Microscopy Studies of the Catalyst Inks for PEM Fuel Cells

The microstructure of the catalyst layer in proton exchange membrane fuel cells (PEMFC) is one of the key factors that determine fuel cell performance. The ink preparation, including dispersion solvent, mixing time, and mixing power, are among the less reported parameters that would influence the ionomer distribution on the catalyst surface and the continuity of the carbon network. In this work, novel characterization approaches have been used to investigate the effect of the Pt/C catalyst ink preparation conditions on the morphology and structures of the catalyst layer. Microscopy analysis revealed that longer mixing time led to better performing electrode structures than shorter mixing time. The longer mixing time enabled improved continuity of the ionomer network and high porosity in the cathode layer that contributes to improved proton conductivity and mass transport. This has been reflected in performance and durability tests, where the electrode made from a 5-day catalyst ink displayed improved performance compared to the one made from a 3-day ink. Durability studies showed 26% and 43% loss of the initial mass activity for 5 days and 3 days mixing, respectively. Finally, in addition, the catalyst layer prepared with ethylene glycol as the dispersion solvent showed better durability than water/1-propanol based solution.

25 ENERGY STORAGE↗

PFSA-Ionomer Adsorption to C and Pt/C Particles in Fuel-Cell Inks

Catalyst inks used to make fuel-cell electrodes consist of Pt/C catalyst particles and a perfluorosulfonic acid (PFSA) ionomer dispersed in water/alcohol solvent mixtures. PFSA ionomer in the ink adsorbs to the surface of the catalyst particles, dictating the dispersion colloid properties. Following adsorption, the subsequent distribution of excess nonadsorbed ionomer in the ink then governs the final structure of the electrode. Here, we characterize the adsorption of the PFSA ionomer onto Pt/C catalyst particles. PFSA adsorption is largely irreversible. Adsorbed sulfonic-acid moieties impart a negative charge on the catalyst surface, causing electrostatic repulsion between the free ionomer in solution and the ionomer-covered Pt/C particle surface. The amount of adsorption is limited by the resulting electrostatic charge that grows as more ionomer adsorbs, and the catalyst surface becomes more negatively charged. Attenuating electrostatic repulsion by increasing the ink ionic strength promotes ionomer adsorption. Electrostatically limited adsorption is observed, irrespective of the solvent water/n-propanol ratio or the catalyst particle porosity and Pt loading. Experimentally measured ionomer adsorption isotherms are well predicted by a Smoluchowski-based kinetic adsorption model, in which the electrostatic energy barrier for adsorption is predicted from DLVO theory. These findings help to unravel the complex phenomena within these colloidal dispersions, allowing for subsequent tailoring of inks to optimize fuel-cell electrode structure and performance.

Adsorption↗

Dictating Pt-Based Electrocatalyst Performance in Polymer Electrolyte Fuel Cells, from Formulation to Application

In this study, in situ electrochemical diagnostics designed to probe ionomer interactions with platinum and carbon were applied to relate ionomer coverage and conformation, gleaned from anion adsorption data, with O 2 transport resistance for low-loaded (0.05 mg Pt cm -2 ) platinum-supported Vulcan carbon (Pt/Vu)-based electrodes in a polymer electrolyte fuel cell. Coupling the in situ diagnostic data with ex situ characterization of catalyst inks and electrode structures, the effect of ink composition is explained by both ink-level interactions that dictate the electrode microstructure during fabrication and the resulting local ionomer distribution near catalyst sites. Electrochemical techniques (CO displacement and ac impedance) show that catalyst inks with higher water content increase ionomer (sulfonate) interactions with Pt sites without significantly affecting ionomer coverage on the carbon support. Surprisingly, the higher anion adsorption is shown to have a minor impact on specific activity, while exhibiting a complex relationship with oxygen transport. Ex situ characterization of ionomer suspensions and catalyst/ionomer inks indicates that the lower ionomer coverage can be correlated with the formation of large ionomer aggregates and weaker ionomer/catalyst interactions in low-water content inks. These larger ionomer aggregates resulted in increased local oxygen transport resistance, namely, through the ionomer film, and reduced performance at high current density. In the water-rich inks, the ionomer aggregate size decreases, while stronger ionomer/Pt interactions are observed. The reduced ionomer aggregation improves transport resistance through the ionomer film, while the increased adsorption leads to the emergence of resistance at the ionomer/Pt interface. Overall, the high current density performance is shown to be a nonmonotonic function of ink water content, scaling with the local gas (H 2 , O 2 ) transport resistance resulting from pore, thin film, and interfacial phenomena.

30 DIRECT ENERGY CONVERSION↗

Effects of Ink Formulation on Construction of Catalyst Layers for High-Performance Polymer Electrolyte Membrane Fuel Cells

Rational design of catalyst layers in a membrane electrode assembly (MEA) is crucial for achieving high-performance polymer electrolyte membrane fuel cells. Establishing a clear understanding of the property (catalyst ink)–structure (catalyst layer)–performance (MEA) relationship lays the foundation for this rational design. Here, a synergistic approach was taken to correlate the ink formulation, the microstructure of catalyst layers, and the resulting MEA performance to establish such a property–structure–performance relationship. The solvent composition (n-PA/H 2 O mixtures) demonstrated a strong influence on the performance of the MEA fabricated with an 830-EW (Aquivion) ionomer, especially polarization losses of cell activation and mass transport. The performance differences were studied in terms of how the solvent composition affects the catalyst/ionomer interface, ionomer network, and pore structure of the resulting catalyst layers. The ionomer aggregates mainly covered the surface of catalyst aggregates acting as oxygen reduction reaction active sites, and the aggregate sizes of the ionomer and catalyst (revealed by ultrasmall angle X-ray scattering and cryo-transmission electron microscopy) were dictated by tuning the solvent composition, which in turn determined the catalyst/ionomer interface (available active sites). In n-PA/H 2 O mixtures with 50~90 wt % H 2 O, the catalyst agglomerates could be effectively broken up into small aggregates, leading to enhanced kinetic activities. The boiling point of the mixed solvents determined the pore structure of ultimate catalyst layers, as evidenced by mercury porosimetry and scanning electron microscopy. For mixed solvents with a higher boiling point, the catalyst–ionomer aggregates in the ink tend to agglomerate during the solvent evaporation process and finally form larger catalyst–ionomer aggregates in the ultimate catalyst layer, resulting in more secondary pores and thus lower mass transport resistance. Both the enlarged catalyst/ionomer interface and appropriate pore structure were achieved with the catalyst layer fabricated from an n-PA/H 2 O mixture with 90 wt % H 2 O, leading to the best MEA performance.

25 ENERGY STORAGE↗

Influence of Pt-Metal Alloy Catalysts with Various Ionomers on Oxygen Reduction Reaction in Fuel Cell Application

Pt-M/C (M = Co, Ni, Mn, etc.) alloy catalysts exhibit superior oxygen reduction reaction (ORR) activity compared to pure Pt/C, leading to a high energy efficiency in hydrogen fuel cells. However, many Pt-M/C alloy catalysts were synthesized and evaluated at the lab scale in model test-bed systems like rotating disc electrodes, which don't always correlate to performance within a fuel cell system; there is a clear need to evaluate catalysts in electrodes that can be prepared at industrially relevant scales to evaluate how factors like ink formulation can greatly affect device-level of fuel cell performance. Herein, three commercial Pt-M/C alloy catalysts (two Pt-Co/C and one Pt-Ni/C) were comprehensively characterized by various techniques. The results show that the average particle sizes of the three catalysts are close to 5 nm; the atomic ratio of Pt/M is around 4; and the M was successfully embedded into Pt lattice, resulting in the positive shift of Pt 4f in XPS spectra and XRD patterns. These catalytic materials were incorporated into 9 different cathode catalyst layers (CCLs) with three kinds of ionomers (Nafion D2020, high oxygen permeability ionomer (HOPI), and Aquivion D79-25BS), and their performance in proton exchange membrane fuel cells (PEMFCs) were investigated. The results demonstrate that the Pt-Co/C catalysts possess a higher mass activity (MA) than Pt-Ni/C; the cathodes with Nafion ionomer provide the highest MA while electrodes with Aquivion ionomer showed the lowest activity, attributed to poor H+ conductivity resulting from suboptimal ionomer incorporation. Finally, these alloys were shown to exceed DOE targets for MA and H2/Air performance reported in the recent publications at beginning of life and after 90k cycle catalyst AST protocol. This study provides valuable performance benchmarks for these materials guiding future Pt-M/C catalyst design and material integration for heavy duty PEMFC applications.

08 HYDROGEN↗

Designing the Platinum Catalyst Layer for Improved Performance and Durability in Anion Exchange Membrane Water Electrolysis

To lower the cost of hydrogen produced by anion exchange membrane water electrolysis (AEMWE), it is critical to reduce the use of platinum group metal (PGM) catalysts within the device. While iridium has been successfully replaced with PGM-free catalysts at the anode, platinum-based (Pt) cathode catalysts are still required to meet the activity and durability targets. This study investigates the impact of commercial Pt/C catalyst loading, ionomer type and content, and electrode fabrication method on the cathode catalyst layer properties and AEMWE performance with the aim of determining the feasibility of reduced Pt loadings. While increased Pt loading is found to improve beginning-of-life performance, the effects are minimal above 0.6 mg/cm 2 . Ink characterization shows that ionomer type and content affect the ink stability, particle size, and percent of unbound ionomer, which further impact the homogeneity of the sprayed catalyst layers. The 5% PiperION cathode exhibited the highest performance, which may be attributed to a balance between the small particle size and the low proportion of unbound ionomer, minimizing kinetic and transport losses. Theoretical calculations show that the ionomers interact differently with the Pt surface, causing different surface charges and water adsorption strength and activating different mechanisms for hydrogen evolution. Pt-PiperION lowered the enthalpy of water-splitting by 0.1 eV compared to Pt alone and allowed for equal site access between adsorbed H* and OH* (both adsorbed at circa −2.2 eV). Although catalyst-coated membrane (CCM) fabrication techniques are desirable for scale-up, no performance enhancement is observed compared with the catalyst-coated substrate approach. Durability, as measured by degradation rates, Pt loss, and catalyst layer restructuring, was found to improve with increased Pt loadings, higher ionomer content, and CCM architectures. These findings provide important insight into the significant role of the cathode in AEMWE and strategies for maintaining the performance with low Pt loading or PGM-free catalysts.

08 HYDROGEN↗

Influence of Coating Method on the Performance of Roll-to-Roll Coated PEM Fuel Cell Catalyst Layers

As production of fuel cell vehicles and power systems increases there is a need to understand the process science of fuel cell manufacturing. Industrial production of polymer electrolyte membrane fuel cell (PEMFC) electrodes will rely on continuous roll-to-roll (R2R) coating methods to meet the rates needed for mass production. There are a variety of coating methods that could be used to coat catalyst layers. The different physics of each method may result in different morphologies and performance. Here we present the results of a study comparing fuel cell catalyst layers coated using two R2R coating methods: slot-die and gravure. These two methods were selected because the physics of applying the liquid to the substrate is very different between the two cases. Pt/C catalysts layers were coated directly onto carbon-fiber gas diffusion media to create gas diffusion electrodes (GDEs), without the use of a decal transfer process. These GDEs were assembled into membrane electrode assemblies (MEAs) by hot pressing to Nafion membranes. In situ performance and other electrochemical diagnostics were used to determine the influence of coating method on catalyst layer electrochemical properties. Electron microscopy was utilized to understand the influence of coating method on electrode morphology and its influence on electrochemical properties. We also explored the influence of solvent ratio to understand the potential coupling between ink formulation and coating methodology.

DIRECT ENERGY CONVERSION,MATERIALS SCIENCE↗

Integration of a high oxygen permeability ionomer into polymer electrolyte membrane fuel cell cathodes for high efficiency and power density

In this work, we present a study on the integration of a high oxygen permeability ionomer (HOPI) with high durability carbon supported platinum (Pt/C) catalysts to prepare cathode catalyst layers (CCLs) for polymer electrolyte membrane fuel cells (PEMFCs). A key motivation is the production of PEMFCs with high efficiency and durability for heavy-duty fuel cell vehicles. Our results from integrating a pre-commercial HOPI with robust, state-of-the-art catalysts with medium and low surface area carbon supports show significant increases in specific activities (67% increase over the standard commercial ionomer) at low current densities and reduced oxygen (O 2 ) transport resistances (R O2 ’s) at high current densities, enabling both higher efficiency and peak power density. The reduction in the R O2 with the HOPI is most significant at low relative humidity (RH), due to its more rigid backbone structure resisting compaction at lower water contents. In our ink optimization analysis, we show that the HOPI in this study achieves its peak performance with an ionomer to carbon ratio (I/C) of 0.6 and a moderately alcohol-rich ink solvent when fabricating catalyst layers by the decal method with an automatic wet film coater.

08 HYDROGEN↗