At least 19 records

Auger spectroscopy analysis of lubrication with zinc dialkyldithiophosphate of several metal combinations in sliding contact

Sliding friction experiments were conducted with aluminum and other riders rubbing on disks of various elemental metals in the presence of a thin film of zinc dialkyldithiophosphate (ZDP). Auger emission spectroscopy was used to in situ monitor the changes in surface chemistry with rubbing under various loads. The metal disks examined included iron, titanium, rhodium, tungsten, molybdenum, and copper. For equivalent films of ZDP the film is a more effective lubricant for some metals than it is for others. The important active element in the compound varies with the metal lubricated and is a function of metal chemistry. The zinc in the ZDP is susceptible to electron beam induced desorption.

Buckley, D. H.↗

Ultrafine gradient microstructure induced by severe plastic deformation under sliding contact conditions in copper

Highlights: • Sliding contact produces a gradient microstructure by severe plastic deformation. • Nanohardness is increased strongly by grain size and dislocation hardening. • The texture components in the deformed layer correspond to pure shear. • Grain size distribution, boundary misorientation and KAM were analysed. • Strain induced effects compete with crystallisation to determine the microstructure. - Abstract: Sliding contact induces severe plastic deformation (SPD) at the surface of ductile materials and induces a microstructural gradient associated to a significant increase of hardness toward the surface. This gradient allows observing all stages of grain refinement in SPD, as illustrated here by the analysis of polycrystalline electrolytic copper tested in a coaxial tribometer. Materials tested in the cold-rolled state and after annealing were characterised by high-resolution electron backscattering diffraction and nano-indentation. The incremental plastic strain produces an ultrafine microstructure in the top layers, which gradually changes to the original size in unaffected material. In cold-rolled material, an intermediate recrystallised layer is observed. The separation of the Misorientation Angle Distribution (MAD) in a low-angle portion and a high angle portion allows characterising the accumulation of strain induced misorientation, while the Kernel Average Misorientation (KAM) provides information on the evolution of substructure at the finest levels. The results point toward a process where strain-induced effects compete continuously with recrystallisation, except for the surface layer in the cold-rolled material, where dynamic recrystallisation is dominant. Combining the information from KAM and subgrain size distribution, the measured hardness can be explained as a combination of grain size and dislocation hardening.

36 MATERIALS SCIENCE↗

The friction and wear of ceramic/ceramic and ceramic/metal combinations in sliding contact

The tribological characteristics of ceramics sliding on ceramics are compared to those of ceramics sliding on a nickel based turbine alloy. The friction and wear of oxide ceramics and silicon-based ceramics in air at temperatures from room ambient to 900 C (in a few cases to 1200 C) were measured for a hemispherically-tipped pin on a flat sliding contact geometry. In general, especially at high temperature, friction and wear were lower for ceramic/metal combinations than for ceramic/ceramic combinations. The better tribological performance for ceramic/metal combinations is attributed primarily to the lubricious nature of the oxidized surface of the metal.

Sliney, Harold E.↗

The friction and wear of ceramic/ceramic and ceramic/metal combinations in sliding contact

The tribological characteristics of ceramics sliding on ceramics are compared to those of ceramics sliding on a nickel-based turbine alloy. The friction and wear of oxide ceramics and silicon-based ceramics in air at temperatures from room ambient to 900 C (in a few cases to 1200 C) were measured for a hemispherically-tipped pin on a flat sliding contact geometry. In general, especially at high temperature, friction and wear were lower for ceramic/metal combinations than for ceramic/ceramic combinations. The better tribological performance for ceramic/metal combinations is attributed primarily to the lubricious nature of the oxidized surface of the metal.

Sliney, Harold E.↗

Infrared emission spectra from operating elastohydrodynamic sliding contacts

Infrared emission spectra from an operating EHD sliding contact were obtained through a diamond window for an aromatic polymer solute present in equal concentration in four different fluids. Three different temperature ranges, three different loads, and three different speeds for every load were examined. Very sensitive Fourier spectrophotometric (Interferometric) techniques were employed. Band Intensities and band intensity ratios found to depend both on the operating parameters and on the fluid. Fluid film and metal surface temperatures were calculated from the spectra and their dependence on the mechanical parameters plotted. The difference between these temperatures could be plotted against shear rate on one curve for all fluids. However, at the same shear rate the difference between bulk fluid temperature and diamond window temperature was much higher for one of the fluids, a traction fluid, than for the others.

Lauer, J. L.↗

Sliding Contact Bearings for Service to 700 C

Cylindrical, sliding contact bearings made entirely of a self-lubricating powder metallurgy composite (PM212) or of super alloy shells lined with clad PM212 were tested in an oscillating mode at temperatures from 25 to 700 C. Tests of 100 hr duration or longer were conducted at a bearing unit load of 3.45 Mpa (500 psi). Shorter duration tests at various unit loads up to 24.1 Mpa (3500 psi) were also conducted. In comparison tests, bearings lubricated with PM212 had superior anti-wear characteristics compared to the baseline, unlubricated, super alloy bearings: no galling of PM212-lubricated bearings occurred, while severe surface damage including galling occurred, especially at high loads, during the baseline tests. A heat treatment procedure, which dimensionally stabilizes PM212 and thereby minimizes clearance changes during high temperature bearing operation, is described.

Sliney, Harold E.↗

Determination of near-surface plastic deformation in sliding contacts

It is pointed out that substantial plastic deformation occurs on and near the contact surfaces, when two solid bodies slide against each other without lubrication. It has been found that this deformation plays an important role in the tribological behavior of the sliding contact. The present investigation has the objective to develop an analytical model to predict the near-surface plastic deformation resulting from a single pass of one metallic surface over another. A finite element viscoplasticity program was written relating velocities to forces in a two-dimensional domain. The program was employed in the study of plastic deformation during a single pass of a hardened tool steel slider over a copper rub specimen. It was found that essentially the only material set in motion by the slider was directly under the contact zone. The agreement between values obtained in the analysis and experimental data is reasonably good.

Kennedy, F. E., Jr.↗

Antiwear Additive Mechanisms in Sliding Contacts

The possible mechanisms associated with wear in a sliding contact and how an oil and antiwear additive can mitigate wear or prevent catastropic seizure of the contacting parts was examined. The various load and temperature regimes are examined and the mechanisms which are predominant under these conditions are determined. The critical mechanism(s) depend on the test parameters, particularly load and temperature, although sliding speed is also a factor. Different ways to improve the efficiency of antiwear additives are suggested.

Baldwin, B. A.↗

A thermal, thermoelastic, and wear simulation of a high-energy sliding contact problem

This paper describes an investigation of the sliding contact problem encountered in high-energy disk brakes. The analysis includes a simulation modeling, using the finite element method, of the thermoelastic instabilities that cause transient changes in contact to occur on the friction surface. In order to include the effect of wear of the concentrated contacts on the friction surface, a wear criterion is proposed that results in prediction of wear rates for disk brakes that are quite close to experimentally determined wear rates. The thermal analysis shows that the transient temperature distribution in a disk brake can be determined more accurately by use of this thermomechanical analysis than by a more conventional analysis that assumes constant contact conditions. It is also shown that lower, more desirable, temperatures in disk brakes can be attained by increasing the volume, the thermal conductivity, and especially, the heat capacity of the brake components.

Kennedy, F. E., Jr.↗

Boosting contact sliding and wear protection via atomic intermixing and tailoring of nanoscale interfaces

Friction and wear cause energy wastage and system failure. Usually, thicker overcoats serve to combat such tribological concerns, but in many contact sliding systems, their large thickness hinders active components of the systems, degrades functionality, and constitutes a major barrier for technological developments. While sub-10-nm overcoats are of key interest, traditional overcoats suffer from rapid wear and degradation at this thickness regime. Using an enhanced atomic intermixing approach, we develop a ~7- to 8-nm-thick carbon/silicon nitride (C/SiN x ) multilayer overcoat demonstrating extremely high wear resistance and low friction at all tribological length scales, yielding ~2 to 10 times better macroscale wear durability than previously reported thicker (~20 to 100 nm) overcoats on tape drive heads. We report the discovery of many fundamental parameters that govern contact sliding and reveal how tuning atomic intermixing at interfaces and varying carbon and SiN x thicknesses strongly affect friction and wear, which are crucial for advancing numerous technologies.

36 MATERIALS SCIENCE↗

Friction and wear behavior of single-crystal silicon carbide in sliding contact with various metals

Sliding friction experiments were conducted with single-crystal silicon carbide in contact with various metals. Results indicate the coefficient of friction is related to the relative chemical activity of the metals. The more active the metal, the higher the coefficient of friction. All the metals examined transferred to silicon carbide. The chemical activity of the metal and its shear modulus may play important roles in metal transfer, the form of the wear debris and the surface roughness of the metal wear scar. The more active the metal, and the less resistance to shear, the greater the transfer to silicon carbide and the rougher the wear scar on the surface of the metal. Hexagon shaped cracking and fracturing formed by cleavage of both prismatic and basal planes is observed on the silicon carbide surface.

Miyoshi, K.↗

Friction and wear behavior of single-crystal silicon carbide in sliding contact with various metals

Sliding friction experiments were conducted with single-crystal silicon carbide in contact with various metals. Results indicate the coefficient of friction is related to the relative chemical activity of the metals. The more active the metal, the higher the coefficient of friction. All the metals examined transferred to silicon carbide. The chemical activity of the metal and its shear modulus may play important roles in metal-transfer, the form of the wear debris and the surface roughness of the metal wear scar. The more active the metal, and the less resistance to shear, the greater the transfer to silicon carbide and the rougher the wear scar on the surface of the metal. Hexagon-shaped cracking and fracturing formed by cleavage of both prismatic and basal planes is observed on the silicon carbide surface.

Miyoshi, K.↗

Metallic transfer between metals in sliding contact examined by auger emission spectroscopy

Metallic transfer between polycrystalline metals in sliding contact was examined. Hemispherical riders of iron, nickel, and cobalt were slid on tungsten, tantalum, niobium, and molybdenum disks in ultrahigh vacuum. Auger emission spectroscopy was used to monitor the elemental composition of the disk surfaces. Iron, nickel, and cobalt transferred to tungsten, whereas only cobalt transferred to tantalum, niobium, and molybdenum. The results of this investigation are discussed in terms of the cohesive energy and strain hardening characteristics of the specimen materials.

Pepper, S. V.↗

Elasto-plastic finite element analyses of two-dimensional rolling and sliding contact deformation of bearing steel

An elastoplastic finite element analysis of repeated rolling-plus-sliding contact is presented for the elastic-linear-kinematic hardening-plastic properties of hardened bearing steel at room temperature. Contacts in the absence of frictional heating are found to produce peak cyclic strain ranges and residual stresses that are similar to the values obtained for pure rolling. For the cases considered, the energy dissipated as heat by plastic deformation is found to be 3-15 percent of the energy dissipated at the surface by friction.

Kumar, A. M.↗

Ceramic wear in indentation and sliding contact

The various wear mechanisms involved with single-crystal ceramic materials in indentation and in sliding contacts. Experiments simulating interfacial events have been conducted with hemispherical, conical and pyramidal indenters (riders). With spherical riders, under either abrasive or adhesive conditions, two types of fracture pits have been observed. First, spherical-shaped fracture pits and wear particles are found as a result of either indenting or sliding. These are shown to be due to a spherical-shaped fracture along the circular or spherical stress trajectories. Second, polyhedral fracture pits and debris, produced by anisotropic fracture, and also found both during indenting and sliding. These are primarily controlled by surface and subsurface cracking along cleavage planes. Several quantitative results have also been obtained from this work. For example, using a pyramidal diamond, crack length of Mn-Zn ferrite in the indentation process grows linearly with increasing normal load. Moreover, the critical load to fracture both in indentation and sliding is essentially isotropic and is found to be directly proportional to the indenter radius.

Miyoshi, K.↗

Friction and Wear of Nanoadditive-Based Biolubricants in Steel–Steel Sliding Contacts: A Comparative Study

The present work deals with the study of tribo-pair interaction in lubricated sliding contacts. By considering the environmental issues, the sunflower oil was extracted from the sunflower seeds and used as a base lubricant. The two types of the nanoadditives, i.e., CuO and CeO{sub 2}, varying concentrations from 0.10 to 0.50% w/v were used to formulate the nanolubricants. The compatibility/synergism of the nanoadditives was examined from antifriction and antiwear behavior study with four-ball tester. Also, sunflower oil was modified by the chemical method to improve its fatty acid structure. A comparative tribological and compatibility study was also done in modified oil at similar concentration levels with both types of nanoparticles. The tribological test result exhibits 0.10% w/v concentration of the nanoadditive as optimum due to lowest wear scar and coefficient of friction. Higher concentration of the nanoparticles impaired the base oil performance. Different analytical tools were used to characterize the oil modification and worn surfaces. Moreover, the role of subsurface of the contacting material with the tribological performance has been reported.