layer, carbonation depth and CO 2 uptake are increased. Binders containing 12–18% zeolite Y by volume consumed all the calcium hydroxide from OPC during hydration and reduced the Ca/(Si+Al) ratio of the amorphous products to near 0.67. In these cases, higher carbonation depths were observed after exposure to ambient air with decalcification of C-(A)-S-H as the main source of CO 2 buffering. Binders with either 0% or 4% zeolite Y contained calcium hydroxide in the hydrated microstructure, had higher Ca/(Si+Al) ratios, and formed a calcite-rich passivation layer that halted deep carbonation. Although the carbonated layer in the samples with 12% and 18% zeolite Y contained 70% and 76% less calcite than the OPC respectively, their higher carbonation depths resulted in total CO 2 uptakes that were 12x greater than the OPC sample. Passivation layer formation in samples with calcium hydroxide explains this finding and was further supported by thermodynamic modeling. High Si/Al zeolite additives to OPC should be balanced with the calcium content for optimal carbonation resistance.

36 MATERIALS SCIENCE↗

Time-resolved 3D characterisation of early-age microstructural development of Portland cement

Abstract Time-resolved in-situ synchrotron X-ray microtomography reveals new levels of detail about the chemical and physical processes that take place as Portland cement hardens. The conversion of a fluid paste into a hardened product can be monitored on a sub-minute time-scale, and with sample movement/settlement corrections applied to enable individual particles to be tracked as they react, hydrate, and become interconnected into a single strong monolith. The growth of the strength-giving hydrate phases surrounding cement grains, and of the fluid-filled pore network that surrounds them, is able to be directly viewed at the level of individual cement particles through the application of this tracking protocol. When cement is brought into contact with water, a layer which differs in density from the bulk of the cement grains becomes observable on the grain surfaces during the induction period (during which time the heat evolution from the paste is relatively low). As hydration continues, reaction products grow both from particle surfaces into the initially fluid-filled region, and also into the space originally occupied by the cement particles, forming a density gradient within the microstructure. As the reaction accelerates and larger volumes of solid phases precipitate, the newly-formed solid structure percolates via interconnection of agglomerated low-density outer hydrates, which then densify as hydration continues. This eventually leads to solidification of the structure into a hardened porous matrix. Graphical abstract

36 MATERIALS SCIENCE↗

In-situ neutron radiography of pore-water movement in portland cement mortar under subzero temperature exposure: Insights from D 2 O-H 2 O systems

Neutron radiography was employed in this study to monitor real-time pore water movement in portland cement mortar exposed to subzero temperatures, providing novel insights into freeze-thaw (F-T) damage mechanisms. Deuterated water (D 2 O) was used to hydrate the cement in the mortar specimens, and the pore structure was saturated with water (H 2 O), allowing for a contrast that enabled detailed tracking of water movement predominantly in the pore structure. Furthermore, the mortar sample was placed on a chiller plate set to subzero temperatures, thereby providing a one-dimensional temperature gradient vertically in the sample. Neutron radiography revealed that unfrozen water migrated upward as the freezing front advanced, which can create hydraulic pressure within the mortar microstructure and may contribute to the initiation and propagation of microcracks during F-T cycles. Additional characterization of the concrete made with D 2 O showed a marked contrast to the samples made with H 2 O, including delayed hydration, diminished compressive strength, and greater porosity. Therefore, while mortar made with D 2 O allowed for greater neutron contrast to the pores filled with H 2 O, further study is required to produce mortars with similar properties to those made with H 2 O. In addition, further refinement is needed to the radiography experiment to allow for greater control of temperatures and potential quantification of the water concentration.

Air-void system↗

Real Time 3D Observations of Portland Cement Carbonation at CO2 Storage Conditions

Depleted oil reservoirs are considered a viable solution to the global challenge of CO 2 storage. A key concern is whether the wells can be suitably sealed with cement to hinder the escape of CO 2 . Under reservoir conditions, CO 2 is in its supercritical state, and the high pressures and temperatures involved make real-time microscopic observations of cement degradation experimentally challenging. Here, we present an in situ 3D dynamic X-ray micro computed tomography (μ-CT) study of well cement carbonation at realistic reservoir stress, pore-pressure, and temperature conditions. The high-resolution time-lapse 3D images allow monitoring the progress of reaction fronts in Portland cement, including density changes, sample deformation, and mineral precipitation and dissolution. By switching between flow and nonflow conditions of CO 2 -saturated water through cement, we were able to delineate regimes dominated by calcium carbonate precipitation and dissolution. For the first time, we demonstrate experimentally the impact of the flow history on CO 2 leakage risk for cement plugging. In-situ μ-CT experiments combined with geochemical modeling provide unique insight into the interactions between CO 2 and cement, potentially helping in assessing the risks of CO 2 storage in geological reservoirs.

58 GEOSCIENCES↗

Mineralogical and microstructural alterations in a portland cement paste after an accelerated decalcification process

Cement paste leaching and concomitant decalcification is a common cause of concrete structure deterioration. Such alterations entail microstructural changes that condition concrete durability. This study analysed those changes in cement pastes exposed to accelerated decalcification, layer-by-layer, from the surface in contact with the leaching agent, 6 M NH{sub 4}NO{sub 3,} to the unaltered area. The microstructural changes were analysed with BSEM, MIP and BET whilst the mineralogical and nanostructural alterations in each layer were assessed with XRD, FTIR, {sup 29}Si and {sup 27}Al MAS NMR and BSD. Decalcification affected not only portlandite and CSH gel, but also the anhydrous clinker and ettringite, inducing major micro- and nano-structural changes, particularly in the two layers closest to the leaching agent. CSH gel decalcification was more intense in the outer layers where long chain gels co-existed with silicon rich gels. BDS, in turn, revealed differences between the amount of bound water in the surface interfacing with the leaching agent and in the leaching front. More specifically, larger numbers of water molecules were tightly bound to silanol groups in the outer, whereas hydroxyl group distribution was more orderly in the inner layers.

36 MATERIALS SCIENCE↗