At least 19 records

Interface morphology and dislocation-mediated processes during rapid solidification of thin films

Rapid solidification experiments have, in recent years, revealed a wealth of new microstructural phenomena that suggest a strong connection between the kinetics of solidification and the crystalline structures that emerge as a result. In this work, we investigate the interplay between interface morphology and defect-mediated processes during rapid solidification conditions using a Phase Field Crystal (PFC) model, enabling us to simultaneously and efficiently explore the physics of solidification and elasto-plasticity in the formalism of a single-field theory. We predict that there are two mechanisms by which dislocations emitted directly from the solid–liquid interface induce orientation gradients as well as the formation of subgrain boundaries within a single solidifying cell. We relate these mechanisms to the morphology of the moving solid–liquid interface and identify a suitable control parameter in the PFC model with which we can go between said morphologies by effectively changing the relative strength of the capillary length and kinetic coefficients of the solid–liquid interface. Thus, we are able to provide mechanistic explanations for several microstructural features (with an emphasis on orientation gradients and subgrain boundaries) observed during the rapid solidification of pure materials. We also provide a simple explanation for the formation of “jagged” subgrain boundaries, which is consistent with our experimental observations in rapidly solidified samples of Aluminum, whose mechanisms have thus far been unknown.

Interface morphology

Splat Quenching as a High Throughput Rapid Solidification Testing Method for Developing Additive Manufacturing Alloys

Splat quenching as a high throughput rapid solidification screening tool is evaluated. Samples were made using known alloys (SS316, IN625, Ti-5553) to evaluate and establish the microstructures for a variety of alloy systems as well as the predicted cooling rates. The samples are inductively heated and levitated prior to being struck between two platens that produce a high contact pressure and a thin sample resulting in cooling rates on the order of 10 6 to 10 7 K/s. Process parameters were evaluated with analytical models in addition to numerical simulations to provide an effect of process variables such as substrate material, melt superheat, and platen velocity on the resulting solidification. The splat thickness was found to be controlled by platen velocity, melt superheat, as well as the feedstock volume. The sample thickness is the key controlling factor for varying the average cooling rate experienced by the splat quenched sample. The splat quenching techniques can reach regions of rapid solidification space that meet and exceed laser and electron beam techniques across the sample. In conclusion, the results of the study provide a useful foundation in understanding the splat quenching technique and its potential as a low effort tool to explore rapid solidification effects on alloys.

Alloy Design

Rapid Solidification Effects in Additively Manufactured Si and SiGe Compositions

SiGe alloys have a proven track record as robust high-temperature thermoelectric materials, powering NASA missions like SNAP-10A, LES-9, and Voyager 1 and 2. Enhancing thermoelectric efficiency hinges on minimizing thermal conductivity while preserving electrical conductivity. Rapid solidification via LPBF can generate microstructural features such as subgrain cellular boundaries and twinning, which may help reduce thermal conductivity while preserving semiconducting behavior. Here, this study investigates the potential of laser powder bed fusion (LPBF) additive manufacturing to fabricate nanostructured Si and SiGe thermoelectric materials. High cooling rates (10 5 to 10 7 K/s) rates inherent to the LPBF process are conducive to forming such nanostructures. Moreover, this fabrication technique could also be suitable for fabricating complex geometries needed to achieve improved device level performance. Process mapping of commercial Si powder with irregular morphology was first performed to understand the LPBF processing behavior of this semiconductor material. Subsequent studies included in-house synthesized B-doped (p-type) Si7 8 Ge 22 spherical powder that was produced via ultrasonic atomization. Scan strategies involved multiple laser exposures to mitigate solidification cracking: a high density of >98% was achieved, but solidification cracking could not be fully eliminated. Subsequently, a high electrical resistivity (i.e., low conductivity) was observed, but the measured Seebeck coefficient, ∼230 μV/K @ 500 °C, proved that good semiconductor material was being fabricated. A subgrain cellular structure (5–10 μm) was observed as defined by Ge segregation to the intercellular boundaries. The remelting strategies helped lower the cooling rates in processing SiGe, but this still resulted in high residual stresses, which induced a remarkably high density of twins (78–95%) to accommodate the deformation. This unique grain structure offers an avenue for phonon scattering and potential improvements in thermoelectric performance.

figure of merit

Evolution of dislocations during the rapid solidification in additive manufacturing

Materials processed by fusion-based additive manufacturing (AM) typically exhibit relatively high dislocation densities, along with cellular structures and elemental segregation. This representative structural feature significantly influences material performance; however, post-mortem microstructure characterizations of AM materials cannot capture the dynamic evolution of dislocations during the manufacturing process, thereby offering limited mechanism-based guidance for further advancing AM techniques and facilitating the qualification and certification of AM products. In this study, we conduct operando high-energy synchrotron X-ray diffraction experiments on wire-laser directed energy deposition of 316 L stainless steel. Through a unique configuration, our operando synchrotron experiments semi-quantitatively probe the dislocation density in solid phases and their dynamic changes during solidification and subsequent cooling. By integrating this advanced synchrotron technique with multi-physics simulation, in-situ neutron diffraction, and multi-scale electron microscopy characterization, our mechanistic study aims to elucidate the effects of rapid cooling and subsequent thermal cycling on the dislocation generation and evolution.

36 MATERIALS SCIENCE

Microstructural evolution and phase stability in Nb-containing interstitial Fe-Mn-Co-Cr-C high-entropy alloys: An in-situ synchrotron X-ray diffraction study during laser melting

The influence of Nb on phase stability and microstructural evolution in an interstitial Fe-Mn-Co-Cr-C high-entropy alloy was investigated using in-situ synchrotron X-ray diffraction (SXRD) during laser melting. Scheil-Gulliver simulations predict the formation of σ and γ-f.c.c. phases in all three alloys, along with NbC in Nb-containing compositions. SXRD confirmed the presence of most predicted phases, but the σ phase was absent. Nb promotes crystallite refinement and increases dislocation density, though excessive additions reduce refinement efficiency due to solubility limits and secondary phase formation. Furthermore, Nb addition also enhances ε-h.c.p. phase formation by reducing stacking fault energy through NbC-induced carbon depletion. Analysis of intensity peak evolution reveals that Nb alters preferred grain orientations, reducing {111} γ intensity while enhancing {220} γ , leading to a more isotropic grain distribution. Overall, Nb plays a key role in phase selection, microstructure refinement, and preferred orientation evolution, allowing the tailored microstructure of high-entropy alloys via rapid solidification.

Interstitial high entropy alloys

Enhancing microsegregation during rapid directional solidification through ternary microalloying

The nano-cellular dendritic microstructure formed during rapid directional solidification in powder bed fusion additive manufacturing creates unique properties such as simultaneous improvement in strength and ductility. However, process control of microsegregation features remains challenging due to low sensitivity of critical solidification mechanisms to process parameters. This study leverages microalloying to achieve large changes in dendrite composition, microstructure, and interdendritic zone width during laser powder bed fusion without modifying process parameters. CALPHAD simulations predict that the addition of Zr significantly steepens the solidus line of the dilute Cu-Cr alloy system, leading to enhanced Cr rejection into the melt and greater than 95% reduction in solubility of Cr in the solidified Cu matrix. Experimental validation using time-of-flight secondary ion mass spectrometry and Kelvin probe force microscopy reveals that the ternary alloy containing 0.01 wt% Zr exhibited wider interdendritic regions compared to the binary, a significantly higher number of Cr-rich particles within interdendritic regions, near-complete ejection of oxygen impurities from the matrix, and greater nanoscale work function contrast. These features indicate more aggressive Cr segregation in the presence of Zr and a purer Cu matrix and provide a potentially robust method for engineering the nano-cellular dendritic solidification microstructure.

CALPHAD

Unravelling Microstructure Selection in an Additively Manufactured Eutectic High‐Entropy Alloy

High-entropy alloys (HEAs) are promising candidates for advanced structural applications due to their excellent mechanical properties. Additive manufacturing (AM), with its rapid solidification conditions, enables the creation of unique nonequilibrium microstructures. To fully leverage the synergy between AM and HEAs, understanding how processing affects structure and properties is essential. Here, how solidification rate influences microstructure evolution and phase transformation pathway in laser additively manufactured AlCrFe2Ni2 eutectic HEAs is investigated. By increasing the laser scan speed and hence the solidification rate, distinct solidification modes evolving from coupled eutectic to anomalous eutectic and eventually to single-phase solidification are revealed. These transitions result in distinct microstructures and a wide range of mechanical properties. Thermodynamic modeling and molecular dynamics simulations reveal that low cooling rates allow for sufficient atomic diffusion and phase separation, facilitating coupled eutectic growth. In contrast, rapid cooling suppresses diffusion and destabilizes the solid–liquid interface, promoting anomalous or single-phase solidification. This integrated experimental and computational approach provides a multiscale understanding of solidification mechanisms in HEAs and underscores how kinetic effects can over-ride thermodynamic predictions under nonequilibrium conditions. Furthermore, these results demonstrate that AM can serve as a powerful tool to design HEAs with tailored microstructures and properties.

36 MATERIALS SCIENCE

A high strength Al-2Ni-0.5Zr conductor alloy fabricated via laser powder bed fusion

There is a current need for new aluminum alloy design strategies to target applications requiring high strength and conductivity with reductions in mass. A new lightweight Al-2Ni-0.5Zr (wt. %) conductor alloy was fabricated using laser powder bed fusion. A design of experiments probed the alloy's solidification cracking susceptibility. It was observed that solidification cracking was generally reduced with fast scan speeds, above 1500 mm/s, and smaller hatch spacings. The different cooling rates throughout the melt pool produced a heterogeneous distribution of cellular and equiaxed Al 3 Ni precipitates in the as-printed alloy. Additionally, the rapid solidification characteristic of laser powder bed fusion created a super-saturated Zr solid solution. An aging heat treatment at 375 °C for 24 h imparted strengthening through the precipitation of L1 2 -Al 3 Zr nanoprecipitates, which counteracted the softening caused by the fragmentation and coarsening of Al 3 Ni precipitates. The yield strength increased from 138 MPa in the as-printed condition to 168 MPa after aging, while the ductility remained constant at ∼21%. The aging treatment simultaneously increased the electrical conductivity from 40.8% IACS (International Annealed Copper Standard) to 53.5% IACS. Modeling of the strengthening mechanisms and electrical conductivity contributions rationalized the simultaneous increase in strength and conductivity upon aging. Furthermore, the strengthening efficacy of the Al 3 Ni and L1 2 -Al 3 Zr precipitates, combined with the low Ni and Zr solubility in the FCC Al matrix, facilitated both high strength and electrical conductivity. Overall, the combination of strength and electrical conductivity positions this alloy as a suitable choice for additively manufactured lightweight conductors.

Additive manufacturing

Laser‐Powder Melt Pool Solidification Dynamics and Microstructural Engineering of Ti‐5553 Microlattices

The fine geometric and topological control afforded by additive manufacturing technologies has enabled the manufacture of architected materials across length scales, and enabling tunable mechanical performance as a function of local and global design. Progress has been made to tune the mechanical response of architected materials through geometry, but understanding how the geometry and processing conditions will inform the microstructure remains a challenge due to the rapid solidification in laser powder bed fusion. This study uses in situ X-ray imaging and electron backscatter diffraction microscopy to demonstrate that the melt pool size, microstructure morphology, and elastic strain distribution is influenced by a combination of lattice geometry and laser processing conditions. These results indicate that within larger melt pools the local thermal gradients are sufficient to enable a columnar-to-equiaxed transition across the melt pool. Furthermore, the solidification mechanisms producing these microstructures are examined across the first 5 ms of melting and solidification, described via in situ high-speed X-ray imaging and mirrored via multiphysics simulation.

additive manufacturing

Nanoscale interfacial melting enables bonding during high velocity microparticle impacts

Melting during high-velocity particle impact has been understood to be typically detrimental to bonding by lowering the strength at the interface and promoting rebound before solidification can occur. Here we establish a possible remedy to this challenge: by dramatically restricting the volume of molten material, its resolidification is accelerated, effectively forming a nanoscale, braze-type joint during impact. In-situ single particle impact imaging is combined with post-mortem structural and chemical analyses to reveal a regime where adhesion is governed not by extensive plastic deformation, but by the kinetics of melt layer resolidification. Furthermore, these findings redefine the role of melting in impact-based processes, establishing transient melting and rapid solidification as a viable strategy for engineering successful adhesion events.

Additive manufacturing

The Study of Dopant Segregation Behavior During the Growth of GaAs in Microgravity

An investigation into the segregation behavior of selenium doped gallium arsenide during directional solidification in the microgravity environment was conducted using the Crystal Growth Furnace (CGF) aboard the first United States Microgravity Laboratory (USML-1). The two crystals grown were 1.5 cm in diameter and 16.5 cm in length with an initial melt length of 14 cm. Two translation periods were executed, the first at 2.5 microns/s and after a specified time, which was different between the two experiments, the translation rate was doubled to 5.0 microns/s. The translation was then stopped and the remaining sample melt was solidified using a gradient freeze technique in the first sample and a rapid solidification in the second experiment. Measurement of the selenium dopant distribution, using quantitative infrared transmission imaging, indicates that the first sample initially achieved diffusion controlled growth as desired. However, after about 1 cm of growth, the segregation behavior was driven from a diffusion controlled growth regime to a complete mixing regime. Measurements in the second flight sample indicated that the growth was always in a complete mixing regime. In both experiments, voids in the center line of the crystal, indicative of bubble entrapment, were found to correlate with the position in the crystal when the translation rates were doubled.

D H Matthiesen

Localized orientation gradients in additively manufactured stainless steel 316H structures

The high solidification rates during additive manufacturing cause highly localized thermal and strain gradients. The effect of these gradients on the evolution of local orientation misorientations within a grain is not well understood. In this study, stainless steel 316H parts were fabricated via laser powder bed fusion using three different energy densities: 43, 71, and 135 J/mm 3 . Electron backscatter diffraction showed that the maximum misorientations of the grains can be up to 25° along the build direction. Misorientation gradients (RM g ) within grains are process-dependent and can change from 0.036°/μm to 0.015°/μm with increased volumetric energy densities. In conclusion, the characterized misorientation gradients are an indication of the level of dislocations and, to an extent, the plastic deformation resulting from the rapid solidification during laser powder bed fusion.

316H

Suppressing Ordering in Equiatomic Fe-Co via Laser Powder Bed Fusion

Neutron and electron diffraction was employed to evaluate the effectiveness of thermal management strategies in suppressing the formation of the equilibrium-ordered B2 (CsCl) phase in equiatomic binary Fe-Co specimens fabricated by laser powder bed fusion additive manufacturing. Specimens with a tensile dogbone geometry were fabricated using various combinations of process parameters (laser power and raster speed) and thermal management strategies (no support struts, struts only in the top gauge section, and struts throughout the gauge section). Diffraction results demonstrate that the rapid solidification during PBF-L effectively minimized B2 formation, with laser power and effective scan velocity having no significant impact on the degree of ordering. Furthermore, the inclusion of support struts in the top grip region had no perceivable impact on ordering, whereas specimens with support struts in the gauge region exhibited no detectable ordering. Results are discussed in the context of thermal finite element analysis predictions.

Laser Material Processing

Massively parallel phase-field simulations targeting exascale

The interface thickness in the phase-field (PF) method limits its simulation scales. Consequently, large-scale PF simulations become prohibitively expensive for resolving the extremely fine microstructures that typically form during rapid solidification processing. This challenge is significant in predicting microstructure evolution in metal additive manufacturing and has been identified by the United States Department of Energy’s Exascale Computing Project. Here, to address this, we develop a multi-GPU and MPI-based massively parallel simulation code, utilizing state-of-the-art algorithms, software, and libraries, for large-scale three-dimensional (3D) PF simulations. We report the first GPU-parallel PF simulations on Frontier (currently the second TOP500 exascale cluster) and Summit machines, taking dendritic growth as an example problem. We evaluate the parallel performance of our implementation using scaling studies with more than 24 000 GPUs (among the largest known computations to date) and the acceleration performance using large-scale simulations of dendritic growth in 3D. Finally, massively parallel GPUs in these supercomputers enabled the first coupled multiscale simulations of laser melting and subsequent dendritic solidification on the scale of a full melt-pool, demonstrating the feasibility of performing PF simulations with a point total over 2 billion grid points within an acceptable time.

Exascale

Crystallographic stability of the BCC phase during quenching of metastable beta titanium alloy Ti-5553 and comparison of structural criteria for the predictive capability of α” martensite

This work evaluates the compositional standard currently developed for Ti-5553 powder and explores the metastable β region for sensitivity to martensitic formation during rapid quenching from the melt. Ti-5553 is a beta-stabilized titanium alloy that is increasingly being used in additive manufacturing applications. A series of alloys within the Ti-5553 compositional space was processed using two-piston spat quenching to perform rapid solidification and quenching for each of these alloy compositions. Typical empirical models such as molybdenum equivalency are not able to fully separate the retained BCC and martensitic compositions. Further, the use of thermodynamic data to estimate the transformation energy needed to form martensite can differentiate the alloys and provide a metric to further develop compositional limits for metastable beta titanium alloy development.

36 MATERIALS SCIENCE

Investigation of CO2 Sorption Characteristics of Imidazolium Ionic Liquid Crystals

This work is focused on advancing of the understanding the carbon dioxide (CO2) sorption characteristics of imidazolium ionic liquid crystals based on the 1-alkyl-3-methylimidazolium (Cnmim) ionic liquid family. Specifically, the mechanism of sorption across the melting, liquid crystal, and isotropic liquid transitions is investigated for 1-tetradecyl-3-methylimidazolium tetrafluoroborate (BF4-) and hexafluorophosphate (PF6-). A unique reversible CO2 occlusion was observed in 1-tetradecyl-3-methylimidazolium tetrafluoroborate (C14mim BF4) under rapid temperature quench from the liquid phases to the solid phase, while complete desorption occurred upon heating above the melting point (40 degrees C). In situ wide-angle x-ray scattering revealed that the lamellar structure of C14mim BF4 liquid crystal phases provides a high concentration of dynamically accessible anion and cation interaction sites for CO2, facilitating CO2 occlusion upon rapid solidification. The selective occlusion of CO2 in C14mim BF4 suggests a new mechanism for CO2 sorption processes.

08 HYDROGEN

Influence of minor Ce additions on magnetic and electrical properties in Fe–6.5 wt. % Si alloy

Fe–6.5 wt. % Si alloys exhibit lower core loss at higher frequency than the dominating electrical steel containing 3.2% Si due to its lower magneto-crystalline anisotropy energy (MAE) and higher electrical resistivity. However, compared to nanocrystalline and amorphous soft-magnetic materials, 6.5% Si steel, although being cost effective and having high saturation magnetization, still has much to improve, especially with respect to MAE and resistivity. To explore further improvement, the effects of minor Ce additions (due to its mixed valence 4f-electron configuration) on the microstructure, electrical and magnetic behaviors of Fe–6.5 wt. % Si alloys were investigated. Due to its limited solubility in Fe, Ce exhibits condition-dependent effects on electrical resistivity, showing only marginal improvement under rapid solidification. In contrast, Ce addition degrades magnetic performance, reducing saturation magnetization (from 1.86 to 1.76 T) and increasing coercivity (from 88 to 171 A/m), which results in an 83.4% increase in core loss (W 10/1000 condition). Overall, Ce addition provides limited benefit in electrical resistivity while deteriorating magnetic properties, making it ineffective for enhancing the soft magnetic performance of Fe–6.5 wt. % Si alloys.

36 MATERIALS SCIENCE

Beyond the eutectic paradigm: nanolamellar patterns in a rapidly solidified peritectic alloy

Peritectic transformations are central to many structural alloys, yet pattern formation remains poorly understood due to complex growth dynamics and limited three-dimensional data. Here, we report an unusual two-phase microstructure in a Zn–Ag peritectic alloy subjected to rapid solidification by laser surface remelting. Synchrotron X-ray nanotomography reveals a lamellar structure of primary 𝜀-AgZn 3 and peritectic Zn with ∼700 nm spacing. Although resembling a eutectic morphology, this pattern forms without a eutectic reaction through non-steady coupled growth from the liquid. SEM and TEM-EDS confirm interface shapes and phase compositions. These findings expand the design space of peritectics for refined microstructural control.

36 MATERIALS SCIENCE