Search NASA⌕ Search

SEARCH · Search NASA

Results for “Prelithiated Anode”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Li 3– x Zr x (Ho/Lu) 1– x Cl 6 Solid Electrolytes Enable Ultrahigh-Loading Solid-State Batteries with a Prelithiated Si Anode

We report two new families of lithium metal chloride solid electrolytes Li 3–x Zr x (M) 1–x Cl 6 (0 ≤ x ≤ 0.8; M = Ho or Lu) with ionic conductivities of up to 1.8 mS cm –1 and a low activation energy of 0.34 eV. Structural elucidation via high-resolution neutron diffraction determines the Li ion distribution in trigonal Li 3 HoCl 6 , orthorhombic-I Li 3 LuCl 6 , and orthorhombic-II Li 2.4 Zr 0.6 (Ho/Lu) 0.4 Cl 6 . The last compound exhibits well-connected Li-ion pathways and abundant Li-ion carriers/vacancies to promote diffusion. All-solid-state batteries with Li 2.6 Zr 0.4 (Ho/Lu) 0.6 Cl 6 solid electrolytes and NCM85 cathodes exhibit stable cycling up to 4.6 V vs Li + /Li, which is even preserved up to 4.8 V. Stable cathode interphases are formed for both electrolytes upon cycling to 4.3, 4.6, and 4.8 V cutoff potentials, as identified by a ToF-SIMS analysis. Solid-state cells with a prelithiated Li 0.7 Si anode exhibit a significantly increased initial coulombic efficiency of 94.5% compared to Si and a high areal capacity of up to 16.3 mAh·cm –2 .

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High-performance all-solid-state Li–S batteries enabled by an all-electrochem-active prelithiated Si anode

The development of all-solid-state Li–S batteries has been greatly impeded by dendrite growth and dendrite penetration, which are both related to the Li metal anode. As a compromised alternative, we report lithium silicide (Li x Si) as a dendrite-free and high-capacity anode with Li source. Here, the as-synthesized Li x Si is relatively soft, highly electronically conductive, and with a high Li diffusivity. These distinctive properties make Li x Si anode viable as an “all-electrochem-active” electrode (consisted of 100 wt.% Li x Si). Compared with the typical composite electrode, the all-electrochem-active electrode not merely maximizes the electrode-level energy density but also minimizes the electrolyte-related interfacial degradation. Li x Si symmetric cell demonstrates a reversible cycling at 4 mA cm –2 for over 320 h. Stress change and morphological evolution of the Li x Si electrode are investigated upon dealloying/alloying. When paired with a S cathode (active mass loading of 3 mg cm –2 ), Li x Si–S full cell shows a good cycling behavior over 500 cycles and rate performance (69% capacity retained at 1.2C) even at 25 °C.

25 ENERGY STORAGE↗

Mitigation of rapid capacity decay in silicon-LiNi 0.6 Mn 0.2 Co 0.2 O 2 full batteries

Silicon (Si)-based materials have been considered as the most promising anode materials for high-energy-density lithium-ion batteries because of their higher storage capacity and similar operating voltage, as compared to the commercial graphite (Gr) anode. But the use of Si anodes including silicon-graphite (Si-Gr) blended anodes often leads to rapid capacity decay in Si-Gr/LiNixMnyCo z O 2 (x+y+z=1) full cells, which has been attributed to surface instability of the Si component. In addition to stabilizing the surface, this work investigates the potential of the Si-Gr blended anodes in a full-cell configuration and its impact on the capacity contribution from active components. Using dQ/dV plots of the full cells, a powerful but simple-to-implement differential potential approach is developed to decouple the capacity contribution and degradation from the graphite and silicon components. Data collected from three-electrode cells confirm the results from the differential potential approach, which suggests a voltage slippage to a higher voltage at the blended anode side. Additionally, the voltage slippage causes a reduced utilization of the Gr component and exacerbates side reactions between the Si-Gr anode and carbonate electrolytes. Furthermore, based on these failure mechanisms, we adopted a mitigation strategy to tune the open circuit voltage of the prelithiated anode while stabilizing the surface. As a result, the full cells with the modified Si-Gr anodes (mass loading, 2.5 mAh/cm 2 ) offer a highly reversible full-cell energy density of 390 Wh/kg (based on the mass of both anode and cathode materials in a full cell) with a cycling CE of 99.9% over 200 cycles.

25 ENERGY STORAGE↗

High Throughput Solvent-free Manufacturing of Battery Electrodes

The project goal is to develop and demonstrate an advanced solvent-free lithium-ion battery electrode process through proposed Advanced Dry Electrode Process (ADEP) equipment, which is expected to exhibit a better binder fibrillization and high throughput and suitable for high performance electrode manufacturing, and commonize the anode and cathode dry processing equipment, supply chain and operation for lithium-ion battery OEMs for replacing the solvent-based slurry casting. Our proposed approach will facilitate low-cost battery production by addressing the following gaps in present dry electrode processing: • Extend the dry electrode fabrication process to lithium-ion battery anode manufacturing • Increase the active material content for anodes and cathodes • Intensify the process through improved mixing, powder rheology and surface modifications • Enable processing of next-generation electrode materials that are not stable to solvent or ambient air exposure. The project objectives include the development of anode-compatible binder and binder fibrillization promoter for low irreversible capacity loss, low electrode binder content yet higher film mechanical strength, and the optimization of solvent-free anode and cathode process for low cost (>60% electrode cost reduction), high performance (10% increase in energy density without sacrificing cycle life) and high throughput to enable next generation lithium-ion battery electrode production. Solvent-free electrode manufacturing will also enable next-generation cell designs based on prelithiated anodes or solid-state electrolytes.

25 ENERGY STORAGE↗

Solid‐State Prealkylation of Electrode Architectures (SPEAR): Direct Control of Prelithiation Levels in Silicon Anodes and Electrochemical Cycling

The Solid-state Prealkylation of Electrode ARchitectures (SPEAR) is different than traditional electrochemical prealkylation processes. Through SPEAR, alkylation is driven by solid-state diffusion without the simultaneous SEI formation concomitant with polarization. Here, we investigate the prelithiation of 80 wt. % Si-based anodes to varying amounts (up to Li 1.38 Si) to understand the trade-off between improved Li capacity and expansion-induced stress. Through dilatometry, we found that solid-state lithiation led to filling of the electrode pores through silicon expansion. This swelling changed the SEI formation process and accessibility of the silicon compared to an electrochemically lithiated electrode. Indeed, optimal prelithiation to Li 0.82 Si increases the initial C/3 cycling capacity post-SEI formation up to 43%, consistent with deeper Si activation through the electrode bulk. Prelithiation and cycling cells prelithiated beyond Li 0.82 Si results in a state of charge (SOC) close to 100% which facilitates parasitic degradation mechanisms and volume expansion of the Si electrode. The results demonstrate a pathway to modify silicon activation/SEI formation to enable high-energy electrodes.

Musgrove, Amanda L. [Oak Ridge National Laboratory↗

Li2O-Based Cathode Additives Enabling Prelithiation of Si Anodes

Low first-cycle Coulombic efficiency is especially poor for silicon (Si)-based anodes due to the high surface area of the Si-active material and extensive electrolyte decomposition during the initial cycles forming the solid electrolyte interphase (SEI). Therefore, developing successful prelithiation methods will greatly benefit the development of lithium-ion batteries (LiBs) utilizing Si anodes. In pursuit of this goal, in this study, lithium oxide (Li2O) was added to a LiNi0.6Mn0.2Co0.2O2 (NMC622) cathode using a scalable ball-milling approach to compensate for the initial Li loss at the anode. Different milling conditions were tested to evaluate the impact of particle morphology on the additive performance. In addition, Co3O4, a well-known oxygen evolution reaction catalyst, was introduced to facilitate the activation of Li2O. The Li2O + Co3O4 additives successfully delivered an additional capacity of 1116 mAh/gLi2O when charged up to 4.3 V in half cells and 1035 mAh/gLi2O when charged up to 4.1 V in full cells using Si anodes.

25 ENERGY STORAGE↗

Advanced Anode Manufacturing through Ultra-Thin Li Deposition

During the program's tenure, Applied Materials delivered high-quality (>99.9%) ultra-pure thin lithium metal in sheets and in roll to roll (R2R) formats to program partners for testing, cell builds and evaluation. The thickness range of the deposited Lithium can be controlled between 1-20 μm (<3% nonuniformity). A second R2R tool was commissioned for Li processing and inline CO 2 passivation module was validated. Additionally, S2S deposition tools were used to explore five different surface protection materials for Li-metal. One surface passivation chemistry was down selected for testing and showed improved performance. Key results are summarized in this final report.

25 ENERGY STORAGE↗

Insights into Chemical Prelithiation of SiO x /Graphite Composite Anodes through Scanning Electron Microscope Imaging

Initial Coulombic efficiency (ICE) is critical for determining the energy density of lithium-ion batteries (LIBs) used for practical applications; however, it is typically disregarded in anode research. We used SiO x and graphite composite anodes for commercial lithium-ion batteries in our preliminary research to achieve a balance between ICE, capacity, and cycling life. ICE reached 88%; however, it needs further improvement for commercial applications. Prelithiation is a process that involves the introduction of extra lithium ions into LIBs during their manufacturing to enhance the overall performance of the LIBs. We applied a chemical prelithiation method on our SiO x /graphite composite anodes, which comprised 95 wt % of the active material mass loading on the electrode. The ICE increased from 88% to 98% using an aryllithium reagent impregnation method within 2 min of prelithiation. The anode’s specific capacity density, rate, and cycle performance also significantly improved. Scanning electron microscopy (SEM) imaging enhanced by an osmium tetroxide staining method indicated that the P-anode contained a stable solid electrolyte interface (SEI) layer after the prelithiation process and cycling electrochemical test. The P-anode’s stable charge differential peak over 500 cycles also showcases a robust artificial SEI layer that was generated by the prelithiation procedure. Here, this prelithiation process has significant potential for adoption in the LIB industry’s current electrode manufacturing process.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Prelithiation of Lithium Peroxide for Silicon Anode: Achieving a High Activation Rate

The use of lithium peroxide (Li2O2) as a cost-effective low-weight prelithiation cathode additive was successfully demonstrated. Through a series of studies on the chemical stability of Li2O2 and the activation process of Li2O2 on the cathode, we revealed that Li2O2 is more compatible with conventional electrolyte and cathode laminate slurry than lithium oxide. Due to the significantlysmaller size of commercial Li2O2, it can beused directly as a cathode additive. Moreover, the activation of Li2O2 on the cathode leads to the impedance growthof the cathode possibly resulting from the release of dioxygen andevacuation of Li2O2 inside the cathode. Withthe introduction of a new Li2O2 spread-coatingtechnique on the cathode, the capacity loss was suppressed. Si||NMCfull cells using Li2O2 spread-coated cathodedemonstrated a highly promising activation rate of Li2O2 and significantly enhanced specific capacity and cyclingstability compared to the uncoated full cells.

cathode additive↗

Free-standing ultrathin lithium metal–graphene oxide host foils with controllable thickness for lithium batteries

Thin (≤20 μm) and free-standing Li metal foils would enable precise prelithiation of anode materials and high-energy-density Li batteries. Existing Li metal foils are too thick (typically 50 to 750 μm) or too mechanically fragile for these applications. Here, we developed a facile and scalable process for the synthesis of an ultrathin (0.5 to 20 μm), free-standing and mechanically robust Li metal foil within a graphene oxide host. In addition to low areal capacities of ~0.1 to 3.7 mAh cm –2 , this Li foil also has a much-improved mechanical strength over conventional pure Li metal foil. Our Li foil can improve the initial Coulombic efficiency of graphite (93%) and silicon (79.4%) anodes to around 100% without generating excessive Li residue, and increases the capacity of Li-ion full cells by 8%. In conclusion, the cycle life of Li metal full cells is prolonged by nine times using this thin Li composite anode.

25 ENERGY STORAGE↗

Designing Li 4 Ti 5 O 12 /LiMn 2 O 4 Cells: Negative-to-Positive Ratio and Electrolyte

Li 4 Ti 5 O12/LiMn2O 4 (LTO/LMO) system is a promising candidate for behind-the-meter storage (BTMS) applications due to its critical-material-free chemistry exhibiting good safety and long lifetime. In this paper we design LTO/LMO cells to mitigate their major degradation mechanism, loss of Li inventory, and improve their long-term cyclability. First, LMO electrodes with different loadings (2.61, 3.29, and 4.26 mAh cm -2 ) are paired with an LTO electrode (3.35 mAh cm -2 ) to create varying negative-to-positive ratios (N/P>1, =1, and <1). Additionally, conventional ethylene carbonate (EC)/ethyl methyl carbonate (EMC) mixture electrolyte and safety enhanced EC-only electrolyte are examined. We show that storing additional Li inventory in the cathode (i.e., using a thicker electrode and having N/P<1) is a convenient method to enhance the capacity retention of LTO/LMO cells, but only if the electrode utilization is not limited by the Li + ion transport. For systems that suffer from limited transport properties, prelithiating the anode will be more effective since LTO (~165 mAh g -1 LTO ) can store the same amount of capacity using less material compared to LMO (~100 mAh g -1 LMO ). In this work, we demonstrate how the electrolyte properties and the electrode thickness of LTO/LMO cells can be designed to enhance their performance.

25 ENERGY STORAGE↗

Failure analysis and design principles of silicon-based lithium-ion batteries using micron-sized porous silicon/carbon composite

Significant progresses have been made to overcome the fundamental challenges in silicon (Si)-based lithium-ion batteries (LIBs). However, much less work have been reported on the design and failure analysis these batteries for practical applications. In this work, we analyzed various cell design parameters affecting the performance of pouch cells using micron-sized porous Si with nano-pore structure and coated by pitch-carbon (p-Si/C). The correlation among particle level, electrode level, and cell level properties, especially the effect of electrode density on the volumetric capacity density of Si anode and full batteries have been systematically investigated. It is found that the corrosion of p-Si/C particle surface is the main failure mechanisms on the eventual capacity loss, while Li plating on anode electrode surface is the main reason for the fast capacity loss in later stage of cycling. The volumetric capacity of Si anode highly depends on both electrode density and the Si content. Moreover, the prelithiation of Si anodes is found to increase energy density while decreasing cycle life of Si-based full cells. Finally, the pathways and strategies for adoption of micron-sized p-Si/C anodes in LIBs have been proposed for their practical applications.

25 ENERGY STORAGE↗

Implanting Transition Metal into Li 2 O-Based Cathode Prelithiation Agent for High-Energy-Density and Long-Life Li-Ion Batteries

Compensating the irreversible loss of limited active lithium (Li) is essentially important for improving the energy-density and cycle-life of practical Li-ion battery full-cell, especially after employing high-capacity but low initial coulombic efficiency anode candidates. Introducing prelithiation agent can provide additional Li source for such compensation. Herein, we precisely implant trace Co (extracted from transition metal oxide) into the Li site of Li 2 O, obtaining (Li 0.66 Co 0.11$\square$0.23 ) 2 O (CLO) cathode prelithiation agent. Further, the synergistic formation of Li vacancies and Co-derived catalysis efficiently enhance the inherent conductivity and weaken the Li-O interaction of Li 2 O, which facilitates its anionic oxidation to peroxo/superoxo species and gaseous O 2 , achieving 1642.7 mAh/g ~Li2O prelithiation capacity (≈980 mAh/g for prelithiation agent). Coupled 6.5 wt % CLO-based prelithiation agent with LiCoO 2 cathode, substantial additional Li source stored within CLO is efficiently released to compensate the Li consumption on the SiO/C anode, achieving 270 Wh/kg pouch-type full-cell with 92 % capacity retention after 1000 cycles.

25 ENERGY STORAGE↗

Synthesizing High-Capacity Oxyfluoride Conversion Anodes by Direct Fluorination of Molybdenum Dioxide (MoO 2 )

High-capacity metal oxide conversion anodes for lithium-ion batteries (LIBs) are primarily limited by their poor reversibility and cycling stability. In this study, a promising approach has been developed to improve the electrochemical performance of a MoO 2 anode by direct fluorination of the prelithiated MoO 2 . The fluorinated anode contains a mixture of crystalline MoO 2 and amorphous molybdenum oxyfluoride phases, as determined from a suite of characterization methods including X-ray diffraction, Raman spectroscopy, and X-ray photoelectron spectroscopy, and scanning transmission electron microscopy. Electrochemical measurements indicate that fluorination facilitates the conversion reaction kinetics, which leads to increased capacity, higher coulombic efficiency, and better cycling stability as compared to the nonfluorinated samples. Overall, these results suggest that fluorination after prelithiation not only favors formation of the oxyfluoride phase but also improves the lithium-ion diffusivity and reversibility of the conversion reaction, making it an attractive approach to address the problems of conversion electrodes. These findings provide a new route to design high-capacity negative electrodes for LIBs.

25 ENERGY STORAGE↗

Prelithiated SiO x /Graphite-NMC811 Cells: Capacity Loss, Impedance Rise and Hidden Degradation Pathways Revealed Using Three-Electrode Diagnostics

Electrodes containing SiO x /graphite (Gr) materials are attractive as anodes for high-energy lithium-ion batteries. However, their mechanical deformation, electrochemical response, and impedance evolution during long-term cycling are strongly coupled, complicating accurate diagnosis of performance fade mechanisms. In this work, the behavior of electrochemically prelithiated SiO x /Gr anodes paired with NMC811 cathodes is systematically investigated using techniques that include in-situ dilatometry, three-electrode electrochemistry, and multiscale post-cycling microscopy. The SiO x /Gr electrode exhibits a maximum expansion of 49% upon lithiation to 10 mV vs Li + /Li, with 84% of the expansion and 91% of the capacity being reversible. In full cells, relatively stable cycling with only 12% capacity fade over 500 cycles is observed. Three-electrode experiments reveal cell-level impedance growth, which is dominated by the NMC811 cathode: the SiO x /Gr anode exhibits minimal net impedance rise and an initial impedance decrease at low potentials. Despite this apparent electrochemical stability, cross-sectional SEM, PFIB tomography, and cryo-STEM reveal irreversible anode thickening caused by the accumulation of an inorganic-rich solid electrolyte interphase (SEI) permeating the anode bulk. Electrode potential-shift analysis further demonstrates that Li + ions released from lithium reservoirs in the prelithiated anode mask true lithium inventory loss during aging. These results demonstrate that low-expansion SiO x /Gr anodes can simultaneously exhibit favorable cycling and impedance metrics while undergoing substantial, hidden degradation, underscoring the importance of electrode-resolved diagnostics for evaluating prelithiated silicon-based anodes.

25 ENERGY STORAGE↗

Long-term cyclability of Li 4 Ti 5 O 12 /LiMn 2 O 4 cells using carbonate-based electrolytes for behind-the-meter storage applications

Li 4 Ti 5 O 12 /LiMn 2 O 4 (LTO/LMO) chemistry was evaluated as a potential candidate for behind-the-meter storage (BTMS) applications. Its long-term cycle performance at 45 °C was tested using ethylene carbonate (EC) and propylene carbonate (PC) solvent electrolytes. Over 1000 cycles, LTO/LMO cells exhibited ~80% capacity retention and Coulombic efficiency higher than 99.96%. Electrochemical test results showed the major degradation mode of LTO/LMO cells arises from continuous electrolyte decomposition at the LTO anode and loss of Li inventory. EC and PC electrolytes created distinct surface layers, where the EC reduction products were more effective in passivating the LTO electrode surface. Dissolution and migration of Mn from the cathode was probed as Mn 2+ species distributed throughout the surface layer at the anode. By utilizing a prelithiated LTO electrode, the LTO/LMO cell performance was significantly enhanced with EC electrolyte. On the other hand, PC electrolyte resulted in accelerated electrolyte decomposition at the lithiated LTO surface due to the lack of surface passivation. Thus, mitigating parasitic reactions at the LTO electrode is the key to developing successful LTO/LMO cells.

25 ENERGY STORAGE↗

Direct Prelithiation of Silicon-Based Composite Electrodes via Island-like Thermal Evaporation

Irreversible losses of Li during solid electrolyte interface (SEI) conditioning is a key contributor to the lower specific capacities observed in silicon-containing Li-ion batteries. Herein, thermal evaporation of between 1 and 20 µm of Li onto Si-based composite anodes has been investigated as a prelithiation method to account for such losses. To account for mechanical strain caused by Li-Si alloying during the deposition, a stainless-steel mesh is applied to the electrodes before prelithiation to form “island-like” deposition on the electrode surface. The open circuit potential was also found to decrease as a function of increased Li evaporation, consistent with the potentials of electrochemically prepared LixSi alloys. Prelithiating to account for irreversible Li losses to SEI formation resulted in full cells with a 15.8% increase in initial coulombic efficiency and a 47.8% reduction in irreversible capacity loss after SEI formation cycling. Subsequent C/3 cycling showed up to a 62.9% increase in specific capacity in prelithiated cells. X-ray photoelectron spectroscopy (XPS) revealed differences in the SEI composition that was formed by electrochemical cycling and reactively formed in prelithiated cells upon exposure to Gen2 + 3% FEC electrolyte. The reactively formed SEI from the spontaneous reaction with lithiated silicon was carbonate-rich while the electrochemical SEI formation showed significantly more LiPFx species, which could play a role in overall cycling performance.

Musgrove, Amanda↗