At least 19 records

In situ probing the origin of interfacial instability of Na metal anode

The unstable and fragile solid electrolyte interphase (SEI) has restricted the application of Na metal anodes. Despite numerous research efforts being put into understanding its chemical composition and physical properties, direct observation of its formation remains a challenge due to the lack of temporal and spatial resolution. Here, through combined in situ probing techniques, we exhibit two pivotal stages associated with SEI instability during the often -neglected formation process. It is revealed that Na metal that is not uniformly passivated at the initial (passivating) stage will trigger unrestricted electrolyte decomposition and homogeneous components distribution during the subsequent (growing) stage. SEI with homogenously distributed components is found to have higher solubility than that with a layered structure evolved from a compact passivation layer. Furthermore, through demonstrating an SEI dissolution model that is closely related to its formation process and compositional distribution, this work sheds light on an uncharted territory of Na metal batteries.

25 ENERGY STORAGE↗

Chemical and Structural Insights into Solid Electrolyte Interphase Evolution for Sodium Metal Electrodes

The solid electrolyte interphase (SEI) critically governs the reversibility of sodium metal batteries, through dynamically mediating ion transport and interfacial reactions. However, its kinetic evolution under operating conditions, and how it influences interfacial stability, remains poorly understood. Here, in this study, we reveal that the SEI undergoes coupled chemical and mechanical changes during sodium plating and stripping, leading to spatial and temporal heterogeneity that drives interfacial degradation. Synchrotron operando grazing-incidence wide-angle X-ray scattering and soft X-ray absorption spectroscopy capture the sequential formation and dissolution of inorganic SEI phases (NaF, NaH, NaOH, Na 2 PO 3 F), accompanied by depth-dependent alterations in organic SEI components. Mesoscale modeling connects this evolving SEI heterogeneity to localized current density fluctuations and stress accumulation at the Na interface, identifying pathways to electrically isolated sodium formation. These findings show that SEI instability fundamentally limits reversibility in sodium metal batteries, and that controlling SEI chemistry–mechanics coupling is essential to achieving its durability.

36 MATERIALS SCIENCE↗

Extending the low-temperature operation of sodium metal batteries combining linear and cyclic ether-based electrolyte solutions

Nonaqueous sodium-based batteries are ideal candidates for the next generation of electrochemical energy storage devices. However, despite the promising performance at ambient temperature, their low-temperature (e.g., < 0 °C) operation is detrimentally affected by the increase in the electrolyte resistance and solid electrolyte interphase (SEI) instability. Here, to circumvent these issues, we propose specific electrolyte formulations comprising linear and cyclic ether-based solvents and sodium trifluoromethanesulfonate salt that are thermally stable down to –150 °C and enable the formation of a stable SEI at low temperatures. When tested in the Na||Na coin cell configuration, the low-temperature electrolytes enable long-term cycling down to –80 °C. Via ex situ physicochemical (e.g., X-ray photoelectron spectroscopy, cryogenic transmission electron microscopy and atomic force microscopy) electrode measurements and density functional theory calculations, we investigate the mechanisms responsible for efficient low-temperature electrochemical performance. We also report the assembly and testing between –20 °C and –60 °C of full Na||Na 3 V 2 (PO 4 ) 3 coin cells. The cell tested at –40 °C shows an initial discharge capacity of 68 mAh g –1 with a capacity retention of approximately 94% after 100 cycles at 22 mA g –1 .

25 ENERGY STORAGE↗

Stable Potassium Metal Anodes with an All-Aluminum Current Collector through Improved Electrolyte Wetting

This is the first report of successful potassium metal battery anode cycling with an aluminum-based rather than copper-based current collector. Dendrite-free plating/stripping is achieved through improved electrolyte wetting, employing an aluminum-powder-coated aluminum foil “Al@Al,” without any modification of the support surface chemistry or electrolyte additives. The reservoir-free Al@Al half-cell is stable at 1000 cycles (1950 h) at 0.5 mA cm -2 , with 98.9% cycling Coulombic efficiency and 0.085 V overpotential. The pre-potassiated cell is stable through a wide current range, including 130 cycles (2600 min) at 3.0 mA cm -2 , with 0.178 V overpotential. Al@Al is fully wetted by a 4 m potassium bis(fluorosulfonyl)imide-dimethoxyethane electrolyte (θCA = 0°), producing a uniform solid electrolyte interphase (SEI) during the initial galvanostatic formation cycles. On planar aluminum foil with a nearly identical surface oxide, the electrolyte wets poorly (θCA = 52°). This correlates with coarse irregular SEI clumps at formation, 3D potassium islands with further SEI coarsening during plating/stripping, possibly dead potassium metal on stripped surfaces, and rapid failure. The electrochemical stability of Al@Al versus planar Al is not related to differences in potassiophilicity (nearly identical) as obtained from thermal wetting experiments. Additionally, planar Cu foils are also poorly electrolyte-wetted and become dendritic. The key fundamental takeaway is that the incomplete electrolyte wetting of collectors results in early onset of SEI instability and dendrites.

25 ENERGY STORAGE↗

Experimental considerations and applications for time-resolved impedance on silicon-anode battery systems

Dynamic electrochemical impedance spectroscopy (dEIS) utilizes a superimposed multi-sinusoidal waveform and enables temporally resolved investigations on various electrochemical processes; however, the signal-to-noise ratio must be maximized while retaining linearity and stationarity within the system. In the present work, we probe the impact of the waveform’s total amplitude as well as the waveform and phase profiles. The equal amplitude multi-sinusoidal waveform with 35 mV total amplitude (<1 mV per frequency) and random phase profile exhibits the lowest impedance noise. This input signal is sufficient in avoiding the high frequency signal attenuation from the potentiostat’s low-pass filter. Additionally, we demonstrate the optimized dEIS waveform’s utility in investigating surface passivation within thin-film and composite silicon (Si) anodes. Within a two-electrode Si-lithium metal coin cell, the charge transfer resistance (RCT) associated with alloying kinetics dominates the overall impedance. RCT increases with state of charge indicating a kinetic bottleneck at higher lithiation states. To explore this further, we utilize a three-electrode Si-LiNi0.8Mn0.1Co0.1O2 pouch cell to deconvolute the Si impedance contributions. The evolution of the solid electrolyte interphase (SEI) and charge transfer resistances correlate to specific Li–Si alloy phases. We attribute this to the influence of Si particle volume expansion on SEI instabilities and a kinetic bottleneck at higher lithiation states.

Lam, Steven [ORNL]↗

Understanding the Origin of the Nonpassivating Behavior of Si-Based Anodes during the Initial Cycles

In this contribution, we combined electrochemical cycling and X-ray photoelectron spectroscopy (XPS) to understand the nonpassivating behavior of the solid electrolyte interphase (SEI) on Si anodes during the first cycles. Based on galvanostatic measurements, we show that the irreversible capacity loss is reduced after the first cycle, and it stays almost constant from the second cycle onwards. XPS was used to determine the root causes of the Coulombic inefficiency, showing that the rate of decomposition of the organic solvents strongly decreased after the first cycle, whereas the rate of salt decomposition is almost unchanged between cycles. We determine that the inhibition of the decomposition reaction of the organic solvent is responsible for the lower Coulombic loss during the second electrochemical cycle in comparison to the first, whereas the nonpassivating behavior toward the salt decomposition is one of the main causes of capacity loss upon cycling. Here, we further revisit the role of cracking in contributing to capacity loss. Whereas high volumetric expansion remains an issue plaguing the performance of Si anodes, our chronoamperometry studies reveal that the SEI formed on Si anodes does not passivate even when the electrode is fully expanded, and no additional surface is exposed. Overall, our work establishes the need to address the chemical and electrochemical instability of the SEI on the Si anode in addition to the more notorious issue of cracking.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Design principles of heterointerfacial redox chemistry for highly reversible lithium metal anode

High electrochemical reversibility is required for the application of high-energy-density lithium (Li) metal batteries; however, inactive Li formation and SEI (solid electrolyte interface)-instability-induced electrolyte consumption cause low Coulombic efficiency (CE). The prior interfacial chemical designs in terms of alloying kinetics have been used to enhance the CE of Li metal anode; however, the role of its redox chemistry at heterointerfaces remains a mystery. Herein, the relationship between heterointerfacial redox chemistry and electrochemical transformation reversibility is investigated. It is demonstrated that the lower redox potential at heterointerface contributes to higher CE, and this enhancement in CE is primarily due to the regulation of redox chemistry to Li deposition behavior rather than the formation of SEI films. Low oxidation potential facilitates the formation of the surface with the highly electrochemical binding feature after Li stripping, and low reduction potential can maintain binding ability well during subsequent Li plating, both of which homogenize Li deposition and thus optimize CE. In particular, Mg hetero-metal with ultra-low redox potential enables Li metal anode with significantly improved CE (99.6%) and stable cycle life for 700 cycles at 3.0 mA cm -2 . This work provides insight into the heterointerfacial design principle of next-generation negative electrodes for highly reversible metal batteries.

25 ENERGY STORAGE↗

Design of a multi-functional gel polymer electrolyte with a 3D compact stacked polymer micro-sphere matrix for high-performance lithium metal batteries

We report lithium metal batteries (LMBs) are considered as promising high energy density batteries. However, they still suffer from poor cyclability due to the instability of solid electrolyte interphases (SEIs) and Li dendrite issues. Herein, a novel 3D densely packed multifunctional crosslinked gel polymer electrolyte (PHGPE) has been synthesized by in situ copolymerization of pentaerythritol tetraacrylate and 2-hydroxyethyl acrylate in a liquid electrolyte via a thermal initiation method. Due to intermolecular hydrogen bonding in the frameworks, the PHGPE exhibits a 3D compact-stacked and crosslinked micro-sphere structure, which benefits the construction of homogeneous Li + flux, enabling uniform Li plating/stripping and formation of robust SEIs onto the lithium electrode. Benefiting from the above advantages, symmetric Li cells in the PHGPE deliver excellent cyclabilities of 6000 h at a current density of 1 mA cm -2 (1 mA h cm -2 ) and 7700 h at 0.5 mA cm -2 (2 mA h cm -2 ). Moreover, the PHGPE has such a wide electrochemical window that it is compatible with both high-voltage LiNi 0.8 Co 0.1 Mn 0.1 O 2 and sulfur cathodes to realize long cycle life. Additionally, a LiFePO 4 based pouch size LMB also presents promising performance. Therefore, this study of the PHGPE has opened a new avenue for high-performance LMBs with excellent versatility and practicality.

25 ENERGY STORAGE↗

Concentration dependent properties and plastic deformation facilitate instability of the solid-electrolyte interphase in Li-ion batteries

Lithium-ion batteries (LIBs) often suffer from capacity fading and poor cyclic performance due to mechanical degradation of the solid-electrolyte interphase (SEI). Here we perform numerical simulations and theoretical analysis to elucidate the role of plasticity in wrinkling and ratcheting behaviors of an SEI/electrode system. A coupled diffusion and finite deformation framework is formulated and numerically implemented as a user-element subroutine (UEL) to describe transient lithium diffusion and accompanying elastic–viscoplastic deformation of the electrode. It is found that concentration dependent properties and plastic deformation facilitate wrinkling in such a system. A wrinkled morphology may further lead to ratcheting and related failure under cycling. A phase diagram of four types of cyclic behaviorsis identified in terms of the charging rate and time. Our analysis suggests several potential strategies to avoid wrinkling and ratcheting instabilities, such as charging/discharging the electrode at a sufficiently slow rate, and/or introducing a thick artificial SEI with a pre-tension.

25 ENERGY STORAGE↗

Interfacial solvation-structure regulation for stable Li metal anode by a desolvation coating technique

Rechargeable lithium (Li) metal batteries face challenges in achieving stable cycling due to the instability of the solid electrolyte interphase (SEI). The Li-ion solvation structure and its desolvation process are crucial for the formation of a stable SEI on Li metal anodes and improving Li plating/stripping kinetics. This research introduces an interfacial desolvation coating technique to actively modulate the Li-ion solvation structure at the Li metal interface and regulate the participation of the electrolyte solvent in SEI formation. Through experimental investigations conducted using a carbonate electrolyte with limited compatibility to Li metal, the optimized desolvation coating layer, composed of 12-crown-4 ether-modified silica materials, selectively displaces strongly coordinating solvents while simultaneously enriching weakly coordinating fluorinated solvents at the Li metal/electrolyte interface. This selective desolvation and enrichment effect reduce solvent participation to SEI and thus facilitate the formation of a LiF-dominant SEI with greatly reduced organic species on the Li metal surface, as conclusively verified through various characterization techniques including XPS, quantitative NMR, operando NMR, cryo-TEM, EELS, and EDS. The interfacial desolvation coating technique enables excellent rate cycling stability (i.e., 1C) of the Li metal anode and prolonged cycling life of the Li||LiCoO 2 pouch cell in the conventional carbonate electrolyte (E/C 2.6 g/Ah), with 80% capacity retention after 333 cycles.

42 ENGINEERING↗

Investigating the Chemical Reactivity of Lithium Silicate Model SEI Layers

Silicon anodes suffer from an unstable solid electrolyte interphase (SEI) layer that contributes to undesirable capacity fade with cycling. A key part to addressing this unstable SEI formation is to examine how certain components of the SEI react with the electrolyte over time. One SEI component that has not been thoroughly studied in the context of the chemical reactivity against the electrolyte is lithiated silicate. Four model silicate thin films with increasing lithium content were deposited by radio frequency (RF) magnetron sputtering to study how the lithiation of the native oxide on a silicon anode affects the chemical stability of the anode surface. SiO2, Li2Si2O5, Li2SiO3, and Li3SiOx films were exposed to 1.2 M LiPF6 in the 3:7 wt% ethylene carbonate/ethyl methyl carbonate (EC/EMC) electrolyte for periods of time that are representative of the amount of time it takes to undergo cell formations. Soaked samples were rinsed, dried, and characterized by a combination of attenuated total reflectance-infrared spectroscopy (ATR-IR), focused ion beam-secondary electron microscopy (FIB-SEM), and X-ray photoelectron spectroscopy (XPS) depth profiling. It was found that the rate of the decrease in film thickness of the silicates exposed to the electrolyte over time increases as a function of the lithium content in the thin film. This reaction involves HF etching and LiPF6 salt degradation leading to silicate loss and fluorination throughout the bulk. Understanding this chemical instability is critical to determining the overall mechanism of SEI degradation over time.

ADVANCED PROPULSION SYSTEMS,ENERGY STORAGE↗

Electrochemical Reactivity and Passivation of Silicon Thin-Film Electrodes in Organic Carbonate Electrolytes

This work focuses on the mechanisms of interfacial processes at the surface of amorphous silicon thin-film electrodes in organic carbonate electrolytes to unveil the origins of the inherent nonpassivating behavior of silicon anodes in Li-ion batteries. Attenuated total reflection Fourier-transform infrared spectroscopy, X-ray absorption spectroscopy, and infrared near-field scanning optical microscopy were used to investigate the formation, evolution, and chemical composition of the surface layer formed on Si upon cycling. Herein, we found that the chemical composition and thickness of the solid/electrolyte interphase (SEI) layer continuously change during the charging/discharging cycles. This SEI layer “breathing” effect is directly related to the formation of lithium ethylene dicarbonate (LiEDC) and LiPF6 salt decomposition products during silicon lithiation and their subsequent disappearance upon delithiation. Furthermore, the detected appearance and disappearance of LiEDC and LiPF6 decomposition compounds in the SEI layer are directly linked with the observed interfacial instability and poor passivating behavior of the silicon anode.

25 ENERGY STORAGE↗

Fine‐Tuning Li‐Ion Solvation Structure by Enhanced Solvent‐Diluent Interactions for Long‐Cycling Lithium Metal Batteries

Achieving durable lithium (Li) metal anodes in liquid electrolytes remains challenging, primarily due to the instability of the formed solid-electrolyte interphases (SEIs). Modulating the Li-ion solvation structures is pivotal in forming a stable SEI for stabilizing Li metal anodes. Here a strategy is developed to fine-tune the Li-ion solvation structures through enhanced dipole–dipole interactions between the Li-ion-coordinated solvent and the non-Li-ion-coordinating diluent, for creating a stable SEI in the developed binary salt electrolyte. The enhanced dipole–dipole interactions weaken the coordination between Li-ions and the solvents while strengthening the interaction between Li-ions and dual anions, thereby facilitating the Li-ion transport and a robust anion-derived SEI with a distinct bilayer structure. Consequently, the developed electrolyte exhibited exceptional electrochemical performance in high energy-density Li||LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cells, with long calendar life, stable cyclability at 1 C, and reliable operation between 25 and −20 °C, and it also demonstrat remarkable cycling stability for a Li||NMC811 pouch cell with projected energy density of 402 Wh kg −1 , maintaining 80% capacity retention over 606 cycles under practical conditions.

25 ENERGY STORAGE↗

The Effect of the SEI Layer Mechanical Deformation on the Passivity of a Si Anode in Organic Carbonate Electrolytes

The solid electrolyte interphase (SEI) on a Si negative electrode in carbonate-based organic electrolytes shows intrinsically poor passivating behavior, giving rise to unsatisfactory calendar life of Li-ion batteries. Moreover, mechanical strains induced in the SEI due to large volume changes of Si during charge-discharge cycling could contribute to its mechanical instability and poor passivating behavior. This study elucidates the influence that static mechanical deformation of the SEI has on the rate of unwanted parasitic reactions at the Si/electrolyte interface as a function of electrode potential. Further, the experimental approach involves the utilization of Si thin-film electrodes on substrates with disparate elastic moduli, which either permit or suppress the SEI deformation in response to Si volume changes upon charging-discharging. We find that static mechanical stretching and deformation of the SEI results in an increased parasitic electrolyte reduction current on Si. Furthermore, attenuated total reflection and near-field Fourier-transform infrared nanospectroscopy reveal that the static mechanical stretching and deformation of the SEI fosters a selective transport of linear carbonate solvent through, and nanoconfinement within, the SEI. These, in turn, promote selective solvent reduction and continuous electrolyte decomposition on Si electrodes, reducing the calendar life of Si anode-based Li-ion batteries. Finally, possible correlations between the structure and chemical composition of the SEI layer and its mechanical and chemical resilience under prolonged mechanical deformation are discussed in detail.

25 ENERGY STORAGE↗

Heterogeneous Solid Electrolyte Interphase Interactions Dictate Interface Instability in Sodium Metal Electrodes

Sodium (Na) metal batteries have attracted recent attention due to their low cost and high abundance of Na. However, the advancement of Na metal batteries is impeded due to key challenges such as dendrite growth, solid electrolyte interphase (SEI) fracture, and low Coulombic efficiency. This study examines the coupled electro‐chemo‐mechanical interactions governing the electrodeposition stability and morphological evolution at the Na/electrolyte interface. The SEI heterogeneities influence transport and reaction kinetics leading to the formation of current and stress hotspots during Na plating. Further, it is demonstrated that the heterogeneity‐induced Na metal evolution and its influence on the stress distribution critically affect the mechanical overpotential, contributing to a faster SEI failure. The analysis reveals three distinct failure mechanisms—mechanical, transport, and kinetic—that govern the onset of instabilities at the interface. Finally, a comprehensive comparative study of SEI failure in Na and lithium (Li) metal anodes illustrates that the electrochemical and mechanical characteristics of the SEI are crucial in tailoring the anode morphology and interface stability. This work delineates mechanistic stability regimes cognizant of the SEI attributes and underlying failure modes and offers important guidelines for the design of artificial SEI layers for stable Na metal electrodes.

25 ENERGY STORAGE↗

Interdependence of Support Wettability - Electrodeposition Rate- Sodium Metal Anode and SEI Microstructure

Here, this study examines how current collector support chemistry (sodiophilic intermetallic Na 2 Te vs. sodiophobic baseline Cu) and electrodeposition rate affect microstructure of sodium metal and its solid electrolyte interphase (SEI). Capacity and current (6 mAh cm -2 , 0.5–3 mA cm -2 ) representative of commercially relevant mass loading in anode-free sodium metal battery (AF-SMBs) are analyzed. Synchrotron X-ray nanotomography and grazing-incidence wide-angle X-ray scattering (GIWAXS) are combined with cryogenic ion beam (cryo-FIB) microscopy. Highlighted are major differences in film morphology, internal porosity, and crystallographic preferred orientation e.g. (110) vs. (100) and (211) with support and deposition rate. Within the SEI, sodium fluoride (NaF) is more prevalent with Te-Cu versus sodium hydride (NaH) and sodium hydroxide (NaOH) with baseline Cu. Due to competitive grain growth the preferred orientation of sodium crystallites depends on film thickness. Mesoscale modeling delineates the role of SEI (ionic conductivity, morphology) on electrodeposit growth and onset of electrochemical instability.

36 MATERIALS SCIENCE↗

Chemo‐Mechanics Interplay Dictates Interface Instability and Asymmetry in Plating and Stripping of Sodium Metal Electrodes

Abstract The development of practical sodium (Na) metal batteries is hindered by key challenges including dendrite growth, dead metal formation, and unstable solid electrolyte interphase (SEI) growth. A fundamental understanding of the chemo‐mechanical interactions at the Na/SEI interface is critical for designing stable Na metal electrodes. In this work, the coupled electrochemical‐mechanical processes governing the morphological evolution and stability of Na metal during plating and stripping are investigated. The heterogeneous nature of transport and morphological interactions at the Na/SEI interface is revealed to result in nonuniform mechanical overpotentials and reaction fronts, eventually leading to Na filaments or pits. The spatio‐temporal evolution of stress heterogeneities during Na plating and stripping is shown to be asymmetric, manifesting in varying morphological nonuniformities and instability modes. The crucial role of external pressure in modulating the electrochemical‐transport interactions, the mechanical response of Na, and the localized reaction currents and stresses at the Na/SEI interface is demonstrated. At different external pressure conditions, the correlation between transport heterogeneities in the SEI and the onset and propagation of interface instability has been delineated. This work highlights the need for synergistic tailoring of external pressure and SEI heterogeneity toward achieving stable electrodeposition and dissolution in Na metal electrodes.

Singla, Aditya [School of Mechanical Engineering P↗

Interdependence of Support Wettability ‐ Electrodeposition Rate‐ Sodium Metal Anode and SEI Microstructure

Abstract This study examines how current collector support chemistry (sodiophilic intermetallic Na 2 Te vs. sodiophobic baseline Cu) and electrodeposition rate affect microstructure of sodium metal and its solid electrolyte interphase (SEI). Capacity and current (6 mAh cm −2 , 0.5–3 mA cm −2 ) representative of commercially relevant mass loading in anode‐free sodium metal battery (AF‐SMBs) are analyzed. Synchrotron X‐ray nanotomography and grazing‐incidence wide‐angle X‐ray scattering (GIWAXS) are combined with cryogenic ion beam (cryo‐FIB) microscopy. Highlighted are major differences in film morphology, internal porosity, and crystallographic preferred orientation e.g. (110) vs. (100) and (211) with support and deposition rate. Within the SEI, sodium fluoride (NaF) is more prevalent with Te−Cu versus sodium hydride (NaH) and sodium hydroxide (NaOH) with baseline Cu. Due to competitive grain growth the preferred orientation of sodium crystallites depends on film thickness. Mesoscale modeling delineates the role of SEI (ionic conductivity, morphology) on electrodeposit growth and onset of electrochemical instability.

Lo, Chang‐An↗