Solvari SR, Simplifying Residential Solar to 1 SKU, with Extended Testing

Accelerated weathering and material compatibility testing for polymeric and asphaltic materials. NLR will be testing the durability of the polymeric materials proposed for use in the supporting structures designed by TESCI solar. This will include the bare materials and coupons attached to asphalt shingles. The exposure will be in damp heat and separately heat, humidity and UV light, all followed by mechanical evaluation. Modification 1 is an extension of the first round of testing with both a continuation of some of the same testing and addition of new testing methods and materials. The testing of materials in the condition of A3 looking at mechanical durability will be continued looking at the materials used in the mounting brackets. We will be adding in testing of the silicone adhesive to the module and of the module itself. For the mounting brackets, testing will also be conducted at multiple temperatures and humidity levels to allow for extrapolation to the field.

14 SOLAR ENERGY↗

The combined effect of temperature and seawater on the compression properties of carbon fiber vinyl ester composites for sandwich structures

For naval applications, composite sandwich structures are of significant interest, and are often manufactured using thin (2 to 4 mm) composite facings made from carbon or glass fiber reinforcement, attached to a thick (25 to 50 mm) section of PVC cellular foam or balsa wood-based core materials using a suitable polymeric resin. In the present study, we focus on the hygrothermal effect on the fiber-dominated compression properties of carbon fiber reinforced vinyl ester resin based polymeric composite (CF/VE), used as “skin” for a polymeric composite sandwich material. Hygrothermal conditioning is achieved by saturating samples in simulated seawater at 40°C. Compression properties are evaluated for coupons extracted along warp and fill undergoing- no conditioning, conditioning till saturation (up to 6 months), and long-term conditioning (2 years). Sea-water saturation yields in up to 12% drop in compression strength with a further 3–4% drop resulting from long-term conditioning. No statistically significant modulus degradation is noticed due to short or long-term hygrothermal exposure. The failure mechanism of the warp extracted coupon, which fails in a splitting failure mode originating due to the delamination between the 0/90 interface, or the fill extracted coupon, which fails due to the instability caused by tow micro-buckling, remains unchanged due to combined exposure (short or long-term) of seawater and temperature. The loss in strength is attributed to the degradation of the fiber-matrix interface, which is validated via conducting single fiber push-in tests with a nominal diameter of 7 micron for conditioned and unconditioned coupons.

Engineering↗

Compatibility of Elastomers with Polyoxymethylene Dimethyl Ethers and Blends with Diesel

Polyoxymethylene dimethyl ethers (PODEs) have shown promise as candidates for diesel fuel blendstocks due to their low sooting tendency, high cetane number, and diesel-comparable boiling point range. However, there is a lack of literature regarding compatibility of PODEs with common automotive elastomers, which would be a prerequisite to their adoption into the marketplace. To address this need, an exposure study and complementary solubility analysis were undertaken. A commercially available blend of PODEs with polymerization degree ranging from 3 to 6 was blended with diesel certification fuel at 0, 33, 50, 67, at 100% by mass. Elastomer coupons were exposed to the various blends for a period of 4 weeks and evaluated for volume swell. The elastomer materials included multiple fluoroelastomers (Viton and fluorosilicone) and acrylonitrile butadiene rubbers (NBR), as well as neoprene, polyurethane, epichlorohydrin (ECO), PVC-nitrile blend (OZO), ethylene propylene diene monomer (EPDM), styrene-butadiene rubber (SBR), and silicone. The exposure results indicated overall poor compatibility for PODE, with every elastomer except for fluorosilicone exhibiting greater than 30% volume swell at the 33% blend level. The general trend across the elastomers was either a consistent increase in volume swell with PODE concentration, or maximum in volume swell at an intermediate blend fraction. One notable exception is EPDM, which is not generally compatible with diesel fuel and which exhibited a reduction in volume swell with increasing PODE concentration. The same elastomers and PODE/diesel blends were evaluated using Hansen solubility parameter analysis, which predicted similar trends to the exposure study with the exception of ECO. From these results, we conclude that adoption of PODEs as a diesel fuel blendstock will require either the development of specialized elastomers, or that the blend fraction be kept to a low level to maintain compatibility with existing elastomers.

42 ENGINEERING↗

Corrosion-Resistant Coatings on Spent Nuclear Fuel Canisters to Mitigate and Repair Potential Stress Corrosion Cracking (FY23 Status)

This report summarizes the activities performed by Sandia National Laboratories in FY23 to identify and test coating materials for the prevention, mitigation, and/or repair of potential chloride-induced stress corrosion cracking in spent nuclear fuel dry storage canisters. This work continues efforts by Sandia National Laboratories that are summarized in previous reports from FY20 through FY22 on the same topic. In FY23, Sandia National Laboratories, in collaboration with five industry partners through a memorandum of understanding, evaluated the physical, mechanical, and corrosion-resistance properties of eight different coating systems. The evaluation included thermal and radiation environments relevant to various time periods of storage for spent nuclear fuel canisters. The coating systems include polymeric (polyetherketoneketone, modified polyimide/polyurea, modified phenolic resin, epoxy), organic/inorganic ceramic hybrids (silane-based polyurethane hybrid and a quasi-ceramic sol-gel polyurethane hybrid), and coatings utilizing a Zn-rich primer applied to stainless steel coupons. The results and implications of these tests are summarized in this report. These analyses will be used to identify the most effective coatings for potential use on spent nuclear fuel dry storage canisters and to identify specific needs for further optimization of coating technologies for application on spent nuclear fuel canisters.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Degradation in Photovoltaic Encapsulant Transmittance: Results of the Second PVQAT TG5 Artificial Weathering Study

The optical degradation of encapsulants from ultraviolet (UV) radiation has historically resulted in a significant loss in performance throughout the life of a photovoltaic (PV) module. International Electrotechnical Commission (IEC) test methods have recently been developed to screen for PV encapsulants prone to loss in optical performance. The present study was performed to benchmark polymeric packaging materials relative to IEC 62788-1-4 (covering the measurement of optical transmittance) and IEC 62788-1-7 (on the durability of transmittance), provide feedback toward improvement of the methods, and develop insight regarding optical degradation. Contemporary materials were examined, including poly(ethylene-co-vinyl acetate) (EVA), thermoplastic polyolefin (TPO), polyolefin elastomer (POE), and polyvinyl butyral (PVB) encapsulants; a poly(ethene-co-tetrafluoroethene)/poly(ethylene terephthalate) (ETFE/PET) transparent backsheet; and a polystyrene (PS) working reference material. The use of silica-, specialty-, and rolled-glass was also compared in laminated coupons. Specimen size was separately examined from 2.5 to 12.5 cm. Weathering was performed with a xenon source, using IEC TS 62788-7-2 methods A2, A3, A4, and A5 (chamber temperature of 55 degrees C, 65 degrees C, 75 degrees C, or 85 degrees C), respectively. Characterizations were made using a UV-visible-near-infrared (UV-VIS-NIR) spectrophotometer (transmittance and reflectance, with and without an integrating sphere), a UV-VIS fluorescence spectrophotometer, a camera, and an optical microscope. Performance was analyzed, including solar weighted transmittance, yellowness index, UV cut-off wavelength, and haze (scattering). Separate Arrhenius analyses were performed to assess retention of transmittance and changes in yellowness index. The activation energy for both characteristics was found to range from 15-80 kJ mol-1, with an average of 48 kJ mol-1, similar to the average of 45 kJ mol-1 identified in the previous international PV Quality Assurance Task Force (PVQAT) Task Group 5 (TG5) study of more traditional encapsulants. The separate degradation modes of discoloration and scattering were distinguished in the encapsulants using a comprehensive spectral characterization. Based on these results, the IEC 62788-1-7 pass/fail criteria of 5% change in transmittance was confirmed to identify a known bad encapsulant.

durability↗

Molecular Imaging of Microbially Induced Corrosion of Synthetic Archeological Glasses by a Rhizosphere Bacterium

Microbially induced corrosion (MIC) focuses on the degradation of solid materials, such as glass or metal. Soil microbes are often associated with the corrosion of foreign objects in the rhizosphere. Paenibacillus polymyxa SCE2, a facultative anaerobic bacterium in soil, is of the same genus as bacteria found near nuclear waste disposal sites. Time-of-flight secondary ion mass spectrometry (ToF-SIMS) was used for imaging surface changes induced by P. polymyxa SCE2 cultured on two synthetic glass coupons to represent natural analogs of materials that were studied in relation to the vitrification of nuclear waste. Multimodal imaging was used to verify bacterial coverage across the glass surface after long-term growth. ToF-SIMS spectral analysis showed detection of glass component ions, such as silicon oxide (m/z – 59.96 SiO 2 – ) and aluminum oxide (m/z – 101.95 Al 2 O 3 – ), and biofilm’s extracellular polymeric substance (EPS) components, such as pentadecanoic acid (m/z – 241.22 C 15 H 29 O 2 – ) and sterol lipids (m/z – 311.16 C 20 H 23 O 3 – ). ToF-SIMS spectral, imaging, and depth profiling analyses showed that the glass rich in silica and other light elements (“granite glass”) had more “corrosion related” peaks than the glass that was less silica-rich and contained more iron (“dike glass”). Furthermore, these surface and interface compositional and spatial differences observed in the mass spectra and imaging were attributed to bacterial metabolism and an electron transfer mechanism influenced by morphological and compositional differences between the two types of glasses. ToF-SIMS is effective in studying microbial effects, bringing new molecular insights into MIC in a broader context of materials degradation.

Amorphous materials↗

Degradation in Photovoltaic Encapsulant Transmittance: Results of the Second PVQAT TG5 Artificial Weathering Study

The optical degradation of encapsulants from ultraviolet (UV) radiation has historically resulted in a significant loss in performance throughout the life of a photovoltaic (PV) module. IEC test methods have recently been developed to screen for PV encapsulants prone to loss in optical performance. The present study was performed to benchmark polymeric packaging materials relative to IEC 62788-1-4 (covering the measurement of optical transmittance) and IEC 62788-1-7 (on the durability of transmittance), provide feedback toward improvement of the methods, and develop insight regarding optical degradation. Contemporary materials were examined, including: poly(ethylene-co-vinyl acetate) (EVA), thermoplastic polyolefin (TPO), polyolefin elastomer (POE), and polyvinyl butyral (PVB) encapsulants; a poly(ethene-co-tetrafluoroethene)/poly(ethylene terephthalate) (ETFE/PET) transparent backsheet; and a polystyrene (PS) working reference material. The use of silica-, specialty-, and rolled-glass was also compared in laminated coupons. Specimen size was separately examined from 2.5 cm to 12.5 cm. Weathering was performed with a xenon source, using IEC TS 62788-7-2 methods A2, A3, A4, and A5 (chamber temperature of 55 Degrees C, 65 Degrees C, 75 Degrees C, or 85 Degrees C), respectively. Characterizations were made using a UV-VIS-NIR spectrophotometer (transmittance and reflectance, with and without an integrating sphere), a UV-VIS fluorescence spectrophotometer, a camera, and an optical microscope. Performance was analyzed, including solar weighted transmittance, yellowness index, UV cut-off wavelength, and haze (scattering). Separate Arrhenius analyses were performed to assess retention of transmittance and changes in yellowness index. The activation energy for both characteristics was found to range from 15 kJ?mol-1-80 kJ/mol-1, with an average of 48 kJ/mol-1, similar to the average of 45 kJ/mol-1 identified in the previous international PV Quality Assurance Task Force (PVQAT) Task Group 5 (TG5) study of more traditional encapsulants. The separate degradation modes of discoloration and scattering were distinguished in the encapsulants using a comprehensive spectral characterization. Based on these results, the IEC 62788-1-7 pass/fail criteria of 5% change in transmittance was confirmed to identify a known bad encapsulant.

durability↗

Development of a Robust Reference Electrode in Aggressive Chemical and Radiation Environments in the Hanford Waste Tanks

The Hanford site stores more than 200 million liters of radioactive and chemically hazardous wastes from the production of weapons materials. The wastes are stored in 177 underground carbon-steel storage tanks, separated between 149 single shell tanks (SSTs) and 28 double shell tanks (DSTs). The DSTs provide critical retrieval and interim storage before the waste is vitrified in the Waste Treatment and Isolation Plant (WTP). The tanks will need to remain in-service far beyond the initial 40-year design life, and effective corrosion control practices must remain in force to extend the tanks’ lifespans. This effort includes direct measurements of corrosion rate (e.g., ultrasonic measurements and corrosion coupons) and electrochemical processes (e.g., linear polarization measurements and open circuit potential measurements). The Hanford site began monitoring the corrosion potential in select DSTs in 2008. Of the 45 reference electrodes that have been installed, 29 have failed and 6 others provided unreliable results. DOE-EM is supporting a 3-year program to develop a chemical and radiation resistant reference electrode for application in the Hanford tanks. The first year of the program focused on understanding the failure mechanism for the reference electrodes and identification of candidate construction materials that would mitigate degradation of the electrodes in the waste environment. During the second year of the program, the objectives were to: 1) test candidate materials under simulated waste conditions, 2) design components that will extend the service life of the electrode, 3) fabricate materials for prototype reference electrodes, and 4) assemble prototype reference electrodes for accelerated testing. The reference electrode is constructed of four principal parts: 1) junction, 2) casing, 3) inner chamber backfill materials, and 4) the sensing wire. Principally, improvements of the junction, casing, and inner chamber backfill materials are being pursued. The junction material at the interface between the waste and the inner chamber of the reference electrode was identified as a critical component in the failure of the reference electrodes. Nine candidate replacement junction materials were tested under simulated waste conditions to evaluate permeation rate. These materials included a variety of polymeric and ceramic materials, some of which were 3-D printed. Thus far, porous polyvinylidene fluoride materials have performed satisfactorily and are being considered for prototype development. The commercial electrode casing materials in general have performed well. Additionally, 3-D printing of chemically and mechanically stable materials is being investigated as a means for further improvement in fabrication consistency. SRNL has also investigated altering the reference electrode design to extend the service life. The new design of the interior of the reference electrode casing creates a longer, more tortuous path between the junction material and the electrode sensing wire. A finite element model was used to optimize the design without adversely impacting the circuit resistance of the electrode during the measurements, thus preserving the measurement accuracy while enhancing the service life. The inner chamber back fill materials are also critical to the performance of the reference electrode. Materials that are resistant to intruding tank waste and provide a conductive path to the sensing wire were investigated. Gel and powder materials that are interspersed with a conductive chloride bearing material were tested for their influence on diffusion and electrode resistance. All the investigated materials and components will be assembled, with collaboration from commercial vendors, to fabricate the initial prototypes. Accelerated testing of the prototypes will be initiated in Year 2 of the program and will be completed in Year 3. A recommendation on the materials of construction and the design of the new robust reference electrode will be presented to the Hanford tank farm facility.

Sykes, Kiana [Savannah River National Laboratory (↗