Search NASA⌕ Search

SEARCH · Search NASA

Results for “Plasma-Facing Tungsten”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Retention and surface morphology evaluation of fine-grain dispersion-strengthened tungsten for plasma-facing component applications

This study exposed novel fine-grain dispersion-strengthened tungsten (W) to high fluence, low energy deuterium (D) and helium (He) plasmas to evaluate how material microstructure and composition affect hydrogen retention and surface morphology. Tested materials included fine-grain dispersion-strengthened tungsten (DSW) with 3 wt% zirconium carbide (ZrC) dispersoids, fine-grain dense W without any dispersoids (FGW), and coarse-grained polycrystalline ‘ITER-grade’ W. Samples were exposed to D 2 + and He + plasmas at fusion-relevant fluences (∼10 25 m -2 ) and ion energies (75 eV) over a range of temperatures (200 °C, 300 °C, 450 °C for D, 850 °C for He). Helium ion microscopy was performed on the exposed samples to evaluate surface morphology changes and material integrity. After D plasma exposure, the ZrC dispersoids showed near-surface degradation at exposure temperatures above 300 °C, but no detrimental morphology changes were observed for the adjacent W grains. After He plasma-exposure, nano-structured fuzz formation was observed in the tungsten matrix of all samples. The ZrC dispersoids maintained their integrity despite the surrounding fuzz growth, with clear delineation between the W fuzz and dispersoid regions. Thermal desorption spectroscopy showed that ZrC DSW consistently retained more D than the FGW by about a factor of 2 across all temperatures. At 200 °C and 300 °C, the ITER-W displayed lower D retention than both the DSW and FGW, however at 450 °C ITER-W showed the highest retention, about 50% more than DSW. He retention was comparable across all samples, with the highest retention observed in the fine-grain W, only 26% higher than in ITER-W. These insights on retention behavior will inform further optimization of these novel fine-grained tungsten materials with and without dispersoid additives.

Dispersion-strengthened tungsten↗

Recrystallization, cracking, and erosion of dispersoid-strengthened tungsten materials during exposure to divertor plasmas

In this study, we investigated the effects of combined intense particle and heat flux exposure on advanced tungsten plasma-facing materials within the DIII-D fusion facility. Our test matrix included two types of dispersoid-strengthened tungsten (containing either 100 nm diameter TiO 2 or Ni particles), along with high-purity polycrystalline tungsten as a reference. This experiment relied on a sample geometry angled at 15° relative to the divertor surface, thereby allowing the surfaces to intercept steady-state perpendicular heat fluxes (q ⟂ ) ranging from 10.1 to 19.6 MW/m 2 . During each shot, the samples were exposed to 42 Hz edge-localized modes (ELMs), allowing us to test the material response to transient heating. We correlated the exposure conditions with extensive post-test surface composition analysis and microscopy to determine how the plasma modified each surface. The angled specimens closest to the strike point received the highest combined heat and particle flux and melted midway through the experiment. EBSD analysis revealed they were completely recrystallized throughout, with an average grain size >100 µm. On the other hand, the specimens that received a lower steady state heat flux survived with more superficial surface damage. Whereas the high-purity polycrystalline tungsten exhibited a higher surface roughness, the dispersoid-strengthened material exhibited more extensive shallow inter-granular cracking. In addition, the surface was depleted of dispersoids following plasma exposure, possibly because of evaporation and/or sputtering. The results described here provide insights into the performance of these materials in a fusion environment which can guide further optimization for use in long-pulse devices.

Kolasinski, Robert D. [Sandia National Laboratorie↗

Developing the hybrid scenario in DIII-D and KSTAR for W-compatible long-pulse operation

Long-pulse, high-performance operation with tungsten plasma-facing components is a crucial challenge for achieving steady-state (SS) goals in ITER and future fusion devices. This paper presents a joint international effort between the DIII-D and KSTAR tokamaks aimed at demonstrating the compatibility of the high q 95 ~ 6 hybrid scenario with a tungsten divertor and superconducting coils. A DIII-D hybrid scenario recipe is successfully tailored to KSTAR’s operational constraints, which facilitates cross-device studies. The results show successful 30 s long-pulse operation in KSTAR at a normalized beta (β N = 2.4) with a benign m/n = 4/3 mode and effective mitigation of tungsten accumulation. Despite this success, the KSTAR scenario exhibits a greater than 25% reduction in thermal confinement compared to the DIII-D reference. To investigate this discrepancy, we performed a predictive TGYRO validation study, which suggests that the difference is likely caused by a weaker temperature pedestal in the KSTAR discharge due to a higher and narrower density pedestal. In addition, such lower thermal confinement leads to higher impurity accumulation, possibly due to a change in neoclassical transport with increased inward pinch, which further degrades global confinement. We also report that stationary, long-pulse operation with sustained thermal confinement requires consistent fueling and wall conditioning. These findings highlight the importance of optimized fueling and real-time wall conditioning in achieving a high temperature pedestal and strong global confinement during stable long-pulse operation. We propose potential approaches toward fully SS, long-pulse operation, including real-time wall conditioning using an impurity dropper in KSTAR and future tokamaks.

DIII-D↗

Power and particle exhaust in the ST-E1 fusion power plant

Power exhaust challenges and potential solutions for a 5 m major radius, low-aspect ratio burning tokamak have been explored. 1D edge plasma models have been used to screen for access to detachment using short and long outer divertor legs in double and single null configurations, using Ar as the primary impurity and assuming tungsten plasma-facing components (PFCs). These show that detachment access can be accessed for all but the most conservative assumptions on scrape-off layer (SOL) width and power, but that trade-offs will be required between magnet engineering and the size of the acceptable window of as-yet uncertain plasma parameters. SOLPS-ITER was used to further model selected plasma scenarios, confirming that Ar seeding can be used to achieve dissipative divertor scenarios with peak deposited heat fluxes below 15 MWm -2 . Initial scoping of first wall loads and positioning of limiters has been carried out, showing the feasibility of protecting the breeding blanket wall during steady state without impeding tritium breeding. Initial PFC technology selection is also presented, identifying this as a critical area where further work is needed to find an attractive solution for helium-cooled PFCs that can handle high heat fluxes without excessive power requirements. Key questions and trade-offs for concept development have been identified, including: how to achieve high radiation for reduction of SOL power without core performance degradation; whether power exhaust can be well-controlled in a double null plasma; mechanical design and materials challenges of high-heat flux PFCs; and control of material erosion, redeposition and tritium retention.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

The effect of high-power transient events on tungsten and tungsten coatings used for radio frequency launcher applications

High-temperature plasma-facing material coatings used for radio frequency (RF) launchers need to be robust enough to survive RF breakdown arcing or other transient events from the plasma (e.g., an edge localized mode) without causing a catastrophic failure of the coating. High-power transient effects are being explored by using an RF-induced vacuum arc to determine the robustness of tungsten coatings made by a variety of manufacturing methods. A 1/4-wavelength resonant section of vacuum transmission line terminated with an open circuit electrode structure with a well-defined electric field (30-60 kV/mm) produces repeatable arcing conditions. The initial focus is on tungsten as a plasma-facing material, including sintered tungsten, tungsten coatings on steel produced via physical vapor deposition (PVD), and functionally graded tungsten/steel coatings deposited by low-pressure plasma-spraying (LPPS). Thin PVD coatings (1-2 microns) fail catastrophically from an arc and result in severe delamination of the coating. The arc-induced damage of thicker coatings, such as those made via LPPS, tend to be restricted to the top few microns of the surface. Arcing often initiates on sharp surface microstructures and causes localized melting of tungsten at the surface of all the materials studied and results in resolidified melt pools with surface cracks. The resolidified surface results in a reduction in overall deuterium retention when exposed to typical RF plasma sheath conditions.

Caughman, John [ORNL] (ORCID:0000000206091164)↗

Simulations of grain growth in tungsten armor materials under ARC plasma edge operation conditions using an integrated plasma-edge/materials model

An integrated model of grain growth deuterium-exposed tungsten polycrystals, consisting of a two-dimensional vertex dynamics model fitted to atomistic data, has been developed to assess the grain growth kinetics of deuterium-exposed polycrystalline tungsten (W). The model tracks the motion of grain boundaries under the effect of driving forces stemming from grain boundary curvature and differential deuterium concentration accumulation. Here, we apply the model to experimentally synthesized tungsten polycrystals under deuterium-saturated conditions relevant to the ARC concept design. The results indicate rapid grain growth kinetics in the near-surface region adjacent to the plasma, where the temperature reaches 1400 K, whereas the microstructure remains stable deeper in the material with the lower temperature of 1000 K. The combined modeling and analysis further reveal that monolithic tungsten produced via conventional fabrication routes is highly susceptible to grain coarsening at temperatures exceeding 1000 K, largely independent of the magnitude of the applied driving force. Moreover, the accumulation of deuterium near grain boundaries has a pronounced inhibitory effect on grain boundary migration. High-angle grain boundaries ( > 50°) contribute more significantly to the overall grain growth process.

36 MATERIALS SCIENCE↗

Toward Verification of RANS Simulations of the T-Tube Modular Divertor Using Large Eddy Simulations of Impinging Turbulent Plane Jets

Turbulent impinging jets have been proposed to cool high heat flux plasma-facing components such as the solid tungsten target plates of the divertor in long-pulse magnetic fusion energy reactors. In particular, the T-tube modular divertor, originally developed by the ARIES Team, consists of two concentric cylindrical tubes where helium flows through a slot in the inner tube, forming an approximately planar jet that impinges upon and cools the inner surface of the pressure boundary (namely, the outer tube) and the ~15-cm 2 plasma-facing W target. The objective of this work is to demonstrate that large eddy simulations (LESs) accurately simulate the thermal transport in canonical flows that comprise the cooling flow in the T-tube, as well as validate temperatures from LES with experimental measurements in a simplified T-tube geometry. Wall‑resolved LESs, validated by experimental data and verified by direct numerical simulations (DNSs), provide benchmark data for two canonical flows in the T‑tube, namely, planar impinging and wall jets, for Reynolds numbers Re B = 4 × 10 3 to 2 × 10 4 . Our LES results are within 4% to 12% root-mean-square error (RMSE) of surface Nusselt number distributions (Nu) from experiments and DNSs. The validated LES results are then used as the ground truth to evaluate four Reynolds‑averaged Navier-Stokes (RANS) turbulence closures, namely, the k‑ω SST, realizable k‑ε, GEKO, and γ‑SST models. The k‑ω SST model has the best overall performance in terms of heat transfer, giving surface Nu within 12% RMSE of the LES results for high‑ReB impinging jets and reduced overprediction in the wall‑jet region. The GEKO model with default constants has the next best performance, providing slightly better Nu predictions for low ReB impinging jets (versus k-ω SST) but worse overall performance over the full range of ReB studied here. The realizable k‑ε turbulence model significantly overestimates turbulence near the stagnation point, while the γ‑SST model suppresses near‑wall production, biasing the simulations toward simulating laminar surface heat transfer. Simulations of the simplified T‑tube show that LES and RANS simulations with the k‑ω SST model give nearly identical average heat transfer coefficients (HTCs) over the impingement surface. The realizable k‑ε model predicts significantly lower wall temperatures due to overestimation of HTC in the outlet flow.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Novel additive manufacturing for plasma facing materials ‐ creating a research pathway for minority students

This project addresses two critical and intertwined challenges in fusion energy, namely the shortage of a broadly trained scientific workforce and the lack of scalable manufacturing solutions for plasma-facing components (PFCs). Through a collaboration among Florida International University (FIU), Miami Dade College (MDC), and Purdue University, the project established structured, reproducible educational and research pathways that recruit and advance students from institutions historically outside the fusion energy enterprise, building the human capital that this field urgently needs. The project integrates the complementary research strengths of FIU and Purdue to investigate flash sintering as a transformative processing route for tungsten-based PFCs. Unlike conventional sintering approaches, flash sintering offers rapid densification at significantly reduced thermal budgets, making it a compelling candidate for fabricating complex tungsten geometries that must withstand extreme plasma-facing environments. Systematic experimental and modeling efforts will elucidate the fundamental mechanisms governing microstructure evolution, grain boundary chemistry, and thermomechanical response during flash sintering — knowledge that is presently lacking but essential for translating this technology into reliable manufacturing practice. The convergence of workforce development and cutting-edge manufacturing research positions this project to deliver measurable, durable impact: a pipeline of fusion-ready researchers cultivated through expanded institutional partnerships, and a validated materials processing framework that accelerates domestic readiness for next-generation fusion reactor construction.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Radiation damage in tungsten under high-energy He-ion irradiation

Tungsten (W) is a primary candidate for plasma-facing components (PFCs) in fusion reactors and hybrid fission-fusion reactors. However, W suffers from severe microstructural damage under Helium (He) ion irradiation in operation conditions. Key irradiation parameters, including incident ion energy, fluence, and irradiation temperature, are known to determine the formation of He bubbles and dislocation loops, which ultimately lead to the degradation of mechanical properties, such as radiation hardening and ductile-to-brittle transition temperature (DBTT) shifts. Various strategies, for instance, interface engineering and alloying, have been developed to enhance He irradiation tolerance in W to address these challenges. Studies in the recent two decades have enhanced the understanding of the underlying mechanisms that drive defect evolution and mechanical performance degradation, thereby offering more insights into the design of more resilient W-based materials for extreme environments.

Liu, Yinghang [Purdue University]↗

Overview of advanced plasma-facing materials testing for Fusion Pilot Plants at DIII-D

Characterization and testing of advanced plasma-facing materials (PFMs) for Fusion Pilot Plants (FPP) is being conducted at the DIII-D National Fusion Facility through the ongoing two-year FPP Candidate Materials Thrust. Year one tested 17 novel materials utilizing the Divertor Materials Evaluation System (DiMES), with samples analyzed pre- and post-experiment via SEM, EDS, and confocal microscopy. Repeatable reference discharges were developed to ensure uniformity between experiments, including a new strike-point rastering scenario to provide more uniform heat/particle flux across DiMES during ELMing H-mode discharges. Various sample geometries and temperatures were used to achieve FPP-relevant conditions, including samples angled 10° towards the incident plasma flux and pre-heating up to 500 °C. The first exposure of liquid lithium (Li) capillary porous structures in a tokamak demonstrated uniform emission of Li vapor and suppression of Li droplets in H-mode when preheated to 350 °C. Dispersoid-strengthened W with 1 wt% TaC, TiC, and ZrC exposed to H-mode showed cracking and dispersoid ejection for all varieties except TiC, providing a clear down-selection. Ultra-high temperature ceramic materials TiB 2 and ZrB 2 showed minimal degradation under L-mode exposure. Silicon carbide (SiC) fiber composites showed arcing along edges, while CVD SiC remained pristine. Atmospheric plasma-sprayed W and SiC coatings endured H-mode exposure without macroscopic delamination; SiC exhibited granular ejection, while W showed increased outgassing. Additional W-based alloys were stress tested in H-mode, including Ni-based W heavy alloys, W f SiC f /W composites, W multi-principle element alloys, and functionally-graded W/SiC, to varying degrees of success.

DIII-D↗

Analysis and modeling of tungsten emission and net erosion in the DIII-D divertor using updated atomic data

Tungsten (W) is one of the leading candidate materials for plasma-facing components. However, its main drawback is its high radiative efficiency; if W penetrates the plasma, it can lead to core degradation or even collapse. Since eroded tungsten tends to ionize in the sheath and redeposit promptly, the net erosion flux that escapes prompt redeposition can differ significantly from the gross erosion. This work presents a modeling framework to estimate net erosion and photon emission from W coatings exposed to the lower divertor of DIII-D using the DiMES material exposure probe. The approach couples RustBCA for sputtering yields with a Monte Carlo transport code (LPTMC) that models redeposition and W emission. Computation is carried out with new atomic data, based on R-matrix and Mons calculations, leading to lower ionization probabilities and a twofold increase in net erosion estimates compared to calculations done with OPEN-ADAS atomic data. The model results are benchmarked against experimental measurements, showing quantitative agreement for erosion, although the trends in W emission are reproduced only qualitatively. The model is also used to assess whether W II emission can serve as a direct measurement of the net erosion of W in the lower divertor of DIII-D. Simulations show that this is not valid if the electron pressure is above ~120 Pa or if the toroidal length of the eroded material is smaller than the parallel-to-B distance traveled by impurity ions before steady-state conditions are reached. Finally, simulations suggest that when W is sputtered by carbon ions with high impact energies (≳300 eV) in DIII-D, W net erosion scales with W gross erosion and can be numerically approximated using W I flux alone as input.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

In situ studies on heavy ion irradiation and partial oxidation induced stacking faults and nanograins in tungsten nanolaminates

Understanding the microstructural evolution of tungsten (W) under extreme irradiation environments is critical for its application as a plasma-facing material in future fusion reactors. Heavy ion irradiation study offers expedited damage accumulation and thus allows irradiation tolerance property prediction in a short period of time. In this study we explore in situ Kr ion irradiation of W nanolaminates at 800 °C and uncover a complex interplay of irradiation-induced transformations, including the emergence of stacking faults, nanograin formation, and generation of thickened grain boundaries defined as GB regions with the thickness of up to 15 nm. High-resolution transmission electron microscopy studies reveal the formation of extended planar faults and a metastable hexagonal close-packed (hcp) phase within the body-centered cubic (bcc) matrix. These structural transitions are facilitated by irradiation-induced shear. They are further stabilized by the presence of oxygen, which promotes stacking fault formation and vacancy trapping. Elevated temperatures enhance defect mobility, enabling dynamic recrystallization into ultrafine grains and the thickening of GBs due to defect absorption and impurity segregation. These findings unravel non-equilibrium phase transformation pathways in heavy ion irradiated W and highlight the critical role of impurity-mediated defect dynamics in governing its radiation tolerance properties.

Wazeer, Adil [Purdue University]↗

Informing ARC divertor design and plasma facing material selection through integrated modeling

This INFUSE 2023 project between UCLA and Commonwealth Fusion Systems used computer modeling to test whether tungsten materials can survive in CFS's ARC fusion reactor divertor. The team simulated plasma conditions and material responses, finding that tungsten-rhenium alloys resist grain growth better than pure tungsten, and that hydrogen buildup depends more on particle flux than temperature. The work helps CFS design durable plasma-facing components for their fusion power plant.

36 MATERIALS SCIENCE↗

The effectiveness of D 2 pellet and gas injection in reducing intra-ELM tungsten erosion and heat flux in the DIII-D small angle slot divertor

Edge localized modes (ELMs) in H-mode plasmas can melt and erode plasma-facing components (PFCs) and lead to impurities in the core, reducing confinement. This study analyzes the use of D 2 pellet and gas injection for ELM mitigation on the DIII-D tokamak during the 2022 Small Angle Slot V-shaped Tungsten (W) (SAS-VW) divertor campaign, reducing W erosion and heat flux during ELMs. D α (656 nm) and WI (400.9 nm) filterscopes and Langmuir probes provide photon emission and electron density/temperature to estimate W atom erosion using the S/XB method, while surface eroding thermocouples measured ELM peak heat flux at the outer strike point (OSP). Thomson Scattering measurements of pedestal T e and n e provided input to predict W divertor erosion and heat flux during ELMs via the Free-Streaming plus Recycling Model (FSRM). While a greater D 2 mass injection rate decreased the ELM peak heat flux, the impact on W erosion was not monotonic. The average ‘large’ intra-ELM W erosion was lower for plasma shots with D 2 mass injection compared to the plasma shots without any D 2 mass injection in the SAS-VW divertor. However, plasma shots did not see significant changes in ‘large’ intra-ELM W divertor erosion as the D 2 mass injection rate increased. On average, the FSRM overestimated SAS-VW experimental intra-ELM W erosion by a factor of 6.9, but the overestimation is reduced to a factor of 3.6 with the implication of C deposition effects. Generally, experimentally measured and predicted quantities were worse for plasma shots with a lower D 2 mass injection rate and corresponding higher plasma carbon (C) impurity percentage (f C ). The discrepancies are postulated to be due to C/W material mixing, for which a simple analytic mixed-material model is presented. These results highlight the importance of incorporating and improving the robustness of a mixed-material layer model in the analysis of PFC erosion on present and future tokamak devices.

Carbon (C)↗

Active Divertor Heat Flux Control using Impurity Powder Dropper

Divertor plasma-facing components (PFCs) in a tokamak are typically designed to withstand average steady-state heat loads of about 5–10 MW/m 2 , a limit that applies to both solid and liquid lithium (LL) PFCs. Exceeding these design values can result in surface damage to tungsten PFCs or excessive lithium (Li) evaporation in liquid lithium divertor (LLD) PFCs. Since exceeding the divertor heat load limits has serious consequences, it is therefore prudent to develop a tool to reduce the divertor heat load and bring the heat load to within the design limit without affecting the plasma performance. Active low Z impurity injection such as Li has been suggested as a potential solution to mitigate excess heat flux as suggested previously, given that non-coronal radiation can be quite large ~ 20–30 MJ per mole of injected Li. Li is considered desirable for reducing the edge neutral recycling helping to improve plasma energy confinement. In this paper, we model the Impurity Power Dropper (IPD) to investigate its potential of divertor heat flux control. The IPD is typically located at the top of the tokamak device and uses a vertical drift tube of a few meters. In the 2 m drift tube case, the IPD powder is accelerated to ~ 6 m/sec before reaching the plasma with the upper divertor configuration, matching the condition for the in-board side pellet injection case. By modeling the IPD geometry we determined the IPD powder deposition profile, and thus the non-coronal radiation and ionization profiles in time as well. From the enhanced radiation power loss, it is therefore possible to reduce the divertor heat load using the divertor simulation code. In conclusion, the IPD divertor heat flux control can be tested in the facilities with IPD including ST-40, DIII-D, EAST, WEST and NSTX-U.

Active lithium injection↗

Coupling Microstructural Evolution Simulations to Material Property Degradation Predictions for Plasma-Facing Materials

Reliable material performance is required for plasma-facing material (PFM) candidates. Previous research has shown that plasma and neutron radiation exposure induces microstructural changes in PFMs; changes in thermal and electrical conductivities and in material hardening and embrittlement were also observed after neutron irradiation. These material property changes will negatively impact the performance of the PFMs in a fusion reactor. Despite the well-known connection between material microstructure, properties, and performance, there is a need for validated modeling capabilities connecting PFM property degradation with microstructural evolution under fusion-relevant conditions. We are developing a simulation capability to couple plasma-induced microstructural evolution to material property degradation. Our approach relies on deliberate mapping between individual simulation models and experimental characterization for validation. The open-source Multiphysics Object-Oriented Simulation Environment (MOOSE) software was used for this simulation capability development. A MOOSE phase-field model was coupled with the cluster dynamics code, Xolotl, to predict microstructural evolution. Microstructure characterization techniques, including scanning electron microscopy (SEM), transmission electron microscopy (TEM), and laser scanning confocal microscopy (LSCM) are used to validate these microstructural evolution simulations. Calculation of thermal and electrical conductivities with first principles simulations was performed for bulk material and for grain boundaries; these results are used within MOOSE models to calculate effective thermal and electrical conductivities as a function of grain characteristics. Thermoreflectance and four-probe techniques were employed to measure the thermal and electrical conductivities, respectively. A MOOSE crystal plasticity model was adapted to predict microstructure-sensitive deformation behavior, and X-ray diffraction (XRD) was used to collect bulk dislocation density data for validation. After individual simulation validation, these models are coupled to predict material property changes resulting from plasma exposure. We focused here on an experimental design to emphasize the separate effects of moderate thermal loads and plasma exposure using tungsten. Annealing of tungsten was performed under a protective environment for temperatures ranging from 500 C to 1500 C. The plasma exposure was completed in the Tritium Plasma Experiment at Idaho National Laboratory under a deuterium flux of 1e22 D/m^2-s. This incremental approach is employed to build confidence in the modeling capability: separate-effects tests ensure that the models capture key mechanisms from single environmental conditions before predicting PFM property degradation under combined loads. We will show our early results from coupling these simulation models to predict PFM property changes from microstructural evolution. Comparisons of the simulation results with preliminary validation data will be discussed.

36 - MATERIALS SCIENCE↗

Continuum radiated power density $(P^{\textrm{C}}_{\textrm{rad}})$ and effective charge $(Z_{\textrm{eff}})$ estimates from multi-energy photon-counting measurements

Multi-energy soft x-ray pinhole cameras have been designed, built, calibrated, and operated at Madison symmetric Torus, Alcator C-Mod, and more recently at Tokamak a configuration variable and Tungsten Environment in Steady-State Tokamak (WEST), to measure plasma emission across multiple energy ranges. Here we describe a new methodology to estimate the local continuum radiated power density and the plasma effective charge (Z eff ) directly from photon-counting measurements of the line-free continuum emission (Bremsstrahlung and Radiative Recombination) in several energy bands between 11 and 18 keV. This capability is particularly valuable for confinement systems using metal plasma-facing components, where x-ray losses from interactions with the sputtered wall can represent a significant fraction of the total radiated power (P rad ). The approach leverages a well-characterized detector responsivity, modeled by a complementary error function, and interprets the differential multi-energy measurements between adjacent energy levels through the probability density function of a Gaussian distribution. The implementation of this diagnostic technique is currently under development on the WEST tokamak, aiming at the goal of providing real-time P rad and Z eff measurements during long-pulse operation (up to 1000 s) in the 2026 campaign.

WEST↗

Plasma Surface Interactions: Predicting the Performance and Impact of Dynamic PFC Surfaces

This project focused on the development and integration of high-performance simulation tools to predict the operating behavior of Plasma-Facing Components in magnetic confinement fusion systems. A key objective at Illinois was to assess the impact of the dynamic interplay between the evolving material surface and the magnetized plasma sheath, and characterize the impact of tungsten-based PFCs on plasma contamination, including phenomena such as surface erosion, dynamic recycling of fuel species, and tritium retention, which are critical for the success of future magnetic fusion devices.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗