Materials Data on Pd4S by Materials Project

Pd4S crystallizes in the tetragonal P-42_1c space group. The structure is three-dimensional. Pd is bonded in a distorted bent 150 degrees geometry to two equivalent S atoms. There are one shorter (2.37 Å) and one longer (2.51 Å) Pd–S bond lengths. S is bonded in a 8-coordinate geometry to eight equivalent Pd atoms.

36 MATERIALS SCIENCE↗

The influence of hydrogen sulfide-to-hydrogen partial pressure ratio on the sulfidization of Pd and 70 mol% Pd-Cu membranes

The influence of H2S-to-H2 partial pressure ratio on the sulfidization of Pd and 70 mol% Pd–Cu membrane alloys was studied using various H2S-containing gas mixtures. The Pd membranes exposed to various H2S mixtures were in very good agreement with the thermodynamic calculations used in this study, resisting sulfidization when exposed to H2S-to-H2 ratios below the equilibrium value predicted for Pd4S formation, and experiencing sulfidization when exposed to ratios above the equilibrium values. The 70 mol% Pd–Cu membranes, however, exhibited deviations from the predicted values, resisting sulfidization at some conditions close to the equilibrium values at which sulfidization was expected, and experiencing sulfidization at some conditions at which resistance was expected. This phenomenon was attributed to deviations of the Pd–Cu alloy from ideality, probably due to Cu segregation at the membrane surface.

08 HYDROGEN↗

First-principles studies of H 2 S adsorption and dissociation on metal surfaces

Density functional theory calculations were employed to investigate the molecular and dissociative adsorption of H 2 S On the closed packed surfaces of a number of important noble metals (Ag(111), Au(111) and Cu(111)) and transition metals (Ir(111), Ni(111), Pd(111) and Pt(111)). Energy Minima Corresponding to adsorbed states were identified with H 2 S binding preferentially at the top sites. The adsorption of other S moieties (SH and S) was also examined. SH and S were found to prefer bridge sites and hollow sites, respectively. The binding of H 2 S and its Scontaining dissociated species is stronger on the transition metals. The elementary reactions of abstraction of H from H 2 S to form a surface SH intermediate and abstraction of H from SH to form a surface S intermediate as model pathways for the dissociation of H 2 S were examined. Our results suggest that H 2 S decomposition on the aforementioned transition metal Surfaces is more facile, both thermodynamically and kinetically.

36 MATERIALS SCIENCE↗

Hydrogen Dissociation on Pd 4 S Surfaces

Exposure of Pd-based hydrogen purification membranes to H 2 S, a common contaminant in coal gasification streams, can cause membrane performance to deteriorate, either by deactivating surface sites required for dissociative H 2 adsorption or by forming a low-permeability sulfide scale. In this work, the composition, structure, and catalytic activity of Pd 4 S, a surface scale commonly observed in Pd-membrane separation of hydrogen from sulfur-containing gas streams, were examined using a combination of experimental characterization and density functional theory (DFT) calculations. A Pd 4 S sample was prepared by exposing a 100 μm Pd foil to H 2 S at 908 K. Both X-ray photoemission depth profiling and low energy ion scattering spectroscopic (LEISS) analysis reveal slight sulfur-enrichment of the top surface of the sample. This view is consistent with the predictions of DFT atomistic thermodynamic calculations, which identified S-terminated Pd4S surfaces as energetically favored over corresponding Pd-terminated surfaces. Activation barriers for H 2 dissociation on the Pd 4 S surfaces were calculated. Although barriers are higher than on Pd(111), transition state theory analysis identified reaction pathways on the S-terminated surfaces for which hydrogen dissociation rates are high enough to sustain the separation process at conditions relevant to gasification applications.